• 제목/요약/키워드: initiation stress

검색결과 647건 처리시간 0.027초

MIXED-MODE CRACK PROPAGATION BY MOVABLE CELLULAR AUTOMATA METHOD

  • Pak, Mik-Hail;Lee, Choon-Yeol;Chai, Young-Suck
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2007년도 춘계학술대회A
    • /
    • pp.1754-1759
    • /
    • 2007
  • Propagation of a mixed-mode crack in Soda-Lime silica glass using Movable Cellular Automata (MCA) method is demonstrated in this study. In MCA method, special fracture criterion is used to describe the process of crack initiation and propagation. Comparison between MCA and other crack initiation criteria results are made. The crack resistance curves and bifurcation angles under different loading angles are found. In comparisons with results of maximum circumferential tensile stress criterion, MCA result showed the sufficient agreement.

  • PDF

變動荷重下의 疲勞壽命 豫測 第2報 (Fatigue Life Predictions for Variable Load Histories - Part II : Computer Software for Predictions of Fatigue Crack Initiation Life -)

  • 이시중;송지호;하재선
    • 대한기계학회논문집
    • /
    • 제12권6호
    • /
    • pp.1350-1357
    • /
    • 1988
  • A computer software was developed for predictions of fatigue crack initiation life of notched members under variable loadings. The software was constructed based on a new fatigue life prediction method utilizing modified .epsilon.-N curves, which can account for the stress interaction effect. The effect of mean plastic strain on low-cycle fatigue life was also incorporated in the software. The software can be utilized for the first step approximation when fundamental data of material fatigue properties are not available.

Response of Millet and Sorghum to Water Stress in Converted Poorly Drained Paddy Soil

  • Jung, Ki-Yuol;Yun, Eul-Soo;Park, Chang-Young;Hwang, Jae-Bok;Choi, Young-Dae;Oh, In-Seok
    • 한국토양비료학회지
    • /
    • 제46권6호
    • /
    • pp.409-416
    • /
    • 2013
  • Millet and sorghum are major dryland cereal crops, however their growth and productivity is limited by soil water stress with varying intensity. The major objective of this study was to evaluate water stress of millet and sorghum yield under drainage classes of poorly drained soil and to test the effect of the installed pipe drainage in poorly drained paddy soil to minimize crop stress. The research was carried out in poorly drained paddy fields located at alluvial slopping area resulting in non-uniform water content distribution by the inflow of ground water from the upper part of the field. Stress Day Index (SDI) was determined from a stress day factor (SD) and a crop susceptibility factor (CS). SD is a degree of measurement by calculating the daily sum of excess water in the profile above 30cm soil depth ($SEW_{30}$). CS depends on a given excess water on crop stage. The results showed that sum of excess water day ($SWD_{30}$) used to represent the moisture stress index was lower on somewhat poorly drained soil compared with poorly drained soil on 117 days. CS values for sorghum were 57% on $3^{rd}$ leaf stage, 44% on $5^{th}$ leaf stage, 37% on panicle initiation, 23% on boot stage, and 16% on soft dough stage. For proso millet CS values were 84% on $3^{rd}$ leaf stage, 70% on $5^{th}$ leaf Stage, 65% on panicle initiation, 53% on boot stage, and 28% on soft dough stage. And for foxtail millet the values were 73% on $3^{rd}$ leaf stage, 61% on $5^{th}$ leaf stage, 50% on panicle initiation, 29% on boot stage, and 15% on soft dough stage. SDI of sorghum and millet was more susceptible to excess soil water during panicle initation stage more poorly drained soil than somewhat poorly drained soil. Grain yield was reduced especially in proso millet and Foxtail millet compared to Sorghum.

SM 490 A 재질에 대한 용접 유형에 따른 피로특성 연구 (A study on the fatigue characteristics of SM 490 A material due to the welding type)

  • 김재훈;구병춘
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 추계학술대회
    • /
    • pp.274-278
    • /
    • 2004
  • This study investigates the fatigue characteristics of SM 490 A material specimens for the railway vehicle due to the welding type. The more stress ratio decreases, the more strength of fillet welded specimen decreases. At speciallly, when the stress ratio of TN(Plate with transverse fillet welded rib) specimens decreases 0.5, 0.1, and -0.1, the fatigue limit decreases unifomly. The strength of TN is higher than it of NCN in the compare of fillet welding type, but the strength of NCN(Non load-carrying cruciform fillet welded joint) is higher than it of CN(Load-carrying cruciform fillet welded joint), which these specimens have the rib in the both side. We analysis the strains on the weld positions of the TN specimens during the fatigue test for the investigation of crack initiation and crack growth. In the theses results, we could find the fatigue crack initiation point and time.

  • PDF

구형 인덴테이션 평가에 의한 비대칭적 층상형 세라믹 부품의 설계연구 (The Optimum Design Study of Asymmetric Layered Ceramic Component by Spherical Indentation)

  • 이기성;김태우;김철
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 추계학술대회
    • /
    • pp.297-301
    • /
    • 2004
  • The optimum design against contact crack initiation is investigated to find major parameters in designing desirable surface-coated asymmetric layered components. Hard ceramic coated soft materials with various elastic modulus mismatch are prepared for the analysis. Spherical indentation is conducted for producing contact cracks from the surface or interface between the coating and the substrate layer. A finite element analysis of the stress fields in the loaded layer components enables a direct correlation between the damage patterns and the stress distributions. Implications concerning the design of asymmetric layered components indicate that the coating thickness and the elastic modulus mismatch are important parameters for designing layered component to prevent the initiation of contact cracks.

  • PDF

Optimal response of conical tool semi angle in ductile metal sheets indentation and its governing mechanics

  • Nazeer, Malik M.;Khan, M. Afzal;Haq, A-Ul
    • Structural Engineering and Mechanics
    • /
    • 제16권1호
    • /
    • pp.47-62
    • /
    • 2003
  • The nonlinear dependence aspect of various conical tool indentation parameters leading to an optimum tool semi angle value for easiest perforation is plotted and discussed explicitly in this work with the conclusion that tool angle has an optimum response towards most of the indentation parameters. Around this optimum angle, the aluminium sheets showed minimum fracture toughness as well as minimum work input to overcome the offered resistance. At the end, the mechanism leading to this phenomenon is presented with the conclusion that plastic flow dominates as the dimple semi cone angle reaches 35 and both pre and post plastic flow perforations lead the tool semi cone angle value towards this dimple cone semi angle of plastic flow initiation for its optimum performance. It is also concluded that specimen material failure is solely under tensile hoop stress and hence results into radial cracks initiation and propagation.

스퍼기어의 피팅 수명 예측 및 실험 (Experiments and Prediction of Pitting Life in Spur Gears)

  • 김종성;주진욱;이상돈;조용주
    • Tribology and Lubricants
    • /
    • 제25권6호
    • /
    • pp.399-403
    • /
    • 2009
  • The objective of this paper is to predict pitting initiation by using a contact analysis and subsurface stress. Contact stresses are obtained by contact analysis of a semi-infinite solid based on the use of influence functions. Subsurface stress field is obtained using rectangular patch solutions. It is used Mesoscopic multiaxial fatigue criterion to predict contact fatigue life. It is important to predict pitting initiation to enhance reliability of the mechanical elements. Pitting life prediction in the spur gears which are fundamental mechanical element is presented in this paper.

복합재료내의 계면균열의 인성과 균열진전 거동 (Toughness and Crack Propagation Behavior of The Interfacial Crack in Composite Materials)

  • 최병선
    • 한국산업융합학회 논문집
    • /
    • 제6권4호
    • /
    • pp.291-298
    • /
    • 2003
  • Interfacial crack problems between fiber and matrix in composite materials are discussed. A series of interfacial crack initiation and propagation experiments are conducted using the biaxial loading device for various mode-mixes. Normal crack opening displacement (NCOD) is measured near crack front by a crack opening interferometry and used for extracting fracture parameters. From mixed mode interfacial crack initiation experiments, large increase in toughness with shear components is observed. Initial velocity of crack propagation is very dependent upon the mode-mixes. It increased with positive mode-mix due to the increase of stress singularities ahead of crack front and decreased with negative mode-mix resulting from the increase of the degree of compressive stress behind the crack front. Crack propagation was less accelerated with positive mode-mix than the negative mode-mix.

  • PDF

강도적 불균질재의 노치 표면에서의 연성크랙 발생 거동 (Behavior of ductile crack initiation with strength mismatch from notch root)

  • 안규백;대연윤;방한서;풍전정남
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2004년도 춘계 학술발표대회 개요집
    • /
    • pp.246-248
    • /
    • 2004
  • It has been well known that ductile fracture of steels is accelerated by triaxial stresses. The characteristics of ductile crack initiation in steels are evaluated quantitatively using two-parameters criterion based on equivalent plastic strain and stress triaxiality. This study provides the fundamental clarification of the effect of strength mismatching, which can elevate plastic constraint due to heterogeneous plastic straining, loading mode and loading rate on critical condition to initiate ductile crack from notch root using equivalent plastic strain and stress triaxiality based on the two-parameter criterion obtained on homogeneous specimens under static tension. The critical condition to initiate ductile crack from notch root for strength mismatched bend specimens under both static and dynamic loading would be almost the same as that for homogeneous tensile specimens with circumferential sharp notch under static loading.

  • PDF

Thermal Shock Resistance of $Al_{2}O_{3}$- and Fe-$Al_{2}TiO_{5}$-based Castable Refractories

  • Liu, T.;Latella, B.A.;Bendeich, P.
    • The Korean Journal of Ceramics
    • /
    • 제4권4호
    • /
    • pp.345-351
    • /
    • 1998
  • Thermal shock resistance of $Al_2O_3$- and Fe-$Al_2TiO_5$-based Castable Refractories was studied using a central heating technique. Ring type specimens, 10mm thick and 20 and 100mm inner and outer diameters, respectively, were rapidly heated on the internal surface of the centre hole using a high power electrical heating element. The temperature field was measured experimentally and modelled using finite element analysis (FEA). The thermal stress field was also modelled using FEA. A radial notch was introduced to the ring specimens to enable calculation of the thermal stress intensity factors (SIF). A special LVDT device was incorporated in the thermal shock tester to monitor crack mouth opening displacement (COD). The thermal shock fracture initiation and crack propagation behaviour of the castable refractories were ascertained using the COD measurements and the fracture mechanics analysis data.

  • PDF