• Title/Summary/Keyword: joint thickness

Search Result 686, Processing Time 0.026 seconds

Static strength of collar-plate reinforced tubular T-joints under axial loading

  • Shao, Yong-Bo
    • Steel and Composite Structures
    • /
    • v.21 no.2
    • /
    • pp.323-342
    • /
    • 2016
  • To study the effect of collar-plate reinforcement on the static strength of tubular T-joints under axial loading, fundamental research work is carried out from both experimental test and finite element (FE) simulation. Through experimental tests on 7 collar-plate reinforced and 7 corresponding un-reinforced tubular T-joints under axial loading, the reinforcing efficiency is investigated. Thereafter, the static strengths of the above 14 models are analyzed by using FE method, and it is found that the numerical results agree reasonably well with the experimental data to prove the accuracy of the presented FE model. Additionally, a parametric study is conducted to analyze the effect of some geometrical parameters, i.e., the brace-to-chord diameter ratio ${\beta}$, the chord diameter-to-chord wall thickness ratio $2{\gamma}$, collar-plate thickness to chord wall thickness ratio ${\tau}_c$, and collar-plate length to brace diameter ratio $l_c/d_1$, on the static strength of a tubular T-joint. The parametric study shows that the static strength can be greatly improved by increasing the collar-plate thickness to chord wall thickness ratio ${\tau}_c$ and the collar-plate length to brace diameter ratio $l_c/d_1$. Based on the numerical results, parametric equations are obtained from curving fitting technique to estimate the static strength of a tubular T-joint with collar-plate reinforcement under axial loading, and the accuracy of these equations is also evaluated from error analysis.

The Static Strength Analysis of Prying Action for T-flange Shape Structure Using F10T High Strength Bolt (F10T 고장력 볼트를 이용한 T-형 플랜지형 구조물의 Prying Action에 따른 정적강도 해석)

  • Park, Myung-Kyun;Lee, Joong-Won;Koo, Bon-Sung
    • Journal of the Korean Society of Safety
    • /
    • v.23 no.4
    • /
    • pp.19-24
    • /
    • 2008
  • This paper presents and discusses the experimental results on the F10T high strength bolts used in the T-flange joint structure. The experimental works were carried out for the parameters which are flange web thickness, the distance between bolts, prying ratio. The results show that the working stress imposed to bolts decreases as the flange web thickness increases on the other hand the imposed stress to the bolts increases as the distance between two bolts increases. In other words the strength of the T-flange joint increased as the web flange thickness increases and the distance between two bolts decreases. The prying ratio is increased as the distance between two bolts increases and as the flange web thickness decreases However, the degree of stress decrease in flange thickness variation is not that high as the distance variation between two bolts. Finally the equation for predicting the failure stress in T-flange joint structure using F10T high strength bolts was suggested.

Effect of Thoracic Joint Mobilization and Breathing Exercise on The Thickness of The Diaphragm, Expansion of The Chest, Respiratory Function, and Endurance in Chronic Stroke Patients

  • Hyunmin Moon;Jang-hoon Shin;Wan-hee Lee
    • Physical Therapy Rehabilitation Science
    • /
    • v.12 no.3
    • /
    • pp.278-292
    • /
    • 2023
  • Objective: This study was performed to investigate the effects of thoracic joint mobilization and breathing exercises on diaphragmatic thickness, chest expansion, respiratory function, and endurance in patients with chronic stroke. Design: Randomized controlled trial Methods: The study included 24 chronic stroke patients who were randomly divided into two groups. The experimental group (12 people) performed 15 minutes of thoracic joint mobility exercises and 15 minutes of breathing exercises, three times a week for 6 weeks, 30 minutes each time. The control group (12 people) received 15 minutes of conservative physical therapy and 15 minutes of breathing exercises, 3 times a week for 6 weeks, 30 minutes per session, the same as the experimental group. The experimental and control groups performed the same breathing exercises. To assess training effectiveness, changes in diaphragm thickness, chest expansion, respiratory function, and endurance were measured. Results: As a result, the experimental group exhibited significant improvements in diaphragm thickness, chest expansion, and respiratory function. The endurance mode also displayed significant enhancement (p<0.05), a finding consistent with the control group. However, the experimental group displayed more substantial improvements in non-affected diaphragm thickness and thoracic expansion compared to the control group (p<0.05). Conclusions: Drawing from these findings, breathing exercise which combine thoracic mobilization, will be actively utilized in addition to physical therapy interventions in clinical trials as an effective intervention method.

Ultrasonographic evaluation of the masseter muscle in patients with temporomandibular joint degeneration

  • Busra Arikan;Numan Dedeoglu;Aydin Keskinruzgar
    • Imaging Science in Dentistry
    • /
    • v.53 no.4
    • /
    • pp.355-363
    • /
    • 2023
  • Purpose: Sonographic elastography can be used to evaluate the hardness of muscle tissue through the application of compression. Strain elastography gauges hardness through the comparison of echo sets before and after compression. This study utilized ultrasonography to measure the thickness and hardness of the masseter muscle in individuals with temporomandibular joint(TMJ) osteoarthritis. Materials and Methods: This study included 40 patients who presented with joint pain and were diagnosed with TMJ osteoarthritis via diagnostic cone-beam computed tomography, along with 40 healthy individuals. The thickness and hardness of each individual's masseter muscle were evaluated both at rest and at maximum bite using ultrasonography. The Mann-Whitney U test and the chi-square test were employed for statistical analysis, with the significance level set at P<0.05. Results: The mean thickness of the resting masseter muscle was 0.91 cm in patients with osteoarthritis, versus 1.00 cm in healthy individuals. The mean thickness of the masseter muscle at maximum bite was 1.28 cm in osteoarthritis patients and 1.36 cm in healthy individuals. The mean masseter elasticity index ratio at maximum bite was 4.51 in patients with osteoarthritis and 3.16 in healthy controls. Significant differences were observed between patients with osteoarthritis and healthy controls in both the masseter muscle thickness and the masseter elasticity index ratio, at rest and at maximum bite (P<0.05). Conclusion: The thickness of the masseter muscle in patients with TMJ osteoarthritis was less than that in healthy controls. Additionally, the hardness of the masseter muscle was greater in patients with TMJ osteoarthritis.

Connections of sleeve joint purlin system

  • Tan, S.H.;Seah, L.K.;Li, Y.
    • Structural Engineering and Mechanics
    • /
    • v.13 no.1
    • /
    • pp.1-16
    • /
    • 2002
  • This paper presents the findings of an investigation carried out to determine the most appropriate connections, in terms of rotational stiffness, to use for the optimum design of cold-formed Zed section sleeve joint purlin system. Experiments and parametric studies were conducted to investigate the effects of geometric variables on the behavior of the sleeve-purlin and cleat-purlin connections of the sleeve joint purlin system. The variables considered were purlin size and thickness, sleeve size, thickness, length and bolt position. The test results were used to verify the empirical expressions, developed herein, employed to determine the rotational stiffness of connections. With the predicted connection stiffness, the most suitable sleeve-purlin and cleat-purlin connections can be selected so as to produce an optimum condition for the sleeve joint purlin system.

Fatigue Strength Evaluation on the IB-Type Spot Welded Lap Joint of 304 Stainless Steel Part 2 : Strain energy Density (304 스테인레스 박강판 IB형 용접이음재의 피로강도 평가 Part 2 : 변형에너지 밀도에 의한 평가)

  • 손일선;오세빈;배동호
    • Journal of Welding and Joining
    • /
    • v.17 no.6
    • /
    • pp.32-37
    • /
    • 1999
  • Since stainless steel plates have good mechanical properties, weldability, appearance and resistance of corrosion, these are traditionally used for vehicles such as the bus and the train. And they are mainly fabricated by spot welding. But fatigue strength of their spot welded joint is considerably influenced by welding conditions as well as geometrical factors. Thus a reasonable and systematic criterion for long life design of spot welded body structure must be established. In this report, strain energy density was analyzed by using 3-dimensional finite element model about the IB-type spot welded lap joint under tension-shear load. Fatigue tests were conducted on them having various thickness, joint angle, lapped length and width. From their results, it was found that fatigue strength of the IB-type spot welded lap joints could be effectively and systematically rearranged by strain energy density at the edge of nugget.

  • PDF

Variation of Welded-Joint Tensile Strength of GMA Welded Accelerated-Cooled Steel (가속냉각강 GMAW 용접이음부의 강도 변화)

  • 방국숙;정성욱
    • Journal of Welding and Joining
    • /
    • v.18 no.6
    • /
    • pp.83-88
    • /
    • 2000
  • Variation of welded-joint hardness and tensile strength of a accelerated-cooled fine-grained ferritic-pearlitic steel with heat input was investigated. In a weld heat-affected zone, a softened zone was formed and it had lower hardness than that of a base metal. While the width of a softened zone increased continuously with an increase of heat input up to 100kJ/cm. the minimum hardness in a softned zone was almost constant after a continuos decrease up to 60KJ/cm. Because of a softened zone, the welded-joint was fractured in the HAZ and its maximum reduction of tensile strength was about 20%. Measured welded-joint tensile strength and calculated minimum tensile strength in a welded-joint was almost same, which means that the plastic restraint of a softened zone did not occur in this experiment. It is believed that as a softened zone width-to-specimen thickness ratio is as high as 2~6 in this experiment, the plastic restraint effect does not occur. Theoretical analysis shows that the plastic restraint effect occurs only when the ratio is below 0.5.

  • PDF

Intra- and inter-rater reliability of muscle thickness measurement of the tibialis anterior using different inward pressures

  • Lee, Seong-Joo;Lim, Ji Young;Lee, Chang-Hyung;Park, Dae-Sung
    • Physical Therapy Rehabilitation Science
    • /
    • v.8 no.4
    • /
    • pp.218-224
    • /
    • 2019
  • Objective: This reliability study examined the effects of applying varying induced inward pressures using a transducer placed at 0° neutral ankle position (NEU) and 15° ankle dorsiflexion (DF) on tibialis anterior (TA) muscle thickness using a custom-made device with a force indicator during rehabilitative ultrasound imaging. Design: Cross-sectional study. Methods: Twenty-four healthy subjects were recruited in this study. Two examiners measured the muscle thickness of the TA at 0° NEU and 15° DF in 3 conditions of inward pressures (1.0 N, 2.0 N, and 4.0 N) using a custom-made holder. The muscle thickness was measured three times for each of the conditions arranged in random order. For intra- and inter-rater reliability, the intraclass correlation coefficients (ICCs) with 95% confidence intervals, standard error of measurement, minimal detectable change, and coefficient of variation were analyzed. One-way repeated measures analysis of variance was conducted for investigating changes of TA muscle thickness according to the inward pressures of the transducers. Results: The intra-rater reliability of TA muscle thickness measurement was excellent (ICC3,1: 0.92-0.96) for all conditions (at both ankle joint angles per varying inward pressure). Likewise, the inter-rater reliability of TA muscle thickness measurement was excellent (ICC2,1: 0.89-0.97) under same conditions. The mean of TA thickness showed the trend of decreasing significantly with increased inward pressures at all ankle joint angles (p<0.05). Conclusions: Use of this custom-made device with a force indicator is useful to accomplish the high intra- and inter-rater reliability of TA muscle thickness measurement at both ankle joint angles in reducing the measurement error.

Micro-EHL Analysis of a Ball Joint Contact with Surface Roughness (표면 거칠기를 고려한 볼 조인트 접촉의 미세 탄성유체윤활 해석)

  • 김태종
    • Tribology and Lubricants
    • /
    • v.19 no.3
    • /
    • pp.123-132
    • /
    • 2003
  • The effect of surface texture on elastohydrodynamic lubrication (EHL) point contact of a ball Joint mechanism in small reciprocating compressors is studied numerically by using multigrid method. Pressure and film thickness profiles have been calculated for surface roughness with waviness of different orientations and transverse ridge and dent at minimum and maximum Hoes M parameter conditions. The influence of the amplitude and the wavelength of the surface roughness was also studied. Results show that the oblique waviness with orientation angle of 30$^{\circ}$generates the smallest minimum film thickness as compared with those of longitudinal, transverse, and other oblique roughness. The influence of transverse waviness on the minimum film thickness is smaller than for the longitudinal waviness case.

Assessment of the Thickness of the Roof of the Glenoid Fossa Using Cone Beam Computed Tomography in Orthognathic Surgery Patients: A Preliminary Study

  • Park, Hyun-Jeong;Seo, Yo-Seob;Lim, Sung-Hoon;Ryu, Ji-Won
    • Journal of Oral Medicine and Pain
    • /
    • v.44 no.4
    • /
    • pp.154-159
    • /
    • 2019
  • Purpose: The aim of this study was to assess the change in thickness of the roof of the glenoid fossa (RGF) in patients undergoing orthognathic surgery using cone-beam computed tomography (CBCT) images. Methods: This retrospective study measured the thickness of the RGF in 19 patients (10 males, 9 females) who underwent orthognathic surgery at Chosun University Dental Hospital. The thickness of the RGF was measured perpendicularly between the 'glenoid fossa line' and 'middle cranial fossa line' on parasagittal and paracoronal reconstructions. Results: The mean RGF thickness increased from 0.83±0.44 mm to 0.86±0.46 mm after surgery. The average change in thickness of the RGF was 0.17±0.18 mm. The thickness of the RGF in the temporomandibular joint (TMJ) showed no significant difference by sex, and the change in thickness of the TMJ did not vary by surgical method. Conclusions: We found that the thickness of the RGF increased after orthognathic surgery, as revealed by CBCT. Further studies including larger numbers of subjects and long-term follow-up are needed to confirm the results of this study.