• 제목/요약/키워드: polymer precursor

검색결과 237건 처리시간 0.026초

유기물과 유무기 혼합 폴리머 게이트 절연체를 사용한 유기 박막 트랜지스터의 특성 (Characteristics of Organic Thin Film Transistors with Organic and Organic-inorganic Hybrid Polymer Gate Dielectric)

  • 배인섭;임하영;조수헌;문송희;최원석
    • 한국전기전자재료학회논문지
    • /
    • 제22권12호
    • /
    • pp.1009-1013
    • /
    • 2009
  • In this study, we have been synthesized the dielectric layer using pure organic and organic-inorganic hybrid precursor on flexible substrate for improving of the organic thin film transistors (OTFTs) and, design and fabrication of organic thin-film transistors (OTFTs) using small-molecule organic semiconductors with pentacene as the active layer with record device performance. In this work OTFT test structures fabricated on polymerized substrates were utilized to provide a convenient substrate, gate contact, and gate insulator for the processing and characterization of organic materials and their transistors. By an adhesion development between gate metal and PI substrate, a PI film was treated using $O_2$ and $N_2$ gas. The best peel strength of PI film is 109.07 gf/mm. Also, we have studied the electric characteristics of pentacene field-effect transistors with the polymer gate-dielectrics such as cyclohexane and hybrid (cyclohexane+TEOS). The transistors with cyclohexane gate-dielectric has higher field-effect mobility, $\mu_{FET}=0.84\;cm^2/v_s$, and smaller threshold voltage, $V_T=-6.8\;V$, compared with the transistor with hybrid gate-dielectric.

정전분무법으로 제작된 열경화성 Phenol-formaldehyde resin 코팅층의 1차원적 미세구조 형성 메카니즘 (1-D Microstructure Evolution of Electrostatic Sprayed Thermosetting Phenol-formaldehyde Resin Coating)

  • 김백현;배현정;고유민;권도균
    • 한국재료학회지
    • /
    • 제26권9호
    • /
    • pp.472-477
    • /
    • 2016
  • Microstructure evolutions of thermosetting resin coating layers fabricated by electrostatic spray deposition (ESD) at various processing conditions were investigated. Two different typical polymer systems, a thermosetting phenol-formaldehyde resin and a thermoplastic polyvinylpyrrolidone (PVP), were employed for a comparative study. Precursor solutions of the phenol-formaldehyde resin and of the PVP were electro-sprayed on heated silicon substrates. Fundamental differences in the thermomechanical properties of the polymers resulted in distinct ways of microstructure evolution of the electro-sprayed polymer films. For the thermosetting polymer, phenol-formaldehyde resin, vertically aligned micro-rod structures developed when it was deposited by ESD under controlled processing conditions. Through extensive microstructure and thermal analyses, it was found that the vertically aligned micro-rod structures of phenol-formaldehyde resin were formed as a result of the rheological behavior of the thermosetting phenol-formaldehyde resin and the preferential landing phenomenon of the ESD method.

Continuous Nanocomposite Coatings on a Phosphor for the Enhancement of the Long-term Stability

  • Kim, Jong-Woung;Song, Jung-Oh;Kim, Chang-Keun
    • 한국고분자학회:학술대회논문집
    • /
    • 한국고분자학회 2006년도 IUPAC International Symposium on Advanced Polymers for Emerging Technologies
    • /
    • pp.233-233
    • /
    • 2006
  • [ $Y_{2}O_{2}S:Eu$ ], a red phosphor, coated with silica nanoparticles or nanocomposites composed of silica nanoparticles and polymeric materials such as PMMA and PVP was prepared via sol-gel process. Samples were prepared from four different methods coded P1, P2, P3, and P4. P1 includes a conventional sol-gel process and a dip-coating method while P2 has the same procedure with P1 except that nanocomposites containing both silica nanoparticles and polymer prepared by sol-gel process were used as coating materials. In P3 method, phosphors were dispersed in a solution containing silica precursor, i.e., TEOS and then polymerization was performed to coat onto the phosphors surface while P4 followed the same procedure with P3 except that a solution containing both TEOS and organic monomer were used in preparing coating materials. Among various coating methods examined in this study, uniform coating of phosphor could be achieved by using method P4, i.e., phosphor surface coating in a solution containing hydrophobic monomer and TEOS. Furthermore, $Y_{2}O_{2}S:Eu$ red phosphor coated with nanocomposite composed of PMMA matrix and silica nanoparticles exhibited enhanced PL intensity and long-term stability.

  • PDF

액상공정을 이용한 탄화규소 세라믹 후막의 제조 (Preparation of Silicon Carbide Ceramic Thick Films by Liquid Process)

  • 김행만;김준수;이홍림;안영철;윤존도
    • 한국세라믹학회지
    • /
    • 제49권1호
    • /
    • pp.95-99
    • /
    • 2012
  • Silicon carbide ceramics are used for oxidation resistive coating films due to their excellent properties like high strength, good oxidation resistance, and good abrasion resistance, but they have poor formability and are prepared by vapor process which is complicated, costly, and sometimes hazardous. In this study, preparation of silicon carbide coating film by liquid process using polymer precursor was attempted. Coating film was prepared by dip coating on substrate followed by heat treatment in argon at $1200^{\circ}C$. By changing the dipping speed, the thickness was controlled. The effects of plasticizer, binder, or fiber addition on suppression of crack generation in the polymer and ceramic films were examined. It was found that fiber additives was effective for suppressing crack generation.

A Study on the Characteristics of Ammonia Doped Plasma Polymer Thin Film with a Controlled Plasma Power

  • 서현진;황기환;주동우;유정훈;이진수;전소현;남상훈;윤상호;부진효
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2014년도 제46회 동계 정기학술대회 초록집
    • /
    • pp.242.2-242.2
    • /
    • 2014
  • Plasma-polymer thin films (PPTF) have been deposited on a Si(100) wafer and glass under several conditions such as different RF power by using plasma-enhanced chemical vapor deposition (PECVD) system. Ethylcyclohexane, ammonia gas, hydrogen and argon were utilized as organic precursor, doping gas, bubbler gas and carrier gases, respectively. PPTFs were grown up with RF (ratio frequency using 13.56 MHz) powers in the range of 20~60 watt. PPTFs were characterized by FT-IR (Fourier Transform Infrared), FE-SEM (Scanning Electron Microscope), AFM (Atomic Force Microscope), Contact angle and Probe station. The result of FT-IR measurement showed that the PPTFs have high cross-link density nitrogen doping ratio was also changed with a RF power increasing. AFM and FE-SEM also showed that the PPTFs have smooth surface and thickness. Impedance analyzer was utilized for the measurements of C-V curves having different dielectric constant as RF power.

  • PDF

폴리에틸렌옥사이드와 주기적인 중간세공 유리실리카 복합재료 제조 (Preparation of Poly(ethylene oxide)/Periodic Mesoporous Organosilica Composite)

  • 이돈;서길수
    • 공업화학
    • /
    • 제20권5호
    • /
    • pp.527-531
    • /
    • 2009
  • 전구체로서 bis(triethoxy silyl) benzene (BTEB), 구조유도체로서 dodecyl trimethyl ammonium bromide (DTMA)를 사용하여 periodic mesoporous organosilicas (PMO) 합성하였다. PMO를 XRD, TEM, 그리고 NMR로 확인한 결과 육각 벌집형태의 메조포러스한 물질임을 확인하였다. 합성한 PMO에 polyethylene oxide (PEO)를 삽입하여, DSC와 XRD로 확인한 결과 고분자가 PMO에 삽입되는 과정에서 고분자의 결정성 용융 온도가 감소하다가 결국 사라짐을 확인하였다. 이러한 결과는 고분자 사슬이 PMO의 기공에 삽입되었다는 것이며, 삽입된 고분자 사슬은 PMO의 골격구조에 의하여 제한 받아서 비결정성 형태의 구조를 지니고 있음을 보여주고 있다.

폴리머 매트릭스를 전구체로 사용한 SrAl2O4:Eu2+,Dy3+ 축광성 형광체의 합성 및 형광 특성 (Synthesis and Photo Luminescent Characteristics of SrAl2O4:Eu2+,Dy3+ Phosphor using Polymer Matrix)

  • 김수종;권혁실
    • 한국전기전자재료학회논문지
    • /
    • 제20권8호
    • /
    • pp.671-679
    • /
    • 2007
  • [ $SrAl_2O_4:Eu^{2+},\;Dy^{3+}$ ] phosphor was synthesized using the impregnation method, and its photoluminescence and long-afterglow properties were investigated, A mixture of $Sr(NO_3)_2,\;Al(NO_3)_2\;9H_2O,\;EuCl_3\;6H_2O,\;DyCl_3\;6H_2O,\;NdCl_3\;6H_2O$ salts were dissolved in distilled water and impregnating into the polymer precursor. After drying, the impregnated mixture was heat treated at $900-1400^{\circ}C$ for 2h in a $N_2-H_2$ reduction atmosphere. The microstructure and crystal structure of the $SrAl_2O_4:Eu^{2+},\;Dy^{3+}$ powders were examined by scanning electron microscopy and X-ray diffraction, respectively. The photoluminescence spectra showed an excitation band along over wide wavelength of 250-450nm, and a broaden emission with a maxima peak at 360nm. In addition, the spectra also showed a good long after glow that decayed over a 1000sec period after 10 min excitation illumination.

Carbon-Supported Ordered Pt-Ti Alloy Nanoparticles as Durable Oxygen Reduction Reaction Electrocatalyst for Polymer Electrolyte Membrane Fuel Cells

  • Park, Hee-Young;Jeon, Tae-Yeol;Lee, Kug-Seung;Yoo, Sung Jong;Sung, Young-Eun;Jang, Jong Hyun
    • Journal of Electrochemical Science and Technology
    • /
    • 제7권4호
    • /
    • pp.269-276
    • /
    • 2016
  • Carbon-supported ordered Pt-Ti alloy nanoparticles were prepared as a durable and efficient oxygen reduction reaction (ORR) electrocatalyst for polymer electrolyte membrane fuel cells (PEMFCs) via wet chemical reduction of Pt and Ti precursors with heat treatment at $800^{\circ}C$. X-ray diffraction analysis confirmed that the prepared electrocatalysts with Ti precursor molar compositions of 40% (PtTi40) and 25% (PtTi25) had ordered $Pt_3Ti$ and $Pt_8Ti$ structures, respectively. Comparison of the ORR polarization before and after 1500 electrochemical cycles between 0.6 and 1.1 V showed little change in the ORR polarization curve of the electrocatalysts, demonstrating the high stability of the PtTi40 and PtTi25 alloys. Under the same conditions, commercial carbon-supported Pt nanoparticle electrocatalysts exhibited a negative potential shift (10 mV) in the ORR polarization curve after electrochemical cycling, indicating degradation of the ORR activity.

Pulverization and Densification Behavior of YAG Powder Synthesized by PVA Polymer Solution Method

  • Im, Hyun-Ho;Lee, Sang-Jin
    • 한국재료학회지
    • /
    • 제30권11호
    • /
    • pp.573-580
    • /
    • 2020
  • YAG (Yttrium Aluminum Garnet, Y3Al5O12) has excellent plasma resistance and recently has been used as an alternative to Y2O3 as a chamber coating material in the semiconductor process. However, due to the presence of an impurity phase and difficulties in synthesis and densification, many studies on YAG are being conducted. In this study, YAG powder is synthesized by an organic-inorganic complex solution synthesis method using PVA polymer. The PVA solution is added to the sol in which the metal nitrate salts are dissolved, and the precursor is calcined into a porous and soft YAG powder. By controlling the molecular weight and the amount of PVA polymer, the effect on the particle size and particle shape of the synthesized YAG powder is evaluated. The sintering behavior of the YAG powder compact according to PVA type and grinding time is studied through an examination of its microstructure. Single phase YAG is synthesized at relatively low temperature of 1,000 ℃ and can be pulverized to sub-micron size by ball milling. In addition, sintered YAG with a relative density of about 98 % is obtained by sintering at 1,650 ℃.

거대기공 다공질 탄화규소 세라믹스의 꺾임강도 (Flexural Strength of Macroporous Silicon Carbide Ceramics)

  • 임광영;김영욱;송인혁;배지수
    • 한국세라믹학회지
    • /
    • 제48권5호
    • /
    • pp.360-367
    • /
    • 2011
  • Macroporous silicon carbide (SiC) ceramics were fabricated by powder processing and polymer processing using carbon-filled polysiloxane as a precursor. The effects of the starting SiC polytype, template type, and template content on porosity and flexural strength of macroporous SiC ceramics were investigated. The ${\beta}$-SiC powder as a starting material or a filler led to higher porosity than ${\alpha}$-SiC powder, owing to the impingement of growing ${\alpha}$-SiC grains, which were transformed from ${\beta}$-SiC during sintering. Typical flexural strength of powder-processed macroporous SiC ceramics fabricated from ${\alpha}$-SiC starting powder and polymer microbeads was 127 MPa at 29% porosity. In contrast, that of polymer-processed macroporous SiC ceramics fabricated from carbon-filled polysiloxane, ${\beta}$-SiC fillers, and hollow microspheres was 116MPa at 29% porosity. The combination of ${\alpha}$-SiC starting powder and a fairly large amount (10 wt%) of $Al_2O_3-Y_2O_3$ additives led to macroporous SiC ceramics with excellent flexural strength.