• 제목/요약/키워드: initial velocity of molten metal

검색결과 2건 처리시간 0.016초

진공흡입주형 주조법에서 탕구방안에 따른 주형 충전 양상 (Mold Cavity Filling by Gating Design in Vacuum Molding Process)

  • 강복현;김기영;김명한;홍영명
    • 한국주조공학회지
    • /
    • 제27권1호
    • /
    • pp.42-47
    • /
    • 2007
  • Vacuum molding process(V-process) has several benefits such as a lower total production cost and a high quality casting comparing to the conventional sand molding. Influence of the gating design on the molten metal flow was investigated in this study. General criteria for the gating design of the castings and commercial codes for the flow and solidification analysis were used to attain the optimized gating design in V-process. Though mold cavity was filled smoothly under the low initial velocity of molten metal, molten metal dashed against the upper part of the mold before the completion of the mold filling with higher initial molten metal velocity and fell soon. This phenomenon may affect collapsing the mold shape, however it is thought that the possibility of burning out of the vinyl by the molten metal is not so high because vinyl is coated with refractory material.

VOF 방법을 이용한 GMA 용접의 금속 이행에 관한 동적 해석 (II) - 단락 이행 모드의 해석 - (Dynamic Analysis of Metal Transfer using VOF Method in GMAW (II) - Short Circuit Transfer Mode -)

  • 최상균;고성훈;유중돈;김희진
    • Journal of Welding and Joining
    • /
    • 제15권3호
    • /
    • pp.47-55
    • /
    • 1997
  • Dynamic characteristics of the short circuit mode are investigated using the Volume of Fluid (VOF) method. When the initial molten drop volume, contact area and wire feed rate are given, rate change of the molten bridge profiles, pressure and velocity distributions are predicted. The electromagnetic force with proper boundary conditions are included in the formulation to consider the effects of welding current. It is found that the molten metal is transferred to the weld pool mainly due to the pressure difference caused by the curvatures in the initial stage, and electromagnetic force becomes dominant factor in the final stage of short circuit transfer. Necking occurs at the contact position between the molten drop and weld pool, and the initial molten drop volume and welding current have significant effects on break-up time.

  • PDF