• 제목/요약/키워드: mortars

검색결과 435건 처리시간 0.025초

PMMA 모르타르의 성질에 미치는 불포화 폴리에스테르 수지 첨가율의 영향 (Effect of Unsaturated Polyester Resin Content on Properties of PMMA Mortars)

  • 최낙운;이철웅;김완영;소양섭
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2004년도 춘계 학술발표회 제16권1호
    • /
    • pp.332-335
    • /
    • 2004
  • Polymethyl Methacrylate(PMMA) mortars using EPS solution-based binders are prepared with various unsaturated polyester resin(UP) contents of binder, and tested for working life. heat exothorm temperature, length change. compressive strength and temperature dependence of compressive strength. As a result, the working life of PMMA mortar is lengthened with raising UP content of binder. Length change of the mortar was condensed from expansion to shrinkage with increasing UP content, and non shrinkage of the mortar is obtained at about UP content of $2.5\%$. The compressive strength of the mortar is increased with an increase in the UP content and reach maximum at UP content of $5\%$. However thermal resistance improvement of the mortar by increasing UP content was not recognized. UP resin was recommended as an effective agent for shrinkage control and strength development of PMMA mortar.

  • PDF

재유화형 분말수지를 혼입한 폴리머 시멘트 모르타르의 건조수축 (Drying Shrinkage of Polymer-Modified Mortar Using redispersible Polymer Powder)

  • 주명기;이윤수;연규석;조규우
    • 한국농공학회:학술대회논문집
    • /
    • 한국농공학회 2002년도 학술발표회 발표논문집
    • /
    • pp.165-168
    • /
    • 2002
  • The effects of polymer-cement ratio, antifoamer agent content and shrinkage-reducing agent content on the drying shrinkage of polymer-modified mortars using redispersible polymer powder are examined. As a result, irrespective of the antifoamer content, the drying shrinkage of the polymer-modified mortars using redispersible polymer powder tend to decrease with increasing polymer-cement ratio and shrinkage-reducing agent content. Such a drying shrinkage development is due to the effect of reducing water from incorporation of EVA redispersible polymer powder and antifoamer agent.

  • PDF

Predicting the high temperature effect on mortar compressive strength by neural network

  • Yuzer, N.;Akbas, B.;Kizilkanat, A.B.
    • Computers and Concrete
    • /
    • 제8권5호
    • /
    • pp.491-510
    • /
    • 2011
  • Before deciding if structures exposed to high temperature are to be repaired or demolished, their final state should be carefully examined. Destructive and non-destructive testing methods are generally applied for this purpose. Compressive strength and color change in mortars are observed as a result of the effects of high temperature. In this study, ordinary and pozzolan-added mortar samples were produced using different aggregates, and exposed to 100, 200, 300, 600, 900 and $1200^{\circ}C$. The samples were divided into two groups and cooled to room temperature in water and air separately. Compression tests were carried out on these samples, and the color change was evaluated by the Munsell Color System. The relationships between the change in compressive strength and color of mortars were determined by using a multi-layered feed-forward Neural Network model trained with the back-propagation algorithm. The results showed that providing accurate estimates of compressive strength by using the color components and ultrasonic pulse velocity design parameters were possible using the approach adopted in this study.

적산온도법에 의한 에폭시 수지 모르터의 초기강도 예측에 관한 연구 (A Study on the Early Strength Prediction of Epoxy Resin Mortars by the Maturity Method)

  • 김철영;연규석;;이윤수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1999년도 봄 학술발표회 논문집(I)
    • /
    • pp.325-330
    • /
    • 1999
  • The objectives of this study were to compare the development of compressive strength of epoxy resin mortars used as repairing materials with respect to maturity, and to propose a predictive model for strength development of epoxy resin mortar. A series of tests were carried out for the hardener contents of 30, 40 and 50 percentage of resin and compressive strength were measured at the of 6, 12, 24, 72, 120 and 168 hours respectively under temperature of 0, 10, 20 and 3$0^{\circ}C$. The datum temperature was estimated by measured strength, and the maturity is calculated with the estimated datum temperature. The compressive strength of epoxy resin mortar could be predicted by regression analysis from the maturity-compressive strength relationship.

  • PDF

Effects of Sand/Binder Ratios on the Mechanical Properties of Mortars Containing Fly ash and Silica fume

  • Park, Ki-Bong;Lee, Han-Seung
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 추계 학술발표회 제17권2호
    • /
    • pp.777-780
    • /
    • 2005
  • The paper presents details of an investigation into the effect of sand content upon the strength and shrinkage of mortar. This strategy was to produces more durable strength mortar with less cement. Cement mortars containing $20\;wt.\;\%$ Class F fly ash, and/or $6\;wt.\;\%$ silica fume were prepared at a water/binder ratio of 0.45 and sand/binder ratios of 2.0, 2.5, 2.7, and 3.0. The increase in sand/binder ratio caused a decrease in the mortar flow. However, the sand/binder ratio did not affect the strength development. Drying shrinkage decreased with increasing the sand contents.

  • PDF

저온양생한 폴리우레탄 모르타르의 강도특성에 관한 연구 (A Study on the Strengths of Polyurethane Morthar Cured under Low Temperature Condition)

  • 오종석;정효석;박홍신;조영국;소양섭
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1999년도 봄 학술발표회 논문집(I)
    • /
    • pp.337-342
    • /
    • 1999
  • The Purpose of this study is to evaluate the strength characteristics of polyurethane(PUR) mortar cured under low temperature condition. PUR mortars are prepared with various catalyst content, methylene chloride(MC) content as a viscosity reducing agent, and curing age at low temperature condition of $0^{\circ}C$, -5$^{\circ}C$ and -1$0^{\circ}C$, tested for working life, compressive and flexural strengths. From the test results, the catalyst and MC contents affect the degree of hardening and blowing of PUR mortar. Strengths increase with an increasing catalyst content at low temperature. Flexural and compressive strength of PUR mortar are about 177kgf/$\textrm{cm}^2$ and 490kgf/$\textrm{cm}^2$ respectively at curing temperature of -1$0^{\circ}C$ with catalyst content of 0.4%. Therefore, it is apparent that this PUR mortars have a sufficient strengths for repair of concrete structures.

  • PDF

중질탄산칼슘을 혼입한 시멘트 모르타르의 황산염침식 저항성 평가 (Sulfate Attack Resistance of Cement Mortar containing Ground Calcium Carbonate)

  • 정호섭;김종필;이승태;김성수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 춘계 학술발표회 논문집(II)
    • /
    • pp.217-220
    • /
    • 2006
  • This paper describes a study undertaken to determine the effect of ground calcium carbonate(GCC) cement mortar with respect to sulfate attack. It were investigated visual appearance and expansion of cement mortars with GCC immersed in artificial solution of 5% sodium sulfate during 510days. According to increasing replacement of GCC, the expansion ratio was comparatively superior to GCC0 mortar specimen. The test results indicated that cement mortars with GCC was benefit the resistance of sulfate attack due to micro filler effect.

  • PDF

급결제를 첨가한 고로슬래그 모르타르의 성능평가 (Evaluation of Performance on the Slag Mortars with Accelerator)

  • 박광필;김성수;김동규;정호섭;이승태;이정배
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2009년도 춘계 학술대회 제21권1호
    • /
    • pp.515-516
    • /
    • 2009
  • 산업의 발전과 국토의 효율적인 활용을 위하여 많은 도로 및 철도 터널이 축조되어 사용되어 왔다. 하지만 이러한 터널 구조물의 지하수와 토양의 오염 물질 등으로 인한 손상에 의하여 많은 열화가 진행되고 있는 실정이다. 이러한 노후터널의 보수 보강에 있어 유해이온에 대한 저항성을 높이고 보수 보강 시간의 단축을 위하여 광물질 혼화재료인 고로슬래그 미분말과 급결제를 사용한 모르타르의 최적 배합을 찾는데 목적을 두었다.

  • PDF

팽창재 및 팽윤재를 병용한 에폭시수지 혼입 시멘트 모르타르의 강도특성 (Strength Properties of Epoxy-Modified Mortars with Expansive and Swelling Agents)

  • 함성민;김주영;김완기
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2014년도 춘계 학술논문 발표대회
    • /
    • pp.288-289
    • /
    • 2014
  • The purpose of this research is to examine strength properties of epoxy-modified mortar with expansive and swelling agent contents. The polymer-modified mortars (PMMs) using epoxy resin are prepared with various polymer-binder ratios, expansive and swelling agent contents. The PMMs using epoxy resin are tested for compressive, flexural and tensile strengths. As a result, the strength properties of the PMMs using epoxy resin are depending on the polymer-binder ratio rather than expansive and swelling agent content, and are remarkably improved over unmodified mortar (UMM).

  • PDF

목초액 담지체를 골재로 사용한 폴리머 시멘트계 내장마감재의 성능평가 (Performance Evaluation of Polymer Cementitious Interior Finish Using Light-Weight Aggregates Containing Pyroligneous Liquid)

  • 이채영;김주영;김완기
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2014년도 춘계 학술논문 발표대회
    • /
    • pp.218-219
    • /
    • 2014
  • The purpose of this study is to develop eco-friendly internal material of acrylic emulsion mortars using light-weight aggregate carrier which contains pyroligneous liquid. Four types of light-weight aggregates (vermiculite, perlite, charcoal, zeolite) that are widely used in building materials are selected and the properties such as adhesion, water absorption coefficient, antibiosis, crack and impact resistance are evaluated in accordance with KS F 4715. As a result, the properties of acrylic emulsion mortars using light-weight aggregate carrier are satisfied with KS requirements. The antibiosis is improved with increasing zeolite light-weight carrier content.

  • PDF