• Title/Summary/Keyword: pH leaching

Search Result 399, Processing Time 0.036 seconds

Bioleaching of Mn(II) from Manganese Nodules by Bacillus sp. MR2 (Bacillus sp. MR2에 의한 망간단괴의 생물용출)

  • Choi, Sung-Chan;Lee, Ga-Hwa;Lee, Hong-Keum
    • Korean Journal of Microbiology
    • /
    • v.45 no.4
    • /
    • pp.411-415
    • /
    • 2009
  • Some microorganisms are capable of leaching Mn(II) from nonsulfidic manganese ores indirectly via nonenzymatic processes. Such reductive dissolution requires organic substrates, such as glucose, sucrose, or galactose, as a source of carbon and energy for microbial growth. This study investigated characteristics of Mn(II) leaching from manganese nodules by using heterotrophic Bacillus sp. strain MR2 provided with corn starch as a less-expensive substrate. Leaching of Mn(II) at 25.6 g Mn(II) $kg^{-1}$ nodule $day^{-1}$ was accompanied with cell growth, but part of the produced Mn(II) re-adsorbed onto residual $MnO_2$ particles after 24 h. Direct contact of cells to manganese nodule was not necessary as a separation between them with a dialysis tube produced similar amount [24.6 g Mn(II) $kg^{-1}$ nodule $day^{-1}$]. These results indicated an involvement of extracellular diffusible compound(s) during Mn(II) leaching by strain MR2. In order to optimize a leaching process we tested factors that influence the reaction, and the most efficient conditions were $25\sim35^{\circ}C$, pH 5~7, inoculum density of 1.5~2.5% (v/v), pulp density of 2~3 g/L, and particle size <75 ${\mu}m$. Although Mn(II) leaching was enhanced as particle size decrease, we suggest <212 ${\mu}m$ as a proper size range since more grinding means more energy consumption The results would help for the improvement of bioleaching of manganese nodule as a less expensive, energy-efficient, and environment-friendly technology as compared to the existing physicochemical metal recovery technologies.

Lead Content Leached out from Glazed Potteries (식품저장용 옹기유의 납 용출에 관한 연구)

  • LEE Goon-Ja;PARK Chung-Kil
    • Korean Journal of Fisheries and Aquatic Sciences
    • /
    • v.14 no.3
    • /
    • pp.158-164
    • /
    • 1981
  • Leaching of lead from glazed potteries was studied under various conditions. The amount of lead was determined by atomic absorption spectrophotometry. Lead content was tended to increase with lowering PH of the solution below pH 4, but it was not detected at above pH 6 during the storage period of six weeks. More lead was leached out from the glazed potteries with red color than those of black color at the same pH. No lead was detected when the medicine-boiling pots were boiled with water or $4\%$ acetic acid solution for six hours. A significant accumulation of lead, however, was shown in Kimchi and mixed solutions of organic acids when they stored in the glazed potteries more than three weeks, although they appeared lead-free by the Korean Industrial Standard Test Method.

  • PDF

A Study on the Bioleaching of Cobalt and Copper from Cobalt Concentrate by Aspergillus niger strains (Aspergillus niger 균주를 이용(利用)한 코발트 정광(精鑛)으로부터 코발트 및 구리의 미생물(微生物) 침출(浸出) 연구(硏究))

  • Ahn, Hyo-Jin;Ahn, Jae-Woo;Bang, Duk-Ki;Kim, Meong-Woon
    • Resources Recycling
    • /
    • v.22 no.2
    • /
    • pp.44-52
    • /
    • 2013
  • Bioleaching behavior of metal ions for recovery of cobalt and copper from cobalt concentrate was investigated by employing three Aspergillus niger strains. Various factors, such as organic acid generation with fungi type, pH of the culture and pulp density were studied. The results showed that the best fungi for organic acid(citric acid and oxalic acid) generation was A. niger KCTC 6144 using Malt Extract Broth culture at initial pH 3.5. But A. niger KCTC 6985 was more effective for the leaching of cobalt and copper from cobalt concentrate. Our results showed that 82% cobalt and 98% copper was dissolved by A. niger KCTC 6985 at 10g/L pulp density, at pH 3.5 and $24^{\circ}C$ after 15 days incubation.

Solvent Extraction Separation of Nd and Pr from Chloride Solution using Organophosphorus Acid Extractants (염산용액에서 유기인산계 추출제에 의한 Nd와 Pr의 분리추출)

  • Park, Joo-Ho;Jeon, Ho-Seok;Lee, Man-Seung
    • Resources Recycling
    • /
    • v.23 no.2
    • /
    • pp.37-45
    • /
    • 2014
  • Solvent extraction experiments have been performed to separate Nd and Pr from chloride leaching solution of monazite sand using single Cyanex272 and mixed extractants as PC88A+Cyanex272 and PC88A+TBP. For this purpose, the effect of the concentration of extractants on the extraction and separation of the two metals were studied by varying the pH of aqueous solution. In the experimental ranges conducted in this study, the distribution coefficients of Nd were higher than those of Pr. In Cyanex272 system, our results indicated that concentration of extractant and initial pH did not affect distribution coefficients, but separation factor was increased with increasing initial pH. In binary extractant system, distribution coefficients were lower than those of single PC88A system, whereas separation factor was similar in both mixed and single extractant system.

Microbial Leaching of Iron from Magnetite (미생물을 이용한 자철석으로부터 철 침출에 관한 연구)

  • Roh, Yul;Oh, Jong-Min;Seo, Yong-Jae;Jang, Hee-Dong
    • Journal of the Mineralogical Society of Korea
    • /
    • v.19 no.4 s.50
    • /
    • pp.265-275
    • /
    • 2006
  • It is in its infancy to use bacteria as a novel biotechnology for leaching precious and heavy metals from raw materials. The objective of this study was to investigate biogeochemical processes of iron leaching from magnetite reduction by iron-reducing bacteria isolated from intertidal flat sediments, southwestern part of Korea. Microbial leaching experiments were performed using commercial magnetite, Aldrich magnetite, in well-defined mediums with and without bacteria. Water soluble Fe production was determined by ICP analysis of bioleached samples in comparison to uninoculated controls, and the resulting precipitated solids were characterized by X-ray diffraction (XRD) and scanning electron microscopy (SEM). The extent of iron leaching from magnetite in the aerobic conditions (Fe = 107 ppm) was higher than that in the anaerobic environments (Fe = 94 ppm). In the anaerobic conditions, Fe(III) in commercial magnetite was also reduced to Fe(II), but no secondary mineral phases were observed. Amorphous iron oxides formed in the medium under aerobic conditions where there was sufficient supply of oxygen from the atmosphere. SEM observation suggests that the reduction process involves dissolution-precipitation mechanisms as opposed to solid state conversion of magnetite to amorphous iron oxides. The ability of bacteria to leach soluble iron and precipitate amorphous iron oxides from crystalline magnetite could have significant implications for biogeochemical processes in sediments where Fe(III) in magnetite plays an important role in the largest pool of electron acceptor as well as the tool as a novel biotechnology for leaching precious and heavy metals from raw materials.

Experimental Studies for Analyzing Salt Movement and Desalinization Effects on Reclaiming New Manguem Tideland (새만금지구 간석지토양의 염분거동해석 및 제염효과분석을 위한 실험적연구)

  • 구자웅;한강완;서승덕
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.31 no.2
    • /
    • pp.92-103
    • /
    • 1989
  • This study was performed in order to produce the basic data for devising irrigation project and desalinization countermeasure through analyzing salt movement and desalinzation effects. The Desalinization experiments with water management practices were carried out, using the soil samples collected in New Manguem tideland. The changes of electrical conductivity, exchangeable sodium percentage, pH and hydraulic conductivity during the desalinization experiments, and the correlations between various factors influencing desalinization, were analyzed by the statistical method. The results obtained from this study were summarized as follows: 1. The sample soils used in this study were salin-sotlic soils with the high electrical conductivity and the high exchangeable sodium percentage, and the soil texture was silt loam. 2. A large amount of the soluble salts was removed in the begining of desalinization experiments. The initial electrical conductivity and the initial exchangeable sodium percentage decreased considerably in the beginning, and were gradually slow in the rate of decrease 3. The value of pH showed a tendency to increase during the desalinization and were little by little slow in the rate of increase, and could be estimated by the regression equation. 4. The initial hydraulic conductivity were raised greatly with gypsum treatment and the penmeability was maintained adequately, The hydraulic conductivity and the leaching time elapsed during the desalinization could be estimated by the regression equation. 5. The water requirement for desalinization with various water management practices could be estimated for a given electrical conductivity, exchangeable sodium percentage, and pH reading respectively.

  • PDF

A study on the manufacture of the ZnO by the wet method from the EAF dust (제강분진을 이용한 ZnO분말의 제조에 관한 연구)

  • Jeong, Rae-Youn;Lee, Jin-Hui
    • Journal of the Korean Applied Science and Technology
    • /
    • v.28 no.2
    • /
    • pp.251-257
    • /
    • 2011
  • The processes for the preparation of ZnO powder by using EAF(electric arc furnace)dust was studied by wetting method which are divided to two steps, carried out of the elution processes by various concentrations of sulfuric acid is reacted with EAF dust as the former, and the latter were performed by a number of specified processes, which are leaching process depends on various pH, cementation, ozone and heat treatment processes etc. Experimental results showed that the appropriate pH range is pH7.5~8.0 and the resulting zinc content is range of 37~38%, the residual quantities of the heavy metals are less than 3ppm individually by cementation process except Mn, even though the Mn metal could not be removed by cementation process but was removed up to 0.2ppm by the ozone process from 70ppm initially. Finally, 80.2% of ZnO was obtained by the heat treatment at $500^{\circ}C$.

An Experimental Study on the Utilization of Phosphogypsum as Daily and Intermediate Cover Materials (일일 및 중간복토재로서 인산석고 재활용을 위한 실험 연구)

  • 이용수;정형식
    • Journal of the Korean Geotechnical Society
    • /
    • v.18 no.1
    • /
    • pp.133-140
    • /
    • 2002
  • Phosphogypsum is a by-product from the phosphoric acid process for manufacturing fertilizers. It consists mainly of $(CaSO_4.2H_2O)$ and contains some impurities such as$(P_2O_5)$, 불소$(F_-)$, and organic substances. The annual world production of this material is up to 150 million tons and is up to 1.57 million tons in Korea. Therefore studies describe application of phosphogypsum to daily and middle cover materials in landfill. For this Purpose, experiments were performed to evaluate the engineering properties of the material by sieve analysis, specific gravity, consistency of soil, compaction, CBR, permeability, mi environmental characteristics of leaching test, reactor test. The results of this study are as follows : The mixing and layer conditions of CBR value are 6.2~6.3%, coefficient of permeability is $\alpha$$\times10_{-5}~10_{-6}cm/sec$. And leaching test results are far below than those of regulatory requirement of Waste Management Act, Soil Environment Preservation Act in Korea and RCRA in USA. Therefore phosphogypsum can be used as daily and intermediate cover materials in landfill.

Solvent Extraction Separation of Re (VI) from Hydrochloric Acid Leaching Solution of Spent Super Alloy by Alamine 304-1 (폐 초내열합금 염산침출 용액으로부터 Alamine304-1을 이용한 레늄의 용매추출분리)

  • Ahn, Jong-gwan;Jung, Hee-Kyeoung;Jang, Jae-Young;Kim, Min-Seuk
    • Resources Recycling
    • /
    • v.24 no.5
    • /
    • pp.56-62
    • /
    • 2015
  • Solvent extraction experiments for the separation and recovery of Re from hydrochloric acid leaching solution of spent super alloy by Alamine 304-1 were carried out. The effects of some variables, such as the nature and concentration of the extractants, HCl concentration, and the presence of impurities were investigated. The synthetic solutions of Re were prepared by dissolving ammonium perrhenate (APR), Alamine304-1, Cyanex272 and $D_2EHPA$ were used solvent extractants distilled in kerosene. The extraction percentage of Re by Alamine304-1 was higher than the other extractants as Cyanex272 and $D_2EHPA$ and the percentage is about 99%. Only 99% of Re was extracted in the presence of Al, Co and V in HCl solution.

A Study on the Cementation Reaction of Cadmium by Zinc Powders from Leaching Solution of Waste Nickel-Cadmium Batteries (폐니켈-카드뮴 전지 침출액으로부터 아연 분말을 이용한 카드뮴의 치환반응에 대한 연구)

  • Kim, Min-Jun;Park, Il-Jeong;Kim, Dae-Weon;Jung, Hang-Chul
    • Resources Recycling
    • /
    • v.28 no.1
    • /
    • pp.23-31
    • /
    • 2019
  • Cementation is one of economical and efficient recycling method precipitating the metal ion in solution by adding another active metal. In this study for optimizing cadmium recovery efficiency, it was performed as a function of the effect of pH, temperature, particle size, and input amount of zinc in 0.1 M $CdSO_4$ solution and Ni-Cd battery leaching solutions, respectively. The particle size of zinc and temperature were key factors for Cd cementation and it was confirmed that the input amount of 2.6 of Zn/Cd ratio using granular-type zinc was optimal condition for selective Cd recovery efficiency at $25^{\circ}C$.