Epoxidized polybutadiene (EPB) was prepared by polybutadiene (PB) with m-chloroperbenzoic acid (MCPBA) in homogeneous solution. EPB was blended with poly(3-hydroxybutyrate) (PHB) up to 30 wt% by solution-precipitation procedure. The thermal decomposition of PHB/EPB blends was studied by thermogravimetric analysis (TGA), differential scanning calorimetry (DSC) and differential thermal analysis (DTA). The thermograms of PHB/EPB blends contained a two-step degradation process, while that of pure PHB sample exhibited only one-step degradation process. This degradation behavior of PHB/EPB blends, which have a higher thermal stability as measured by maximum decomposition temperature and residual weight, is probably due to crosslinking reactions of the epoxide groups in the EPB component with the carboxyl chain ends of PHB fragments during the degradation process, and the occurrence of such reactions can be assigned to the exothermic peaks in their DTA thermograms.
The purpose of this dissertation is to increase oxidation resistance for Polybutadiene & Polyisoprene, and to investigate the energetics of inhibited oxidation of Polybutadiene & Polyisoprene stabilized with various types of antioxidants using DSC. The results of the study are as fellows: 1. In the DSC SCREEN for the onset temperature of oxidation, Polybutadiene was faster than Polyisoprene for the samples containing no antioxidant in air. 2. In the DSC evaluation for Polybutadiene, Recipe BG-4 with 2.0phr compounds of antioxidant was the best effective, and Recipe BS-4 with 2.0phr compounds of antioxidant was the worst effective, and the degrees of effect of antioxidant were exhibited in the ranking of G-1, D, BHT, and SP, roughly. 3. In the DSC evaluation for the Polyisoprene, Recipe IG-4 with 2.0phr compounds of antioxidant was the best effective, and Recipe ID-4 with 2.0phr compounds of antioxidant was the worst effective, and the degrees of effect of antioxidant were exhibited in the ranking of G-1, SP, BHT, and D roughly. 4. In the study on enthalpy which depends on exothermal reaction, the enthalpy of Polyisoprene was gloater than that of Polybutadiene. However, the problem was not solved completely, and it needs further studies.
Kim, Young-Joon;Chang, Ki-Young;Kim, Gu-Ni;Chun, Yong-Chul;Yoo, Chong-Sun;Park, Sang-Wook
Elastomers and Composites
/
v.31
no.2
/
pp.104-110
/
1996
The polyurethane was synthesized by the reaction of polycaprolactone diol(Mw 2000), 4,4'-diphenylmethane diisocyanate and 1,4-butanediol as the chain extender. Also, the modified polyurethane polymers based on liquid polybutadiene as a part of soft segment and dimethylolpropionic acid as a chain extender, giving polyurethane with various polarity, were synthesized. The thermal, mechanical, adhesion properties and water contact angles of the polyurethanes were examined. From the result of the water contact angle, the polarity of the acid modified PU containing 6% acid content was unchanged but mechanical and adhesion properties were improved. The water contact angles on polybutadiene modified PU films were increased with increasing polybutadiene content. The mechanical properties of the polybutadiene modified PU were higher than that of acid modified PU. However, the mechanical properties were reduced as polybutadiene content increased. The result is presumably due to phase separation between hard segment and soft segment. The peel strength of the polyurethane introduced with 5wt% polybutadiene was improved about 150% than that of unmodified PU. The same as the mechanical properties, the more polybutadiene was introduced, the lower peel strength was obtained.
Carboxyl-terminated polybutadiene was prepared by free-radical polymerization using 4,4'-azobis-[4-cyano valeric acid] as an initiator and the effect of initiator concentration on polymer properties was investigated. Polymerization of the carboxyl-terminated polybutadiene was carried out varying the initiator concentration reacting with a constant butadiene concentration. The carboxyl weight percent decreased with increasing initiator concentration. The conversion was proportional to the square root of initiator concentration, giving a functionality greater than 2.0 which is consistent with the general tendency of free radical polymerization.
Polybutadiene(PB) was epoxidized to various extents with m-chloroperbenzoic acid (MCPBA) in homogeneous solution. The thermal properties of the epoxidized PBs were investigated by differential scanning calorimetry (DSC) and thermogravimetric analysis (TGA). As a result of epoxidation the glass transition temperature (Tg) of PB increased by approximately $0.8^{\circ}$ for each 1 mol% of epoxidation. The thermal decomposition of the epoxidised PBs occurred in two-step process, while that of PB exhibited apparent one-step degradation process.
Novel bio-polybutadiene polymers with controlled molecular weight (MW), MW distribution, chemical composition and micro structure were synthesized by a living anionic polymerization of butadiene and the subsequent coupling reaction of the thus obtained living polybutadiene and a vegetable oil. Anionic polymerization of butadiene was carried out in THF solvent using n-BuLi initiator. The resulting living polybutadienyllithium polymer was then reacted with epoxidized soybean oil (ESO) to obtain a star-polymer of polybutadiene and vegitable oil. Three different bio-elastomers were prepared by coupling living polybutadienes of MWs 1000, 5000 and 1000g/mol with ESO. The molecular structure and MW of the polybutadienes and bioelastomers were characterized by $^1H$-NMR, FTIR and GPC techniques.
The effect of maleinized polybutadiene (MPB) on the mechanical properties of epoxy resins including adhesion strength, elongation and impact peel resistance was investigated in this study, in which MPB is an anhydride-functionalized polybutadiene prepolymer. Different molecular weights (3.1K and 5.6K) of MPB were added to diglycidyl ether bisphenol-A (DEGBA), an epoxy resin, to increase its impact peel strength and elongation. At various loading percent (5, 10, 15, 20 and 25 wt%) of MPB in the epoxy resin, significant improvements of mechanical properties were observed. According to the comparative analysis results, the modified epoxy system with 15 wt% (3.1K) MPB exhibited the highest lap shear strength, about 40% higher than that of neat epoxy. The tensile strength and elongation steadily and simultaneously increased as the loading percent of MPB increased. The impact peel strengths at low (-40℃) and room (23℃) temperatures were substantially improved by MPB incorporation into epoxy resins. Reactive and flexible MPB prepolymer seems to construct strong nano-structured networks with rigid epoxy backbones without sacrificing the tensile and adhesion strengths while increasing impact resistance/toughness and elongation properties. For higher impact peel while maintaining adhesion and tensile strengths, approximately 10-15 wt% MPB loading in epoxy resin was suggested. Consequently, incorporation of functionalized MPB prepolymer into epoxy system is an easy and efficient way for improving some crucial mechanical properties of epoxy resins.
Lee, Sangmook;Hong, In-Kwon;Lee, Jae Wook;Jeong, Won Bok
Polymer(Korea)
/
v.38
no.4
/
pp.417-424
/
2014
Reactivity and rheological behavior of highly concentrated polymer bonded explosives (PBX) simulant was studied. As a binder, thermosetting hydroxyl terminated polybutadiene (HTPB) was used. By using bimodal $CaCO_3$ (size ratio 10:1) and sugar particles (size ratio 25:1) as fillers, maximum 75 v% filling was possible during melt mixing. The relative viscosities of bimodal suspension were much lower than those of unimodal one and showed minimum values at 0.25 of fine particle fraction. In curing experiment, as curing temperature increased, the time of initiation and completeness of curing reaction became shortened, the torque kept low, and the change of internal temperature decreased.
To separate carbon dioxide from a flue gas, membranes for gas separation was fabricated from polystyrene-b-polybutadiene (SB) diblock copolymer blends with poly(phenylene oxide), PPO. SB diblock copolymer formed miscible blends with PPO in the experimental range (lower than or equal to 70 wt% PPO). When the blend contained PPO whose composition is in the range of 40-50 wt%, the discontinuous phase of polybutadiene block in SB diblock copolymer, was changed to discrete phase, while polystyrene blocks containing PPO was changed to the continuous phase. A sudden decrease of the gas permeability and a sudden increase of the gas selectivity was observed at these blend compositions. A gas separation membranes having excellent mechanical properties and exhibiting advantages in gas permeability and selectivity could be fabricated from blends containing more than 50 wt% PPO.
In this study, microstructure and gel content (C-C) of polybutadiene rubber (PBR) were investigated using various techniques including ASTM D 3616, attenuated total reflectance Fourier transform infrared spectrometry (ATR FTIR), differential scanning calorimetry (DSC) and nuclear magnetic resonance spectroscopy (NMR). The ATR FTIR spectra of the samples were investigated to determine the cis, trans, 1, 2-vinyl and the C-C gel content in PBR. The absorbance ratios of specific peaks in different grades of PBR were correlated with the C-C gel content measured by the ATR FTIR techniques. Physico-mechanical and rheological properties of rubber compounds based on BR with various amounts of gel were determined. The results showed that there is an acceptable correlation between these properties and the C-C gel content of PBR.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.