• Title/Summary/Keyword: micro fracture

Search Result 438, Processing Time 0.024 seconds

Effects of diamond abrasive and lubricants on mechanical properties and wearing resistance of microblades (첨가된 다이아몬드 abrasive와 윤활제의 함량이 마이크로블레이드의 내구성과 기계적 특성에 미치는 영향)

  • Kim, Song-Hui;Mun, Jong-Cheol;Kim, Sang-U
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2007.11a
    • /
    • pp.134-135
    • /
    • 2007
  • Graphite and MoS2 were added respectively as a lubricant to improve the cutting efficiency of micro blades which contains diamond abrasive. Strength, fracture toughness, and life span of micro-blades were observed to decrease with the increase in diamond abrasive and lubricant content. Wearing mode of micro-blades and the cutting efficiency were also found to be affected by the content of diamond abrasive and the addition of lubricants.

  • PDF

Study on Fracture Toughness and Heat Input in Weld HAZ of Cr-Mo Steel (I) (welding structure) (Cr-Mo강 용접열영향부의 파괴인성과 용접입열량에 관한 연구(I) (HAZ 고유조직을 중심으로))

  • 임재규;정세희
    • Journal of Welding and Joining
    • /
    • v.2 no.2
    • /
    • pp.54-61
    • /
    • 1984
  • Construction of welding structure is greatly dependent upon welding heat cycle. Fracture toughness is decreased remarkablely due to coarse grained HAZ and inequal residual stress of three dimensions to originate in welding. Post weld heat treatment(PWHT) is carried out to increase the fracture toughness of HAZ and to remove the residual stress. There occur some problem such as toughness decrement and stress relief cracking(SRC) in the coarse grained HAZ subject to the effect of tempering treatment. Therefore, in this paper, the effect of heat inputs affecting cooling rate and PWHT under the no stress on fracture toughness were evaluated by crack opening displacement (COD), SEM and micro-hardness test. Experimental results are as follows; 1. Fracture toughness of weld HAZ is dependent upon weld heat cycle and it is decreased with increment of heat input, but the degree of improvement of fracture toughness after PWHT was linearly increased with heat input. 2. Hardness of the parent metal is not changed, but the softening of coarse grained HAZ is remarkable due to PWHT. 3. Fracture surface of as-weld show the perfect brittle fracture with the cleavage fracture, but after PWHT they appear the ductile fracture surface with dimple.

  • PDF

The Effect of Sintongchukea-tang (Shentongzhuyu-tang) on Bone Fusion in Rib Fractured Rats (신통축어탕(身痛逐瘀湯)이 늑골골절 유발 Rat의 골유합에 미치는 영향)

  • Nam, Dae-Jin;Oh, Min-Seok
    • Journal of Korean Medicine Rehabilitation
    • /
    • v.30 no.3
    • /
    • pp.1-21
    • /
    • 2020
  • Objectives This study was designed to evaluate the bone regeneration effects of Sintongchukea-tang (SC) on rib fractured rats. Methods Rats were randomly divided into 5 groups (normal, control, positive control, SC low [SC-L] and SC high [SC-H]). All groups were subject to fractured rib except normal group. Normal group received no treatment at all. Control group was orally fed with phosphate buffered saline, and positive control group was medicated with tramadol (20 mg/kg). SC group was orally medicated with SC (50 mg/kg, 100 mg/kg) once a day for 14 days. The fracture healing process was observed by x-ray, micro CT and fracture tissue slide was observed by immunohistochemical staining. We analysed levels of transforming growth factor-β1, Ki67, alkaline phosphatase (ALP), runt-related transcription factor 2 (Runx2), receptor activator of nuclear factor kappa-β, tartrate resistant acid phosphatase (TRAP) and analysed levels of Osteocalcin in plasma. We measured levels of aspartate aminotransferase (AST), alanine aminotransferase (ALT), ALP, blood urea nitrogen (BUN) and creatinine in plasma, for hepatotoxicity and nephrotoxicity of SC. Results Though X-ray and micro-computed tomography, more callus formation was observed and bone union was progressing. Through Hematoxylin and Eosin, callus formation was increased compared to the control group. Runx2 level at SC-H was significantly increased and TRAP level at SC-L was significantly decreased compared with the control group. AST, ALT, ALP, BUN and creatinine were not statistically different from the control group. Conclusions As described above, SC promoted fracture healing by stimulating the bone regeneration factor. And SC shows no hepatotoxicity and nephrotoxicity. In conclusion, it seems that SC helps to promote fracture regeneration and it can be used clinically to patients with fracture.

Optimum Shape Design of Cemented Carbide Micro-Drill in Consideration of Productivity

  • Kim, Gun-Hoi;Kwon, Ji-Yong;Lee, Sung-Goo
    • 제어로봇시스템학회:학술대회논문집
    • /
    • 2003.10a
    • /
    • pp.264-268
    • /
    • 2003
  • Recently reduction of industrial products in size and weight has been increased by application of micro-drills in gadgets of high precision and a great interest of a micro-drilling has been raised. Due to the lack of tool stiffness and the chip packing, the micro-drilling requires not only the robust tool structure which has not affected by vibration but also effective drilling methods designed to prevent tool fracture from cutting troubles. This paper presents an optimum design shape of a 0.15 mm micro-drill associated with a new manufacturing process to improve the production rate and to lengthen the tool life and suggestions on the micro-drilling characteristic properties associated with the tool life and workpiece quality.

  • PDF

Optimum Manufacturing Processes of Micro-drill (마이크로 드릴의 최적 생산설계)

  • Kim, Gunhoi
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.1 no.1
    • /
    • pp.109-116
    • /
    • 2002
  • Resently, reduction of industrial products in size and weight has increased by the application of micro-drill for gadgets of high precision and gave rise to a great interest in a micro-drilling. Due to the lack of tool stiffness and the chip packing, micro-drilling requires not only the robust tool structure which has not affected by the vibration, but also the effective drilling methods designed to prevent tool fracture from cutting troubles. Firstly, this paper presents a new manufacturing process of micro-drill for improving the product rate and an optimum shape of micro-drill for lengthening the tool life, and secondly suggests between tool life and drilling torque acquired in the inprocess monitoring system.

  • PDF

Optimum Shape Design of Cemented Carbide Micro-drill in Consideration of Productivity (생산성을 중시한 초경합금 소재 마이크로 드릴의 최적 형상설계)

  • 김건회
    • Transactions of the Korean Society of Machine Tool Engineers
    • /
    • v.13 no.3
    • /
    • pp.133-140
    • /
    • 2004
  • Recently reduction of industrial products in size and weight has been increased by application of micro-drills in gadgets of high precision and a great interest of a micro-drilling has been raised. Due to the lack of tool stiffness and the chip packing, the micro-drilling requires not only the robust tool structure which has not affected by vibration but also effective drilling methods designed to prevent tool fracture from cutting troubles. This paper presents an optimum design shape of a 0.15 mm micro-drill associated with a new manufacturing process to improve the production rate and to lengthen the tool life and suggestions on the micro-drilling characteristic properties associated with the tool life and workpiece quality.