• Title/Summary/Keyword: galvanic current density

Search Result 41, Processing Time 0.024 seconds

The Study on the Corrosion Characteristics of Al-Alloy Shell for Cooler (알루미늄합금 원통냉각기의 부식 특성에 관한 연구)

  • 임우조;김성진;윤병두
    • Journal of the Korean Society of Fisheries and Ocean Technology
    • /
    • v.39 no.2
    • /
    • pp.152-157
    • /
    • 2003
  • Most Recently, with rapid development in marine industries such as marine structures and ship, there occurs much interest in the study of corrosion characteristics which play an important role in design of cooling water system like heat-exchanger. Especially, as operating environment of fresh cooling water system in vessels is acidified, this system is seriously corroded. In this study, to study on the corrosion characteristics of Al-alloy shell for cooler, the electrochemical polarization test of materials for the marine fresh water cooler such as Al-alloy, Cu and naval brass was carried out in fresh water. And thus the polarization resistance and anodic polarization behavior of Al-alloy, Cu and naval brass are investigated. Also, galvanic corrosion characteristics of Al-alloy coupled with Cu and naval brass is considered. The main results obtained are as follows ; (1) The current density of corrosion is high in order of Al-alloy > naval brass > Cu (2) As anodic potential increases, the corrosion resistance of naval brass is better than that of Cu. (3) The galvanic corrosion of Al-alloy coupled with Cu and naval brass is activated than corrosion of Al-alloy.

A Study on the Influence of Al Alloy Sacrificial Anode Efficiency due to Marine Environmental Variation (해양환경 변화가 알루미늄합금 희생양극의 효율에 미치는 영향에 관한 연구)

  • 김도형
    • Journal of Ocean Engineering and Technology
    • /
    • v.14 no.2
    • /
    • pp.106-111
    • /
    • 2000
  • Recently it was reported that the life of Al Sacrifical anode is being used in port piers has been significantly shortened compared with the original design life (e.g. average life shortened from 20 years to 13-15 year) Those factors involving these problems mentioned above were seemed to be a quality of anode material and diverse environmental factors such as pH flow rate temperature Dissolved oxygen Chemical oxygen demand and resistivity etcm In this study flow rate and contamination degree(pH) of sea water affecting to sacrificial anode life hve been investigated in terms of electrochemical characteristics of Al alloy sacrificial anode It was known that the lifetime of Al alloy anode was shortened not only by increasing of self-corrosion quantity by varying flow rate of sea water but also by increasing corrosion current density due to the potential difference increment between Al anode and steel structure cathode by varying contamination degree of sea water. Especially when anode current density is from 1mA/cm2 to 3mA/cm2 and flow rate of sea water is under 2m/s anode current efficiency is 90% above However flow rate is over 2m/s anode current efficiency fell down sharply due to erosion corrosion as well as galvanic corrosion.

  • PDF

Micro-electrochemical Characteristics of Sensitized 304 Stainless steel Using Micro-droplet cell Techniques (마이크로 드로플릿 셀 기법을 이용한 예민화 된 304 스테인리스강의 미세전기화학 특성)

  • Kim, Kyu-Seop;Lee, Jae-Bong
    • Corrosion Science and Technology
    • /
    • v.9 no.6
    • /
    • pp.300-309
    • /
    • 2010
  • The influences of sensitization on localized corrosion resistance of 304 stainless steel, were investigated, using micro-dropletcell techniques. Micro-droplet cell allows one to align the micro-electrode to the desired spot of the working electrode and measure directly local current with the potentiodynamic polarization, linear polarization and a.c. impedance. Micro-electrochemical tests were carried out inside of the grain and on grain boundaries separately. It was found that sensitization decreased the pitting potential, increasing corrosion current density around grain boundaries. Galvanic current density was also measured between grain and grain boundaries.

Hollow Sb93Pt7 Nanospheres Prepared by Galvanic Displacement Reaction for a Highly Li Reactive Material

  • Kim, Hyun-Jung;Cho, Jae-Phil
    • Journal of the Korean Electrochemical Society
    • /
    • v.11 no.3
    • /
    • pp.154-158
    • /
    • 2008
  • The synthesis of hollow ${Sb_93}{Pt_7}$ nanospheres smaller than 30 nm with a shell consisting of smaller nanoparticles, with an average particle size of ${\sim}$ 3 nm is reported. The formation of this alloy is driven by galvanic replacement reaction involving Sb nanoparticles and ${H_2}{PtCl_6} $ without need for any additional reductants. Further, the reaction proceeds selectively as long as the redox potential between two metals is favorable. The capacities of the hollow samples are 669 and 587mAh/g at rates of 1 and 7C, respectively, while those values for the nanoparticles are 647 and 480mAh/g at rates of 1, 7C, respectively. This result shows the significantly improved capacity retention of the hollow sample at higher C rates, indicating that high surface area of the hollow nanospheres makes the current density more effective than that for the solid counterpart.

A Study on the Galvanic Corrosion for Zirconium with Titanium and 316L Stainless Steel

  • Baik, Shin-Young
    • Journal of the Korean Society of Marine Environment & Safety
    • /
    • v.19 no.3
    • /
    • pp.285-289
    • /
    • 2013
  • The coastal area of Republic of Korea is very clean compared to other countries. In this reason, west coastal area of our country is a good place for breeding up a fish such as shrimp. In winter season, the heating system is required for preventing shrimp death caused by freezing in the farm. The heater in the heating system for fishery's farm is operated very severe combating corrosion due to high accumulation by feeding material and high temperature in heated sea water. Almost all manufactured heaters of STS 316L and Ti material are scrapped every year due to heavy corrosion such a general and crevice corrosion. For comparing the general and galvanic corrosion in new heater material, the test material of Zirconium (Zr), Titanium (Ti) and STS 316L are tested by potentiodynamic polarization, electrochemical impedance spectroscopy (EIS), current density-time methods and microscopic examination in a 3.5% NaCl solution. The corrosion potential (Ecor) measured by potentiodynamic polarization for Zr, Ti and STS 316L reveals -198, -250 and -450mV, corrosion current density 0.5, 2.5 and $6.5{\mu}A/cm^2$ respectively. The film resistance measured by EIS are Zr 63,000, Ti 39,700 and 316L $3,150{\Omega}$, and the current of Zr-Ti couple is $0.03{\mu}A$, whereas Zr-316L SS is $0.1{\mu}A$. According to the result of this experiment in 3.5% NaCl solution, Zr is excellent corrosion resistance material than Ti and STS 316L.

Galvanic Anode Charactristics of Grounding Cell Design for Corrosion Protection of Pipings (배관 방식용 접지전지 설계를 위한 유전양극의 특성에 관한 연구)

  • 임우조
    • Journal of the Korean Society of Fisheries and Ocean Technology
    • /
    • v.19 no.1
    • /
    • pp.57-62
    • /
    • 1983
  • The galvanic anodes have three kinds of Zn alloy anode, Al alloy anode and Mg alloy anode, which are widely used in cathodic protection for all metal structures in water or under ground. This paper to be used for designing of the grounding cell has reached the following conclusion as the results of an experimental study on the characteristics of such galvanic anodes for corrosion protection of pipings: 1) Zn alloy anode was the best when the specific resistance of the environment was bellow 1000 $\Omega$.cm, and when above 1000 $\Omega$.cm, Mg alloy anode to be used for designing of the grounding cell was the best. 2) Al alloy anode was better than Mg alloy anode for grounding cell when the specific resistance was bellow 500 $\Omega$.cm, but the Al alloy anode in all the environments reduced the characteristics of galvanic anode to the lower grade than those of Zn alloy anode. 3) Each impressed voltage (E) of the anodes at which drainage current density ($\rho$) begins rapidly increasing is quantitatively presented as follows: \circled1 E sub(Zn)=log (4.9465/$\rho$super(0.0639))+11$\times$10 super(-6)$\rho$super(0.8923i) \circled2 E sub(Al)=log (4.9306/$\rho$super(0.0525))+13$\times$10 super(-6)$\rho$super(0.9314i) \circled3 E sub(Mg)= log (3.7086/$\rho$super(0.0988))+181$\times$10 super(-6)$\rho$super(0.5406i) 4) The empirical equations between the drainage current density (i) and impressed environment are modeled as the following type. logi=g+root(n.E+r)(g,n,r; constants)

  • PDF

Study on the Cathodic Protection Characteristics of Hot Water Boiler by Mg-Alloy Galvanic Anode(1) (Mg 합금 유전양극에 의한 온수Boiler의 음극방식특성에 관한 연구(1))

  • 임우조;윤병두
    • Journal of the Korean Society of Fisheries and Ocean Technology
    • /
    • v.37 no.2
    • /
    • pp.147-152
    • /
    • 2001
  • Corrosion damage of boiler, factory equipment and so forth occur quickly due to using of the polluted water, resulting in increasing leak accident. Especially, working life of hot water boiler using the polluted water becomes more short, and energy loss increases. The cathodic protection method is the most economical and reliable one to prevent corrosion damage of steel structures. Mg-base alloys galvanic anode protection of cathodic protection methode is suitable for the application of hot water boiler using water with high specific resistance such as tap water. This paper is studied on the cathodic protection characteristics of hot water boiler. In tap water solution, the measurement of cathodic protection potential according to the time elapsed is carried out, and behavior of cathodic polarization with current change is investigated. The main results obtained are as follows. In hot water boiler shell, the open circuit potential of base metal become less noble than that of weld Bone, and the current density of base metal becomes low than that of weld zone. The further distance from Mg-alloy galvanic anode, the higher cathodic protection potential of hot water boiler appears. And protective potential becomes high according to pass cathodic protection time and after 6∼10 days become stable.

  • PDF

Study on the Characteristics of Corrosion for Epoxy Coated Steel Structure (에폭시도막 강구조물의 부식특성에 관한 연구)

  • Lim, U-Jo;Cheun, Jeong-Hyun;Jeong, Gi-Cheol
    • Journal of the Korean Society of Fisheries and Ocean Technology
    • /
    • v.34 no.2
    • /
    • pp.223-230
    • /
    • 1998
  • Recently, with the rapid development in the industries such as mechanical plants, automobiles, ships and marine structures, it is enlarged by the use of the SS 41 steel. This mechanical plants and marine structures are exposed m corrosion because of Cl-under marine environments. To protect their accidents, mainly applied anti-corrosion epoxy coating and various protective its structures. In this study, corrosion control characteristics on the epoxy coating were investigated by the galvanic corrosion of impressed voltage tester under marine environments The main results obtained are as follows; 1. Corrosion current density of amine-epoxy coating becomes more increased than that of other epoxy coating and the time area rate of pin hole and pit until 5% becomes most rapid. 2. The potential of SUS 304 stainless steel(cathode) for Al-epoxy coating is nearly zero potential. 3. Corrosion current density of Amine-epoxy by shot blast becomes more decreased than that of not shot blast and cathodic potential becomes more noble. 4. As distance of anode and cathode is more decreased, corrosion current density of epoxy coating is more increased and cathodic potential becomes less noble.

  • PDF

Electrical Characteristics of Porous Carbon Electrode According to NaCl Electrolyte Concentration (NaCl 전해질 농도 변화에 따른 다공질 탄소전극의 전기적 특성)

  • Kim, Yong-Hyuk
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.23 no.10
    • /
    • pp.814-819
    • /
    • 2010
  • Porous carbon electrodes with wooden materials are manufactured by molding carbonized wood powder. Electrical properties of the interface for electrolyte and porous carbon electrode are investigated from viewpoint of NaCl electrolyte concentration, capacitance and complex impedance. Density of porous carbon materials is 0.47~0.61 g/$cm^3$. NaCl electrolytic absorptance of the porous carbon materials is 5~30%. As the electrolyte concentration increased, capacitance is increased and electric resistance is decrease with electric double layer effect of the interface. The electric current of the porous carbon electrode compared in the copper and the high density carbon electrode was improved on a large scale, due to a increase in surface area. The circuit current increased as the distance between of the porous carbon electrode and the zinc electrode decreased, due to increase in electric field. Experimental results indicated that the current properties of galvanic cell could be improved by using porous carbon electrode.