• Title/Summary/Keyword: leaching stability

Search Result 54, Processing Time 0.036 seconds

Evaluation of Lead, Copper, Cadmium, and Mercury Species in the Leachate of Steel Making Slag by Seawater (해수에 의한 제강 슬래그의 납, 구리, 카드뮴 및 수은 화합물의 용출특성 평가)

  • Lee, Han-Kook;Lee, Dong-Hoon
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.27 no.1
    • /
    • pp.75-84
    • /
    • 2005
  • The aim of this study is to evaluate the leaching characteristics of lead, copper, cadmium, and mercury from steel making slag by seawater. To demonstrate the leaching characteristics of heavy metals from steel making slag by seawater, it was carried to various leaching tests such as regular leaching tests, liquid/sold(LS) leaching test and pH static test. From the leachability of $Pb^{+2},\;Cu^{+2},\;and\;Cd^{+2}$ from steel making slag in pH static test, it is distinguished between distilled water and seawater. With distilled water, it is very low between pH 7-8 and pH 11-12. On the other hands, with the seawater, its leaching is higher than that of distilled water. In particular, concentration of $Hg^{+2}$ leached from slag by seawater is lower than that of distilled water. Meanwhile, we found that the heavy metals from steel making slag would be dissolved and precipitated using geochemcial equilibrium program such as visual minteq. Lead and copper leached from steel making slag with seawater were dissolved nearly in the range of pH 11-12, but in the range of pH 7-10 those were precipitated about 90%. And cadmium leached from steel making slag with seawater were dissolved completely. On pH static test with distilled water, lead leached from steel making slag seemed to be similar to pH static test with seawater. However, copper and cadmium leached from steel making slag were dissolved. In general, the species of lead leached from steel making slag were formed mainly of $PbCl^+,\;PbSO_4$, the species of copper were formed mainly of $CuSO_4,\;CuCO_3$, the species of cadmium were formed mainly of $CdCl^+,\;CdSO_4$ due to being sorbed with the anions($Cl^-,\;CO_3^{-2},\;SO_4^{-2}$) of the seawater. Both pH static test with seawater and distilled water, it is not in the case of the mercury. Most of mercury leached from steel making slag was precipitated(SI=0). Because the decreasing of $Hg^{+2}$ concentrations depends ferociously on the variation of chloride($Cl^-$) existed in the seawater. $Hg^{+2}$ leached from steel making slag could be sorbed strongly with chloride($Cl^-$) compared of carbonate($CO_3^{-2}$) and sulfate($SO_4^{-2}$) in the seawater. On the basis of that result, we found that the species of mercury was formed of calomel($Hg_2Cl_2$) as one of finite solid. Due to forming a calomel($Hg_2Cl_2$) in the seawater, the stability of mercury species by steel making slag should be higher than those of lead, copper, and cadmium species. Regarding the results stated above, we postulated that the steel making slag could be recycled to sea aggregates due to being distinguishing leachability of heavy metals($Pb^{+2},\;Cu^{+2},\;Cd^{+2},\;and\;Hg^{+2}$) between leaching tests by distilled water and seawater.

Manufacturing of Ultra-light Ceramsite from Slate Wastes in Shangri-la, China

  • Li, Zhen;Zhang, Haodong;Zhao, Pengshan;He, Xiaoyun;Duan, Xiaowei
    • Journal of the Korean Ceramic Society
    • /
    • v.55 no.1
    • /
    • pp.36-43
    • /
    • 2018
  • The physical and chemical analyses of mineral waste such as moisture content, water absorption, freezing-thawing resisting sexual, chemical composition and crystal structure were investigated. In the technological process of crushing, screening, molding, drying, preheating, sintering and cooling, many parameters were changed to eliminate the influence of freeze thaw stability and the ball billets were processed into slate ceramsites eventually. Adopting orthogonal experiment and range analysis, the optimal technology parameters were confirmed as preheating temperature of $300^{\circ}C$ for 25 minutes and sintering temperature of $1230^{\circ}C$ for 20 minutes. Slate wastes in Shangri-la could foam and expand without any additive. The ultra-light ceramsite could be directly used as building aggregate, since the analysis results of its leaching toxicity were eligible. Besides, effects of sintering temperature on physical property and crystal phase were also explored in this study.

A Study on Performance Improvement of Glucose Sensor Adopting a Catalyst Using New Cross Liker (새로운 가교제를 적용한 촉매를 이용한 글루코스 센서의 성능향상 연구)

  • Chung, Yongjin;Kwon, Yongchai
    • Korean Chemical Engineering Research
    • /
    • v.53 no.6
    • /
    • pp.802-807
    • /
    • 2015
  • In this study, we synthesized a new biocatalyst consisting of glucose oxidase (GOx), polyethyleneimine (PEI) and carbon nanotube (CNT) with addition of terephthalaldehyde (TPA) (TPA/GOx/PEI/CNT) for fabrication of glucose sensor that shows improved sensing ability and stability compared with that using other biocatalysts. Main bonding of the new TPA/GOx/PEI/CNT catalyst is formed by Aldol condensation reaction of functional end groups between GOx/PEI and TPA. Such formed bonding structure promotes oxidation reaction of glucose. Catalytic activity of TPA/GOx/PEI/CNT is evaluated quantitatively by electrochemical measurements. As a result of that, large sensitivity value of $41{\mu}Acm^{-2}mM^{-1}$ is gained. Regarding biosensor stability of TPA/GOx/PEI/CNT catalyst, covalent bonding formed between GOx/PEI and TPA prevents GOx molecules from becoming leaching-out and contributes improvement in biosensor stability. With estimation of the biosensor stability, it is found that the TPA/GOx/PEI/CNT catalyst keeps 94.6% of its initial activity even after three weeks.

A Study on the Development of Rapidly Hardening Grouting Method for the Effective Filling in the Underground Cavity (지하공동의 효율적 충전을 위한 급결 충전 그라우트공법개발에 관한 연구)

  • Kim, Soo-Lo;Kim, Tae-Heok;Shin, Dong-Chun;Kwon, Hyun-Ho
    • Tunnel and Underground Space
    • /
    • v.19 no.6
    • /
    • pp.534-544
    • /
    • 2009
  • The collapse of the underground cavity can cause the abrupt local subsidence of the ground surface. It can be hazardous to the stability of road and building for human activity. Therefore it is necessary to develop reinforcement methods for the filling of the underground cavity. This study was executed to improve the material quality and systems to fill the calcium-aluminate mineral $(C_{12}A_7)$ environmentally, and minimize the loss of filling materials for the steep underground cavity. Filling material which was developed in this study is composed of rapid hardening material and additives. The developed material had rapid hardening and non-separation ability in the water cavity condition, so it made the effective underground dam in the cavity with prevention of material loss when it was poured in the water cavity. Results of heavy metal leaching test for environmental assessment showed that it was environmentally suiTable material for the filling in the mine cavity.

Conducting Polymer-Silica Composites for Immobilization of Enzymes

  • Kwon, Sang-Woon;Jeong, Bo-Ock;Lee, Eun-Hee;Kim, Yong-Shin;Jung, Yong-Ju
    • Bulletin of the Korean Chemical Society
    • /
    • v.33 no.5
    • /
    • pp.1593-1596
    • /
    • 2012
  • A new enzyme immobilization method based on hydrophobic interaction between supporting material and enzyme has been successfully developed. The efficacy of the new technique has been investigated by loading a horse radish peroxidase (HRP) enzyme on the surface of conducting polymer-silica composites and by measuring the enzyme activity and leaching property of HRP loaded within polymer-silica composites. The immobilized HRP enzyme showed activity profiles similar to that of free HRP in phosphate buffer (pH 6). Above all, HRP adsorbed on the polymer-silica composites has showed excellent stability over 10 days, compared to HRP adsorbed on the pristine silica. It is thought that with appropriate optimization works, the present method would be used as a cost-effective and facile route for the immobilization of biomolecules.

Manufacture of the Non-Sintered Aggregate Using the Industrial By-products and the Municipal Waste Incineration Fly-Ash (도시 쓰레기 소각 비산재와 산업부산물을 이용한 비소성 인공골재의 제조)

  • 김대규;윤성진;문경주;소양섭
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2002.10a
    • /
    • pp.69-74
    • /
    • 2002
  • Incineration method of municipal solid waste is the general method for reduction it's quantity and weight. Municipal solid waste incineration ash is classified two general types of ash : fly ash((MWFA) and bottom ash(MWBA)). MWFA containing a high degree heavy-metal may give rise to a serious environmental trouble. Therefore, this study was carried out to examine utilization of fly ash. In this study, we tried to find the recycling method of fly ash as a environmental-friendly artificial aggregate. The artificial aggregate using fly ash was tested for the various aspects, including physical properties and environmental stability. The qualities of artificial aggregate are similar to it of lightweight aggregate, and the heavy metal leaching concentration are very lower than a limitation of KSLT and EP.

  • PDF

Solidification/stabilization of Hazardous Wastes Using Cementitious Materials(III) (특수시멘트 고형화재를 이용한 지정폐기물의 고형화/안정화(III))

  • Lim, Chae-Yong;Ku, Ki-Dae;Um, Tae-Sun;Lee, Jong-Ryul;Choi, Long;Oh, Byoung-Hwan
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.05a
    • /
    • pp.289-294
    • /
    • 2001
  • This study concerns the cement-solidification/stabilization of the waste with high concentration heavy metals. Compressive strength and leaching test of heavy metals were evaluated for ing types of cements and the effect of the additives of Hauyne clinker and slag were also cussed. Using ordinary portland cement, rapid hardening portland cement and the cement with additives solidification materials, it shows that the strength and stability of concrete is satisfactory and superiority is in the order of rapid hardening portland cement > the cement with additives > nary portland cements.

  • PDF

Properties of artificial lightweight aggregates made from waste sludge

  • Chiou, I.J.;Chen, C.H.
    • Computers and Concrete
    • /
    • v.8 no.6
    • /
    • pp.617-629
    • /
    • 2011
  • In this investigation, reservoir sediment and municipal sewage sludge were sintered to form the artificial lightweight aggregates. The sintered aggregates were compared with the commercialized lightweight aggregates to in terms of potential alkali-silica reactivity and chemical stability based on analyses of their physical and chemical properties, leaching of heavy metal, alkali-silica reactivity, crystal phase species and microstructure. Experimental results demonstrated that the degree of sintering of an aggregate affected the chemical resistance more strongly than did its chemical composition. According to ASTM C289-94, all potential alkali-silica reactivity of artificial lightweight aggregates were in the harmless zone, while the potential reactivity of artificial lightweight aggregates made from reservoir sediment and municipal sewage sludge were much lower than those of traditional lightweight aggregates.

Influence of Frit Surface on the Transmittance of Transparent Dielectric in PDP

  • Kim, Hyung-Sun;Cha, Myung-Lyoung
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2005.07b
    • /
    • pp.828-831
    • /
    • 2005
  • Producing high transparency dielectric is still one of the most important subjects in the PDP process for improving luminous efficiency. It has been reported by many workers that transparency is improved by controlling the composition of the frit, the frit size and distribution, and the firing atmosphere. To understand the mechanism of discoloration of frit, $Bi_2O_3$ and $B_2O_3$ glasses were used for a leaching test using water and alcohol solution in milling. As a result, the frit prepared by wet milling had lower chemical durability than that prepared by dry milling. The leached layer around the frit showed high stability for heat treatment because the frit surface was covered with hydroxides or hydrates which was resulted from a reaction between the frit and the solution during milling.

  • PDF

Fabrication of Metallic Tantalum Powder by Magnesium-gas Reduction of Tantalum Oxide (탄탈륨 산화물의 마그네슘 가스환원에 의한 탄탈륨 금속분말 제조)

  • Lee, Dong-Won
    • Journal of Powder Materials
    • /
    • v.25 no.5
    • /
    • pp.390-394
    • /
    • 2018
  • Metallic tantalum powder is manufactured by reducing tantalum oxide ($Ta_2O_5$) with magnesium gas at 1,073-1,223 K in a reactor under argon gas. The high thermodynamic stability of magnesium oxide makes the reduction reaction from tantalum oxide into tantalum powder possible. The microstructure after the reduction reaction has the form of a mixture of tantalum and magnesium oxide, and the latter could be entirely eliminated by dissolving in weak hydrochloric acid. The powder size in SEM microstructure for the tantalum powder increases after acid leaching in the range of 50-300 nm, and its internal crystallite sizes are observed to be 11.5 to 24.7 nm with increasing reduction temperatures. Moreover, the optimized reduction temperature is found to be 1,173 K as the minimum oxygen concentration is approximately 1.3 wt.%.