Degradation Degree Evaluation of Heat Resisting Steel by Electrochemical Technique Part 2 : Effect of Testing Conditions on Evaluation Value of Degradation Degree and Changes of Mechaical Properties (전기화학적 방법에 의한 내열강의 열화도측정 제2보 : 열화도측정치에 미치는 측정조건들의 영향과 기계적성질 변화에 대해서)

  • 정희돈;권영각;장래웅
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.17 no.2
    • /
    • pp.300-312
    • /
    • 1993
  • The material deterioration of service-exposed boiler tube steels in fossil power plant was evaluated by using the electrochemical technique namely, modified electrochemical potentiokinetic reactivation(EPR). It was focused that the passivation of Mo$_{6}$C carbide which governs the mechanical properties of Mo alloyed steels did not occur even in the passivity region of steel in sodium molybdate solution and the reactivation peak current (Ip) observed as the result of non-passivation indicating the precipitation of Mo$_{6}$C carbides. To obtain the optimal test conditions for the field test by using the specially designed electrochemical cell, the effects of scan rate, the surface roughness and the pH of electrolyte on Ip value were also investigated. Furthermore, the change of mechanical properties occurred during the long time exposure at high temperature was evlauated quantitatively by small punch(SP) tests and micro hardness test taking account of the metallurgical changes. It is known that reactivation peak current (Ip) has a good relationship with Larson-Miller Parameter(LMP) which represents the information about material deterioration occurred at high temperature environment. In addition it was possible to estimate the ductile-brittle transition temperature (DBTT) by means of the SP test. The Sp test could be, therefore, suggested as a reliable test method for evaluating the material degradation of boiler tube steels. From the good correaltion between the SP DBTT and Ip values shown in this study, it was knows that the change of mechanical properties could be evaluated non-destructively by measurring only Ip values.ues.

Optimal Maintenance Decisions for Power Supply Timber Poles

  • G., Chattopadhyay;A., Rahman
    • International Journal of Reliability and Applications
    • /
    • v.5 no.4
    • /
    • pp.115-128
    • /
    • 2004
  • Reliability of a power supply timber pole depends on complex combination of age, environmental factors involved in deterioration process ans inspection and maintenance actions influencing reliability and safety. In this paper soil and human factors are identified, models have been developed and analyzed for optimal maintenence decisions related to electrical power supply timber poles.

  • PDF

Effect of Admix Ratio of Free-machining Agent 'KSX' that Contains Complex Calcium Oxide Powder on Machinability

  • Furuta, Satoshi;Masuda, Shinsuke
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.297-298
    • /
    • 2006
  • Free-machining agent 'KSX' contains complex calcium oxide is developed. The effect of admix ratio of KSX on mechanical properties and machinability with two different cutting speeds is reported. KSX displays improved machinability without deterioration of mechanical properties up to 0.3mass% addition. It was observed that KSX is effective with a small addition of 0.1mass% at slower cutting speed, and increased of admix ratio is effective at faster cutting speed.

  • PDF

Evaluation of the Mechanical Properties of Field-Cast Shotcrete and Long-Term Durability by Combined Deterioration Test (현장타설 숏크리트의 역학적 성능 평가 및 복합열화시험을 통한 장기내구성 평가)

  • Ma, Sang-Joon;Jang, Phil-Sung;Kim, Dong-Min;Choi, Jae-Seok
    • Journal of the Korea Concrete Institute
    • /
    • v.19 no.1
    • /
    • pp.47-56
    • /
    • 2007
  • Recently, tunnels are increasingly constructed in this country with the increased construction of highways, high-speed railways and subways. Shotcrete is one of the major processes in the tunnel construction. Many problems, however, exist in the current shotcrete practice. The purpose of the study is, therefore, to explore the trobles in the current shotcreting practice, and to develop high-quality silica fume shotcrete. For the purpose of security a long-term durability of shotcrete, this study conducted combined deterioration tests. In this study, a combined deterioration test in consideration of a variety of deterioration factors were proceeded. Especially, micro-silica fume that was used frequently in overseas because of a outstanding strength-promotion effect was applied to combined deterioration test, and a long-term durability of shotcrete was investigated according to additions mixing. As a result of test, the shotcrete mixed Micro-silica fume showed a good deterioration quality compared with the other mixes. And is shows that the Micro-silica fume has an outstanding strength-promotion effect and is effective to secure a long-term durability of shotcrete by means of decreasing a deterioration caused by steel fiber mixed.

The Effect of Hot Isostatic Pressing on Mechanical Properties of Cast Aluminum Alloy (주조된 AI 합금의 기계적 성질에 미치는 HIP의 영향)

  • Kim, Gi-Tae;Yang, Hun-Cheol;Choe, Jae-Yun
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.26 no.3
    • /
    • pp.461-470
    • /
    • 2002
  • The present paper investigates the effect of hot isostatic pressing (HIPing) on mechanical properties, e.g., tensile strength, ductility and impact absorption energy of sand and die casted aluminum alloys. After HIPing at various temperatures and pressure conditions, uniaxial tensile test and Izod impact test of the samples were carried out. The experimental results showed improvements in uniaxial tensile strength, elongation and Izod impact toughness of sand casted aluminum alloy, while deterioration of a tensile strength fur die casted aluminum alloy. The effect of HIPing for microstructure of the cast aluminum alloy was also investigated.

Mechanical Deterioration Characteristics of ACSR due to a Flame (화염으로 인한 ACSR의 기계적 열화 특성)

  • 박창기;이광식;강지원;김영달
    • Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
    • /
    • v.17 no.6
    • /
    • pp.160-168
    • /
    • 2003
  • In Korea, a large portion of aerial power-transmission cables is installed in the mountains. In the case of a fire in the mountains, steel wires coated with zinc and aluminum wires of those power cables exposed to the fire or near around will be deteriorated by the blaze and the high temperature. Deterioration proceeds by interactions of a variety of factors like quality, manufacturing process, the condition of installation and exposure environment of a wire, and so on. Generally, the characteristic of a conductor affect by a forest fire can not be analyzed without the effect through simulating a forest fire. However, there are little research accomplishments of that kind of simulation about it, and there's been no analysis of a sample exposed to an actual forest fire. This thesis shows the experimental results that apply to a new wire by an artificial flame-maker because it's difficult to directly analyze the characteristic of deterioration by a forest fire. Those results include the intensity of extension and wrench for a conductor. In addition, there's been an experiment and analysis about the mechanical characteristics of the wire of ACSR 480[$\textrm{mm}^2$] which was removed from Pohang area by a forest fire. Then, the database will be made to predict the state of deteriorated wires by a forest fire using those two data, and data necessary to diagnose the life state of an ACSR wire affected by a forest fire will be given.

Reliance Analysis for Mechanical Characteristics of ACSR Transmission Line due to a Flame (화염에 의한 ACSR 송전선의 기계적 특성에 관한 신뢰성 분석)

  • 김영달
    • Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
    • /
    • v.17 no.6
    • /
    • pp.138-146
    • /
    • 2003
  • This paper deals with the experimental results that apply to a new wire by an artificial flame-maker because it's difficult to directly analyze the characteristic of deterioration by a forest fire. Those results include tension load, extension rate and torsion number for a conductor. In addition, there's been an experiment and analysis about the mechanical characteristics of the wire of ACSR 480$\textrm{mm}^2$ which was removed from Pohang area by a forest fire. Then, the database will be made to predict the state of deteriorated wires by a forest fire using those two data, and data necessary to diagnose the life state of an ACSR wire affected by a forest fire will be given.

Influence of Residual Bending Fatigue Strength on Impact Damage of CFRP Composites (CFRP 적층판의 충격손상이 잔류 굽힘 피로강도에 미치는 영향)

  • Yang, Yong Jun;Yang, In Young
    • Journal of the Korean Society of Safety
    • /
    • v.30 no.3
    • /
    • pp.7-12
    • /
    • 2015
  • CFRP composites are used as primary structural members in various industrial fields because their specific strength and specific stiffness are excellent in comparison to conventional metals. Their usage is expanding to high added-value industrial fields because they are more than 50% lighter than metals, and have excellent heat resistance and wear resistance. However, when CFRP composites suffer impact damage, destruction of fiber and interface delamination occur. This causes an unexpected deterioration of strength, and for this reason it is very difficult to ensure the reliability of the excellent mechanical properties. Therefore, for the destruction mechanism in bending with impact damage, this study investigated the reinforcement data regarding various external loads by identifying the consequential strength deterioration. Specimens were damaged by impact with a steel ball propelled by air pressure. Decrease in bending strength caused by the tension and compression of the impact side, and depending on the lamination direction of fiber and interface inside the specimen. From the bending test it was found that the bending strength reduced when the impact energy increased. Especially in the case of compression on the impact side, as tensile stress occurred at the damage starting point, causing rapid failure and a substantially reduced failure strength.

Evaluation for mechanical hardness of gas turbine rotor bolt according to deterioration of specimen (시편의 열화에 따른 가스터빈 로터볼트 기계적 강도평가)

  • Gil, D.S.;Ahn, Y.S.;Park, S.K.
    • Journal of Power System Engineering
    • /
    • v.15 no.4
    • /
    • pp.19-24
    • /
    • 2011
  • The operational efficiency of domestic gas turbine is about 25% and it is now in the trend of the gradual growth in spite of the severe temperature, frequent starting and shutdown according to the environmental management and the energy-efficient use. Rotor bolts of gas turbine in power plants have been the cause of defects because these gas turbines have been operated for a long time under the high pressure and temperature environment experiencing the aging change and stress concentration of the bonded part. The connection parts of the bolt revealed various failure shape and these parts were elongated under very low pressure when operated in the relaxed condition. The cause is in the lack of the metal distribution in the bottle lack area and the cap screw of the bolt is broken totally in case that the nut is fastened in most cases. Gas turbine rotor bolts are connected to the rotor wheel and these bolts caused the vibration, the bulk accident of the rotor in the event that the coupling power among these bolts was relaxed. Therefore, we would like to evaluate the soundness of the main part of the gas turbine rotor bolt through the measurement of the inner condition change along with the mechanic deterioration and temperature, stress in the gas turbine rotor material.

Heat Transfer Characteristics on Toroidal Convection Loop with Nanofluids (나노유체 토로이달 자연대류 루프에서의 열전달 특성)

  • Jang, Ju-Chan;Rhi, Seok-Ho;Lee, Chung-Gu
    • Transactions of the Korean Society of Mechanical Engineers B
    • /
    • v.33 no.4
    • /
    • pp.235-241
    • /
    • 2009
  • Experimental studies on single-phase toroidal circulation loop(thermosyphon) have been performed in the present study with Ag-nanofluids as a working fluids. The present paper deals with an experimental study on the heat transfer behavior of single-phase toroidal loop. Toroidal loop charged with nanofluid has been constructed and a number of tests have been carried out. Different geometric parameter, e.g., orientation has been investigated. The tests were conducted employing two fluids: distilled water and Ag-nanofluid of various volume concentrations. The experiments at Rayleigh number from $10^5$ to $10^6$ showed a systematic and slight deterioration in natural convective heat transfer. It was observed that the deterioration due to the particle concentration was in the range of 5-10%. At a given particle concentration of 0.05%, abrupt decrease in the Nusselt number and the Raleigh number was observed. The present study with toroidal loop shows that the application of nanofluids for heat transfer intensification should not be decided only by the effective thermal conductivity with increasing particle concentration.