Combustion characteristics of two imported Indonesia coals as a pulverized fuel of thermal power plants (인도네시아산 발전용 수입 석탄 2종의 연소특성 비교 평가)

  • Lee, Hyun-Dong;Kim, Jae-Kwan
    • Journal of Energy Engineering
    • /
    • v.19 no.2
    • /
    • pp.136-142
    • /
    • 2010
  • Combustion reactivity and thermal behavior of two imported coals used as a pulverized fuel of commercially thermal power plant were investigated by thermogravimetric analysis (TGA) and large scale test furnace of 200 kg/hr. TGA results showed that combustion efficiency of high moisture coal has lower than reference coal due to the slow combustion completion rate although it has the low ignition temperature, and activation energies of high moisture coal with 79 kJ/mol for overall combustion was higher than reference coal of 53 kJ/mol. Test furnace results ascertained that flame of black band of high moisture coal during the combustion in boiler broke out compared to reference coal and then it becomes to unburned carbon due to the less reactivity and combustion rate. But, Blending combustion of high moisture coal with design coal of high sulfur are available because sulfur content of high moisture coal was too low to generate the low SOx content in flue gas from boiler during the combustion. The ash analysis results show that it was not expected to be associated with slagging and fouling in pulverized coal fired systems due to the low alkali metal content of $Na_2O$ and $K_2O$ compared to bituminous coal.

Experimental Study on Moisture Content According to Addition of Surfactants (계면활성제 첨가에 따른 함수율에 관한 실험적 연구)

  • Kim, Nam-Kyun;Rie, Dong-Ho
    • Fire Science and Engineering
    • /
    • v.29 no.2
    • /
    • pp.79-83
    • /
    • 2015
  • The fire accident is a representative type of disaster that can largely impact on business. Therefore, precautionary measures and rapid initial response is very important when a disaster occurs. The storage of porous combustibles is inevitable in coal yard, plywood processing industry, and others that are currently operating. Initial fire fighting of fire and identifying the ignition point in such a porous combustible storage space are so difficult that if the initial response is failed, being led to deep-seated fire, surface fire is likely to result in secondary damage. In addition, deep-seated fire can cause personal injuries and property damage due to a large amount of toxic gases and reignition. Therefore damage reduction measures is required around the storage space to handle a porous flammable. Improving the penetration performance of the concentration of the surfactant is carried out as underlying study, which is about an deep-seated fire extinguishing efficiency augmentation when using wetting agents. The porous materials used in the experiments is radiata pine wood flour, which occupies more than 75% of the domestic wood market. Fire fighting water is selected as Butyl Di Glycol (BDG), which is being used for infiltration extinguishing agent, and the experiment was carried out by producing a standard solution. The experiment was carried out on the basis of the Deep-Seated Fire Test of NFPA 18. The amount of watering, porous material to the internal amount of penetration, and runoff measurement out of the porous material was conducted. According to experimental results, as the surface tension is reduced, the surfactant concentration macroscopic penetration rate decreases, but infiltration to a porous material is shown to have growth characteristics.

A Study on the Confirmation of non-flammabikity of the Cast Resin Mold Transformer in Subway Substation (지하철 변전실용 진공주형형 몰드변압기의 난연성 확인에 관한 연구)

  • 정용기;장성규;곽희로
    • Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
    • /
    • v.12 no.2
    • /
    • pp.99-107
    • /
    • 1998
  • This dissertationhas confirmed the non-flam mability of cast mold transformer that is increasingly used lately. As a research progress, the investigation has been performed on the installation status and each line of the subway system which have the most mold transformer accidents, and the impediment status of the transformer for rectifier and the high-voltage distribution transformer per each manufacturer. Then, a high voltage mold of the actual mold transformer has been installed in the horiwntal heating furnace and the heat has been applied by the standard heating temperature curve of KSF 2257(Fireproof testing meth od of the construction structures: 1993). Accordingly, the combustibility of the mold transformer based on the test results has been found that 78 minutes has been required for the complete burning per the KSF 2257 combustion test curve and that, after stopping the heat application of the horizontal furnace after ignition, the flame progress has not been made but shown as the self-extinguishing characteristics when the flame progress has been checked. Thus, the non-flammability and self-extinguishability of the mold transformer have been confirmed. The result of this dissertation has indicated that the accident involving mold transformer has been progressed and expanded by the dielectric breakdown or void due to the crack in the mold rather than a fire accident caused by a short-circuit or an overload.r an overload.

  • PDF

A Study on the Method for Quantifying CO2 Contents in Decarbonated Slag Materials by Differential Thermal Gravimetric Analysis (DTG 분석법을 활용한 슬래그류 비탄산염 재료의 CO2 정량 측정방법 연구)

  • Jae-Won Choi;Byoung-Know You;Yong-Sik Chu;Min-Cheol Han
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.12 no.1
    • /
    • pp.8-16
    • /
    • 2024
  • Limestone (CaCO3, calcium carbonate), which is used as a raw material in the portland cement and steel industry, emits CO2 through decarbonation by high temperatures in the manufacturing process. To reduce CO2 emissions by the use of raw materials like limestone, it has been proposed to replace limestone with various industrial by-products that contain CaO but less or none of the carbonated minerals, that cause CO2 emissions. Loss of Ignition (LOI), Thermogravimetric analysis (TG), and Infrared Spectroscopy (IR) are used to quantitative the amount of CO2 emission by using these industrial by-products, but CO2 emissions can be either over or underestimated depending on the characteristics of by-product materials. In this study, we estimated CO2 contents by LOI, TG, IR and DTG(Differential Thermogravimetric analysis) of calcite(CaCO3) and samples that contain CO2 in the form of carbonate and whose weight increases by oxidation at high temperatures. The test results showed for CaCO3 samples, all test methods have a sufficient level of reliability. On the other hand, for the CO2 content of the sample whose weight increases at high temperature, LOI and TG did not properly estimate the CO2 content of the sample, and IR tended to overestimate compared to the predicted value, but the estimated result by DTG was close to the predicted valu e. From these resu lts, in the case of samples that contain less than a few percent of CO2 and whose weight increases during the temperature that carbonate minerals decompose, estimating the CO2 content using DTG is a more reasonable way than LOI, TG, and IR.

Marine Environmental Characteristics around the Test Phase of Offshore Wind Farm in the Southwestern Coast of Yellow Sea (서남해 해상풍력 실증단지 해역의 해양 환경 특성)

  • Seo, Jinsung;Maeng, Junho;Lim, Eunpyo;Jin, Seungjoo;Kim, Hyunmin;Kim, Taeyun
    • Journal of Environmental Impact Assessment
    • /
    • v.28 no.5
    • /
    • pp.457-470
    • /
    • 2019
  • This study aims to present the characteristics of marine physics, water quality, and sediment quality around offshore wind farm near the Gochang and Buan sea areas through the analysis of monitoring data. The relationships between suspended solid and wave height as well as suspended solid and flow velocity were analyzed. We found that Correlation Coefficient values of 0.61~0.69 between wave height and suspended solid, and suspended solid concentration reaches 75 mg/L or higher when wave height of more than 1m occurred in the spring (1 month). The water quality index (WQI) was used to identify the status of the water quality in the study area. Most of the measured points were rated first grade (very good). The variation of chlorophyll-a was relatively hight compared to the other criteria, indicating that it is a major factor affecting the quality index. In the sediment column, all heavy metals were detected below the Threshold Effects Level(TEL), and ignition loss and grain size show a positive correlation.

A Study on the Heat Release Characteristics of Fire Load for Performance Based Design of Multiplexes: A Focus on the Heat Release Rate and Fire Spread Rate of Cinema Seats (복합영상관의 성능위주설계를 위한 가연물의 연소발열특성 연구: 객석의자의 열발생률 및 연소확산속도를 중심으로)

  • Nam, Dong-Gun;Jang, Hyo-Yeon;Hwang, Cheol-Hong;Lim, Ohk-Kun
    • Fire Science and Engineering
    • /
    • v.34 no.1
    • /
    • pp.11-17
    • /
    • 2020
  • As performance-based design (PBD) has a direct impact on evacuation safety assessments, designing fire scenarios based on real fire tests is essential. To improve the reliability of the PBD for fire safety in multiplexes, information on fire behavior, such as heat release rate (HRR) and fire spread rate, are provided in this study by conducting a standard fabric flammability test. To this end, several chairs were arranged in a pattern that resembled a theater-style seating. The peak HRR and heating value per unit mass for each chair ranged from 415 kW to 988 kW and 15.2 MJ/kg to 23.8 MJ/kg, respectively. The heating values per unit mass of the new and old chairs were 23.6 MJ/kg and 16.7 MJ/kg, respectively. As the quantity of plastic and cushioning materials in the new chairs was more than that of the old ones, the new chairs were more vulnerable to fire hazards. Furthermore, when the chairs were arranged in a line, the fire spread rate was observed to be 0.39-0.42 m/min, regardless of the ignition location. Finally, a fire growth curve showing the peak HRR and fire spread rate was also demonstrated.

Characteristics of Vitrification Process for Mixture of Simulated Radioactive Waste Using Induction Cold Crucible Melter (유도가열식 저온용융로를 이용한 혼합모의 방사성폐기물의 유리화 공정 특성)

  • 김천우;양경화;박병철;박승철;황태원;박종길;신상운;하종현;송명재
    • Journal of Nuclear Fuel Cycle and Waste Technology(JNFCWT)
    • /
    • v.2 no.3
    • /
    • pp.165-174
    • /
    • 2004
  • In order to simultaneously vitrify the ion exchange resin(IER) and combustible dry active waste(DAW) generated from Korean nuclear power plants, a vitrification pilot test was conducted using an induction cold crucible melter(CCM) . The energy necessary for startup of the glass using a Ti-ring was evaluated as about 290 kWh. The power supplied from a high frequency generator to melt the glass properly was ranged from 160 to 190 kW without any interruption. When the mixture of the IER and DAW was fed into the CCM, the concentration of CO was lowered up to 1/40 compared to feeding the IER solely. It may be caused by the DAW which can produce about 1.8 times higher heat compared to the IER. When the swelling phenomenon occurred in the glass melt, the concentration of $NO_2$, oxidizing gas, was higher than NO, reducing gas. Total feed amounts of the IER and DAW were 368 and 751 kg, respectively. And then, about 74 of volume reduction factor was achieved.

  • PDF

Experimental Study on the Self-extinguishing Performance of Extruded Polystyrene Insulation for Buildings and Suggestions on Institutional Management (건축용 압출법 단열판(XPS)의 자기소화성에 대한 실험적 연구 및 제도적 관리에 관한 제언)

  • Kang, Jung Ki;Choi, Don Mook
    • Fire Science and Engineering
    • /
    • v.34 no.3
    • /
    • pp.141-149
    • /
    • 2020
  • The Korea Industrial Standards (KS) stipulates methods and test procedures for measuring the horizontal combustibility of cellular plastics exposed to small flames (KS M ISO 9772:2018) and recommendations regarding the magnetic digestion of extruded polystyrene insulation (XPS) for measurement results (KS M 3808:2020). Although products that are certified to conform to KS standards must have burning characteristics (self-extinguishing), they are incinerated and spread by welds at construction sites, causing significant human and property damages. In this study, XPS produced by five companies, certified by KS, and sold in the market were purchased and tested for ignition and diffusion caused by a weld bullion at a construction site. The results showed that the five products had differences in performance. Three out of the five products were found to be self-saturated, but the other two were easily ignited and diffused, making it difficult for them to be self-extinguishing. Based on the result of this experimental investigation in line with the KS regulations, all the three types of products, including two types of products that were incinerated through weld defects, were found to be non-self-extinguishing, as specified in KS M 3808.

Study on Reutilization with Aerobic Microbes of Organic Food Waste Leachates (호기성 미생물을 이용한 음폐수의 처리 및 자원화에 관한 연구)

  • Kang, Bo-Mi;Hwang, Hyeon-Uk;Kim, Ji-Hoon;Yang, Yong-Woon;Kim, Young-Ju
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.33 no.1
    • /
    • pp.54-59
    • /
    • 2011
  • This test established the bioavailability and sample input by mixing the maintaining the microbial machine parts and food waste leachates in weight of 2:1 as advanced experiment, maintaining the constant temperature, agitating and observing its weight and property change for 60 hours. And, I injected daily the established microbial machine parts and food waste leachates rate, maintained the temperature in the reactor with $55{\sim}65^{\circ}C$, and agitated with constant speed. I studied the recycling possibility of food waste leachates by extracting the sample after 24 hours, verifying its characteristics, and repeating the food waste leachates input and sample extraction for about 40 days. Considering all about the results of this study, I saw that 87.32% of food waste leachates was reduced, and the solid of bluebug or food included in the food waste leachates was decomposed within 24 hrs. pH for 43 days after 9 days of stabilization period was maintained from 3.7~3.9 and the ignition loss from 88.67~87.3%, and the quantity of organic matter from 77.6~80.88%. With the similar result daily maintained, it is considered to progress more the minimization by inputting the future food waste leachates. C/N rate satisfies the less than 25 that is the composting basis within 8 days, maintaining between 13~15, with 2% of salt not exceeded, it is able to recycle as the compost of food waste leachates as based on the composting with no extracted heavy metal content.

Study on Horizontal and Vertical Temperature Analysis of Cable Fire in Common Duct using Room Corner Experiment (룸코너 실험을 이용한 공동구 케이블 화재 시 수평·수직 방향 온도 분석에 관한 연구)

  • JaeYeop Kim;SeHong Min
    • Journal of the Society of Disaster Information
    • /
    • v.19 no.3
    • /
    • pp.634-643
    • /
    • 2023
  • Purpose: Underground common duct fires are steadily occurring, and the proportion of property damage is particularly large among property and human casualties caused by fires. Especially, cable fires that occur in common areas can spread vertically quickly and pose a great risk. This paper aims to scientifically analyze the nature of the fire by reproducing the fire through experiments. Method: To analyze the characteristics of cable fires in underground common duct, heat release rate and temperature changes were measured through Room-corner (ISO 9705) test, and the vertical and horizontal propagation of cable fires was quantitatively compared and analyzed. Result: The Room Corner Test (ISO 9705) was used to compare the temperature changes at each data logger point. The results showed that the time it took for the fire to reach the ignition temperature in the horizontal and vertical directions from the center point of the first-tier cable was 589 seconds and 536 seconds, respectively, which means that the vertical fire propagation is 53 seconds faster than the horizontal propagation. This proves that the vertical propagation of fire is relatively faster than the horizontal propagation. The horizontal propagation speed of the fire was also compared for each floor cable tray. The results showed that the third-tier cable propagated at 3.4 times the speed of the second-tier cable, and the second-tier cable propagated at 1.5 times the speed of the first-tier cable. This means that the higher the cable is located, the faster the fire spreads and the larger the fire becomes. Conclusion: This study identified the risks of cable fires and analyzed the risks of vertical fire propagation during cable fires based on the results of the Room Corner Test. Studies to prevent the spread of fire and fire response policies to prevent vertical fire propagation are required. The results of this study are expected to be used to assess the fire risk of common areas and other fires.