The comparison of the fatigue crack initiation life in a notch (노치부의 피로균열발생 수명 비교)

  • Kim, S.H.;Bae, S.I.;Ham, K.C.;Song, J.I.
    • Proceedings of the KSME Conference
    • /
    • 2001.06a
    • /
    • pp.217-222
    • /
    • 2001
  • For the life evaluating of notched members, it is the best way that performing the real fatigue test of structure containing notch. But this method required generally much times and costs to evaluate fatigue life. So, generally we use the modified S-N curve or several methods to predict fatigue life. In this study, crack initiation life was evaluated by fatigue testing the SAE keyhole specimen and smooth specimen made of Al 7075-T6 alloys using the constant load then obtained S-N curve of smooth specimen and P-N curve of SAE keyhole specimen. And, fatigue lives of keyhole specimen are predicted using some life prediction methods (Nominal range I method, Nominal range II method, FEM analysis) for investigating experimented results, and that were compared with experimental data. Predicted fatigue lives by FEM analysis were corresponded with experimental data between 1/3times and 3times on the whole, and predicted fatigue lives using modified S-N curve (Nominal range I method, Nominal range II method) were nonconservative compared with that of FEM analysis.

  • PDF

Investigation the fracture behavior of high-density polyethylene PE80 weakened by inclined U-notch with end hole

  • Soltaninezhad, Saeed;Goharrizi, Ataallah Soltani;Salavati, Hadi
    • Structural Engineering and Mechanics
    • /
    • v.74 no.5
    • /
    • pp.601-609
    • /
    • 2020
  • In this article, the Strain Energy Density (SED) averaged over a well-defined control volume at a notch edge was applied in combination with the Equivalent Material Concept (EMC) to assess the fracture behaviors of some keyhole-notched specimens made of a High-Density Polyethylene (HDPE-PE80) material under mixed-mode loading conditions. An experimental program was performed and 54 new experimental data were totally provided. Additionally, different loading mode ratios were regarded by changing the inclination angles of the notches with respect to the applied load directions. The results obtained from the determined criteria were in good agreement with those of the experimental data.

Fatigue Properties of Rail Steel Under Constant Amplitude Loading and Variable Amplitude Loading (일정 및 변동하중하의 레일강의 피로특성)

  • Kim, Cheol-Su;Kim, Jeong-Gyu
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.25 no.4
    • /
    • pp.654-661
    • /
    • 2001
  • In this study, fatigue growth behavior of the transverse crack, which was the most dangerous damage among the various types of rail defects, was investigated using the notched keyhole specimen under constant amplitude loadings. Fatigue limit of smooth specimen in rail steel at R=0 was 110MPa, and the fatigue crack initiation life in the region of the low stress amplitude (ie. long life) occupied the major portion of the total fatigue life. The fatigue strength under variable amplitude loading was converted to the equivalent fatigue strength based upon. Miners rule, which was estimated approximately 9% lower than that under constant amplitude loading. Also, in the low ΔK(sub)rms region ($\leq$21MPa√m), fatigue crack growth rate (da/dN) under constant amplitude loading was higher than that under variable amplitude loading, whereas the tendency was reversed in the high ΔK(sub)rms region. It is believed that this behavior is due to the transition of fracture appearance.

Semicircular Horizontal Approach in Breast Reduction: Clinical Experience in 38 Cases

  • Shin, Hee Su;Lee, Yong Hae;Jung, Sung Gyun;Lee, Doo Hyung;Roe, Young;Cha, Jong Hyun
    • Archives of Plastic Surgery
    • /
    • v.42 no.4
    • /
    • pp.446-452
    • /
    • 2015
  • Background Various techniques are used for performing breast reduction. Wise-pattern and vertical scar techniques are the most commonly employed approaches. However, a vertical scar in the mid-lower breast is prominent and aesthetically less pleasant. In contrast, a semicircular horizontal approach does not leave a vertical scar in the mid breast and transverse scars can be hidden in the inframammary fold. In this paper, we describe the experiences and results of semicircular horizontal breast reductions performed by a single surgeon. Methods Between September 1996 and October 2013, our senior author used this technique in 38 cases in the US and at our institution. We used a superiorly based semicircular incision, where the upper skin paddle was pulled down to the inframammary fold with the nipple-areola complex pulled through the keyhole. Results The average total reduction per breast was 584 g, ranging from 286 to 794 g. The inferior longitudinal pedicle was used in all the cases. The average reduction of the distance from the sternal notch to the nipple was 13 cm (range, 11-15 cm). The mean decrease in the bra cup size was 1.7 cup sizes (range, a decrease of 1 to 3). We obtained very satisfactory results with a less noticeable scar, no complication such as necrosis of the nipple or the skin flap, wound infection, aseptic necrosis of the breast tissue, or wound dehiscence. One patient had a small hematoma that resolved spontaneously. Conclusions This technique is straightforward and easy to learn, and offers a safe, effective, and predictable way for treating mammary hypertrophy.