• 제목/요약/키워드: melting process

검색결과 1,006건 처리시간 0.029초

Melting and draining tests on glass waste form for the immobilization of Cs, Sr, and rare-earth nuclides using a cold-crucible induction melting system

  • Choi, Jung-Hoon;Lee, Byeonggwan;Lee, Ki-Rak;Kang, Hyun Woo;Eom, Hyeon Jin;Park, Hwan-Seo
    • Nuclear Engineering and Technology
    • /
    • 제54권4호
    • /
    • pp.1206-1212
    • /
    • 2022
  • Cold-crucible induction melting (CCIM) technology has been intensively studied as an advanced vitrification process for the immobilization of highly radioactive waste. This technology uses high-frequency induction to melt a glass matrix and waste, while the outer surface of the crucible is water-cooled, resulting in the formation of a frozen glass layer (skull). In this study, for the fabrication of borosilicate glass waste form, CCIM operation test with 60 kg of glass per batch was conducted using surrogate wastes composed of Cs, Sr, and Nd as a representative of highly radioactive nuclides generated during spent nuclear fuel management. A 60 kg-scale glass waste form was successfully fabricated through melting and draining processes using a CCIM system, and its physicochemical properties were analyzed. In particular, to enhance the controllability and reliability of the draining process, an air-cooling drain control method that can control draining through air-cooling near drain holes was developed, and its validity for draining control was verified. The method can offer controllability on various draining processes, such as molten salt or molten metal draining processes, and can be applied to a process requiring high throughput draining.

Transient heat transfer and crust evolution during debris bed melting process in the hypothetical severe accident of HPR1000

  • Chao Lv;Gen Li;Jinchen Gao;Jinshi Wang;Junjie Yan
    • Nuclear Engineering and Technology
    • /
    • 제55권8호
    • /
    • pp.3017-3029
    • /
    • 2023
  • In the late in-vessel phase of a nuclear reactor severe accident, the internal heat transfer and crust evolution during the debris bed melting process have important effects on the thermal load distribution along the vessel wall, and further affect the reactor pressure vessel (RPV) failure mode and the state of melt during leakage. This study coupled the phase change model and large eddy simulation to investigate the variations of the temperature, melt liquid fraction, crust and heat flux distributions during the debris bed melting process in the hypothetical severe accident of HPR1000. The results indicated that the heat flow towards the vessel wall and upper surface were similar at the beginning stage of debris melting, but the upward heat flow increased significantly as the development of the molten pool. The maximum heat flux towards the vessel wall reached 0.4 MW/m2. The thickness of lower crust decreased as the debris melting. It was much thicker at the bottom region with the azimuthal angle below 20° and decreased rapidly at the azimuthal angle around 20-50°. The maximum and minimum thicknesses were 2 and 90 mm, respectively. By contrast, the distribution of upper crust was uniform and reached stable state much earlier than the lower crust, with the thickness of about 10 mm. Moreover, the sensitivity analysis of initial condition indicated that as the decrease of time interval from reactor scram to debris bed dried-out, the maximum debris temperature and melt fraction became larger, the lower crust thickness became thinner, but the upper crust had no significant change. The sensitivity analysis of in-vessel retention (IVR) strategies indicated that the passive and active external reactor vessel cooling (ERVC) had little effect on the internal heat transfer and crust evolution. In the case not considering the internal reactor vessel cooling (IRVC), the upper crust was not obvious.

Fabrication of BSCCO Tube by Melting Centrifugal Process

  • Kim, Ki-Ik;Oh, Sung-Young;Seo, Chang-Eui;Jun, Byung-Hyuk;Kim, Hyoung-Seop;Hyun, Ok-Bae;Kim, Chan-Joong
    • 한국초전도학회:학술대회논문집
    • /
    • 한국초전도학회 2004년도 High Temperature Superconductivity Vol.XIV
    • /
    • pp.96-96
    • /
    • 2004
  • PDF

알루미늄 용탕 보온용기의 단열재 적층구조 변경을 통한 보온성 향상 (Thermal Insulation Improvement by Laminated Adiabatic Structure Change in Holding Furnace with Molten Aluminum Alloy)

  • 황준선;강충길
    • 한국주조공학회지
    • /
    • 제31권6호
    • /
    • pp.336-341
    • /
    • 2011
  • Recently, aluminium usage in the automobile industry has been increased cause of its lightweight. The aluminium has a melting-solidification process in producing line and another melting process was needed in manufacturing process. Two times of melting process for making ingot and casting not only makes the loss of time and money but contaminates the air with Sox, Nox. For this reason, the holding furnace with laminated adiabatic material was developed. This holding furnace can deliver the molten aluminium directly to the industry needing molten aluminium. Recent holding furnace has above $15^{\circ}C/h$ of cooling rate and that causes solidification of molten aluminium. The ANSYS software was used to analysis the heat transfer. The adiabatic materials were laminated with optimized arrangement and holding furnace shape was changed with optimized modelling by ANSYS analysis for reducing the cooling rate of molten aluminium in holding furnace.

초기적으로 과냉각된 수직실린더 내부 물질의 상변화 과정 (Phase change process of the initially subcooled material in a vertical cylinder)

  • 백영렬;이재헌
    • 대한기계학회논문집B
    • /
    • 제21권1호
    • /
    • pp.24-35
    • /
    • 1997
  • Melting process inside in a vertical cylinder has been investigated numerically to observe heat transfer characteristics in the latent heat storage vessel applied to the thermal storage system. The time-dependent boundary fitted coordinate system was introduced to overcome the difficulty caused by the moving boundary. The present results are in good agreement with the available previous data when the initial subcooling effect of the solid phase is not considered. It is found that the melting is promoted by the natural convection, but is delayed by the initial subcooling effect of the solid phase.

열처리 조건에 따른 Bi-2212 초전도 튜브의 특성 (Characteristics of Bi-2212 Superconductor Tube Depending on Heat-treatment Conditions)

  • 박용민;장건익
    • 한국전기전자재료학회논문지
    • /
    • 제14권7호
    • /
    • pp.606-610
    • /
    • 2001
  • Bi-2212 HTS tube was fabricated by centrifugal forming and partial melting processes. Bi-2212 bulk tube has been optimized to achieve smooth surface and uniform thickness. The slurry was prepared in the mixing ratio of 10:1 between Bi-2212 powder and binder and initially charged into the rotating mold under the speed of 300~450 rpm. Heat-treatment was performed at the temperature ranges of 860~89$0^{\circ}C$ in air for partial melting. the HTS tube fabricated by centrifugal forming process at 89$0^{\circ}C$ under the rotating speed of 450 rpm was highly densified and the plate-like grains with more than 20${\mu}{\textrm}{m}$ were well oriented along the rotating axis. The measured Tc and J$_{c}$ at 10K on specimen heat treated at 89$0^{\circ}C$ was around 85 K and 1,200 A/$\textrm{cm}^2$ respectively.y.

  • PDF

전기로 High Current Cable 고장진단 알고리즘 개발 (Developing a fault diagnosis algorithm on a high current cable of arc furnace)

  • 최성진;장유진;김상우
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2005년도 학술대회 논문집 정보 및 제어부문
    • /
    • pp.573-575
    • /
    • 2005
  • In the steel industry, a steel melting electric arc furnace is used to produce both carbon and alloy steels. Steel scrap which is charged into the furnace is heated by means of electric arc between graphite electrodes and the scrap. In this melting process, current is supplied to the furnace through HCC(high current cable) which connect the furnace and transformer. Four HCCs are assigned to each phase in our system to divide the current. Since a sudden cable breaking result in the shutdown of melting process, an aging detection of HCC is very important for both an improvement of productivity and cost reduction. In this paper, the aging of the HCC is estimated by using the current ratio between four HCCs.

  • PDF

수송기기 유압 실린더 블록 재료의 Fe-Cu 계면반응 특성 (A Characteristic of Fe-Cu Interfacial Reaction in the Hydraulic Cylinder Block for Vehicle Parts)

  • 김해지;김남경
    • 한국기계가공학회지
    • /
    • 제3권1호
    • /
    • pp.90-94
    • /
    • 2004
  • Generally, a hydraulic cylinder block which is one of a vehicle parts that plays Important role in excavator power transmission, has copper alloy separation phenomenon by sliding motion between metals in high pressure condition. In this paper, to solve this problem, the interfacial reaction layer of Fe-Cu With SCM440 and copper alloy is studied through the melting method. As the result of this study, it is found that the interfacial reaction layer of $1{\mu}m$ created in the interface of Fe-Cu which has very strong physical bonding. It has been also confirmed that the melting method can improve life of the hydraulic cylinder block.

  • PDF

초음파 가진에 따른 열전달 향상에 관한 연구 (An Experimental Study of enhancing heat transfer by Ultrasonic Vibration)

  • 윤정환;오율권;차경옥
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2001년도 추계학술대회논문집B
    • /
    • pp.235-240
    • /
    • 2001
  • This study presents experimental work on phase change heat transfer, in order to increase heat transfer rate, ultrasonic vibrations were introduced. Solid-liquid phase change occurs in a number of situations of practical interest. This study reveal that ultrasonic vibrations accompany the effects like agitation, acoustic streaming, cavitation, and oscillating fluid motion. Such effects are a prime mechanism in the overall melting process when ultrasonic vibrations are applied. Some common examples include the melting of edible oil, metallurgical process such as casting and welding, and materials science applications such as crystal growth. Therefore, this study presented the effective way to enhance phase change heat transfer.

  • PDF