The ceramic forming materials are getting more important recently since they are used widely in repairing metal structures, welded metal structures and mechanical components etc. The determination of elastic constants for ceramic coating materials takes much time and efforts in experiment due to the brittleness of ceramic material itself. The aim of this research is to determine the Young's Modulus for ceramic metal coating material. In order to achieve the goal, the hybrid method which uses impulse hammer technique for experimental method and modal analysis of finite element method for computational method was used. The results show good agreement with existing experimental data on Young's Modulus.
The success of a porcelain fused to metal (PFM) restoration depends upon the quality of the porcelain-metal bond. The adhesion between metal substructure and dental porcelain is related to the diffusion of oxygen to the reaction layer formed on cast-metal surface during firing. The purposed of this investigation was to study the effects of gold based bonding agent on Ni-Cr alloy-ceramic adhesion between porcelain matrix, gold based bonding agent and metal substructure interface. gold based bonding agent have been applied as an intermediate layer between a metal substructure and a ceramic coating. gold based bonding agent(Aurofilm NP, Metalor, Swiss) was applied on Ni-Cr alloy surface by four method. Surfaces only air abraded with 110${\beta}\neq$ Al2O3 particles were used as control. metal ceramic adhesion was evaluated by a biaxial flexure test(N=5) and volume fraction of adherent porcelain was determined by SEM/EDS analysis. Result of this study suggest that the layering sequence of gold based bonding agent is very important and can improve porcelain adherence to PFM.
Purpose: The purpose of this study was to compare the shear bond strength of the metal-heat pressed glass ceramic bilayer structure. Methods: Metal framework specimens were prepared and surface is spreaded opaque(IPS InLine system opaque, IvoclarVivadent, Liechtenstein). There were 10 specimens for each bilayer dental ceramic group. The first group was porcelain fused metal, Press on metal IPS Inline press group, and press on metal HASS prototype group. Specimens measured for the shear bond strength on Schwickerath test by Instron universal testing machine(Instron3345, Instron Corp., USA). Mean average bond strength values of each specimen group were analyzed using a one-way ANOVA analysis of variance Saphiro-wilk's test. Statistical analysis were performed using IBM SPSS 23.0(IBM Co., Armonk, USA) Results: $RMS{\pm}SD$ The highest mean average HASS POM showed a bond strength value ($47.55{\pm}12.80Mpa$). The lowest mean average values Porcelain fused metal ($33.30{\pm}2.00Mpa$). Independent t-test was conduct to analysis the significant difference (p<0.05) (Table 3). Conclusion: Three kinds of Metal/ glass bilayer dental ceramics bond strength were clinical acceptability. Especially, as lithium disilicate containing represents higher bond strength.
Transactions of the Korean Society of Mechanical Engineers A
/
v.24
no.1
s.173
/
pp.29-37
/
2000
The effect of a ceramic ball inclusion on densification behavior of a metal powder compact was investigated under cold isostatic pressing, pressureless sintering and hot isostatic pressing. To simulate those processes, proper constitutive models were implemented into a finite element program (ABAQUS). Measured density distributions of metal powder compacts were also compared with finite element results and showed the same trend with simulated results. Residual stress distributions were calculated by finite element analysis to study the effect of ceramic ball inclusions with different thermal expansion coefficients. The higher residual stress was observed in a metal powder compact when the difference between thermal expansion coefficients for a ceramic ball and metal powder became larger. Samples produced by Wing showed more uniform density distributions and lower residual stresses compared to those by sintering after cold isostatic pressing. For various sizes of ceramic ball inclusions, densification and deformation of powder compacts were also studied during hot isostatic pressing.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2009.06a
/
pp.388-389
/
2009
The use of arc tubes made of ceramic material further enhanced some of the metal halide lamp's properties. These properties translate into higher efficacy with better color rendering, stable color through lamp long life. Recently, due to an increase in the application of the ceramic metal-halide lamp, the study for the property etc. according to Ballast's driving scheme and the study for arc tube material, optimization of gas and so on are being proceeded to improve the property of the lamp. Especially, to control ceramic metal-halide lamp, the vigorous study and practical use with respect to Electronic Ballast, which has been improved in the disadvantages of the conventional Magnetic Ballast are made. In this paper, Electrical characteristics and gas insulation destroy time are analyzed by comparing magnetic ballast with electronic ballast.
Jun Byung-Hun;Kim Jin-Sung;Kang Hyo-Jin;Oh Sang-Keun
Proceedings of the Korean Institute of Building Construction Conference
/
2005.05a
/
pp.113-117
/
2005
The ceramic metal resin paints for waterproof and anti corrosion is not long history in development of materials even many actual result. So far, no standard have been given to construction and maintenance method, Quality and property, it is real state that cannot afford to proper quality control in job site or production. This study has been test for the ceramic metal resin paints for water and anti corrosion, as the result, it have proper performance of job site and mechanical performance of compare to other existing. In particular, tensile strength indicates more high about $14.1N/mm^2$ than epoxy resin paints, and in elongation per unit length is more high It is shows having better adhesive strength than epoxy resin paint for crack on the concrete structure. Moreover, The ceramic metal paint for water and corrosion proofing have to have main performance is watertightness and resistance for external impact, chloride ion permeation, drinkable water elution.
Objectives : The purpose of this in vitro study was to evaluate the effect of firing cycles on the marginal and internal fit of metal ceramic crown. Methods : Ten same cases of stone models (abutment teeth 11) were manufactured. Ten cobalt-chrome cores were made per each models and the marginal and internal fit was evaluated through a silicone replica technique. The marginal and internal fit of specimens was measured twice. The first measurement was done after manufacturing cobalt-chrome alloy core and the second measurement was done after porcelain firing. T-test of paired sample for statistical analysis was executed with SPSS 12.0K for Windows (${\alpha}$=0.05). Results : Mean(SD) marginal and internal fit were 77.1(23.3) ${\mu}m$ for the cobalt-chrome alloy core group and 84.4(21.9) ${\mu}m$ for the metal-ceramic crown group. They were statistically significant differences between groups for marginal and internal fit (p<.05). Conclusions : All metal ceramic crowns showed marginal and internal fit ranged within the current clinical recommendations.
Purpose: This study aimed to evaluate the effects of a special heat treatment on Pd-Au-Ag metal-ceramic alloy after degassing treatment and on changes in the hardness of the alloy during the firing process. Methods: Specimen alloys were cast and subjected to degassing at 900℃ for 10 minutes. These specimens were then subjected to a special heat treatment at 600℃ for 15 minutes in a dental porcelain furnace. Further, the specimens were subjected to simulated firing in the porcelain furnace. The resulting specimens were then tested for hardness, and changes in the microstructure were observed. Results: There was a decrease in the hardness of the alloy during the simulated firing of the cast alloy due to the coarsening of the particles. Meanwhile, additional heat treatment after degassing was found to play a crucial role in preventing a decrease in hardness. This treatment effectively suppressed the coarsening of the precipitates during repeated firing at high temperatures. Conclusion: Specific heat treatment of the Pd-Au-Ag metal-ceramic alloy prevented a decrease in its hardness and extended the lifespan of the metal-ceramic prosthesis.
The purpose of this study was to evaluate the effects of different bases of ceramic brackets on shear bond strength and to observe failure patterns of bracket bondings. Lower bicuspid brackets whose bases designed for the macromechanical and silane treated chemical bonding those for silane treated chemical bonding, those for micromechanical bonding, and those for macromechanical bonding were tested as experimental groups, and foil mesh-backed metal brackets as a control group. All the brackets were bonded with $Mono-Lok\;2^{(TM)}$ on the labial surface of extracted human lower bicuspids after etching the enamel with $38\%$ phosphoric acid solution for 60 seconds. The shear bond strengths were measured on the universal test machine after 24 hours passed in the $37^{\circ}C$ water bath. The gathered data were evaluated and tested by ANOVA and Duncan's multiple range test, and those results were as follows. The shear bond strengths of brackets for macromechanical and chemical bonding, those for chemical bonding, and those for micromechanical bonding were not different (p>0.05), but showed statistically higher than those of metal bracket and those of ceramic bracket for micromechanical bonding(p<0.05). The shear bond strengths of ceramic bracket for micromechanical bonding showed statistically lower than those of metal bracket(p<0.05). The enamel fractures and/or ceramic bracket fractures were observed in the cases of higher bond strength than that of metal bracket. These results supported that silane treated base of ceramic bracket show higher shear bond strength than that of metal bracket, and suggested that micromechanical form of ceramic bracket bases show higher shear bond strength than that of macromechanical form.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.