• 제목/요약/키워드: magnetic hysteresis loss

검색결과 73건 처리시간 0.024초

Recovery Propagation in Coated Conductors

  • Kim, H.R.;Park, C.R.;Yim, S.W.;Yoo, S.D.;Hyun, O.B.
    • 한국초전도학회:학술대회논문집
    • /
    • 한국초전도학회 2009년도 Korea Superconductivity Society Meeting 2009
    • /
    • pp.82-82
    • /
    • 2009
  • PDF

자기 부상 방식 미세 운동 기구의 동적 모델링 (Dynamic Modeling of an Fine Positioner Using Magnetic Levitation)

  • 정광석;백윤수
    • 대한기계학회논문집A
    • /
    • 제24권5호
    • /
    • pp.1166-1174
    • /
    • 2000
  • In this paper, we introduce a positioner based on magnetic levitation to eliminate the friction which is the most severe effect to limit high resolution on the micro level. Differently from existing electromagnetic device, the proposed positioner consists of air core solenoid and permanent magnet. Although the combination produces small magnetic force, it is suitable for realizing micro motion repeatedly without the accumulation of error because there is no hysteresis caused by ferromagnetic materials, no eddy current loss, no flux saturation. First, the approximate modeling of stiffness and damping effects between the magnetic elements is made and verified experimentally. Then, we have formulated the dynamic equation of one d.o.f magnetic levitation positioner using linear perturbation method and discussed the necessity of optimization for the chief design parameters to maximize the stability performance.

CoFeSiBNi 아몰퍼스 합금의 소자 크기에 대한 자기-임피던스 효과 관찰 (Magneto-Impedance Effect of CoFeSiBNi Amorphous Magnetic Films according to the size)

  • 박병규;황성우;문성욱
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.339-341
    • /
    • 2007
  • Soft ferromagnetic materials are very useful for many sensors using magnetic materials with high permeability, low coercivity and low hysteresis loss. Among them, FeCoSiBNi amorphous magnetic films show us a good impedance change(about 3.05%/Oe, at 12MHz) by the exterior magnetic field in this experiment. These are produced by rapid solidification from the melt and the material is ejected in a jet from a nozzle and quenched in a stream of liquid. After that, we make them a shape of wire with different sizes of width. Thus, we can find that the impedance change (122.16%, at 12MHz) is occurred and the fabricated magnetic wire has the characteristics of good sensor element.

  • PDF

Relationship Between AC and DC Magnetic Properties of an Iron-Based Amorphous Alloy for High Frequency Applications

  • Choi, Y.S.;Noh, T.H.;Lim, S.H.
    • Journal of Magnetics
    • /
    • 제1권1호
    • /
    • pp.24-30
    • /
    • 1996
  • The relationship between effective permeability and the remanence ratio of an Fe-based amorphous alloy (Metglas 2605S3A) is investigated over a wide frequency range, in an effort to understand magnetization behavior of the alloy. In the frequency range from 1 to 200 kHz, the permeability is maximum at the remanence ratio of 0.4-0.5 and, at frequencies over 500 kHz, the correlation with negative coefficients emerges indicating that the permeability decreases with the remanent ratio, except for the ribbon coated with an insulating layer of MgO which exhibits both high values of the effective permeability and remanence ratio. It is considered from the correlation results that the boundary at which the dominant magnetization mechanism changes from domain wall motion to spin rotation is near 500 kHz. The core loss is also investigated as a function of annealing time when the samples are annealed at a fixed temperature of $435^{\circ}C$. The core loss in most cases decreases with the annealing time, the degree of the loss may consist of the hysteresis loss and anomalous eddy current loss. The two loss components are considered to be of similar magnitudes at low frequencies while, at high frequencies, the dominant contribution to the total loss is the anomalous loss.

  • PDF

Analysis of the local superconducting properties in YBCO coated conductors with striations

  • Kim, Muyong;Park, Sangkook;Park, Heeyeon;Ri, Hyeong-Cheol
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제17권2호
    • /
    • pp.25-30
    • /
    • 2015
  • In order to realize economical applications, it is important to reduce the ac loss of 2G high-temperature superconductor coated conductors. It seems to be reasonable that a multi-filamentary wire can decrease the magnetization loss. In this study, we prepared two samples of YBCO coated conductors with striations. We measured local superconducting properties of both samples by using Low Temperature Scanning Laser and Hall Probe Microscopy (LTSLHPM). The distribution of the local critical temperature of samples was analyzed from experimental results of Low Temperature Scanning Laser Microscopy (LTSLM) near the superconducting transition temperature. According to LTSLM results, spatial distributions of the local critical temperature of both samples are homogeneous. The local current density and the local magnetization in samples were explored from measuring stray fields by using Scanning Hall Probe Microscopy (SHPM). From SHPM results, the remanent field pattern of the one bridge sample in an external magnetic field confirms the Bean's critical state model and the three bridge sample has similar remanent field pattern of the one bridge sample. The local magnetization curve in the three bridge sample was measured from external fields from -500 Oe to 500 Oe. We visualized that the distribution of local hysteresis loss are related in the distribution of the remanent field of the three bridge sample. Although the field dependence of the critical current density must be taken into account, the relation of the local hysteresis loss and the remanent field from Bean's model was useful.

Magnetic Characterization of the Nd Based Permanent Magnet by Newly-Developed Bipolar Pulse-Type Hysteresis Loop Tracer

  • Rhee, J.R.
    • Journal of Magnetics
    • /
    • 제4권3호
    • /
    • pp.73-75
    • /
    • 1999
  • By appliying an slternate pulsed magnetic field -generated by using a sequential ignition circuit and a magnet exciting circuit- with peak value of about 10 T to the rod type Nd based magnet Nd2Fe12.7Cr1.3B with length of 5 mm and diameter of 3.6 mm, the basic magnetic properties such as saturation magnetization, residual magnetization, coercivity, maximum energy products, magnetic anisotropy and anisotropic field are investigated with obtaining the major and minor J-H loops of the magnet. The increase in coercivity due to eddy currents in ac measurement of coercivity is calculated considering eddy current loss by analyzing a wave of generating magnetic field. The average coercivity calculated for the magnet is about 12.2 kOe, anisotropy magnetic field and anisotropic constant are measured as 60 kOe 2.43 Mj/$m^3$, respectively.

  • PDF

페라이트기 11Cr 저탄소강의 자기적 특성에 대한 고온 장시간 시효열화 효과 (Effect of Long-Term Aging Degradation on Magnetic Properties of Ferritic 11Cr Low-Carbon Steel)

  • 김정석;류권상
    • 비파괴검사학회지
    • /
    • 제36권5호
    • /
    • pp.377-383
    • /
    • 2016
  • 페라이트기 11Cr 저탄소강의 자기적 특성에 대한 고온 장시간 시효열화의 영향에 대해서 연구하였다. 장시간 시효시간이 증가함에 따라서 자기이력곡선으로부터 구한 보자력, 자기이력손실은 감소하였고 이들은 시효시간에 대해 2차 지수함수 관계를 나타내었다. 비커스 경도 역시 시효시간의 증가에 따라서 감소하여 기계적 물성의 연화를 나타내었다. 미세조직적 분석으로 주사전자현미경, 후방산란전자 및 X-선 회절시험을 수행하였다. 입계에서는 $Cr_{23}C_6$ 석출물의 급격한 성장과 입내의 래스 경계부에서 Laves ($Fe_2W$)상이 발달하였다. 조대한 석출물들로 인해 장시간 시효열화에 따라서 고용원소의 고갈과 래스 하부조직이 소멸되었다. 이는 자기적 물성과 기계적 물성의 연화현상과 밀접한 관련을 갖게 된다.

Ni-Cu-Zn페라이트의 損失과 磁性 特性 (Power Loss and Electro-Magnetic Characteristics of Ni-Cu-Zn Ferrites)

  • 대규열부;김정수
    • 자원리싸이클링
    • /
    • 제13권6호
    • /
    • pp.37-42
    • /
    • 2004
  • NiO, ZnO 조성이 다른 Ni-Cu-Zn 페라이트의 손실 분석을 실시했다. 손실, Ph는 측정 온도의 상승에 따라 감소해 100-120$^{\circ}C$ 근처에서 일정한 값을 얻었다. Pcv의 주파수의존성은 Pcv~f$^n$ 로 표현될 수 있는데, n은 1 MHz까지 일정했다. Pcv는 ZnO/NiO비가 증가함에 따라 감소한다. Pcv를 Hysteresis loss(Ph) 및 잔류손실(Pcv-Ph)로 분리했다. Pcv의 온도특성 및 조성 의존성은 Ph에 기인하지만, Pcv-Ph는 온도 및 조성에 의존하지 않는다. Ph와 초투자율, ${\mu}_i$의 온도 및 조성 의존성을 분석해, 다음과 같은 식이 성립된다는 것을 알 수 있었다. ${\mu}_i{\mu}_0=I_s^2/(K_I+b{\sigma}_0{\lambda}_s)$ Wh=13.5(I$_s^2/{\mu}_i{\mu}_0)$ 여기서, ${\mu}_0$은 진공의 투자율, I$_s$는 포화자화, K$_I$는 이방성상수, ${\sigma}_0$는 내부 불균일 응력, ${\lambda}_s$는 자기이방성 상수, b는 미지의 상수, Wh는 1주기 당의 히스테리시스 손실(Ph=Wh${\times}$f)이다. Ni-Cu-Zn 페라이트의 Steinmetz 상수 m=1.64~2.2는 Mn-Zn 페라이트보다는 적은데, 이는 양 재료 간의 손실 메커니즘의 차가 있음을 암시하는 것이다.

Ni-Cu-Zn페라이트의 손실과 자성 특성 (Power Loss and Electro-Magnetic Characteristics of Ni-Cu-Zn Ferrites)

  • 대규열부;김정수
    • 한국자원리싸이클링학회:학술대회논문집
    • /
    • 한국자원리싸이클링학회 2004년도 13회 산화철워크샵
    • /
    • pp.3-11
    • /
    • 2004
  • NiO, ZnO 조성이 다른 Ni-Cu-Zn 페라이트의 손실 분석을 실시했다. 손실, Ph는 측정 온도의 상승에 따라 감소 해 $100-120^{\circ}C$ 근처에서 일정한 값을 얻었다. Pcv 의 주파수의존성은 $Pcv\~f^n$ 로 표현될 수 있는데, n는 1 MHz 까지 일정했다. Pcv 는 ZnO/NiO 비가 증가함에 따라 감소한다. Pcv 를 Hysteresis loss, Ph 및 잔류손실, (Pcv-Ph)로 분리했다. Pcv 의 온도특성 및 조성 의존성은 Ph에 기인하지만, (Pcv-Ph)는 온도 및 조성에 의존하지 않는다 Ph 와 초투자률, ${\mu}$i의 온도 및 조성 의존성을 분석 해, 다음과 같은 식이 성립된다는 것을 알 수 있었다. $${\mu}\;_i{\mu}\;_o=I_s\;^2/(K_1+b{\sigma}\;_o{\lambda}\;_s)\;\;\;\;(1)$$ $$Wh=13.5(I_s\;^2/{\mu}\;i{\mu}\;0)\;\;\;\;(2)$$ 여기서, ${\mu}\;_o$ 은 진공의 투자율, $I_s$, 는 포화자화, $K_1$는 이방성상수, ${\sigma}_\;o$는 내부 불균일 응력, ${\lambda}_\;s$ 는 자기이방성 상수,b는 미지의 정수, Wh는 1 주기 당의 히스테리시스 손실(Ph=Wh*f)이다. Ni-Cu-Zn 페라이트의 Steinmetz 정수 m=1.64-2.2는 Mn-Zn 페라이트보다는 적은데, 이는 양 재료간의 손실 메커니즘의 차가 있음을 암시하는 것이다.

  • PDF