• Title/Summary/Keyword: near net shape

Search Result 122, Processing Time 0.019 seconds

Numerical Analysis of the Effect of Fuselage of Fan-in-body Aircraft on the Pusher Propeller

  • Kang, Jiwook;Jang, Jisung;You, Younghyun;Hyun, Youngo;Lee, Jonghun
    • 항공우주시스템공학회지
    • /
    • 제15권2호
    • /
    • pp.26-35
    • /
    • 2021
  • In this study, CFD analysis was conducted to compare the aerodynamic performance of the isolated propeller and pusher propeller, which is affected by the wake of wide fuselage. The moving reference frame (MRF) method was used for isolated propeller analysis, while the MRF and sliding mesh method were used sequentially for the pusher propeller to analyze the change in the aerodynamic characteristics based on the azimuth angle. Under the same torque condition, the thrust of the pusher propeller was greater than that of the isolated propeller. Thrust increment of the pusher propeller was mainly generated near the root of the blade where the fuselage wake was concentrated. The net efficiency of the pusher propeller was greater than or equal to that of the isolated propeller. Because of the flat fuselage shape, thrust and torque of the pusher propeller periodically changed with the rotation of the propeller.

Study on failure mechanism of line contact structures of nuclear graphite

  • Jia, Shigang;Yi, Yanan;Wang, Lu;Liu, Guangyan;Ma, Qinwei;Sun, Libin;Shi, Li;Ma, Shaopeng
    • Nuclear Engineering and Technology
    • /
    • 제54권8호
    • /
    • pp.2989-2998
    • /
    • 2022
  • Line contact structures, such as the contact between graphite brick and graphite tenon, widely exist in high-temperature gas-cooled reactors. Due to the stress concentration effect, the line contact area is one of the dangerous positions prone to failure in the nuclear reactor core. In this paper, the failure mechanism of line contact structures composed of IG11 nuclear graphite column and brick were investigated by means of experiment and finite element simulation. It was found that the failure process mainly includes three stages: firstly, the damage accumulation in nuclear graphite material led to the characteristic yielding of the line contact structure, but no macroscopic failure can be observed at this stage; secondly, the stresses near the contact area met Mohr failure criterion, and a crack initiated and propagated laterally in the contact zone, that is, local macroscopic failure occurred at this stage; finally, a second crack initiated in the contact area and developed in to a Y-shape, resulting in the final failure of the structure. This study lays a foundation for the structural design and safety assessment of high-temperature gas-cooled reactors.

직응집성형법을 이용한 질화규소의 실형상 성형공정 및 성형특성 (Near-Net-Shape Forming and Green Properties of Silicon Nitride by Direct Coagulation Casting Technique)

  • 정윤성;;정연길;백운규
    • 한국세라믹학회지
    • /
    • 제39권3호
    • /
    • pp.299-307
    • /
    • 2002
  • 본 연구에서는 복잡 형상의 세라믹체를 효율적으로 성형할 수 있어 새로운 성형기법으로 부각되고 있는 직응집성형(Direct Coagulation Casing, DCC)공정기술에 관하여 콜로이드 계면화학을 이용하여 연구하였다. 높은 고형분량을 가지는 안정된 질화규소 슬립을 제조하기 위하여 분산제, 소결조제 그리고 응집제 각각이 다양한 공정변수에 미치는 영향에 대하여 평가하였다. 1.0 wt% Tetraethylammonium Hydroxide(TEAH)를 첨가하여 염기영역에서 소결조제를 포함한 안정된 51vol%의 질화규소 슬립을 제조할 수 있었다. 질화규소 슬립은 첨가된 $Al(CH_3COO)_2OH$의 온도증가에 따른 열분해를 이용하여 직응집성 유도하였다. 염기영역에서 $Al^{3+}$ 이온들이 aluminum hydroxide$(Al(OH)_3)$ 석출되면서 슬립내 $OH^-$ 농도를 감소시켜 질화규소 슬립을 직응집시켰다.

13%Cr-0.17%C 스테인리스강의 고온 가스질화에 미치는 Al 함량 변화의 영향 (Effect of Al Content Variation on High Temperature Gas Nitriding in 13%Cr-0.16%C Stainless Steel)

  • 박범태;김정민;강희재;공정현;강창룡;성장현
    • 열처리공학회지
    • /
    • 제24권6호
    • /
    • pp.318-326
    • /
    • 2011
  • This study has been performed to investigate the effect of Al addition on High Temperature Gas Nitriding (HTGN) in 13%Cr-0.16%C stainless steel with different Al contents of 0.54%, 1.76% and 2.36%, respectively. HTGN treatment was carried out at $1100^{\circ}C$ for 1 hr, 5 hrs and 10 hrs. Nitrogen-permeated surface layers showed round type carbides of $Cr_{23}C_6$ and needle type nitrides of AlN in the matrix of martensite, representing 600~700 Hv. And the thickness of the surface layer increased with increasing Al content and HTGN treatment time. The inner region that was not permeated nitrogen showed chromium carbides in the mixed phase of martensite and ferrite for the 0.53% Al alloyed steel, however chromium carbides in the matrix of ferrite single phase were shown for the steels with the addition of 1.76%Al and 2.36%Al, representing the hardness of ~200 Hv. During nitrogen permeation from surface to the interior, substitutional elements of Cr, Al and Si moved toward the surface and interstitial element of carbon also moved from interior to the surface. This movement of alloying elements leads high concentration of these elements at the outmost surface, subsequently the lowest peak of substitutional elements were shown in the vicinity of near surface. After showing the lowest peak, the high concentration region of Al and C were formed due to the continuous movement of Al toward the surface. The long discontinuous precipitates of $Cr_{23}C_6$ and AlN were formed along the outmost surface owing to the high concentration of these alloying elements.

SLM 방식으로 적층 제조된 Ti-6Al-4V 합금의 HIP 처리에 따른 준정적 및 동적 기계적 특성 변화 (Influence of Hot Isostatic Press on Quasi-static and Dynamic Mechanical Properties of SLM-printed Ti-6Al-4V Alloy)

  • 장지훈;최영신;김형균;이동근
    • 열처리공학회지
    • /
    • 제33권3호
    • /
    • pp.99-106
    • /
    • 2020
  • Selective laser melting (SLM) is an additive manufacturing process by melting metallic powders and stacking into layers, and can product complex shapes or near-net-shape (NNS) that are difficult to product by conventional processes. Also, SLM process is able to raise the efficiency of production by creating a streamlined manufacturing process. For manufacturing in SLM process using Ti-6Al-4V powder, analysis of microstructural evolution and evaluation of mechanical properties are essential because of rapid melting and solidification process of powders according to high laser power and rapid scan speed. In addition, it requires a post-processing because the soundness and mechanical properties are degraded by defects such as pore, un-melted powder, lack-of-fusion, etc. In this study, hot isostatic press (HIP) was conducted as a post-processing on SLM-printed Ti-6Al-4V alloy. Microstructure of post-processed Ti-6Al-4V alloy was compared to as-built Ti-6Al-4V, and the evolution of quasi-static (Vickers hardness, room temperature tensile characteristic) and dynamic (high-cycle fatigue characteristic) mechanical properties were analyzed.

반응결합 강화 알루미나세라믹스의 제조에 관한 연구 (A Study on the Fabrication of Reinforced Reaction Bonded Alumina Ceramics)

  • 김일수;강민수;박정현
    • 한국세라믹학회지
    • /
    • 제35권4호
    • /
    • pp.311-318
    • /
    • 1998
  • The reaction bonded alumina ceramics with reinforced particles which have low shrinkage were pro-duced by blending of SiC or TiC or ZrO2 powders to the mixture of Al metal and Al2O3 powder. The powd-ers were attrition milled isostantically pressed and preheated tio 110$0^{\circ}C$ with a heating rate of $1.5^{\circ}C$/min The specimens were then sintered at the temperature range 1500 to 1$600^{\circ}C$ for 5 hours with a heating rate of 5$^{\circ}C$/min. The specimens showed 5-9% weight gain and 2-9% dimensional expansion through the complete oxidation of Al after preheating up to 11--$^{\circ}C$ the overall dimensional change of the specimens after the reaction sintering at 1500-1$600^{\circ}C$ was 6-12% The maximum densities were 92% theoretical. The fine grain-ed(average grain size :0.4 ${\mu}{\textrm}{m}$) microstructure were observed in the specimen with ZrO2 and SiC. But the microstructure of specimen with TiC was relatively coarse.(average grain size : 2.1 ${\mu}{\textrm}{m}$) The mullite phase was formed by the reaction of Al2O3 and SiO2 in a specimen with SiC. In the TiC contained specimen TiC was oxidized into TiO2 and finally reacted with Al2O3 to form Al2TiO5 during sintering.

  • PDF

Powder Metallurgy for Light Weight and Ultra-Light Weight Materials

  • Kieback, B.;Stephani, G.;Weiβgarber, T.;Schubert, T.;Waag, U.;Bohm, A.;Anderson, O.;Gohler, H.;Reinfried, M.
    • 한국분말재료학회지
    • /
    • 제10권6호
    • /
    • pp.383-389
    • /
    • 2003
  • As in other areas of materials technology, the tendency towards light weight constructions becomes more and more important also for powder metallurgy. The development is mainly driven by the automotive industry looking for mass reduction of vehicles as a major factor for fuel economy. Powder metallurgy has to offer a number of interesting areas including the development of sintered materials of light metals. PM aluminium alloys with improved properties are on the way to replace ferrous pars. For high temperature applications in the engine, titanium aluminide based materials offer a great potential, e.g. for exhaust valves. The PM route using elemental powders and reactions sintering is considered to be a cost effective way for net shape parts production. Furthermore it is expected that lower costs for titanium raw materials coming from metallurgical activities will offer new chances for sintered parts with titanium alloys. The field of cellular metals expands with the hollow sphere technique, that can provide materials of many metals and alloys with a great flexibility in structure modifications. These structures are expected to be used in improving the safety (crash absoption) and noise reduction in cars in the near future and offer great potential for many other applications.

Al 박육 다이캐스팅 주물에서 기포결함에 미치는 주물두께, 사출속도의 영향 (Effect of Casting Thickness and Plunger Velocity on Porosity in Al Plate Diecasting)

  • 강호정;박진영;김억수;조경목;박익민
    • 한국주조공학회지
    • /
    • 제35권4호
    • /
    • pp.80-87
    • /
    • 2015
  • The Al die casting process has been widely used in the manufacturing of automotive parts when the process requires near-net shape casting and a high productive rate. However, porosity arises in the casting process, and this hampers the wider use of this method for the creation of high-durability automotive components. The porosity can be controlled by the shot condition, but, it is critical to set the shot condition in the sleeve, and it remains difficult to optimize the shot condition to avoid air entrapment efficiently. In this study, the 4.5 mm, 2.0 mm plate die castings were fabricated under various shot conditions, such as plunger velocities of 0.7 m/s ~ 3.0 m/s and fast shot set points of the cavity of -25%, 0%, 25%, and 50%. The mold filling behavior of Al melts in the cavity was analyzed by a numerical method. Also, according to the shot conditions, the results of numerical analyses were compared to those of die-casting experiments. The porosity levels of the plate castings were analyzed by X-ray CT images and by density and microstructural analyses. The effects of the porosity on the mechanical properties were analyzed by tensile tests and hardness tests. The simulation results are in good general agreements with the die-casting experimental results. When plunger velocity and fast shot set point are 1.0 m/s and cavity 25% position, castings had optimum condition for good mechanical properties and a low level of porosity.

A distributed piezo-polymer scour net for bridge scour hole topography monitoring

  • Loh, Kenneth J.;Tom, Caroline;Benassini, Joseph L.;Bombardelli, Fabian A.
    • Structural Monitoring and Maintenance
    • /
    • 제1권2호
    • /
    • pp.183-195
    • /
    • 2014
  • Scour is one of the leading causes of overwater bridge failures worldwide. While monitoring systems have already been implemented or are still being developed, they suffer from limitations such as high costs, inaccuracies, and low reliability, among others. Also, most sensors only measure scour depth at one location and near the pier. Thus, the objective is to design a simple, low cost, scour hole topography monitoring system that could better characterize the entire depth, shape, and size of bridge scour holes. The design is based on burying a robust, waterproofed, piezoelectric sensor strip in the streambed. When scour erodes sediments to expose the sensor, flowing water excites it to cause the generation of time-varying voltage signals. An algorithm then takes the time-domain data and maps it to the frequency-domain for identifying the sensor's resonant frequency, which is used for calculating the exposed sensor length or scour depth. Here, three different sets of tests were conducted to validate this new technique. First, a single sensor was tested in ambient air, and its exposed length was varied. Upon verifying the sensing concept, a waterproofed prototype was buried in soil and tested in a tank filled with water. Sensor performance was characterized as soil was manually eroded away, which simulated various scour depths. The results confirmed that sensor resonant frequencies decreased with increasing scour depths. Finally, a network of 11 sensors was configured to form a distributed monitoring system in the lab. Their exposed lengths were adjusted to simulate scour hole formation and evolution. Results showed promise that the proposed sensing system could be scaled up and used for bridge scour topography monitoring.

SiCp입자강화 Al 복합재료의 내열 및 마모특성 (Heat and Wear Resistance Characterization of SiCp Reinforced Al Matrix Composites)

  • 김석원;김완기;우기도;안행근
    • 한국주조공학회지
    • /
    • 제20권6호
    • /
    • pp.377-385
    • /
    • 2000
  • Al matrix composites as the most promising MMCs can be expected to be excellent engineering materials in the nearest future. So as to improve material properties of composite, many manufacturing processes have been developed. Among them, squeeze casting process which offers fine microstructure and near-net-shape is one of the most successful MMCs manufacturing processes. But, in case of with subsieve size particles (under 44 ${\mu}m$), it is very difficult to homogeneously distribute particles in matrix of Al matrix composite by various casting processes, including squeeze casting used so far. Duplex process which was developed in previous study was used to distribute the particle of subsieve size more homogeneously in matrix of Al matrix composite. Microstructures, wear and heat resistance characterization of Al-Si-Cu-Mg-(Ni)/SiCp manufactured by duplex process were examined to clarify the effect of manufacturing conditions, particle size of reinforcement and alloying elements. Al matrix composites reinforced with SiCp(10 ${\mu}m$) have the lowest wear amount among composites reinforced with 3 ${\mu}m$, 5 ${\mu}m$ and 10 ${\mu}m$ SiCp. The wear amount of Al matrix composites with 10 wt.% SiCp(3, 5, 10 ${\mu}m$) was decreased according to the increase of the sliding speed because abrasive wear takes place at high sliding speed of 4m/s and worn debris with block type occurs at low sliding speed of 1m/s. As for heat resistance, it is made clear that remarkable heat resistance property can be obtained by addition of Ni element in Al matrix composites.

  • PDF