세라미스 파괴인성평가에 있어서 IF법과 AE (Acoustic Emission and Indentation Fracture Method for the Engineering Ceramics)

  • 김부안;문창권
    • 한국해양공학회지
    • /
    • 제15권2호
    • /
    • pp.61-65
    • /
    • 2001
  • The fracture toughness of ceramics can be measure by such various methods as DT (double torsion), CN (chevron notch) etc. But, the application of these methods to the engineering ceramics is very difficult because of its very high hardness. So, IF (indentation fracture) method is generally used for the evaluation of fracture toughness of ceramics. The Median crack induced by the sharp Vickers indenter was compared with the detected AE (acoustic emission) signal. On the silicon nitride ceramics, the AE test results agree fairly well with the median crack occurance and growth process. But, on the alumina, very many complicated crack signals were detected besides median crack. It can be considered that the IF methods must be used in limited engineering ceramics materials.

  • PDF

절단 유리판의 표면결함에 관한 실험적 연구 (Experimental Study on the Surface Defects of Scribed Glass Sheets)

  • 김청균
    • Tribology and Lubricants
    • /
    • 제24권6호
    • /
    • pp.332-337
    • /
    • 2008
  • This paper presents the surface defect analysis based on the experimental investigation of scribed glasses. The scribing process by a diamond wheel cutter is widely used as a reliable and inexpensive method for sizing of glass sheets. The wheel cutter generates a small median crack on the glass surface, which is then propagated through the glass thickness for complete separation. The surface contour patterns in which are formed during a scribing process are strongly related to wheel cutter parameters such as wheel tip surface finish, tip angle and wheel diameter, and cutting process parameters such as scribing pressure, speed and tooling technique. The scribed surface of a glass sheet provides normal Wallner lines, which represent regular median cracks and crack propagation in glass thickness, and abnormal surface roughness patterns. In this experimental study, normal and abnormal surface topographic patterns are classified based on the surface defect profiles of scribed glass sheets. A normal surface of a scribed glass sheet shows regular Wallner lines with deep median cracks. But some specimens of scribed glass sheets show that abnormal surface profiles of glass sheets in two pieces are represented by a chipping, irregular surface cracks in depth, edge cracks, and combined crack defects. These surface crack patterns are strongly related to easy breakage of the scribed glass imposed by external forces. Thus the scribed glass with abnormal crack patterns should be removed during a quality control process based on the surface defect classification method as demonstrated in this study.

Automated assessment of cracks on concrete surfaces using adaptive digital image processing

  • Liu, Yufei;Cho, Soojin;Spencer, Billie F. Jr;Fan, Jiansheng
    • Smart Structures and Systems
    • /
    • 제14권4호
    • /
    • pp.719-741
    • /
    • 2014
  • Monitoring surface cracks is important to ensure the health of concrete structures. However, traditional visual inspection to monitor the concrete cracks has disadvantages such as subjective inspection nature, associated time and cost, and possible danger to inspectors. To alter the visual inspection, a complete procedure for automated crack assessment based on adaptive digital image processing has been proposed in this study. Crack objects are extracted from the images using the subtraction with median filter and the local binarization using the Niblack's method. To adaptively. determine the optimal window sizes for the median filter and the Niblack's method without distortion of crack object an optimal filter size index (OFSI) is proposed. From the extracted crack objects using the optimal size of window, the crack objects are decomposed to the crack skeletons and edges, and the crack width is calculated using 4-connected normal line according to the orientation of the local skeleton line. For an image, a crack width nephogram is obtained to have an intuitive view of the crack distribution. The proposed procedure is verified from a test on a concrete reaction wall with various types of cracks. From the crack images with different crack widths and patterns, the widths of cracks in the order of submillimeters are calculated with high accuracy.

음향방출을 이용한 유리의 비커스 압입 균열 특성 (Characteristics of Cracks under Vickers Indentation in Glass Using Acoustic Emission)

  • 박혜연;이종규;박흥일;이병우
    • 동력기계공학회지
    • /
    • 제16권1호
    • /
    • pp.72-77
    • /
    • 2012
  • Acoustic emission (AE) is known to be sensitive to fracture process and so it was expected that AE data may propose as a means of monitoring the fracture information. The aim of this study is to analyze the characteristic of AE signal emitted from glass during Vickers indentation. To observe AE characteristics by surface effect, both glass and coating glass were studied. During Vickers indentation loading, AE signal resulted from penny-like crack is detected. During Vickers indentation unloading, AE signal resulted from both radial/median crack and lateral crack is detected. In case of indentation on glass, the emission energy(${\epsilon}$) is found to be approximately proportional to the fourth power of the crack length. In case of indentation on coating glass, the emission energy(${\epsilon}$) is approximately proportional to the crack length.

콘크리트 교량 방호벽의 균열원인 및 패턴 분석에 대한 연구 (Study on Cracking Causes and Patterns in Median Barrier and Guardrail Concrete in RC Bridge)

  • 최세진;최정욱;권성준
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제18권5호
    • /
    • pp.19-26
    • /
    • 2014
  • 콘크리트 방호벽 및 중앙분리대는 교량의 부속시설이지만, 슬립폼 시공과 넓은 비표면적으로 인해 초기재령 균열이 발생하기 쉽다. 본 연구에서는 대형 교량의 방호벽과 중앙분리대 콘크리트의 외관조사 및 비파괴실험을 수행하여 균열의 원인과 발생 균열의 패턴을 분석하였다. 이를 위해 시공기간을 고려하여, 건조수축, 수화열 해석이 수행되었으며, 현장의 환경조건을 고려하여 소성수축 특성을 평가하였다. 평가결과 대상구조물의 균열 원인은 철근위치에 따른 소성침하균열, 소성수축 및 건조수축에 의한 복부균열, 재료분리에 따른 상부균열로 추정할 수 있었다. 또한 균열원인과 발생 패턴을 도식화하였으며, 시공 및 재료분야에서 균열제어대책을 제안하였다. 해상위 교량에 설치하는 중앙분리대 및 방호벽 콘크리트는 환경조건 (풍속, 온도, 습도)에 매우 민감하여 초기재령균열이 쉽게 발생하므로 재료선택 및 시공방법에 신중을 기해야 한다.

미끄럼 미소압입에 의한 소다석회 유리의 변형 및 파괴 거동 (Deformation and Fracture Behavioos of Soda-lime Glass by Sliding Microindentation)

  • 안유민;최상현;박상신
    • Tribology and Lubricants
    • /
    • 제13권4호
    • /
    • pp.18-25
    • /
    • 1997
  • The various deformation and fracture behaviors under light loads in soda-lime glass under sliding Vickers indentation have been studied. In soda-lime glass, deformation and fracture behaviors can be classified into four different patterns by applied load. At very light load (<0.1N), plastic deformation only occurred. At low loads (0.1~0.8N), median crack, appear. At intermediate loads (0.8~3.0N), median and lateral cracking occurred leading to a large chipping. At high loads (3.0~6.0N), a crushed zone was observed with median crack. The friction experiment finds that the increasing in the friction coefficients coincides with the onset of crushing in soda-lime glass.

알루미나 세라믹스의 반복적 균열치유 특성 (Cyclic Crack Healing Effect of Al2O3 Ceramics)

  • 문창권;김부안
    • 한국해양공학회지
    • /
    • 제27권2호
    • /
    • pp.69-74
    • /
    • 2013
  • In this study, the crack healing effects of $Al_2O_3$ ceramics based on the heat treatment conditions were investigated. The influence of the additive amounts of SiC nanoparticles and the cycling process of indentation-heat treatment on the crack healing effect of $Al_2O_3$ ceramics were also examined. Three-point bending tests were carried out and the morphological changes in the fracture surface were observed by using FE-SEM. As a result, heat-treated samples in a vacuum or air atmosphere showed improved bending strengths compared to un-heat treated samples. This means that cracked specimens can be healed by heat treatment in a vacuum or air atmosphere. The crack healing effect of $Al_2O_3$ ceramics that were heat treated in an air atmosphere was much higher than that of those heat treated in a vacuum. After heat treatment, the $Al_2O_3$ ceramics with 30 wt% SiC nanoparticles showed a higher bending strength than those with 15 wt% SiC. The cyclic indentation and heat treatment did not remarkably affect the crack healing effect. The SEM images showed that the median crack, indenter mark on the surface, and pores in the fracture surface of a specimen almost disappeared after being heat treated in an air atmosphere.

미소 비커스 압입균열에 의한 초경합금의 파괴 인성치 측정 (Measurement of Fracture Toughness of WC-Co Composites by Micro-Vickers Indentation Cracks)

  • Lee, O.S.;Son, I.S.;Park, W.K.;Hwang, S.K.
    • 한국정밀공학회지
    • /
    • 제12권2호
    • /
    • pp.5-13
    • /
    • 1995
  • Various techniques to measure fracture toughness which is an important parameter to predict fracture behavious of structural materials have been reported. Among these mathods, this paper describes the micro-Vickers indentation crack method to estimate the fracture toughness of some WC-Co composites. Two indentation crack patterns (such as radial-median cracks (orhalf-penny cracks) and Palmqvist cracks generated during indentation) are referred precisely. The fracture toughness of WC-4.7wt%Co, WC-6wr%Co and WE-9wr%Co composites were estimated by using some equations given by Shetty et al., Nihara et al. in this study. We show the reliability of indentation method by comparing the results with those from literatures. The appropriate equation to estimate the fracture toughness in the case of WC-Co composite is given. In addition, some technical informations in terms of the crack length by indentation in estimating the existence of the surface residual stress that prevents to obtain an accurate fracture toughness are presented.

  • PDF

영상처리 기법을 이용한 콘크리트 교량의 균열 검출 (Crack Detection on Concrete Bridge by Image Processing Technique)

  • 김형진;이정호;문영식
    • 대한전자공학회:학술대회논문집
    • /
    • 대한전자공학회 2007년도 하계종합학술대회 논문집
    • /
    • pp.381-382
    • /
    • 2007
  • In this paper, crack detection technique of concrete bridge is proposed robust against shadow and noise. Our technique consists of two steps. In the first step, crack candidate region is detected by preprocessing. Preprocessing techniques such as median filter, isolated point filter and morphological techniques, use utilized for detection of crack candidate regions. In the final step, crack is detected from crack candidate region by considering any connectivity between cracks. By experimental results, performance is improved 6.8% over the existing method.

  • PDF

자기애자의 자기부 균열 식별을 위한 이미지 처리기법 개발 (Development of Image Process for Crack Identification on Porcelain Insulators)

  • 최인혁;신구용;안호성;구자빈;손주암;임대연;오태근;윤영근
    • 한국전기전자재료학회논문지
    • /
    • 제33권4호
    • /
    • pp.303-309
    • /
    • 2020
  • This study proposes a crack identification algorithm to analyze the surface condition of porcelain insulators and to efficiently visualize cracks. The proposed image processing algorithm for crack identification consists of two primary steps. In the first step, the brightness is eliminated by converting the image to the lab color space. Then, the background is removed by the K-means clustering method. After that, the optimum image treatment is applied using morphological image processing and median filtering to remove unnecessary noise, such as blobs. In the second step, the preprocessed image is converted to grayscale, and any cracks present in the image are identified. Next, the region properties, such as the number of pixels and the ratio of the major to the minor axis, are used to separate the cracks from the noise. Using this image processing algorithm, the precision of crack identification for all the sample images was approximately 80%, and the F1 score was approximately 70. Thus, this method can be helpful for efficient crack monitoring.