• 제목/요약/키워드: gas metal arc welding

검색결과 277건 처리시간 0.021초

용접사업장 근로자의 흄 및 금속 노출농도에 대한 평가와 혈중 금속 농도 (Airborne Concentrations of Welding Fume and Metals of Workers Exposed to Welding Fume)

  • 최호춘;김강윤;안선희;박화미;김소진;이영자;정규철
    • 한국산업보건학회지
    • /
    • 제9권1호
    • /
    • pp.56-72
    • /
    • 1999
  • Airborne concentrations of welding fumes in which 13 different metals such as Al, Cd, Cr, Cu, Fe, Mn, Mo, Ni, Pb, Si, Sn, Ti, and Zn were analyzed were measured at 18 factories including automobile assembly and manufactures, steel heavy industries and shipyards. Air samples were collected by personal sampler at each worker's worksite(n=339). Blood levels of Cd, Cu, Fe, Mn, Pb and Zn were also measured from samples taken from 447 welders by atomic absorption spectrometry and compared with control values obtained from 127 non-exposed workers. The results were as follows ; 1. Among various welding types, $CO_2$ welding 70.2 % were widely used, shielded metal arc welding(SMAW) 22.1 % came next, and rest of them were metal inert gas(MIG) welding, submerged arc welding(SAW), spot welding(SPOT) and tungsten inert gas(TIG) welding. 2. Welding fume concentration was $0.92mg/m^3$($0.02{\sim}15.33mg/m^3$) at automobile assembly and manufactures, $4.10mg/m^3$($0.02{\sim}70.75mg/m^3$) at steel heavy industries and $5.59mg/m^3$($0.30{\sim}91.16mg/m^3$) at shipyards, respectively, showing significant difference among industry types. Workers exposed to high concentration of welding fumes above Korean Permissible Exposure Limit(KPEL) amounted to 7.9 % and 12.5 %, in $CO_2$ welding and in SMAW at automobile assembly and manufactures and 62.7 % in $CO_2$ welding, and 12.5 % in SMAW at shipyards, and 66.2 % in $CO_2$ welding and 70.6 % in SMAW at steel heavy industries. 3. Geometric mean of airborne concentration of each metal released from welding fumes was below one 10th of KPEL in all welding types. Percentage of workers, however, exposed to airborne concentration of metals above KPEL amounted to 16.8 % in Mn and 7.6 % in Fe in $CO_2$ welding; 37.5 % in Cu in SAW, 30 % in Cu in TIG; and 25 % in Pb in SPOT welding. As a whole, 76 Workers(22.4%) were exposed to high concentration of any of the metals above KPEL. 4. There were differences in airborne concentration of metals such as Al, Cd, Cr, Cu. Fe. Mn, Mo, Ni, Pb, Si, Sn, Ti and Zn by industry types. These concentrations were higher in shipyards and steel heavy industries than in automobile assembly and manufactures. Workers exposed to higher concentration of Pb above KPEI amounted to 7.4 % of workers(7/94) in automobile assembly and manufactures. In shipyards, 19.2 % of workers(19/99) were over-exposed to Mn and 7.1 % (7/99) to Fe above KPEL. In steel heavy industries, 14.4 %(21/146), 7.5 %(11/146) and 13 %(19/146) were over-exposed to Mn, Fe and Cu, respectively. As a whole, 76 out of 339 workers(22.4%) were exposed to any of the metals above KPEL. 5. Blood levels of Cd, Cu, Fe, Mn, Pb, and Zn in welders were $0.11{\mu}g/100m{\ell}$, $0.84{\mu}g/m{\ell}$, $424.4{\mu}g/m{\ell}$, $1.26{\mu}g/100m{\ell}$, $5.01{\mu}g/100m{\ell}$ and $5.68{\mu}g/m{\ell}$, respectively, in contrast to $0.09{\mu}g/100m{\ell}$, $0.70{\mu}g/m{\ell}$, $477.2{\mu}g/m{\ell}$, $0.73{\mu}g/100m{\ell}$, $3.14{\mu}g/100m{\ell}$ and $6.15{\mu}g/m{\ell}$ in non-exposed control groups, showing significantly higher values in welders but Fe and Zn.

  • PDF

건설현장 용접직종별 용접흄 및 금속류 노출 실태 (Welding Fume and Metals Exposure Assessment among Construction Welders)

  • 박현희;박해동;장재길
    • 한국산업보건학회지
    • /
    • 제26권2호
    • /
    • pp.147-158
    • /
    • 2016
  • Objectives: The objective of this study was to evaluate the assessment of exposure to welding fume and heavy metals among construction welders. Methods: Activity-specific personal air samplings(n=206) were carried out at construction sites of three apartment, two office buildings, and two plant buildings using PVC(poly vinyl chloride) filters with personal air samplers. The concentration of fumes and heavy metals were evaluated for five different types of construction welding jobs: general building pipefitter, chemical plant pipefitter, boiler maker, ironworker, metal finishing welder. Results: The concentration of welding fumes was highest among general building pipefitters($4.753mg/m^3$) followed by ironworkers($3.765mg/m^3$), boilermakers($1.384mg/m^3$), metal finishing welders($0.783mg/m^3$), chemical pipefitters($0.710mg/m^3$). Among the different types of welding methods, the concentration of welding fumes was highest with the $CO_2$ welding method($2.08mg/m^3$) followed by SMAW(shield metal arc welding, $1.54mg/m^3$) and TIG(tungsten inert gas, $0.70mg/m^3$). Among the different types of workplace, the concentration of welding fumes was highest in underground workplaces($1.97mg/m^3$) followed by outdoor($0.93mg/m^3$) and indoor(wall opening as $0.87mg/m^3$). Specifically comparing the workplaces of general building welders, the concentration of welding fumes was highest in underground workplaces($7.75mg/m^3$) followed by indoor(wall opening as $2.15mg/m^3$). Conclusions: It was found that construction welders experience a risk of expose to welding hazards at a level exceeding the exposure limits. In particular, for high-risk welding jobs such as general building pipefitters and ironworkers, underground welding work and $CO_2$ welding operations require special occupational health management regarding the use of air supply and exhaust equipment and special safety and health education and fume mask are necessary. In addition, there is a need to establish construction work monitoring systems, health planning and management practices.

저사이클 피로 영역에서의 Alloy 617 모재와 용접재의 파괴 시험편에 대한 거시적 및 미시적 관찰 (Macro and Microscopic Investigation on Fracture Specimen of Alloy 617 Base Metal and Weldment in Low Cycle Fatigue Regime)

  • 김선진;랜도 디와;김우곤;김응선
    • 대한기계학회논문집A
    • /
    • 제40권6호
    • /
    • pp.565-571
    • /
    • 2016
  • 본 논문은 Alloy 617 모재와 용접재에 대한 저사이클 피로 시험 후의 파괴 시험편에 대한 거시적 및 미시적 파면해석을 나타낸다. 용접재 시험편은 Alloy 617의 가스텅그스텐아크 용접 패드로부터 채취, 제작하였다. 본 연구의 목적은 Alloy 617의 모재와 용접재 시험편의 저사이클 파괴 모드 및 기구의 거시적 및 미시적 양상을 고찰하는 것이다. 전변형률 제어 피로시험이 상온에서 0.6, 0.9, 1.2 및 1.5%에 대하여 수행되었다. Alloy 617 모재의 거시적 파면은 피로하중 축에 수직인 평평한 형태의 양상을 보였으나, 용접재 시험편의 경우는 상대적으로 전단/별모양의 양상의 파괴를 나타내었다. 두 시험편 모두 피로균열전파 영역에서는 명확한 스트라이에이션이 관찰되었다. 한편, 모재의 피로균열은 피로 하중 축에 수직인 방향으로 결정입내를 따라 전파하였으나, 용접재 시험편의 경우 하중 축에 거의 $45^{\circ}$의 경사진 형태의 결정입내로 나타났다.

개조된 GMA용접공정을 이용한 SiC/AI 복합재료의 제조 및 특성 (Manufacturing and Characterization of SiC/AI Metal Matrix Composite by Modified Gas Metal Arc Welding Process ; Manufacturing and Microstructure)

  • 김광수
    • 한국재료학회지
    • /
    • 제6권11호
    • /
    • pp.1090-1098
    • /
    • 1996
  • 개조한 가스 금속 아아크 용접공정을 이용하여 SiC/AI 금속기 복합재료를 제조하고 그 특성을 조사하였다. AI 모재위에 강화입자의 크기와 부피분율을 변화하여 다양한 SiC/AI 복합재료층을 제조하였고, 만들어진 복합재료층의 특성은 미세조직관찰과 미소경도시험을 통하여 이루어졌다. 복합재료층의 두께는 약 7-8mm로 측정되었고 균일한 강화입자의 분포도를 얻을 수 있었다. 분산입자의 부피분률은 Ar가스의 유량에 의하여 조절하였고 분산입자의 부피분률이 증가하고 크기가 작아짐에 따라 기지의 수지상 응고조직은 더욱 미세화되었다. 복합재료의 부피경도는 분산입자의 부피분률이 감소함에 따라 낮아졌으나 입자 크기에는 크게 변화가 없는 것으로 나타났다.

  • PDF

청정도 가스 이송용 재료의 특성과 전해연마에 관한 연구 (A Study on the Characteristics of Electro Polishing and Utility Materials for Transit High Purity Gas)

  • 이종형;박신규;양성현
    • 한국산업융합학회 논문집
    • /
    • 제7권3호
    • /
    • pp.259-263
    • /
    • 2004
  • In the manufacture progress of LCD or semiconductor, there are used many kinds of gas like erosion gas, dilution gas, toxic gas as a progress which used these gas there are required high puritize to increase accumulation rate of semiconductor or LCD materials work progress of semiconductor or LCD it demand many things like the material which could minimize metallic dust that could be occured by reaction between gas and transfer pipe laying material, illumination of the surface, emition of the gas, metal liquation, welding etc also demand quality geting stricted. Material-Low-sulfur-contend (0.007-0010), vacuum-arc-remelt(VAR), seamless, high-purity tubing material is recommend for enhance welding lower surface defect density All wetted stainless steel surface must be 316LSS elecrto polishinged with ${\leq}0.254{\mu}m$($10.0{\mu}in$) Ra average surface finish, $Cr/Fe{\geq}1.1$ and $Cr_2O_3$ thickness ${\geq}25{\AA}$ From the AES analytical the oxide layer thickness (23.5~36 angstroms silicon dioxide equivalent) and chromum to iron ratios is similar to those generally found on electropolished stainless steel., molybdenum and silicon contaminants ; elements characteristic of stainless steel (iron, nickel and chromium); and oxygen were found on the surface Phosphorus and nitrogen are common contaminants from the electropolish and passivation steps.

  • PDF

WELD REPAIR OF GAS TURBINE HOT END COMPONENTS

  • Chaturvedi, M.C.;Yu, X.H.;Richards, N.L.
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.235-243
    • /
    • 2002
  • Ni-base superalloys are used extensively in industry, both in aeroengines and land based turbines. About 60% by weight of most modern gas turbine engine structural components are made of Ni-base superalloys. To satisfy practical demands, the efficiency of gas turbine engines has been steadily and systematically increased by design modifications to handle higher turbine inlet or firing temperatures. However, the increase in operating temperatures has lead to a decrease in the life of components and increase in costs of replacement. Moreover, around 80% of the large frame size industrial/utility gas turbines operating in the world today were installed in the mid-sixties to early seventies and are now 25 to 30 years old. Consequently, there are greater opportunities now to repair and refurbish the older models. Basically, there are two major factors influencing the weldability of the cast alloys: strain-age cracking and liquation cracking. Susceptibility to strain-age cracking is due to the total Ti plus AI content of the alloy; Liquation cracking is due either to the presence of low melting constituents or constitutional liquation of constituents. Though Rene 41 superalloy has 4.5wt.% total Ti and Al content and falls just below the safe limit proposed by Prager et al., controlled grain size and special heat treatments are needed to obtain crack-free welds. Varying heat treatments and filler materials were used in a laboratory study, then the actual welding of service parts was carried out to verity the possibility of crack-tree weld of components fabricated from Rene 41 superalloy. The microstructural observations indicated that there were two kinds of carbides in the FCC matrix. MC carbides were located along the grain boundaries, while M$_{23}$C$_{6}$ carbide was located both inter and intra granularly. Two kinds of filler materials, Rene 41 and Hastelloy X were used to gas tungsten arc weld a patch into the sheet metal, along with varying pre-weld heat treatments. The microstructure, hardness and tensile tests were determined. The service distressed parts were categorized into three classes: with large cracks, with medium cracks and with small or no visible cracks. No significant difference in microstructure among the specimens was observed. Specimens were cut from the corner and the straight edge of the patch repair, away from the corner. The only cracks present were found to be associated with inadequate surface preparation to remove oxidation. Guidelines for oxide removal and the welding procedures developed in the research enabled crack-free welds to be produced.d.

  • PDF

유전자 알고리즘을 이용한 GMA 필릿 용접 비드형상 예측에 관한 연구 (A Study on Bead Geometry Prediction the GMA Fillet Welding using Genetic Algorithm)

  • 김영수;김일수;이지혜;정성명;이종표;박민호
    • Journal of Welding and Joining
    • /
    • 제30권6호
    • /
    • pp.126-132
    • /
    • 2012
  • The GMA welding process involves large number of interdependent variables which may affect product quality, productivity and cost effectiveness. The relationships between process parameters for a fillet joint and bead geometry are complex because a number of process parameters are involved. To make the automated GMA welding, a method that predicts bead geometry and accomplishes the desired mechanical properties of the weldment should be developed. The developed method should also cover a wide range of material thicknesses and be applicable for all welding position. For the automatic welding system, the data must be available in the form of mathematical equations. In this study a new intelligent model with genetic algorithm has been proposed to investigate interrelationships between welding parameters and bead geometry for the automated GMA welding process. Through the developed model, the correlation between process parameters and bead geometry obtained from the actual experimental results, predicts that data did not show much of a difference, which means that it is quite suitable for the developed genetic algorithm. Progress to be able to control the process parameters in order to obtain the desired bead shape, as well as the systematic study of the genetic algorithm was developed on the basis of the data obtained through the experiments in this study can be applied. In addition, the developed genetic algorithm has the ability to predict the bead shape of the experimental results with satisfactory accuracy.

자동차 산업에서 뿌리기술의 중요성 및 최신 용접/접합 기술 (Importance of Fundamental Manufacturing Technology in the Automotive Industry and the State of the Art Welding and Joining Technology)

  • 장인성;조용준;박현성;소득영
    • Journal of Welding and Joining
    • /
    • 제34권1호
    • /
    • pp.21-25
    • /
    • 2016
  • The automotive vehicle is made through the following processes such as press shop, welding shop, paint shop, and general assembly. Among them, the most important process to determine the quality of the car body is the welding process. Generally, more than 400 pressed panels are welded to make BIW (Body In White) by using the RSW (Resistance Spot Welding) and GMAW (Gas Metal Arc Welding). Recently, as the needs of light-weight material due to the $CO_2$ emission issue and fuel efficiency, new joining technologies for aluminum, CFRP (Carbon Fiber Reinforced Plastic) and etc. are needed. Aluminum parts are assembled by the spot welding, clinching, and SPR (Self Piercing Rivet) and friction stir welding process. Structural adhesive boning is another main joining method for light-weight materials. For example, one piece aluminum shock absorber housing part is made by die casting process and is assembled with conventional steel part by SPR and adhesive bond. Another way to reduce the amount of the car body weight is to use AHSS (Advanced High Strength Steel) panel including hot stamping boron alloyed steel. As the new materials are introduced to car body joining, productivity and quality have become more critical. Productivity improvement technology and adaptive welding control are essential technology for the future manufacturing environment.

차체 이음 유발 용접 불량에 대한 분석과 해결 방안 (Evaluation and solution of noise making weldment in automotive body)

  • 조정호;이중재;배승환;이용기;박경배;김용준;문세민
    • Journal of Welding and Joining
    • /
    • 제33권2호
    • /
    • pp.18-22
    • /
    • 2015
  • The importance of emotional quality of car is getting higher in these days. Noise takes great portion in emotional quality because it is detectable problem with just a few rides. The sources of car noise during operation are various and the related technical issues are vast. Sometimes weldments of auto body are referred as the source of noise and the suspicious weldment shows unsatisfactory welding quality in most cases. In this research, cases of noise making weldments are investigated to figure out the solution for welding quality improvement. They are categorized into several groups in according to the inferred types of the error source then appropriate solutions are suggested. Auto body has weldments of resistance spot welding and gas metal arc welding in general. Therefore the solutions are suggested as adjustment of welding process variables and related machineries. Inevitable error source is also referred which is originated from thermal expansion rate difference between ultra high strength steel and mild steel. This new approach is validated through simple calculation then more concrete investigation with numerical analysis is remained as further works to be done.

판재의 비드 용접에서 구속경계조건을 적용한 열응력 및 각변형 해석 (An Analysis of Thermal Stress and Angular Distortion in Bead-on-Plate Welding Incorporating Constrained Boundary Conditions)

  • 배강열;최태완
    • Journal of Welding and Joining
    • /
    • 제17권1호
    • /
    • pp.104-115
    • /
    • 1999
  • 판재의 비드 용접과정에서 열응력과 각변형의 발생기구 및 크기를 판재 단면에 대한 2차원 유한 요소해석을 통해 규명하고자 할 때 판재의 3차원 특성을 판재 길이의 크기효과로 간주하여, 구속경계조 건으로 설정함으로써 2차원 해석으로도 더욱 실제에 근접한 현상해석이 가능함을 제안하고자 하였다. 먼저 용접 입열에 의한 판재 내부의 천이 온도분포를 해석하였고, 이를 열응력 해석에 활용하였다. 2차 원 열응력 해석에 있어, 용접도중에 단면 전체가 길이 방향으로 동일한 크기의 변위를 한다고 가정하여 일정 변위를 길이 방향 경계조건으로 설정하고, 판재의 길이에 따라 각변형의 발생이 구속된다고 가정 하여, 판재의 길이에 의한 구속효과를 상당 구속력으로 간주하여 이를 단면 부재의 회전방향에 대한 경 계조건으로 설정함으로써 판재의 3차원 특성을 고려하고자 하였다. 제안된 방법에 의한 응력 분포 형태, 각변형 크기 등의 해석 결과가 기존의 2차원 해석 결과에 비해 실제에 더 근접함을 보여 주었다.

  • PDF