• 제목/요약/키워드: magnetic powder size

검색결과 198건 처리시간 0.028초

Magnetic Properties of Amorphous FeCrSiBC Alloy Powder Cores Using Phosphate-coated Powders

  • Jang, Dae-Ho;Kim, Kwang-Youn;Noh, Tae-Hwan
    • Journal of Magnetics
    • /
    • 제11권3호
    • /
    • pp.126-129
    • /
    • 2006
  • The phosphate coating on the $(Fe_{0.97}Cr_{0.03})_{76}(Si_{0.5}B_{0.5})_{22}C_2$ amorphous powders with an average size of 10 ${\mu}m$ in diameter has been carried out in aqueous 1.0-2.0 wt% $H_3PO_4$ solutions, and the consolidation behavior and magnetic properties of their compressed powder cores has been investigated. The phosphate coating could provide efficient electrical insulation between amorphous powders and improved consolidation ability at room temperature. Especially when the powders were treated in more concentrated phosphoric acid solution, enhanced phosphate covering and higher frequency/dc-bias stability were achieved. The powder cores phosphate-coated in 2.0 wt% $H_3PO_4$ solution exhibited constant permeability of 21 up to 10 MHz, 110 of the quality factor at 0.9 MHz, 610 mW/cm3 core loss at 100 kHz/0.1 T and 89 of percent permeability at 100 kHz.

분말사출성형으로 제조된 다극 이방성 Sr-페라이트 소결자석 (Multi-pole anisotropic Sr-ferrite sintered magnets fabricated by powder injection molding)

  • 조태식
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집 Vol.14 No.1
    • /
    • pp.284-287
    • /
    • 2001
  • Multi-pole anisotropic Sr-ferrite sintered magnets has been studied by powder injection molding under applied magnetic field. The orientation of anisotropic Sr-ferrite powders higher than 80% during injection molding is achieved at the following conditions; apparent viscosity lower then 2500 poise in 1000 $sec^{-1}$ shear rate and applied magnetic field higher then 4 kOe. For the high fluidity and strength of injection molded compact, and the effective binder removal without defects during solvent extraction and thermal debinding, the optimum multi-binder composition is paraffin wax(PW)/carnauba wax(CW)/HDPE = 50/25/25 wt%. The rate of binder removal is proportional to the mean particle size of Sr-ferrite powders whereas it is inversely proportional to the content of Sr-ferrite powders and the sample thickness. The high magnetic properties of Sr-ferrite sintered magnets are; 3.8 kG of remanent flux density, 3.4 kOe of intrinsic coercivity, and 1.2 kG of surface flux density (l-mm-thick) in the direction of applied magnetic field.

  • PDF

분말사출성형으로 제조된 다극 이방성 SF-폐라이트 소결자석 (Mu7i-pole anisotropic Sr-ferrite sintered magnets fabricated by powder injection molding)

  • 조태식
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집
    • /
    • pp.284-287
    • /
    • 2001
  • Multi-pole anisotropic Sr-fertile sintered magnets has been studied by powder injection molding under applied magnetic field. The orientation of anisotropic Sr-ferrite powders higher than 80% during injection molding is achieved at the following conditions; apparent viscosity lower then 2500 poise in 1000 sec$\^$-1/ shear rate and applied magnetic field higher then 4 kOe. For the high fluidity and strength of injection molded compact, and the effective binder removal without defects during solvent extraction and thermal debinding, the optimum multi-binder composition is paraffin wax(PW)/carnauba wax(CW)/HDPE = 50/25/25 wt%. The rate of binder removal is proportional to the mean particle size of Sr-ferrite powders whereas it is inversely proportional to the content of Sr-ferrite powders and the sample thickness. The high magnetic properties of Sr-ferrite sintered magnets are; 3.8 kG of remanent flux density, 3.4 kOe of intrinsic coercivity, and 1.2 kG of surface flux density (1-mm-thick) in the direction of applied magnetic field.

  • PDF

Wireless Magnetic Pump: Characteristics of Magnetic Impellers and Medical Application

  • Song, Moon Kyou;Kim, Sung Hoon
    • Journal of Magnetics
    • /
    • 제22권2호
    • /
    • pp.344-351
    • /
    • 2017
  • Wireless magnet pumps are used in medical applications and are particularly useful as artificial heart ventricular assist devices (VADs). To investigate wireless operation of magnetic pumps, we fabricated three types of magnetic impellers using bonded magnets by blending magnetic powders of SmFeN, NdFeB, and Sr-ferrite. We investigated the magnetic properties of the fabricated magnetic impellers, which are driven by the application of magnetic coupling with an external driving magnet or external coil system, without a driving motor, shaft, or mechanical bearings. The use of wireless magnetic pumps is therefore not complicated by critical issues of size, heat, and vibration, which are very important issues for blood pumps. The magnetic properties of the impellers, such as their rotational speed, driving torque and hydrodynamic performance, determine their wireless driving ranges. We conducted performance evaluations of the impeller's magnetic wireless manipulation, heat, and vibration. In addition, we carried out an animal test to confirm the suitability of the wireless magnetic pumps for use as biventricular assist devices (BiVADs).

NFC의 자기차폐용 Ni-Zn-Cu 페라이트의 자기특성에 미치는 소결온도의 영향 (Influence of Sintering Temperature on Magnetic Properties of Ni-Zn-Cu Ferrites Used for Mangetic Shielding in NFC)

  • 류요한;김성수
    • 한국분말재료학회지
    • /
    • 제23권2호
    • /
    • pp.132-135
    • /
    • 2016
  • This study investigates the influence of sintering temperature on the magnetic properties and frequency dispersion of the complex permeability of Ni-Zn-Cu ferrites used for magnetic shielding in near-field communication (NFC) systems. Sintered specimens of $(Ni_{0.7}Zn_{0.3})_{0.96}Cu_{0.04}Fe_2O_4$ are prepared by conventional ceramic processing. The complex permeability is measured by an RF impedance analyzer in the range of 1 MHz to 1.8 GHz. The real and imaginary parts of the complex permeability depend sensitively on the sintering temperature, which is closely related to the microstructure, including grain size and pore distribution. In particular, internal pores within grains produced by rapid grain growth decrease the permeability and increase the magnetic loss at the operating frequency of NFC (13.56 MHz). At the optimized sintering temperature ($1225-1250^{\circ}C$), the highest permeability and lowest magnetic loss can be obtained.

연자성 복합체 후막용 슬러리 제조공정의 최적화 (Optimization of Slurry Preparation Process for Soft Magnetic Green Sheet)

  • 오세문;이창현;신효순;여동훈;김진호
    • 한국전기전자재료학회논문지
    • /
    • 제28권12호
    • /
    • pp.792-796
    • /
    • 2015
  • With high integration of electronic components, power inductors are also miniaturized. Recently, thick film processes for small size power inductors were developed and commercialized. However, the thick film process to prepare soft magnetic green sheets was not reported enough. In this study, we used Fe-Si magnetic and CIP (carbonyl iron powders) as starting materials to lead to a bimodal particle size distribution in the sheet. We proposed a newly developed 'Modified slurry preparation process' to get well dispersed condition even at high solid contents. Using the new process, it was possible to prepare a well dispersed slurry over 70 vol% of solid. BYK-103 was better than BYK-111 as dispersant in this slurry and the optimum amount was 0.6 wt%. The optimized slurry was formed into a sheet by tape casting process and then the sheet was laminated. We conformed that small size powder, large size powder, and epoxy resin were well dispersed in the green sheet.

연자성 합금 분말의 입자크기에 따른 전자파 흡수 특성 비교 (Study of Electromagnetic Wave Absorption Properties with Particle Size in Soft Magnetic Alloy Powder)

  • 홍순호;손근용;박원욱;남정미;문병기;송용설
    • 한국분말재료학회지
    • /
    • 제14권4호
    • /
    • pp.261-264
    • /
    • 2007
  • The electromagnetic wave (EM) absorption properties of various particle size have been investigated in a sheet-type absorber using the $Fe_{73}Si_{16}B_{7}Nb_{3}Cu_{1}$ alloy powder. With decreasing the average particle size, the complex permeability (${\mu}_{r}$) and permittivity (${\varepsilon}_{r}$) increased and the matching frequency is shifted toward lower frequency. The fabricated EM wave absorbers showed permeability $2{\sim}6$, permittivity $17{\sim}23$ for a $-325{\sim}+400$ mesh sample, and the calculated power absorption was as high as 80% in the frequency range over 2 GHz.

A New PIM Joining Process

  • Miura, Hideshi
    • 한국분말재료학회지
    • /
    • 제9권4호
    • /
    • pp.203-210
    • /
    • 2002
  • A new PIM in-process joining technique has been developed for more complicated and functional PIM components by application of the exuded wax from the green compacts during solvent debinding step. At first, various stainless steels and iron compacts with rectangular shape were combined, and the joining behaviors and properties were investigated by shear and tensile test, and microscopic observation. Subsequently, perfect joined three pieces of thin and hollow compacts were obtained for the combination of same and different stainless steels, and it was difficult to join the iron and stainless steel compacts in hydrogen atmosphere because of the different starting temperature of shrinkage. However, pretty good joined iron and stainless steel compacts were obtained by consideration of particle size and vacuum atmosphere. Finally, for the combination of ferro-silicon and austenitic stainless steel compacts, high functionality (magnetic (1.60Tes1a) & non-magnetic) and perfect joint were obtained.

$Fe_2O_3$몰비 및 B\ulcorner첨가가 Sr-Ferrite 특성에 미치는 영향 (Effect of Molar Ratio of $Fe_2O_3$ and BaO Addition on the Characteristics of Sr-Ferrite)

  • 문기훈;심영재;조성걸
    • 한국세라믹학회지
    • /
    • 제34권5호
    • /
    • pp.453-460
    • /
    • 1997
  • Sr-ferrite having magnetoplumbite structure is similar to Ba-ferrite in magnetic characteristics, but better magnetic characteristics for using motor application. To improve remanence magnetic flux density(Br) and coercive force(iHc), it is necessary that sintered ferrites must have high density and grain size less than 1 $\mu$m. By varying n values in SrO.nFe2O3 basic composition, calcination temperature, and BaO addition, Sr-ferrite powder and sintered specimen was prepared. The n values, calcination temperature, and BaO addition affected secondary phase formation, particle size, and particle shape. BaO addition enhanced Fe2O3 secondary phase and hexagonal shape particle. Fe2O3 phase reduced sintered density which greatly decreased Br.

  • PDF