비닐하우스용 아연도강관의 강도경년변화 시험(농업시설) (A Secular Change of Strength for Galvanized Steel Pipes for Vinyl Housing)

  • 남상운;김문기;권혁진
    • 한국농공학회:학술대회논문집
    • /
    • 한국농공학회 2000년도 학술발표회 발표논문집
    • /
    • pp.296-301
    • /
    • 2000
  • Bend test for metallic materials was conducted on samples of galvanized steel pipes being used in greenhouse farms. A secular change of yield strength for galvanized steel pipes was analyzed with the part of buried in the ground and exposed in the atmosphere. From those experimental results and corrosion rate of galvanized film, the standard durable years for pipe framed greenhouses are estimated that the small sized pipe houses of movable type is 7∼8 years and the large sized pipe houses of fixed type is 14∼15 years.

  • PDF

Failure Analysis of Welded Pipe in Water Supplies for Apartment

  • Lee, Jong Kwon;Hong, Kyung Tae;Hwang, Woon Seok;Koh, Yong Tae;Park, Yong Soo
    • Corrosion Science and Technology
    • /
    • 제3권2호
    • /
    • pp.67-71
    • /
    • 2004
  • Galvanized Steel pipes have been widely used in industries and apartments, Unexpected early leakage has been found in an apartment. Tunneling corrosion or penetration was found in the water supply pipes. The chemical compositions of the pipes and properties of coating layer were evaluated. The pipes met the specification of KS D 3507. The cause of early failure was analyzed through the examination of macrostructures and microstructures, It was found that the pipes were failed by grooving corrosion, which resulted from galvanic corrosion of weld bead and matrix.

급수관내 염소 주입이 미생물의 증식과 부식에 미치는 영향 (The Influence of Chlorine Application on Corrosion and Bacterial Growth in Home Plumbing Systems)

  • 김태현;이윤진;임승주
    • 한국환경보건학회지
    • /
    • 제32권5호
    • /
    • pp.431-439
    • /
    • 2006
  • This research was conducted using a model home plumbing system composed of copper, stainless steel, galvanized iron, carbon steel, and PVC (polyvinyl chloride) pipe. The number of bacteria present in stainless steel pipe and PVC was higher than other pipes. High turbidity and zinc release were found in galvanized iron pipe material and detected during the first 6 months. Conversely, there was a decrease in turbidity and zinc release after 6 months resulting in levels similar to other pipes. Copper concentration decreased as operation times increased. In this experiment, the number of bacteria detected in biofilm for a copper pipe continued to increase. Pipe material influenced bacterial numbers in biofilm and water. This showed that elevated chlorine could not control bacterial growth in biofilm for galvanized iron and stainless steel systems. It also suggested that the dosing of chlorine might not be available for all kinds of pipes. Therefore, another complementary method should be introduced to manage biofilm effectively in water distribution systems.

수도관의 부기거동에 관한 연구 (Corrosion Behaviour of Water Pipes)

  • 김원만;박영식
    • 환경위생공학
    • /
    • 제7권1호
    • /
    • pp.1-16
    • /
    • 1992
  • Corrosion of pipes Is one of the most serious problems in the maintenance of water worlds. Corrosion is promoted not only by physical factors such as temperature, but also by electrochemical factors including concentration of soluble metal ions, chlorine ion, pH, DO and microorganisms. Corrosion products also affect corrosion rate. In this research, study results are summarized as follows ; 1) Corrosion test was performed for 4 weeks at $70^{\circ}C$, pH 7.0 with specimens of 4 types of metal materials used as service pipes. Corrosion rate and S.E.M were analyzed. The results were showed that corrosion 1.ate of carbon steel pipe was 4.10~5.22 $mg/\textrm{cm}^2$ . week, galvanized steel pipe 0.98~1.34$mg/\textrm{cm}^2$. week, Copper pipe 0.02~0.04$mg/\textrm{cm}^2$. week, stainless steel pipe 0.05~ 0.10$mg/\textrm{cm}^2$ . week. 2) When corrosion rate was tested for tile types of pipes at pH 7 and both $25^{\circ}C$ and $75^{\circ}C$, avaerage corrosion rate for 6 weeks at $25^{\circ}C$ Ivas 2.26$mg/\textrm{cm}^2$ . week in carbon steel pipe, 1.99$mg/\textrm{cm}^2$. week in galvanized steel pipe, 0.26 $mg/\textrm{cm}^2$. week in stainless steel pipe. At $87^{\circ}C$, average corrosion rate for 4 weeks u.3s 4.56 $mg/\textrm{cm}^2$. week in carbon steel pipe,

  • PDF

공동주택의 노후 급수관 개선방안에 관한 연구 : 부천시 공동주택을 중심으로 (The Replacement Plans for Aged Public Water Supply Pipes in Apartment Buildings : Especially Apartment Buildings in Bucheon)

  • 이용화;허용철
    • 설비공학논문집
    • /
    • 제27권4호
    • /
    • pp.228-232
    • /
    • 2015
  • The water supply galvanized steel pipes of apartment buildings in Bucheon city constructed with building permission before 1994 have many problems such as leaks, the water containing rust, and low water pressure due to corrosion. Therefore, this study aims to find a way to renew the water supply pipes under investigation through a survey. As a result, when replacing the galvanized steel pipe with the corrosion-resistant pipe, the water supply system should also be changed from the gravity tank system to the booster pump system and the hygienic water storage tank. It is necessary to redraft the long-term repair plan including the replacement of the water supply system. Also, it is necessary to save the allowance reserve according to the modified long-term repair plan.

아연도금강관의 가스메탈아크용접에서 용접인자가 기공형성에 미치는 영향 (Effects of Welding Parameters on Porosity Formation in Weld Beads of Galvanized Steel Pipes produced with Gas Metal Arc Welding)

  • 임영민;장복수;고진현
    • Journal of Welding and Joining
    • /
    • 제30권5호
    • /
    • pp.46-50
    • /
    • 2012
  • This study was carried out to investigate the effect of welding parameters such as shielding gas compositions welding voltage and welding current on the pore formation in the weld beads of galvanized steel pipes produced with gas metal arc welding. The porosity was evaluated and rated by metallography and radiographic test in terms of weight percentage, number and distribution of pores in weld beads. The porosity increased with increasing welding voltage and current, in which Ar gas produced the most porosity while $Ar+5%O_2$ generated the least porosity. It was found that the porosity could be reduced by selection of the proper gas mixture composition such as $Ar+5%O_2$ and $Ar+10%CO_2$ and by using current (130~150A) and voltage(16~20V).

파이프 골조 온실 구조물의 표준내용연수 연구 (A Study on the Standard Durable Years of Pipe Framed Greenhouses)

  • 남상운
    • 한국농공학회지
    • /
    • 제43권1호
    • /
    • pp.96-101
    • /
    • 2001
  • In designing the greenhouse structures, snow and wind loads must be estimated on the basis of the probability of occurrence of snow or wind storms of a given intensity. The recurrence interval chosen depends on the standard durable years and safety factors of the greenhouse. This study was carried out to find the standard durable years of pipe framed greenhouses. Bend test for metallic materials was conducted on samples of galvanized steel pipes being used in greenhouse frames. A secular change of collapse loads and flexural rigidity for galvanized steel pipes were analyzed with the parts buried in the ground and exposed in the atmosphere. From those experimental results and corrosion rate of galvanized film, the standard durable years for pipe framed greenhouses are estimated as follows ; the small scale pipe houses of movable type is 7∼8 years and the large scale pipe houses of fixed type is 14∼15 years.

  • PDF

설비배관에서 용접봉에 따른 환경오염 (Environments Pollution Caused by Welding Rod in the Process of Pipe Working)

  • 윤영묵;이우람;이철구;김주한
    • 한국생산제조학회지
    • /
    • 제18권3호
    • /
    • pp.300-306
    • /
    • 2009
  • Welding technology is applicable in many kinds of fields, with the help of its advantages such as easy operational procedure and structural simplification. However, in the process of welding, hazardous materials and fumes cause huge fire broke-outs, explosions, and health-conscious problems. Also, as heavy metals in fumes have a harmful effect on the environment, recently, this has emerged as a urgent social issue. This study has been aimed at the recommendation of the most environment-friendly, among materials currently used in plumbing welding, and it has been done at the result of the analysis of amount, ingredient, and size in collected fumes created in the experiment of welding five rods to galvanized steel pipes and steel pipe ones. At the test result, due to the effect of Zn-coating, galvanized steel pipes, when welded to rods, created more fumes than steel pipe ones. In the mean time, when it comes to welding rods, among five, WR-03 produced fumes the least. Therefore, a combination of the test results clearly indicates that the case of welding WR-03 to cast-iron pipes turned out to be the most environment-friendly.

  • PDF

급수관에서 관재에 따른 부식특성과 미생물 재성장 고찰 (Influence of Pipe Materials on Corrosion and Bacteria Regrowth in A Model Home Plumbing System)

  • 김태현;이윤진;이환;이철효;안교철;이우식
    • 한국환경과학회지
    • /
    • 제16권1호
    • /
    • pp.121-128
    • /
    • 2007
  • This study performed in order to evaluate the effects of pipe materials on corrosion and bacteria regrowth using a laboratory scale batch test. Two varieties of feed water with different microbial conditions were selected: tap water, surface river water (Han River water), and five pipe materials; carbon steel, copper, galvanized iron, stainless steel, and PVC, Carbon steel and galvanized iron pipes showed higher corrosion rates than other materials. In terms of attached bacterial growth, pipes with PVC and stainless steel showed higher bacteria concentration compared to other materials. Pseudomonas vesicularis was the predominant bacteria found on biofilm. The behavior of bacterial growth in the pipes was observed using a scanning electron microscope.

소석회와 CO2를 이용한 상수관로의 부식제어(II) - 관종별 부식특성 평가 (Corrosion Control in Water Distribution System using Lime and Carbon Dioxide(II) - Evaluation on the Characteristics of Corrosion as a Function of Pipe Material)

  • 이두진;김영일;송영일;박현아
    • 상하수도학회지
    • /
    • 제22권3호
    • /
    • pp.379-387
    • /
    • 2008
  • The pH & alkalinity adjustment method by lime and carbon dioxide($CO_2$) for corrosion control in water distribution system was investigated to evaluate the corrosion characteristics of metal pipes, such as galvanized iron, copper, stainless steel, and carbon steel. When the pH in sand filtered and ozone+GAC treated water was increased with lime and $CO_2$ from 7.5 to 8.0, the concentration of residual chlorine decreased at higher pH and longer reaction time; the concentration of trihalomethane increased. The corrosion rate of coupons with corrosion control using lime and carbon dioxide was showed much smaller than those without corrosion control using pilot-scale simulated distribution system. The galvanized iron was corroded much faster than carbon steel, copper, and stainless steel. Especially, copper and stainless steel coupons were hardly corroded. The galvanized iron and carbon steel coupons with corrosion control were produced the corrosion products less than those without corrosion control by the results of environmental scanning electron microscope(ESEM) and energy dispersive x-ray spectroscopy(EDS) analyses. The galvanized iron coupon with pH and alkalinity adjustment by lime and carbon dioxide was detected about 30 percent of zinc, when the carbon steel was detected about 30 percent of calcium by calcium carbonate products formation. For the results of X-ray diffraction(XRD) analyses, the goethite(${\alpha}$-FeOOH) was identified as primary corrosion product of galvanized iron without corrosion control, while the Zinc oxide(ZnO) was found on corrosion products of galvanized iron coupon with corrosion control as the results of EDS analyses. However, the carbon steel corrosion products regardless of corrosion control were composed predominantly of maghemite(${\gamma}-Fe_2O_3$) and hematite(${\alpha}-Fe_2O_3$).