Preparation of Nano Titania Sols and Thin Films added with Transition Metal Elements (전이금속원소들이 첨가된 나노 티타니아 졸 및 코팅막 제조)

  • Lee K.;Lee N. H.;Shin S. H.;Lee H. G.;Kim S. J.
    • Korean Journal of Materials Research
    • /
    • v.14 no.9
    • /
    • pp.634-641
    • /
    • 2004
  • The photocatalytic performance of $TiO_2$ thin films coated on porous alumina balls using various aqueous $TiOCl_2$ solutions as starting precursors, to which 1.0 $mol\%$ transition metal ($Ni^{2+},\;Cr^{3+},\;Fe^{3+},\;Nb^{3+},\;and\;V^{5+}$) chlorides had been already added, has been investigated, together with characterizations for $TiO_2$ sols synthesized simultaneously in the same autoclave through hydrothermal method. The synthesized $TiO_2$ sols were all formed with an anatase phase, and their particle size was between several nm and 30 nm showing ${\zeta}-potential$ of $-25{\sim}-35$ mV, being maintained stable for over 6 months. However, the $TiO_2$ sol added with Cr had a much lower value of -potential and larger particle sizes. The coated $TiO_2$ thin films had almost the same shape and size as those of the sol. The pure $TiO_2$ sol showed the highest optical absorption in the ultraviolet light region, and other $TiO_2$ sols containing $Cr^{3+},\;Fe^{3+}\;and\;Ni^{2+}$ showed higher optical absorption than pure sol in the visible light region. According to the experiments for removal of a gas-phase benzene, the pure $TiO_2$ film showed the highest photo dissociation rate in the ultraviolet light region, but in artificial sunlight the photo dissociation rate of $TiO_2$ coated films containing $Cr^{3+},\;Fe^{3+}\;and\;Ni^{2+}$ was measured higher together with the increase of optical absorption by doping.

Synthesis of TiO2 nanoparticles using Water-in-oil microemulsion method (유중수형(油中水型) 마이크로에멀젼법을 이용한 타이타니아 나노입자의 제조)

  • So Min Jin;Hyeon Jin;Seong Ju Kim;Yu Na Kim;Dae-Won Lee
    • Journal of Industrial Technology
    • /
    • v.43 no.1
    • /
    • pp.1-6
    • /
    • 2023
  • TiO2 is a versatile metal oxide material that is frequently used as a photo-catalyst for organic pollutant oxidation and a functional material for ultraviolet-ray protection. To improve its chemical/physical properties and widen the range of industrial application, it is demanded to control the crystalline feature and morphology precisely by applying advanced nano-synthesis methods. In this study, we prepared TiO2 nanoparticles using the water-in-oil (W/O) microemulsion method and compared them with the particles synthesized by the conventional precipitation method. Also, we tried to find the optimum conditions for obtaining nano-sized, anatase-rich TiO2 particles by the W/O microemulsion method. We analyzed the crystalline feature and particle size of the prepared samples using X-ray diffraction (XRD) and Transmission electron microscopy (TEM). In summary, we found the W/O microemulsion is more effective than precipitation in obtaining nano-sized TiO2. The best result was derived when the microemulsion was formed using AOT surfactant, hydrolysis was performed under basic condition and the sample was calcined at 200℃.

Synthesis and Catalytic Characteristics of Thermally Stable TiO2/Pt/SiO2 Hybrid Nanocatalysts (고온에서 안정적인 TiO2/Pt/SiO2 하이브리드 나노촉매의 제작 및 촉매 특성)

  • Reddy, A. Satyanarayana;Jung, Chan-Ho;Kim, Sun-Mi;Yun, Jung-Yeul;Park, Jeong-Young
    • Journal of Powder Materials
    • /
    • v.18 no.6
    • /
    • pp.532-537
    • /
    • 2011
  • Thermally stable $TiO_2$/Pt/$SiO_2$ core-shell nanocatalyst has been synthesized by chemical processes. Citrated capped Pt nanoparticles were deposited on amine functionalized silica produced by Stober process. Ultrathin layer of titania was coated on Pt/$SiO_2$ for preventing sintering of the metal nanoparticles at high temperatures. Thermal stability of the metal-oxide hybrid catalyst was demonstrated heating the sample up to $600^{\circ}C$ in air and by investigating the morphology and integrity of the structure by transmission electron spectroscopy. The surface analysis of the constituent elements was performed by X-ray photoemission spectroscopy. The catalytic activity of the hybrid catalysts was investigated by CO oxidation reaction with oxygen as a model reaction.

Evaluation of Mechanical Properties of Barrier Ribs for Plasma Display Panel Using Nano Indenter Technology (나노 인덴터를 이용한 플라즈마 디스플레이 소자(PDP)내 격벽의 기계적 물성 평가)

  • Jung, Byung-Hae;Kim, Hyung-Sun
    • Korean Journal of Materials Research
    • /
    • v.13 no.1
    • /
    • pp.53-58
    • /
    • 2003
  • For the rib materials in PDP(plasma display panel), an effective method to improve the mechanical properties is to form a composite material by reinforcing a glass matrix with rigid fillers, such as alumina and titania powders. In this study, two types of ribs with different volume percent of fillers and with different glass matrix were tested for hardness, Young's modulus with the Berkovich indentation. As a result, cracks appeared around at the load of 1345 mN for the dense type of rib, while porous one endured until 2427 mN without any crack formation. Young's modulus and hardness decreased at the range: 90∼65 GPa, 9∼4 GPa, respectively as a function of indent load. Thus, a new method with nanoindenter represents a possible evaluation method for mechanical properties of barrier ribs.

The growth of zinc oxide particles by coagulation in aerosol reactor (에어로졸 반응기에서 산화아연 입자의 응집 성장)

  • Lee, Jong Ho;Song, Shin Ae;Park, Seung Bin
    • Particle and aerosol research
    • /
    • v.4 no.2
    • /
    • pp.69-75
    • /
    • 2008
  • Nanosize ZnO particles were prepared by oxidation of zinc vapor and the particle growth was modeled by a coagulation model by assuming that the characteristic time for reaction was much shorter than coagulation time and residence time (${\tau}_{reaction}{\ll}{\tau}_{coagulation}{\ll}{\tau}_{residence}$). Experimental measurement of zinc oxide particles diameter was consistent with the predicted result from the coagulation model. For practical purpose of predicting zinc oxide size in areosol reactor, the constant kernel solution is concluded to be sufficient, Uniqueness of nano-scale property of zinc oxide was confirmed by the higher photocatalytic activity of zinc oxide than nanosize titania particles.

  • PDF

Effects of Electrolyte Concentration and Relative Cathode Electrode Area Sizes in Titania Film Formation by Micro-Arc Oxidation

  • Lee, Yong-K.;Lee, Kang-Soo
    • Corrosion Science and Technology
    • /
    • v.9 no.4
    • /
    • pp.171-174
    • /
    • 2010
  • MAO (micro-arc oxidation) is an eco-friendly convenient and effective technology to deposit high-quality oxide coatings on the surfaces of Ti, Al, Mg and their alloys. The roles of the electrolyte concentration and relative cathode electrode area sizes in the grown oxide film during titanium MAO were investigated. The higher the concentration of the electrolyte, the lower the $R_{total}A$ value. The oxide film produced by the lower concentration of the electrolyte is thinner and less uniform than the film by the higher concentration, which is thick and porous. The cathode area size must be bigger than the anode area size in order to minimize the voltage drop across the cathode. The ratio of the cathode area size to the anode area size must be bigger than 8. Otherwise, the cathode will be another source for voltage drop, which is detrimental to and slows down the oxide growth.

Densification Behavior of Nanocrystalline Ceramic Powder under Cold Compaction (냉간 압축 하에서 나노 세라믹 분말의 치밀화 거동)

  • Lee Sung-Chul;Kim Ki-Tae
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.30 no.10 s.253
    • /
    • pp.1242-1248
    • /
    • 2006
  • Densification behavior of nanocrystalline titania powder was investigated under cold compaction. Experimental data were obtained under triaxial compression with various loading conditions. Lee and Kim proposed the Cap model by developing the parameters involved in the yield function of general Cap model and volumetric strain evolution under cold isostatic pressing. The parameters in the Drucker/Prager Cap model and the proposed model were obtained from experimental data under triaxial compression. Finite element results from the models were compared with experimental data for densification behavior of nanocystalline ceramic powder under cold isostatic pressing and die compaction. The proposed model agreed well with experimental data under cold compaction, but the Drucker/Prager Cap model underestimated at the low density range. Finite element results, also, show the relative density distribution of nanocystalline ceramic powder compacts is severe compared to conventional micron powder compacts with the same averaged relative density.

Development of MBR System Commercialization Technology Using a Membrane with a Good Fouling Resistance (막 오염 저항성이 우수한 분리막을 이용한 MBR 시스템의 실증화 기술개발)

  • Choi, J.H.;Lee, J.B.;Kim, I.C.
    • Membrane Journal
    • /
    • v.18 no.1
    • /
    • pp.35-43
    • /
    • 2008
  • In this study, we tried to solve membrane fouling with membranes made by fine nano-particle in MBR process. And we confirmed good fouling resistance in pilot test. In this test, we confirmed our membrane with titania out-standing quality by testing in the pilot long-term test by comparing to other company product. Our membrane keep up steadily $20{\sim}25 L/m^2{\cdot}hr$ high flux in $7,000{\sim}13,000mg/L$ MLSS high sludge concentration. In addition to this quality, we studied membrane flux character related membrane arrangement, membrane-air line arrangement, air-line hole size, cleaning solution concentration, treatment method, etc. Using the optimization of this additional parameter, we tried to search method of maximizing membrane quality.

Evaluation on the Photodegradation Rate of NOx Using High Efficiency Visible-Light Responsive Photocatalysts (고효율 가시광 반응형 광촉매를 이용한 NOx의 광저감율 평가)

  • Cha, Ji An;An, Sang Hun;Cho, Eun hee;Kim, Tae Oh
    • Particle and aerosol research
    • /
    • v.6 no.4
    • /
    • pp.165-172
    • /
    • 2010
  • Titania is widely used as an effective photocatalyst for the photodegradation of environmental pollutants in air. In this study, novel N-doped $ZrO_2/TiO_2$ photocatalysts were synthesized via sol-gel method and characterized by UV-Vis spectrophotometer, transmission electron microscope, and X-ray diffractometer. N-doped $ZrO_2/TiO_2$ photocatalysts were nano-sized with an average particle size of about 20 nm. The XRD pattern of N-doped $ZrO_2/TiO_2$ photocatalysts showed both anatase and rutile phases. The photocatalytic activity of N-doped $ZrO_2/TiO_2$ photocatalysts was evaluated by degradation of NO under UV and visible light irradiation at various parameters such as amount of photocatalyst, concentration of NO, and intensity of light. The photocatalytic activity of N-doped $ZrO_2/TiO_2$ photocatalysts was effective for the enhancement of the degradation of NO and higher than that of $TiO_2$ photocatlysts under UV and visible light irradiation.

Effect of Microwave Irradiation on Morphology and Size of Anatase Nano Powder: Efficient Photodegradation of 4-Nitrophenol by W-doped Titania

  • Shojaei, Abdollah Fallah;Loghmani, Mohammad Hassan
    • Bulletin of the Korean Chemical Society
    • /
    • v.33 no.12
    • /
    • pp.3981-3986
    • /
    • 2012
  • Anatase nanocrystalline and its tungsten-doped (0.4, 2, and 4 mol %) powders have been synthesized by microwave irradiation through hydrolysis of titanium tetra-isopropoxide (TIP) in aqueous solution. The materials are characterized by XRD, Raman, SEM-EDX, TEM, FT-IR and UV-vis techniques. The nanocrystalline $TiO_2$ particles are 30 nm in nature and doping of tungsten ion decreases their size. As seen in TEM images, the crystallites of W (4 mol %) doped $TiO_2$ are small with a size of about 10 nm. The photocatalytic activity was tested on the degradation of 4-nitrophenol (4-NP). Catalytic activities of W-doped and pure $TiO_2$ were also compared. The results show that the photocatalytic activity of the W-doped $TiO_2$ photocatalyst is much higher than that of pure $TiO_2$. Degradation decreases from 96 to 50%, during 115 min, when the initial 4-NP concentration increases from 10 to 120 ppm. Maximum degradation was obtained at 35 mg of photocatalyst.