The Optical properties of Fe2O3/Na3AlF6/Fe2O3/Cu, Al, Cr Multi Layered Thin Film depending on the Optical Thickness (Fe2O3/Na3AlF6/Fe2O3/Cu, Al, Cr 다층박막의 광학적 두께에 따른 광학특성)

  • Kim, Jun-Sik;Jang, Gang-Jae;Jang, Gun-Eik
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.21 no.7
    • /
    • pp.665-668
    • /
    • 2008
  • Multi-layered thin films of $Fe_2O_3/Na_3AlF_6/Fe_2O_3/Cu$, Cr, Al were deposited on glass substrate by evaporation process. As high and low refractive index material, $Fe_2O_3$ and $Na_3AlF_6$ were selected and additionally Cu, Al and Cr were chosen as mid reflective layer respectively. Optical properties including reflectance were systematically studied depending on optical thickness of $Na_3AlF_6$ especially $0.25{\lambda}$ and $0.5{\lambda}$. In order to expect the experimental result, the simulation program, the Essential Macleod Program(EMP) was adopted and compared with the experimental data. Based on the results taken by spectrophotometer at viewing angle $45^{\circ}C$, the $Fe_2O_3/Na_3AlF_6/Fe_2O_3/Cu$ show the colour rage between red and orange in $0.25{\lambda}$ and green and pupple in $0.5{\lambda}$ respectively. When the Al was used as mid reflective layers in $Fe_2O_3/Na_3AlF_6/Fe_2O_3$ system, typical yellow colour and mixed colour between green and pupple were appeared in $0.25{\lambda}$ and $0.5{\lambda}$ of $Na_3AlF_6$ respectively. As compared the experimental result to simulation data, it was found out that the experimental data is relatively well matched with the EMP simulation data.

The optical properties of ZnS/$Na_3AlF_6$/ZnS/Cr multi-layered thin film with different optical thickness (ZnS/$Na_3AlF_6$/ZnS/Cr 다층 박막의 광학적 두께 변화에 따른 광특성)

  • Kim, Jun-Sik;Jang, Gang-Jae;Jang, Gun-Eik
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.06a
    • /
    • pp.535-536
    • /
    • 2008
  • Multi-layered thin films of ZnS/$Na_3AlF_6$/ZnS/Cr were deposited on glass substrate by evaporation process. ZnS and $Na_3AlF_6$ were selected as high and low refractive index material, and additionally Cr was chosen as mid reflective layer respectively. The multi-layered thin films were prepared in terms of different optical thickness and different staking sequence and layers. The optical properties were systematically characterized with different optical thickness of $Na_3AlF_6$ especially $0.25\lambda$ and $0.5\lambda$. In order to expect the experimental result, the simulation program, the Essential Macleod Program(EMP) was adopted. Based on the results taken by spectrophotometer at viewing angle $45^{\circ}$, the ZnS/$Na_3AlF_6$/ZnS/Cr multi-layered thin film shows purple colour range in $0.25\lambda$, bluish green in $0.5\lambda$, red purple in $0.75\lambda$, and purple in $1.0\lambda$ respectively.