• 제목/요약/키워드: lead free piezoelectric

검색결과 189건 처리시간 0.022초

Two-Step 소결법을 통한 0.96(K0.456Na0.536)Nb0.95Sb0.05-0.04Bi0.5(Na0.82K0.18)0.5ZrO3 무연 압전 세라믹의 밀도 및 압전 특성 향상 (Enhancement of Density and Piezoelectric Properties of 0.96(K0.456Na0.536)Nb0.95Sb0.05-0.04Bi0.5(Na0.82K0.18)0.5ZrO3 Lead-Free Piezoelectric Ceramics through Two-Step Sintering Method)

  • 유일열;박상현;최성희;조경훈
    • 한국재료학회지
    • /
    • 제34권2호
    • /
    • pp.116-124
    • /
    • 2024
  • In this study, we investigated the microstructure and piezoelectric properties of 0.96(K0.456Na0.536)Nb0.95Sb0.05-0.04Bi0.5(Na0.82K0.18)0.5ZrO3 (KNNS-BNKZ) ceramics based on one-step and two-step sintering processes. One-step sintering led to significant abnormal grain (AG) growth at temperatures above 1,085 ℃. With increasing sintering temperature, piezoelectric and dielectric properties were enhanced, resulting in a high d33 = 506 pC/N for one-step specimen sintered at 1,100 ℃ (one-step 1,100 ℃ specimen). However, for one-step 1,115 ℃ specimen, a slight decrease in d33 was observed, emphasizing the importance of a high tetragonal (T) phase fraction for superior piezoelectric properties. Achieving a relative density above 84 % for samples sintered by the one-step sintering process was challenging. Conversely, two-step sintering significantly improved the relative density of KNNS-BNKZ ceramics up to 96 %, attributed to the control of AG nucleation in the first step and grain growth rate control in the second step. The quantity of AG nucleation was affected by the duration of the first step, determining the final microstructure. Despite having a lower T phase fraction than that of the one-step 1,100 ℃ specimen, the two-step specimen exhibited higher piezoelectric coefficients (d33 = 574 pC/N and kp = 0.5) than those of the one-step 1,100 ℃ specimen due to its higher relative density. Performance evaluation of magnetoelectric composite devices composed of one-step and two-step specimens showed that despite having a higher g33, the magnetoelectric composite with the one-step 1,100 ℃ specimen exhibited the lowest magnetoelectric voltage coefficient, due to its lowest kp. This study highlights the essential role of phase fraction and relative density in enhancing the performance of piezoelectric materials and devices, showcasing the effectiveness of the two-step sintering process for controlling the microstructure of ceramic materials containing volatile elements.

Pulsed Laser Deposition 방법으로 증착된 ZnSnO3 압전 박막의 성장과 특성 평가 (Fabrication and Properties of ZnSnO3 Piezoelectric Films Deposited by a Pulsed Laser Deposition)

  • 박병주;윤순길
    • 한국전기전자재료학회논문지
    • /
    • 제27권1호
    • /
    • pp.18-21
    • /
    • 2014
  • Because the Pb-based piezoelectric materials showed problems such as an environmental pollution. lead-free $O_3$ materials were studied in the present study. The $O_3$ thin films were deposited at $640^{\circ}C$ on $Pt/Ti/SiO_2$ substrate by pulsed laser deposition (PLD) and were annealed for 5 min at $750^{\circ}C$ using rapid thermal annealing (RTA) in nitrogen atmosphere. Samples annealed at $750^{\circ}C$ showed a smooth morphology and an improvement of the dielectric and leakage properties, as compared with as-grown samples. However, electrical properties of the $O_3$ thin films obtained in the present study should be improved for piezoelectric applications.

Columbite법으로 제조된 (Na,K,Li)(Nb,Ta,Sb)O3 세라믹스의 하소온도에 따른 유전 및 압전 특성 (Dielectric and Piezoelectric Properties of (Na,K,Li)(Nb,Ta,Sb)O3 Ceramics Manufactured Using Columbite Methods with Calcination Temperature)

  • 라철민;류주현
    • 한국전기전자재료학회논문지
    • /
    • 제29권3호
    • /
    • pp.159-163
    • /
    • 2016
  • In this paper, in order to develop optimum composition ceramics with excellent piezoelectric properties, $(Na_{0.525}K_{0.443}Li_{0.037})(Nb_{0.823}Sb_{0.08}Ta_{0.037})O_3+0.3wt%Bi_2O_3+0.4wt%Fe_2O_3$ lead-free piezoelectric ceramics were synthesized by conventional soild-state method. The calcination temperature of columbite precursors were fabricated at temperature range from $950^{\circ}C$ to $1,150^{\circ}C$ and sintering aids with low melting point were added to densify these ceramics. Effect of calcination temperature on dielectric and piezoelectric properties of ceramics were investigated. the ceramics with B-site columbite precursors at temperature of $1,100^{\circ}C$ obtained the optimal values of $d_{33}=272$ [pC/N], $k_p=0.51$, $Q_m=102$, ${\varepsilon}_r=978$.

MnO2 첨가가 0.985[Li0.04(Na0.545K0.46)0.96(Nb0.81Ta0.15Sb0.04)]O3+0.015KNbO3 세라믹스의 유전 및 압전 특성에 미치는 영향 (Effect of MnO2 Addition on Dielectric and Piezoelectric Properties of 0.985[Li0.04(Na0.545K0.46)0.96(Nb0.81Ta0.15Sb0.04)]O3 Ceramics)

  • 김유석;류주현
    • 한국전기전자재료학회논문지
    • /
    • 제27권6호
    • /
    • pp.361-366
    • /
    • 2014
  • $MnO_2$-doped $0.985[Li_{0.04}(Na_{0.545}K_{0.46})_{0.96}(Nb_{0.81}Ta_{0.15}Sb_{0.04})]O_3+0.015KNbO_3(0.985LNKNTS+0.015KNbO_3)$ lead-free ceramics were fabricated by conventional solid state method to develop excellent dielectric and piezoelectric properties. The result of X-ray diffraction patterns obviously indicated that all of the specimen has pure perovskite structure without secondary phase. In addition, orthorhombic phase and coexistance region of orthorhombic-tetragonal phase (MPB) were observed with amount of $MnO_2$. The optimal values of ${\rho}$=4.70 $g/cm^3$, $d_{33}=238$ pC/N, $k_P=0.46$, $Q_m=121$, ${\varepsilon}_r=849$, and $T_C=225^{\circ}C$ were obtained at 0.01 mol% $MnO_2$ doped $0.985LNKNTS+0.015KNbO_3$ ceramics sintered at $990^{\circ}C$ for 5 h, respectively. Hence, it was indicated that the suitable amount of $MnO_2$ could improve the electrical properties of $0.985[Li_{0.04}(Na_{0.545}K_{0.46})_{0.96}(Nb_{0.81}Ta_{0.15}Sb_{0.04})]O_3+0.015KNbO_3$ ceramics.

과 액상 형성에 의한 비납계 압전 (Na,K)NbO3-Ba(Cu,Nb)O3 결정립의 비정상 성장 거동 및 전기적 특성 (Fast Abnormal Grain Growth Behavior and Electric Properties of Lead-Free Piezoelectric (K,Na)NbO3-Ba(Cu,Nb)O3 Grains through Transient Liquid Phase)

  • 임지호;이주승;이승희;정한보;박춘길;안철우;유일열;조경훈;정대용
    • 한국재료학회지
    • /
    • 제29권4호
    • /
    • pp.205-210
    • /
    • 2019
  • $Pb(Zr,Ti)O_3$ (PZT) is used for the various piezoelectric devices owing to its high piezoelectric properties. However, lead (Pb), which is contained in PZT, causes various environment contaminations. $(K,Na)NbO_3$ (NKN) is the most well-known candidate for a lead-free composition to replace PZT. A single crystal has excellent piezoelectric-properties and its properties can be changed by changing the orientation direction. It is hard to fabricate a NKN single crystal due to the sodium and potassium. Thus, $(Na,K)NbO_3-Ba(Cu,Nb)O_3$ (NKN-BCuN) is chosen to fabricate the single crystal with relative ease. NKN-BCuN pellets consist of two parts, yellow single crystals and gray poly-crystals that contain copper. The area that has a large amount of copper particles may melt at low temperature but not the other areas. The liquid phase may be responsible for the abnormal grain growth in NKN-BCuN ceramics. The dielectric constant and tan ${\delta}$ are measured to be 684 and 0.036 at 1 kHz in NKN-BCuN, respectively. The coercive field and remnant polarization are 14 kV/cm and $20{\mu}C/cm^2$.

Effect of Ta-Substitution on the Ferroelectric and Piezoelectric Properties of Bi0.5/(Na0.82K0.18)0.5TiO3 Ceramics

  • Do, Nam-Binh;Lee, Han-Bok;Yoon, Chang-Ho;Kang, Jin-Kyu;Lee, Jae-Shin;Kim, Ill-Won
    • Transactions on Electrical and Electronic Materials
    • /
    • 제12권2호
    • /
    • pp.64-67
    • /
    • 2011
  • The effect of Ta substitution on the crystal structure, ferroelectric, and piezoelectric properties of $Bi_{0.5}(Na_{0.82}K_{0.18})_{0.5}Ti_{1-x}Ta_xO_3$ ceramics has been investigated. The Ta doping resulted in a transition from coexistence of ferroelectric tetragonal and rhombohedral phases to an electrostrictive pseudocubic phase, leading to degradations of the remnant polarization, coercive field, and piezoelectric coefficient $d_{33}$. However, the electricfield-induced strain was significantly enhanced by the Ta substitution-induced phase transition and reached a highest value of $S_{max}/E_{max}$ = 566 pm/V under an applied electric field 6 kV/mm when 2% Ta was substituted on Ti sites. The abnormal enhancement in strain was attributed to the pseudocubic phase with high electrostrictive constants.

피에조를 이용한 초소형 단일 솔더볼 연결부의 전단 시험장치 개발 (Development of a Shear Testing Machine for a Miniature Single Solder Ball Joint using Piezoelectric Loading Device)

  • 권용상;고국종;김호경
    • Tribology and Lubricants
    • /
    • 제26권1호
    • /
    • pp.44-51
    • /
    • 2010
  • A miniature shear testing machine was designed and developed, adopting a piezoelectric actuator with mechanical advantage using 4 levers in order to investigate shear behavior of a small solder ball. The final output displacement was initially expected to be 2.88 mm without load resistance, considering the lever ratio of 24 and the piezo displacement of 0.12 mm with an exciting voltage of 10 V. However, the final plunger displacement ${\Delta}{\upsilon}$ can be expected as ${\Delta}{\upsilon}=2.88-3.04{\times}10^{-4}F$ as a function of piezoelectric force F due to the stiffness of various levers and connectors and piezo actuator. The shear behavior of lead-free solder ball in diameter of $760{\mu}m$ was successfully investigated in a speed range of 2 mm/s~0.0035 mm/s using this designed device.

MnO2 as an Effective Sintering Aid for Enhancing Piezoelectric Properties of (K,Na)NbO3 Ceramics

  • Jeong, Seong-Kyu;Hong, In-Ki;Do, Nam-Binh;Tran, Vu Diem Ngoc;Cho, Seong-Youl;Taib, Weon Pil;Lee, Jae-Shin
    • 한국분말재료학회지
    • /
    • 제17권5호
    • /
    • pp.399-403
    • /
    • 2010
  • The effects of $MnO_2$ doping on the crystal structure, ferroelectric, and piezoelectric properties of (K,Na)$NbO_3$ (KNN) ceramics have been investigated. $MnO_2$ was found to be effective in enhancing the densification and grain growth during sintering. X-ray diffraction analysis indicated that Mn ions substituted B-site Nb ions up to 2 mol%, however, further doping induced unwanted secondary phases. In comparison with undoped KNN ceramics, the well developed microstructure and the substitution to B-sites in 2 mol% Mn-doped KNN ceramics resulted in significant improvements in both piezoelectric coupling coefficient and electromechanical quality factor.

저온소결 (K0.5Na0.5)NbO3 세라믹스의 분극전계에 따른 압전 및 유전특성 (Piezoelectric and Dielectric Properties of Low Temperature Sintering (K0.5Na0.5)NbO3 Ceramics with the Variation of Poling Electric Field)

  • 이일하;류주현;정영호
    • 한국전기전자재료학회논문지
    • /
    • 제21권11호
    • /
    • pp.1000-1004
    • /
    • 2008
  • In this paper, the influences of poling electric field on piezoelectric properties of $0.95(K_{0.5}Na_{0.5})NbO_3$-$0.05Li(Sb_{0.8}Nb_{0.2})O_3$ (abbreviated as KNN-LSN) ceramics were investigated. The specimens was sintered at sintering temperature of $1050^{\circ}C$. They showed orthorhombic phase structure without secondary phase. Electromechanical coupling factor (kp), dielectric and piezoelectric constant($d_{33}$) increased with poling electric field. However, mechanical quality factor (Qm) decreased. Take into account of poling conditions and piezoelectric properties of KNN-LSN ceramics, the optimum poling condition for KNN-LSN ceramics was poling electric field of 4.5 kV/mm. At the time, kp of 0.458, Qm of 43.97, $d_{33}$ of 278 pC/N, and dielectric constant of 1079 were shown, respectively.

Structural, Dielectric and Field-Induced Strain Properties of La-Modified Bi1/2Na1/2TiO3-BaTiO3-SrZrO3 Ceramics

  • Hussain, Ali;Maqbool, Adnan;Malik, Rizwan Ahmed;Zaman, Arif;Lee, Jae Hong;Song, Tae Kwon;Lee, Jae Hyun;Kim, Won Jeong;Kim, Myong Ho
    • 한국재료학회지
    • /
    • 제25권10호
    • /
    • pp.566-570
    • /
    • 2015
  • $Bi_{0.5}Na_{0.5}TiO_3$ (BNT) based ceramics are considered potential lead-free alternatives for $Pb(Zr,Ti)O_3$(PZT) based ceramics in various applications such as sensors, actuators and transducers. However, BNT-based ceramics have lower electromechanical performance as compared with PZT based ceramics. Therefore, in this work, lead-free bulk $0.99[(Bi_{0.5}Na_{0.5})_{0.935}Ba_{0.065}]_{(1-x)}La_xTiO_3-0.01SrZO_3$ (BNBTLax-SZ, with x = 0, 0.01, 0.02) ceramics were synthesized by a conventional solid state reaction The crystal structure, dielectric response, degree of diffuseness and electric-field-induced strain properties were investigated as a function of different La concentrations. All samples were crystallized into a single phase perovskite structure. The temperature dependent dielectric response of La-modified BNBT-SZ ceramics showed lower dielectric response and improved field-induced strain response. The field induced strain increased from 0.17%_for pure BNBT-SZ to 0.38 % for 1 mol.% La-modified BNBT-SZ ceramics at an applied electric field of 6 kV/mm. These results show that La-modified BNBT-SZ ceramic system is expected to be a new candidate material for lead-free electronic devices.