Recently, the attraction for water-based ink is increasing, Because Solvent ink, based on organic solvent, cause bad effect on environment and rise the cost. Instead of organic solvent that cause environment pollution as well as cost-rise by rise of petroleum price, Binder based on alkali-soluble resin is popular and studied by many other country. However, in domestic, research and development for alkali-soluble resin is not like, because of lack of understanding environmental pollution and safety, therefor alkali-soluble resin development and research for the properties of the water-based ink used by alkali-soluble resin is not study very well. In this paper, we studied dispersion of carbon black in acrylic resin solution and the properties of water-based ink used by carbon black and acrylic binder.
Paper stock could be situated in a cooled environment seasonally and/or regionally otherwise it is stored in a controlled warehouse. In this paper, printing problems on a cooled paper are investigated and characterized in terms of paper properties. For this purpose, various kinds of sample are cooled down under a specially designed freezing device and printed for observing their printability. Causes for poor ink transfer on a cooled paper are suggested due to condensation, surface inactivity, and rheological change in ink film. Paperboards with higher amount of binder, thick and/or multi-coated layers are more vulnerable to poor ink trap. Severe drying of wet coating could cause a similar result as that of the coatings with higher binder formulation. It is shown that more absorptive porous structure is desirable for better ink receptivity in a cooled status. Printing on a dampened surface may be an indicator for ink transferability on a cooled paper. Finally, desirable directions for papermaker and printshop are suggested.
Paper could be situated in a cooled environment seasonally or regionally otherwise it is forced to be in a controlled circumstance. In this paper, printing problems on a cooled paper are investigated and characterized in terms of paper properties. For this purposes, various kinds of sample are cooled down under a specially designed freezing device and printed for observing their printability. Causes for poor ink transfer on a cooled paper are suggested due to condensation, surface inactivity, and rheological change in ink film. Paperboards with higher amount of binder, thick and/or multi coat layers are more vulnerable to poor ink trap. Severe drying could cause the same effect as that of higher binder formulation. It is shown that more absorptive porous structure is desirable for better ink receptivity in a cooled status. Printing on a dampened surface may be an indicator for ink transferability on a cooled paper. Finally, desirable directions for papermaker and printshop are suggested.
This study was carried out to elucidate the potential in substitution of SB latex with eco-friendly starch based bio-binder as a coating binder. The part of SB latex in coating color of pre- and top layer was substituted with starch based bio-binder in order to evaluate the characteristics of coating color and coated paper, and printability. The viscosity and water retention of coating color were increased by substitution of SB latex with starch based bio-binder. Roughness of coated paper was increased by substitution with starch based bio-binder, although there was not significant changes in roughness when SB latex is used as a binder in pre-coating color. Brightness and whiteness of coated paper were not affected, but opacity and print mottle were improved by substitution with starch based bio-binder. The interesting result observed was that dry-pick did not affected significantly, and ink set-off was improved by starch based bio-binder. It is expected that starch based bio-binder can be commercialized if the systematic further research works are carried out.
Bio-binder is well known as a promising alternative binder for SB latex because it is eco-friendly and inexpensive, compared to synthetic latex. SB latex in top coating color was substituted with starch-based bio-binder to investigate its effects on the coating color and its coated paper properties. Bio-binder contributed to the increase of coating color viscosity, and the improvement of water retention. Most optical properties except opacity were deteriorated by the increase of bio-binder dosage. It was also found that the increase of bio-binder substitution in top coating color brought about the increase of roughness, and decrease of coated paper gloss, print gloss, dry and wet pick strength. However the stiffness and the ink set-off of the bio-binder coated paper were improved. Overall, mostly adverse effects of bio-binder on the properties of coating color and its paper were observed. Therefore, it is not recommended to use bio-binder as top coating color.
The coated paper was greatly affected by the basic physical properties of the binder as well as the amount of the coating formula. High glass transition temperature (Tg) of the styrene-butadiene (SB) latex, selected as the binder in our study, gave the high stiffness to the coated paper, but lowered the binding force and print gloss. The average particle size of the SB latex also greatly affected to the coated paper so that the smaller particle size improved the rheological property of the coating formula and increased the binding force and print gloss. Another property of the SBR latex, gel content, was important because when its value was small, the latex was easily deformed at the high temperature and increased air permeability to the coated paper. Therefore, the lower gel content consequently resulted in the higher blistering resistance, especially in the web paper. The larger portion of the SB latex in the coated formula improved the binding force and print gloss, but decreased the ink set-off and ink-trapping to the coated paper. The heavier coating improved optical properties such as opacity, paper gloss and paper smoothness, to the coated paper.
Humectants are chemical compounds which added to water based pigment inks for DTP (Digital Textile Printing) to prevent evaporation of water. The humectants usually have diol or triol type chemical structures and their -OH groups have possibility to react with functional groups of the binder polymers, such as ester, carboxylic acid, and urethane groups, acting as a crosslinking agent. The crosslinking reactions between polymer binders and humectants in inks can affect touch of the printed fabrics. In this regard, this study aims to investigate effect of chemical structures and added amounts of humectants in pigment ink on touch of dyed fabrics by using 1,6-hexanediol, ethylene glycol, diethylene glycol, and 1,4-buthanediol with various amounts added to the mixture of a black pigment and a polyurethane type binder. Then, color, rubbing strength, touch of the fabrics dyed with the prepared pigment inks were evaluated.
To improve rubbing fastness of the printed fabrics, the binder polymers for Digital Textile Printing(DTP) pigment inks were synthesized with miniemulsion polymerization using various acrylic monomers, which are MMA(Methyl methacrylate), BA(Butyl acrylate), and Self-crosslinking monomers, such as NEA(N-Ethylol acrylamide) and MAA (Methacrylic acid). The acrylic monomer compositions were varied when synthesizing the binder polymers and their particle size distributions, average molecular weights, and Tgs were investigated. The prepared binder polymers were applied to prepare Cyan, Black, Yellow and Magenta pigment ink for DTP and the prepared inks were used to dye cotton fabrics. Then, color strength, and rubbing fastness were also investigated to study the effect of the comonomer compositions of the binder polymer on the color strength and rubbing fastness of the resulting pigment inks.
The mottling in coated paper is one of the most difficult problems to solve in the area of offset printing. The prevention of mottling requires optimization of coating color formation, especially the minimum of binder migration. In this paper, we studied a mottling. Kaolin clay and CaCO3 as pigment, starch and latex as binder of coating color were used in this study. We have measured surface property of 24 coated samples through k value, mottle value and transferred ink. In the equation of Walker and Fesko, the value of k was the highest and that of mottle and the mount of transferred ink were the lowest in kaolin 60 part. And it is more easy to analyze the various surface of coated paper when sample was exposed on IR.
Recently, 3D printing technology is a hot issue in various industrial fields. According to the user's application, it allows for the free form fabrication method to be utilized in a wide range. The powder based fusion technique is one of the 3D printing methods. When using this method it is possible to apply the various binder jetting techniques such as piezo, thermal bubble jet, dispenser and so on. In this paper, a multi thermal bubble ink jet was integrated for jetting of powder binding material and developing a power fused 3D printing system. For high quality 3D printing parts, it needs an analysis and evaluation of the behavior of the thermal bubble ink jet head. In the experiment, a correlation between jetting binder quantity and layer thickness of powder was investigated, and a 3D part model was fabricated, which was used by measuring the scale factor.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.