  • In this study, adhesion of plasma spray coated hydroxyapatite film on the two-step anodized dental implant was investigated. The plasma spray was carried out on the dental implant after two step anodization. The adhesion of coated HA film was investigated by FE-SEM after fatigue test. In the case of two-step anodized implant showed a good adhesion between implant and coated film.

  • PDF

성경 대퇴골에 매식된 Titanium Plasma Spray 및 Hydroxyapatite 피복임프란트 주위의 골치유 양상 (HISTOLOGIC EvALUATION OF BONE HEALING AROUND TITANIUM PLASMA SPRAYED AND HYDROXYAPATITE-COATED IMPLANTS IN DOGS)

  • 허기남;정현주
    • Journal of Periodontal and Implant Science
    • /
    • 제25권2호
    • /
    • pp.418-437
    • /
    • 1995
  • The effect of the hydroxyapatite coatings on Titanium implants has been the subject of recent investigations. So far, the use of HA coating remains substantially controversial.This study was aimed to evaluate histologically the bone healing patterns around titanium plasm sprayed(TPS) amd HA-coated implant after implantation into the femur neck of ten adult dogs. After implantation, animals were sacrificed at the intervals of 2,4,6,8 and 12 weeks.The fluorescent dyes were injected on the postoperative 4th and 12th week into the animals supposed to be killed at the 12th week. The morphology and direction of new bone formation was similar in both TPS and HA-coated implants.There was a tendency toward more bone formation in the cortical bone area than in the cancellous bone area. Histologically,in the interface of the HA-coated implants, bone response and bone maturation was faster, compared to the TPS implants in the 2nd and 4th week. By fluorescent microscopy, new bone formation was active in the 4th week around both implants and was directed from the periosteum overlying cortical bone to the cancellous bone. These results suggest that the bone formation and maturation is faster during the early healing stage in the interface of the HA-coated implant and where the cortical bone quality is poor, HA coated implant is superior to the TPS implant in the early phase of new bone formation.

  • PDF

성견에서 수산화인산염 피개 IMZ임플란트와 티타늄 피개 IMZ임플란트주위의 골형성 및 골성숙 정도에 대한 비교연구 (EFFECTS OF HYDROXYAPATITE AND TITANIUM-COATED DENTAL IMPLANTS ON BONE FORMATION AND MATURATION IN DOG)

  • 윤홍철;한동후
    • 대한치과보철학회지
    • /
    • 제33권2호
    • /
    • pp.317-334
    • /
    • 1995
  • The purpose of this study was to compare the bone formation, maturation around HA-and titaniumcoated dental implants in dog. 5 hydroxyapatite coated IMZ implants and 5 titanium coated IMZ implants were placed into the previously extracted site in the mandible of 5 adults dogs. All dogs were injected intravenously Tetracycline, Alizalin red S, and Calcein for bone fluorescent labelling, After the experimental period of 16weeks, the dogs were sacrificed and tissue samples around the implants were obtained. Microscopic observations(ligth, polariged and fluorescence microscope), morphometric analysis, line profile with EPMA, and quantitative analysis for Ca,P, and Ti were performed. The results were as follows ; 1. Bone maturations around the implants were relatively lower than those of natural teeth. No significant differences in bone maturation and remodeling patterns were observed between the two implants groups. 2. Calcification of bone surrounding the implants was initiated in 8-11 weeks for HA-coated implants, while it took 11 weeks or more for Ti-coated implants. 3. Bone-to-implants contact ratio of 82.63% was recorded for HA-coated group and 72.25% for titanium coated group, with no significant difference between the two groups. 4. Bone around the implants exhibited reduced quantity of Ca and P in the $100{\mu}m$ region relative to natural teeth, while the rest of the regions showed no statistical differences. No significant differences were found between the two implant groups. 5. There was a separation of HA layer from the implant core and subsequent infiltration of inflammatory cells into the resulting space in the HA-coated implants, and evidences of phagocytosis of HA particles by macrophages. Bone calcification was more rapid around HA-coated implants compared to titanium-coated implants, but HA coated implants did not show any significant differences either in the degree of calcification or the bone-to-implant contact ratio over Ti coated implants. HA coated implants may have complications associated with HA absorption and separation of HA layer from the implant core.

  • PDF

수산화인회석 코팅 임프란트의 골치유과정에 관한 실험적 연구 (Experimental study about the bony healing of hydroxyapatite coating implants)

  • 엄태관;김종화;조인희;정창모;조용석;김영균
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • 제37권4호
    • /
    • pp.295-300
    • /
    • 2011
  • Introduction: Hydroxyapatite(HA) coating implant can accelerate osseointegration, however, there are many controversies. Materials and Methods: This study examined the early osseointegration of two types of hydroxyapatite coated implants. Twelve adult male miniature pigs (Medi Kinetics Micropigs, Medi Kinetics Co., Ltd., Busan, Korea) were used in this study. In the implants placed in the mandible, a histomorphometric evaluation was performed to evaluate the bone-implant contact (BIC) ratio. Results: The BIC ratio increased with time. TS III HA and Zimmer HA were not significantly different (P>0.05). At 8 weeks, the BIC of Zimmer HA was higher than TS III HA, but there was no significant difference (P>0.05). Conclusion: HA coated implants will accelerate early osseointegration.

수종의 Hydroxyapatite coated 골유착성 임프란트의 임상적 연구 (CLINICAL STUDY OF ENDOSSEOUS HYDROXYAPATITE COATED IMPLANTS)

  • 한종현;김성현;정영철
    • 대한치과보철학회지
    • /
    • 제38권5호
    • /
    • pp.631-639
    • /
    • 2000
  • Root-form endosseous implants which are in use today have a variety of materials, designs and surface characteristics. Among them, pure titanium surface implants and titanium matrix coated with HA are popular as well as are available in many studies. Rate of clinical success is obviously lower in jaw with cancellous bone than dense bone. In order to increase the rate of success in poor bone quality. More advanced techniques of implant surgery and surface treatment of implant fixture body have been developed. As a successful result, the installation of HA coated implant in bone quality type III or IV became highly successful. Since most clinical studies were performed without knowing the characteristics of HA coated implants, it has been impossible to come up with proper clinical data. Therefore the characterization of HA coated implants is essential to understand long term clinical performance and the predictability of HA coated implant system Our results showed that HA coated implants had the success rate at 93.7% in bone quality type III, IV for 3.8 years, and the fixture of Steri-Oss showed more stability with time.

  • PDF

HYDROXYAPATITE GRANULE IMPLANTED Ti-ALLOY

  • Nonami, Toru;Taoda, Hiroshi;Kamiya, Akira;Naganuma, Katsuyoshi;Sonoda, Tsutomu;Kameyama, Tetsuya
    • 한국표면공학회지
    • /
    • 제32권3호
    • /
    • pp.356-359
    • /
    • 1999
  • To obtain a biomaterial that has both biological affinity and high mechanical strength, hydroxyapatite granules were implanted into the surface of pure titanium film coated titanium alloy. The film was coated by reactive DC sputtering method on the alloy substrate. Hydroxyapatite granules (32- $38\mu\textrm{m}$ in diameter)were spread over titanium alloy substrate and pressed to implant the granules in the substrate. They can be implanted into substrate under 17MPa at $800^{\circ}C$ for 10minutes. The only tops of the granules were exposed and they were firmly stuck in substrate. The hydroxyapatite implanted titanium alloy composites were expected to be useful for biomaterials as artificial bones and dental roots.

  • PDF

Sol-Gel법으로 HA코팅된 치과용 임플란트 합금의 표면특성 (Surface Characteristics of HA Coated Dental Implant Alloy by Sol-Gel Method)

  • 최한철;고영무
    • 한국표면공학회지
    • /
    • 제38권4호
    • /
    • pp.167-173
    • /
    • 2005
  • Surface characteristics of HA(hydroxyapatite) coated dental implant alloy by Sol-Gel method were investigated using potentiostat, ICP, SEM, EDX, EPMA and surface roughness tester. Surface roughness of HA coated specimen by Sol-Gel showed higher than that of PVD coated specimen. Corrosion resistance increased in the order of $1\%$ lactic acid, artificial saliva, $0.5\%$ HCI and $0.9\%$ NaCl solution. Amount of Ca element release was higher than that of V and P in the $0.5\%$ HCI and $0.9\%$ NaCl solution.

The effect of Er:YAG laser irradiation on the surface microstructure and roughness of hydroxyapatite-coated implant

  • Kim, Seong-Won;Kwon, Young-Hyuk;Chung, Jong-Hyuk;Shin, Seung-Il;Herr, Yeek
    • Journal of Periodontal and Implant Science
    • /
    • 제40권6호
    • /
    • pp.276-282
    • /
    • 2010
  • Purpose: The present study was performed to evaluate the effect of erbium:yttrium-aluminium-garnet (Er:YAG) laser irradiation on the change of hydroxyapatite (HA)-coated implant surface microstructure according to the laser energy and the application time. Methods: The implant surface was irradiated by Er:YAG laser under combination condition using the laser energy of 100 mJ/pulse, 140 mJ/pulse and 180 mJ/pulse and application time of 1 minute, 1.5 minutes and 2 minutes. The specimens were examined by surface roughness evaluation and scanning electron microscopic observation. Results: In scanning electron microscope, HA-coated implant surface was not altered by Er:YAG laser irradiation under experimental condition on 100 mJ/pulse, 1 minute. Local areas with surface melting and cracks were founded on 100 mJ/pulse, 1.5 minutes and 2 minutes. One hundred forty mJ/pulse and 180 mJ/pulse group had surface melting and peeling area of HA particles, which condition was more severe depending on the increase of application time. Under all experimental condition, the difference of surface roughness value on implant surface was not statistically significant. Conclusions: Er:YAG laser on HA-coated implant surface is recommended to be irradiated below 100 mJ/pulse, 1 minute for detoxification of implant surface without surface alteration.

성견 치주질환 이환 발치와에 즉시 임플란트 매식술시 Titanium plasma sprayed 임프란트와 Hydroxyapatite coated 임프란트의 계면조직에 관한 연구 (HISTOLOGICAL COMPARISONS OF TITANIUM PLASMA SPRAYED IMPLANT AND HYDROXYAPATITE COATED IMPLANT TO BONE INTERFACE IN PERIODONTALLY INVOLVED EXTRACTION SOCKETS IN DOGS)

  • 김진숙;김종관
    • Journal of Periodontal and Implant Science
    • /
    • 제23권3호
    • /
    • pp.400-410
    • /
    • 1993
  • Dental implants have been widely used in the treatment of esthetic and functional problems of the mouth due to alveolar bone loss, after tooth extraction. The success of implantation strongly depends on osseointegration. For osseointegration, implant material, methodology, and design have been investigated. For materials, two popular materials at present are titanium and hydroxyapatite. For methods, immediate implantation is being used recently. The purpose of this study is to evaluate osseointegration between the unthreaded cylindrical TPS implant and the HA-coated implant by a histomorphometric analysis. For this analysis, experimental periodontits was induced on the 3, 4 premolars of adult dogs by the ligation of orthodontic threads. Thereafter, each tooth was extracted. TPS. Implants and HA-coated implants were immediately inserted in the extraction socket. In control group, TPS implants were immediately inserted, and In experimental group, HA implants were immediately inserted. The dogs were sacrificed after 12 weeks, then the specimens were prepared for LM and histomorphometric analysis. The conclusion of this study is as follows l. In both control and experimental group, no inflammatory cells were observed. 2. The results of the histomorphometric analysis showed that the total osseointegration was 48.5% in control group, and 68.8% in expermental group. The experimental group was higher than the control group, and the difference was not statistically significant (p<0.05). 3. The results of the histomorphometric analysis showed that the osseointegration in the hole was 40.6% in control group, and 70.2% in experimental group. The experimental group was higher than the control group, and the difference was statistically significant (p<0.05). In both control and experinental group, no inflammatory cells were observed. 4. The results of the histomorphometric analysis showed that the osseointegration in the lower part was 52.1% in control group, and 73.3% in experimental group. The experimental group was higher than the control group, and the difference was statistically significant (p<0.05). 5. In experimental group, the bone to HA interface seemed to be mixed of bone and HA. We could not distinguish HA from the bone. The HA coating was detached from the titanium surface.

  • PDF