Study on The Development and Economic Evaluation of Solar Drying System for Wood Industry (목재산업용(木材産業用) 태양열(太陽熱) 건조장치(乾燥裝置)의 개발(開發)과 경제성분석(經濟性分析)에 관한 연구(硏究))

  • Lee, Hyoung-Woo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.20 no.1
    • /
    • pp.5-14
    • /
    • 1992
  • Experimental external collector type solar lumber dryer of $1m^3$ of maximum capacity with $1.6m^3$ of collector area was designed and constructed. The seasonal performance of solar dryer, including air-conditions, energy efficiency, and drying characteristics of 3cm-thick red pine and douglas-fir lumber was investigated. Also, the economic analysis was carried out. Annual average solar drying rate was about 2 times faster than air-drying rate with no significant difference in the amount of drying defects. But in initial drying stage air-drying rate in winter was much faster and those in spring and autumn were slightly slower than solar drying rate in each season. Annual average energy efficiency of solar-dryer and-collector was 25% and 57%, respectively. Fuel savings were over 50% at 15% of energy inflation rate and the payback period was estimated as 6.10 years at 30% of energy inflation rate.

  • PDF

Effects of Pruning on Timber Quality of Pinus koraiensis Grown in Korea

  • Chong, Song-Ho;Jung, Doo-Jin;Park, Byung-Su;Chun, Su Kyoung
    • Journal of the Korean Wood Science and Technology
    • /
    • v.31 no.6
    • /
    • pp.22-30
    • /
    • 2003
  • This study was performed to obtain the basic data for high quality timber production and efficient utilization by investigating the effect of pruning on timber quality of domestic plantation-grown Korean pine (Pinus koraiensis Sieb. et Zucc.). The results were summarized as follows:Dead knots (unsound knots) in the pruned logs occurred more at upper parts when compared with in non-pruned ones. The numbers of knots on surface in heavily pruned trees were less than those in non-pruned trees, but there was no significant difference in moderately pruned trees. The required period to reveal clear timber surface without defects after pruning increased proportionally with the increase of knot diameter. The yield of clear lumber production increased by about 10% after 14 years from moderate pruning. The quality grade of log improved with more pruning practices. Knots appeared the most important factor in lowering the log grades.

Heat Treatment of Dimension Lumber and Roundwood Used for Hanok Above $170^{\circ}C$

  • Kang, Ho-Yang
    • Journal of the Korea Furniture Society
    • /
    • v.21 no.6
    • /
    • pp.499-504
    • /
    • 2010
  • Korean traditional buildings, Hanok, are mostly constructed with dimension lumbers and roundwoods. They are hardly kiln-dried without severe defects, thus usually air-dried from some months to an year. Dimension lumbers and roundwoods were heat-treated above $170^{\circ}C$ and drying defects were examined. Temperature rising curves of all dimension timbers used for this study show one or two deflection points. The time when the temperature at 37.5mm depth reached at $100^{\circ}C$ for spruce dimension heat-treated at $170^{\circ}C$ was twice longer than that heat-treated at $190^{\circ}C$. There were many internal checks in roundwoods of $148mm{\Phi}$, while surface checks were apparently closed at the end of heat treatment. The drying time of $300{\times}300mm$ dimensions with 65mm hole was shorter than that without hole by half.

  • PDF

A Study on Quality Improvement of Exporting Wood Products I. Kiln Drying Schedules for Oak, Ramin and Meranti (수출용(輸出用) 목재가공품(木材加工品)의 품질개선(品質改善)에 관(關)한 연구(硏究) I. 참나무, 라민 및 나왕의 인공건조(人工乾燥) 스케줄)

  • Chung, Byung-Jae
    • Journal of the Korean Wood Science and Technology
    • /
    • v.2 no.1
    • /
    • pp.3-18
    • /
    • 1974
  • The exports of plywood are increasing annually and it has ranked first in the world market because of the high quality product and manufactured using mordern techniques. However, it is known that the exports of the other wood products, except plywood, is inactive because of their low quality. Accordingly, to increase the exports of various wood products investigations were carried out on kiln drying techniques to improve the quality of the wood. Wet wood should be kiln dried before use to prevent various drying defects such as distortion, shrinkage etc., which would develop after processing,:and also wet wood is not suitable for cutting, gluing and finishing. Therefore, the kiln drying properties of lumber from such species as oak, ramin and meranti which are used in large quantity for manufacturing exporting wood products have been studied. The results of the research are summarized as follows. (1) The end checks and the time for drying from initial moisture content of about 40 percent to 5 percent moisture content in ovendry were investigated as follows: (2) The kiln dried results, for 30mm stock, which are presented by using kiln schedule table 3 are as follows: (3) The kiln schedules for ramin, meranti and oak are given respectively as follows: Ramin kiln schedule: Table 17 and Table 18. Meranti schedule : Table 12. Oak schedule : Table 15.

  • PDF

Press-drying of Plantation Softwood Lumber (인공조림(人工造林) 침엽수재(針葉樹材)의 열판건조(熱板乾燥))

  • Jung, Hee-Suk;Lee, Nam-Ho;Yeo, Hwan-Myeong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.21 no.3
    • /
    • pp.61-66
    • /
    • 1993
  • 24mm-thick specimens from three species of plantation-grown softwood were press dried under two platen pressures of 1.75kgf/$cm^2$ and 3.50kgf/$cm^2$ to obtain drying information regarding to drying rate, thickness shrinkage and drying defects. The influence of platen pressure on drying fare in range of moisture content (30 to 10 percent) increased for pitch pine and larch, but reduced for korean white pine at higher pressure. Thickness shrinkage was increased at the higher pressure, and estimated thickness shrinkage at final MC of 10 percent became unrealistically greater for specimens containing higher final moisture content under the great influence of compressive strain. The effects of pressure on the amount of surface checks and honeycombing were different from species used. These species should have applied lower temperature than 177$^{\circ}C$ in this study to reduce surface checks and honeycombing.

  • PDF

Effect of Presteaming on the Drying Rate and Drying Defects of Quercus acutissima (증기전처리(蒸氣前處理)가 상수리나무판재(版材)의 건조속도(乾燥速度)와 건조결함(乾燥缺陷)에 미치는 영향(影響))

  • Lee, Hyoung-Woo;Jung, Hee-Suk
    • Journal of the Korean Wood Science and Technology
    • /
    • v.13 no.2
    • /
    • pp.3-13
    • /
    • 1985
  • This study was carried out to investigate the effects of presteaming on the drying rate and drying defects of 3 cm - thick Quercus acutissima. Specimens for presteaming were steamed green at $100^{\circ}C$ for 4 hours and then kiln-dried to 10 percent moisture, content with controls, using the kiln-drying schedule ($T_4-C_2$) recommended by Rasmussen. The results obtained were as follows: 1. Presteaming reduced drying time approximately 18 percent from 70 to 10 percent moisture content. 2. The effect of presteaming on surface checking was not significant. 3. Presteamed specimens showed the reduction in end checking compared with controls. 4. Percents of boards with collapse, cupping, and honeycomb of presteamed specimens were slightly lower than those of controls. 5. Dry lumber grade of presteamed specimens was better than that of controls. Percent of first grade boards of presteamed specimens was 20 percent higher than that of controls and percents of second and third grade boards of presteamed specimens were 15 and 5 percent lower than those of controls, respectively.

  • PDF

Distribution Characteristics of Bending Properties for Visual Graded Lumber of Japanese Larch (육안등급으로 구분된 낙엽송 제재목의 휨성능 분포 특성)

  • Lee, Jun Jae;Kim, Gwang Chul;Kim, Kwang Mo;Oh, Jung Kwon
    • Journal of the Korean Wood Science and Technology
    • /
    • v.31 no.5
    • /
    • pp.72-79
    • /
    • 2003
  • In reliability based design(RBD) method, the distribution characteristics of mechanical properties of material are basic input variable. Therefore, distribution type and parameters of mechanical properties should be determined accurately. Until now, the properties were derived from tests with small, clear specimens. However, the test conditions should emulate as nearly as possible the way in which the timber would be used in practice and the test results should, as closely as possible, reflect the structural end use conditions to which the timber products would be subjected. In this study, structural timbers (38mm by 140mm, 3.0m long) were graded by visual assessment of growth characteristics and defects. And then bending tests were conducted on 498 structural size timbers. For each grade, the distribution type and the parameters of mechanical properties were determined for each grade. For the determination of best-fit distribution type, comparing of square error between distribution types and KS test were conducted. Best-fit distribution type of bending strength(MOR) is weibull distribution for all grade. In case of MOE, normal distribution is best-fit.

A Study on Quality Improvement of Exporting Wood Products (수출용 목재 가공품의 품질개선에 관한 연구)

  • Chung, Byung-Jae;Lee, Eun-Chol;Oh, Kwang-In;Kim, Jong-Yeung
    • Journal of the Korean Wood Science and Technology
    • /
    • v.2 no.2
    • /
    • pp.22-24
    • /
    • 1974
  • 1. Object and importance of the research. The exports of plywood are increasing annually and it has ranked first in the world market because of the high quality product developed and manufactured using modern techniques. However, it is known that the exports of the other wood products, except plywood, is inactive because of their low quality. Accordingly, to increase the exports of various wood products investigations were carried out on kiln drying techniques to improve the quality of the wood. 2. The details and scope of the research Wet wood should be kiln dried before use to prevent various drying defects such as distortion, shrinkage etc, which would develop after processing, and also wet wood is not suitable for cutting, gluing and finishing. Therefore, the kiln drying properties of lumber from such species as Persimmon, Oak, Ramin and Meranti which are used in large quantity for manufacturing exporting wood products have been studied. Also the real state of kiln drying industry in Korea was investigated. 3. Results and proposal for practical use of the research 3. 1 Results of the research 3.1.1 The end checks and the time for drying from intial moisture content of about 40 percent to 5 percent moisture content in ovendry were investigated as Table 1. 3.1.2 The kiln dried results, for 30mm stock, which are presented by using kiln schedule Table 2 are as Table 3. 3.1.3 The kiln schedule for Persimmon which has a normal drying properties is given in Table 4. However, the persimmon which has easy checking properties should be air dried under a relative humidity of above 85% until reaching about 25 percent moisture content. 3.1.4 The kiln schedules for ramin, meranti and oak are given respectively as follows. Ramin kiln schedule ............ Table 5 and Table 6 Meranti kiln schedule ............ Table 7 Oak kiln schedule ............ Table 8 3.2 Proposal for practical use of the research Firms using the above species should be informed the results of the research so they can be used to preventing drying defects and shortening drying time.

  • PDF

On the manufacturing of WPC (Wood Plastic Composites) with Heat-Catalyst Polymerization (I) - On the characteristics of composites made from monomer Methyl MethacryIate and several commercial woods in Korea (가열(加熱)·촉매중합법(觸媒重合法)에 의한 목재(木材)·고분자복합체(高分子複合體) 제조(製造)(I) - MMA에 의한 한국산(韓國産) 주요목재(主要木材)의 복합체특성(複合體特性))

  • Cho, Nam-Seok;Jo, Jae-Myeong;Ahn, Won-Yong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.2 no.3
    • /
    • pp.3-16
    • /
    • 1974
  • One of the disadvantages of. wood and wood products is their hydroscopicity or dimensional instability. This is responsible for the loss of green volume of lumber as seasoning degrade. Dimensional stabilization is needed to substantially reduce seasoning defects and degrades and for increasing the serviceability of wood products. Recently, considerable world-wide attention has been drawn to the so-called Wood-Plastic Composites by irradiation-and heat-catalyst-polymerization methods and many research and developmental works have been reported. Wood-Plastic Composites are the new products having the superior mechanical and physical properties and the combinated characteristics of wood and plastic. The purpose of this experiment was to obtain the basic data for the improvement of wooden materials by manufacturing WPC. The species examined were Mulpurae-Namoo (Fraxinus, rhynchophylla), Sea-Namoo (Carpinus laxiflora), Cheungcheung-Namoo (Cornus controversa), Gorosae-Namoo (Acermono), Karae-Namoo(Juglans mandshurica) and Sanbud-Namoo (Prunus sargentii), used as blocks of type A ($3{\times}3{\times}40cm$) and type B ($5{\times}5{\times}60cm$), and were conditioned to about 10~11% moisture content before impregnation in materials humidity control room. Methyl methacrylate (MMA) as monomer and benzoyl peroxide (BPO) as initiator are used. The monomer containing BPO was impregnated into wood pieces in the vacuum system. After impregnation, the treated samples were polymerized with heat-catalyst methods. The immersed weights of monomer in woods are directly proportionated to the impregnation times. Monomer impregnation properties of Cheungcheung-Namoo, Mulpurae-Namoo and Seo-Namoo are relatively good, but in Karae-Namoo, it is very difficult to impregnate the monomer MMA. Fig. 3 shows the linear relation between polymer retentions in wood and polymerization times; that is, the polymer loadings are increasing with polymerization times. Furthermore species, moisture content, specific gravity and anatomical or conductible structure of wood, bulking solvents and monomers etc have effects on both of impregnation of monomer and polymer retention. Physical properties of treated materials are shown in table 3. Increasing rates of specific gravity are ranged 3 to 24% and volume swelling 3 to 10%. ASE is 20 to 46%, AE 14 to 50% and RWA 18 to 40%. Especially, the ASE in relation to absorption of liquid water increases approximately with increase of polymer content, although the bulking effect of the polymerization of monomer may also be influential. WPCs from Mulpurae-Namoo and Cheungcheung-Namoo have high dimensional stability, while its of Karae-Namoo and Seo-Namoo are-very low. Table 4 shows the mechanical properties of WPCs from 6 species. With its specific gravity and polymer loading increase, all mechanical properties are on the increase. Increasing rate of bending strength is 10 to 40%, compression strength 25 to 70%, ;impact bending absorbed energy 4 to 74% and tensile strength 18 to 56%. Mulpurae-Namoo and Cheungcheung-Namoo with high polymer content have considerable high increasing rate of strengths. But incase of Karae-Namoo with inferior monomer impregnation it is very low. Polymer retention in cell wall is 0.32 to 0.70%. Most of the polymer is accumulated in cell lumen. Effective. of polymer retention is 58.59% for Mulpurae-Namoo, 26.27% for Seo-Namoo, 47.98% for Cheungcheung-Namoo, 25.64% for Korosae-Namoo, 9.96% for Karae-Namoo and 25.84% for Sanbud-Namoo.