Model of Organic Light Emitting Device Emission Characteristics with Alternating Current Driving Method (교류 구동 방법에 의한 유기전계발광소자 발광 특성의 모델)

  • Seo, Jung Hyun;Ju, Sung Hoo
    • Korean Journal of Materials Research
    • /
    • v.31 no.10
    • /
    • pp.586-591
    • /
    • 2021
  • This paper proposes a mathematical model that can calculate the luminescence characteristics driven by alternating current (AC) power using the current-voltage-luminance (I-V-L) properties of organic light emitting devices (OLED) driven by direct current power. Fluorescent OLEDs are manufactured to verify the model, and I-V-L characteristics driven by DC and AC are measured. The current efficiency of DC driven OLED can be divided into three sections. Region 1 is a section where the recombination efficiency increases as the carrier reaches the emission layer in proportion to the increase of the DC voltage. Region 2 is a section in which the maximum luminous efficiency is stably maintained. Region 3 is a section where the luminous efficiency decreases due to excess carriers. Therefore, the fitting equation is derived by dividing the current density and luminance of the DC driven OLED into three regions, and the current density and luminance of the AC driven OLED are calculated from the fitting equation. As a result, the measured and calculated values of the AC driving I-V-L characteristics show deviations of 4.7% for current density, 2.9 % for luminance, and 1.9 % for luminous efficiency.

Properties of MgMoO4:Eu3+ Phosphor Thin Films Grown by Radio-frequency Magnetron Sputtering Subjected to Thermal Annealing Temperature (열처리 온도 변화에 따른 라디오파 마그네트론 스퍼터링으로 성장된 MgMoO4:Eu3+ 형광체 박막의 특성)

  • Cho, Shinho
    • Current Photovoltaic Research
    • /
    • v.4 no.1
    • /
    • pp.25-29
    • /
    • 2016
  • $Eu^{3+}$-activated $MgMoO_4$ phosphor thin films were grown at $400^{\circ}C$ on quartz substrates by radio-frequency magnetron sputter deposition from a 15 mol% Eu-doped $MgMoO_4$ target. After the deposition, the phosphor thin films were annealed at several temperatures for 30 min in air. The influence of thermal annealing temperature on the structural and optical properties of $MgMoO_4:Eu^{3+}$ phosphor thin films was investigated by using X-ray diffraction (XRD), photoluminescence (PL), and ultraviolet-visible spectrophotometry. The transmittance, optical band gap, and intensities of the luminescence and excitation spectra of the thin films were found to depend on the thermal annealing temperature. The XRD patterns indicated that all the thin films had a monoclinic structure with a main (220) diffraction peak. The highest average transmittance of 91.3% in the wavelength range of 320~1100 nm was obtained for the phosphor thin film annealed at $800^{\circ}C$. At this annealing temperature the optical band gap energy was estimated as 4.83 eV. The emission and excitation spectra exhibited that the $MgMoO_4:Eu^{3+}$ phosphor thin films could be effectively excited by near ultraviolet (281 nm) light, and emitted the dominant 614 nm red light. The results show that increasing RTA temperature can enhance $Eu^{3+}$ emission and excitation intensity.

Synthesis and photoluminescence of Ca3Si3O8F2: Ce4+, Eu3+, Tb3+ phosphor

  • Suresh, K.;PoornachandraRao, Nannapaneni V.;Murthy, K.V.R.
    • Advances in materials Research
    • /
    • v.3 no.4
    • /
    • pp.227-232
    • /
    • 2014
  • $Ce^{4+}$, $Eu^{3+}$, $Tb^{3+}$ co-doped $Ca_3Si_3O_8F_2$ phosphor was synthesized via solid state reaction method using $CaF_2$, $CaCO_3$ and $SiO_2$ as raw materials for the host and $Eu_2O_3$, $CeO_2$, and $Tb_4O_7$ as activators. The luminescent properties of the phosphor was analysed by spectrofluorophotometer at room temperature. The effect of excitation wavelengths on the luminescent properties of the phosphor i.e. under near-ultraviolet (nUV) and visible excitations was investigated. The emission peaks of $Ce^{4+}$, $Eu^{3+}$, $Tb^{3+}$ co-doped $Ca_3Si_3O_8F_2$ phosphor lays at 480(blue band), 550(green band) and 611nm (red band) under 380nm excitation wavelength, attributed to the $Ce^{4+}$ ion, $Tb^{3+}$ ion and $Eu^{3+}$ ions respectively. The results reveal that the phosphor emits white light upon nUV (380nm) / visible (465nm) illumination, and a red light upon 395nm / 535nm illumination. RE ions doped $Ca_3Si_3O_8F_2$ is a promising white light phosphor for LEDs. The emission colours can be seen using Commission international de l'eclairage (CIE) co-ordinates. A single host phosphor emitting different colours under different excitations indicates that it is a potential phosphor having applications in many fields.

Photoluminescent Properties of Eu(III) in the Composite Heterocyclic Ligands/Crown Ether Systems

  • Liu, Hong Guo;Jang, Ki-Wan;Feng, Xu Sheng;Kim, Chang-Dae;Yoo, Young-Jae;Lee, Yong-Ill
    • Bulletin of the Korean Chemical Society
    • /
    • v.26 no.12
    • /
    • pp.1969-1974
    • /
    • 2005
  • Composite systems of $Eu(phen)_2Cl_3{(H_2O)}_2$, Eu(DN-bpy)$(phen)Cl_3{(H_2O)}_2$ and Eu(DB-bpy)$(phen)Cl_3{(H_2O)}_2$ (DNbpy: $4,4^\prime$-Dinonyl-$2,2^\prime$-dipyridyl; DB-bpy: $4,4^\prime$-Di-tert-butyl-$2,2^\prime$-dipyridyl) with crown ethers of Benzo-15-crown-5 (B15C5), Benzo-18-crown-6 (B18C6), 18-crown-6 (18C6), Dibenzo-18-crown-6 (DB18C6) and Dibenzo-24-crown-8 (DB24C8) were fabricated successfully and characterized by using photoluminescent spectroscopy and luminescent lifetime measurements. All composites formed show high luminescence mainly in red region. It was found that the heterocyclic ligands such as phen, DN-bpy and DB-bpy as well as the crown ethers have great influences on the photoluminescent properties of $Eu^{3+}$ ion. The environment around $Eu^{3+}$ ion in the composite systems changes greatly,presumably the variation of the first coordination sphere. The $Eu^{3+}$ ion occupies higher symmetrical environment and in more than one kind of symmetrical site in the composite systems studied in this work.

Upconversion Photoluminescence Properties of PbMoO4:Er3+/Yb3+ Phosphors Synthesized by Microwave Sol-Gel Method

  • Lim, Chang Sung
    • Korean Journal of Materials Research
    • /
    • v.25 no.9
    • /
    • pp.480-486
    • /
    • 2015
  • $Pb_{1-x}MoO_4:Er^{3+}/Yb^{3+}$ phosphors with various doping concentrations of $Er^{3+}$ and $Yb^{3+}$ ($x=Er^{3+}+Yb^{3+}$, $Er^{3+}=0.05$, 0.1, 0.2, and $Yb^{3+}=0.2$, 0.45) are successfully synthesized using a microwave sol-gel method, and the up-conversion photoluminescence properties are investigated. Well-crystallized particles, which are formed after heat treatment at $900^{\circ}C$ for 16 h, exhibit a fine and homogeneous morphology with particle sizes of $2-5{\mu}m$. Under excitation at 980 nm, the $Pb_{0.7}MoO_4:Er_{0.1}Yb_{0.2}$ and $Pb_{0.5}MoO_4:Er_{0.05}Yb_{0.45}$ particles exhibit a strong 525 nm emission band, a weak 550 nm emission band in the green region, and a very weak 655 nm emission band in the red region. The Raman spectra of the doped particles indicate the presence of strong peaks at higher and lower frequencies induced by the disordered structures of $Pb_{1-x}MoO_4$ through the incorporation of the $Er^{3+}$ and $Yb^{3+}$ ions into the crystal lattice, which results in the unit cell shrinkage accompanying the new phase formation of the $MoO_{4-x}$ group.

Synthesis of CaS:Eu2+ Phosphor by using a Sealing Vessel and its Photoluminescence Properties

  • Yoo, Hyoung-Sun;Park, Bong-Je;Kang, Jong-Hyuk;Im, Won-Bin;Jeon, Duk-Young
    • Transactions on Electrical and Electronic Materials
    • /
    • v.8 no.6
    • /
    • pp.255-259
    • /
    • 2007
  • We have synthesized $CaS:Eu^{2+}$ phosphor by using a sealing vessel and evaluated its photoluminescence properties. The method using a sealing vessel is simple and economical in comparison with other methods reported up to date. As an activator concentration was increased from 0.1 mol% to 4 mol%, the main emission wavelength of the phosphor was increased from 642 nm to 651 nm due to the crystal field splitting of 5d levels of $Eu^{2+}$ ion. Although the same amount of $Eu_2O_3$ was used, the concentration of the activator ions, which were reduced from $Eu^{3+}\;to\;Eu^{2+}$ and substituted $Ca^{2+}$ ions, was increased with increase of firing temperature. Therefore, the main emission wavelength was also. shifted from 645 nm to 651 nm with increase of firing temperature from $1100^{\circ}C\;to\;1300^{\circ}C$. The critical distance($R_{c1}=20.65\;{\AA}$) between $Eu^{2+}$ ions calculated from the critical concentration was well matched with that($R_{c2}=19.17\;{\AA}$) calculated from the Dexter formula.

Photoluminescence Properties of SrSnO3:Dy3+ White Light-Emitting Phosphors (SrSnO3:Dy3+ 백색광 형광체의 발광 특성)

  • Shin, Johngeon;Cho, Shinho
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.30 no.11
    • /
    • pp.710-716
    • /
    • 2017
  • New white-light-emitting $SrSnO_3:Dy^{3+}$ phosphors were prepared using different concentrations of $Dy^{3+}$ ions via a solid-state reaction. The phase structure, luminescence, and morphological properties of the synthesized phosphors were investigated using X-ray diffraction analysis, fluorescence spectrophotometry, and scanning electron microscopy, respectively. All the synthesized phosphors crystallized in an orthorhombic phase with a major (020) diffraction peak, irrespective of the concentration of $Dy^{3+}$ ions. The excitation spectra were composed of a broad band centered at 298 nm, ascribed to the $O^2-Dy^{3+}$ charge transfer band and five weak bands in the range of 350~500 nm. The emission spectra of $SrSnO_3:Dy^{3+}$ phosphors consisted of three bands centered at 485, 577, and 665 nm, corresponding to the $^4F_{9/2}{\rightarrow}^6H_{15/2}$, $^4F_{9/2}{\rightarrow}^6H_{13/2}$, and $^4F_{9/2}{\rightarrow}^6H_{11/2}$ transitions of $Dy^{3+}$, respectively. As the $Dy^{3+}$ concentration increased from 1 to 15 mol%, the intensities of all the emission bands gradually increased, reached maxima at 15 mol% of $Dy^{3+}$ ions, and then decreased rapidly at 20 mol% due to concentration quenching. The critical distance between neighboring $Dy^{3+}$ ions for concentration quenching was calculated to be $9.4{\AA}$. The optimal white light emission by the $SrSnO_3:Dy^{3+}$ phosphors was obtained when the $Dy^{3+}$ concentration was 15 mol%.

A study on the Mossbauer effect and optical properties of $^{57}Fe$-doped-GaAs ($^{57}Fe$ 도프된 GaAs의 Mossbauer 효과 및 광학적 특성에 관한 연구)

  • 고정대;홍성락;김득영;강태원
    • Journal of the Korean Vacuum Society
    • /
    • v.6 no.4
    • /
    • pp.337-342
    • /
    • 1997
  • We have investigated Mossbauer effect and emission properties of the Fe-doped GaAs grown by liquid phase epitaxy (LPE). The powder type of isotope $^{57}Fe$ was used as a dopant source in LPE-GaAs. From the analysis of Mossbauer effect the value of isomer shift, 0.303$\pm$0.018 mm/sec, is calculated at low temperature. This means that charge state of Fe ion in GaAs is 3+. The results of double crystal x-ray rocking curve (DCRC) and low temperature photoluminescence (PL) show the crystal quality of the epitaxial layers are good. Unusual luminescence peaks from the Fe-GaAs epitaxial layers appeared at emission energy of 0.99 eV and 1.15 eV. We attribute these emissions to Fe-acceptor related two deep radiative centers.

  • PDF

A Study on the Preparation of $ZnGa_{2}O_{4}$ by Polymerized Complex Method and Solution Combustion Method (착체중합법 및 연소합성법에 의한 $ZnGa_{2}O_{4}$ 합성에 관한 연구)

  • Jun, Ae-Kyoung;Ryu, Ho-Jin;Park, Hee-Dong;Lee, Ik-Mo
    • Korean Journal of Materials Research
    • /
    • v.8 no.7
    • /
    • pp.616-620
    • /
    • 1998
  • Zn_{0.994}Mn_{0.006}Ga_2O_4$ green phosphor powders were synthesized using polymerized complex and solution combustion methods, and their powder and luminescence properties were characterized by XRD, SEM, BET, PL, etc. The properties were compared with those of the powders prepared by a solid state reaction method. The powders prepared by polymerized complex and solution combustion methods showed only a single spinel phase at 50$0^{\circ}C$ and 40$0^{\circ}C$, respectively. Their particle sizes were smaller than that of a solid state reaction method. Emission intensity of the phosphor powders prepared by both methods were highest at 90$0^{\circ}C$ and 40$0^{\circ}C$, respectively.

  • PDF

Synthesis of K2TiF6:Mn4+ Red Phosphors by a Simple Method and Their Photoluminescence Properties (Mn4+ 이온 활성 K2TiF6 불화물 적색형광체의 합성과 발광특성)

  • Kim, Yeon;Wu, Mihye;Choi, Sungho;Shim, Kwang Bo;Jung, Ha-Kyun
    • Korean Journal of Materials Research
    • /
    • v.26 no.9
    • /
    • pp.504-511
    • /
    • 2016
  • To prepare $Mn^{4+}$-activated $K_2TiF_6$ phosphor, a precipitation method without using hydrofluoric acid (HF) was designed. In the synthetic reaction, to prevent the decomposition of $K_2MnF_6$, which is used as a source of $Mn^{4+}$ activator, $NH_5F_2$ solution was adopted in place of the HF solution. Single phase $K_2TiF_6$:$Mn^{4+}$ phosphors were successfully synthesized through the designed reaction at room temperature. To acquire high luminance of the phosphor, the reaction conditions such as the type and concentration of the reactants were optimized. Also, the optimum content of $Mn^{4+}$ activator was evaluator based on the emission intensity. Photoluminescence properties such as excitation and emission spectrum, decay curve, and temperature dependence of PL intensity were investigated. In order to examine the applicability of this material to a white LED, the electroluminescence property of a pc-WLED fabricated by combining the $K_2TiF_6$:$Mn^{4+}$ phosphor with a 450 nm blue-LED chip was measured.