• Title/Summary/Keyword: freezing, thawing

Search Result 935, Processing Time 0.03 seconds

An Experimental Study on the Improvement of Freezing-Thawing Resistance of Gutter Concrete (측구 콘크리트의 동결융해 저항성능 개선을 위한 실험적 연구)

  • Lee, Hoi-Keun;Sohn, Yu-Shin;Kim, Han-Jun;Lee, Seung-Hoon
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.11a
    • /
    • pp.577-580
    • /
    • 2006
  • This paper presents the experimental results of frost durability characteristics including freezing-thawing and de-icing salt scaling of the concrete used for gutter of the road. Mixtures were proportioned with the three level of water-binder ratio (W/B), 0.58, 0.53, and 0.48, and two binder compositions corresponding to Type I cement without any supplementary cementitious materials (OPC) and Type I cement with 30% blast-furnace slag replacement (Slag30). Also, two different solutions of calcium chloride and water that contains 0 and 8g of anhydrous calcium chloride in each 100 mL of solution, respectively, were used to evaluate their effect on the frost durability resistance. Test results showed that the Slag30 mixture exhibited higher durability factor and lower mass loss values than those made with OPC. Among the mixture tested in this work, the mixtures (OPC and Slag30) made with a relatively higher W/B of 0.58 exhibited large amount of the de-icing salt scaling regardless of calcium chloride concentration. Finally, the use of slag can be used effectively in terms of economy and frost durability of the concrete designated for gutter.

  • PDF

Effect of Culture Conditions on Survival of Frozen-Thawed Blastocysts Fertilized In Vitro (소 체외수정란의 배양조건이 동결-융해 배반포의 생존에 미치는 영향)

  • 윤종택;이호준;노상호;정연길;박용습;최은주;이종완;김용엽;정혜영
    • Journal of Embryo Transfer
    • /
    • v.14 no.3
    • /
    • pp.163-169
    • /
    • 1999
  • This study was carried out to investigate the effect of co-culture system(bovine oviduct epithelial cells; BOEC) and defined culture system(modified TALP ; mTALP) on the development of IVM-IVF embryos, and survival of in vitro produced blastocysts after freezing and thawing. Occytes from the slaugheterhous ovaries were matured and fertilized using general protocol. The results obtained were as the following: 1. Survival rates of frozen-thawed blastocysts using 10% glycerol as cryoprotectant was higher in day 7 blastocysts than in Day 8 and 9 blastocysts from co-cultrue system, but survival rate of frozen-thawed blastocysts was higher in Day 10 blastocysts than in day 8 and 9 blastocysts from defined culture system. Regardless of their age, survival rate of frozen-thawed blastocysts was significantly higher (p<0.05) in co-culture system than in defined culture system. 2. The cell number of blastocysts was significanlty higher (p<0.05) in Day 7 blasotcysts than in Day 8 and 9 blastocysts from co-cultures, but the cell number of blsstocysts was significantly higher (p<0.05) in Day 10 blastocysts than in Day 8 and 9 blastocysts from defined culture system. Regardless of the culture system, blastocysts with higher cell number showed higher survival rates after freezing and thawing.

  • PDF

Strength and Durability Properties of Polymer Concrete Utilizing Oyster Shell Powder as a Filler (굴 패각 분말을 충전재로 활용한 폴리머 콘크리트의 강도 및 내구 특성)

  • Sung, Chan-Yong;Kim, Young-Ik
    • Journal of The Korean Society of Agricultural Engineers
    • /
    • v.52 no.6
    • /
    • pp.125-134
    • /
    • 2010
  • This study was performed to evaluate the workability, strengths and durability of polymer concrete using oyster shell that are reclaimed at public shore illegally or leaved on the surroundings of shore to prevent the environmental pollution. We investigated the effect of oyster shell powder (OSP) and $CaCO_3$. on the slump, compressive strength, flexural strength, acid sulfuric and freezing and thawing resistance as a filler of polymer concrete. Modified OSP obtained by crushing oyster shell (less than 0.15 mm size) consists of 60.47 wt% of $SiO_2$ and 39.5 wt% of $CaCO_3$. As a result of slump test by OSP and $CaCO_3$. contents, it is found that slump of specimen used OSP is lower than that used $CaCO_3$. and the more OSP contents are, its slump is increased. Compressive and flexural strength of polymer concrete using OSP are similar or slightly lower than that using $CaCO_3$. In acid sulfuric test for 5 % $H_2SO_4$ and freezing thawing test, regardless of kinds of fillers and contents are not found fatal defects in weight change, falling-off in surface and durability factor.

Durability and mechanical performance in activated hwangtoh-based composite for NOx reduction

  • Kim, Hyeok-Jung;Park, Jang-Hyun;Yoon, Yong-Sik;Kwon, Seung-Jun
    • Advances in concrete construction
    • /
    • v.11 no.4
    • /
    • pp.307-314
    • /
    • 2021
  • Activated hwangtoh (ACT) is a natural resource abundant in South Korea, approximately 15.0% of soil. It is an efficient mineral admixture that has activated pozzolanic properties through high-temperature heating and rapid cooling. The purpose of this study is to improve a curb mixture that can reduce NOx outside and investigate durability performance. To this end, mortar curb specimens were manufactured by replacing OPC with ACT. The ACT substitution ratios of 0.0, 10.0, and 25.0% were considered, and mechanical and durability tests on the curb specimens were conducted at 28 and 91 days of age. Steam curing was carried out for three days for the production of curbs, which was very effective to strength development at early ages. The reduction in strength at early ages could be compensated through this process, and no significant performance degradation was evaluated in the tests on chloride attack, carbonation, and freezing and thawing. The mortar curb with an ACT of 10.0~25.0% replacement ratio exhibited clear NOx reduction through photocatalytic (TiO2) treatment. This is due to the increase in physical absorption through surface absorption and the photocatalyst-containing TiO2 coating. In this study, the reasonable range of the ACT replacement ratio for NOx reduction was quantitatively evaluated through a comprehensive analysis of each test.

Durability properties of fly ash-based geopolymer mortars with different quarry waste fillers

  • Tammam, Yosra;Uysal, Mucteba;Canpolat, Orhan
    • Computers and Concrete
    • /
    • v.29 no.5
    • /
    • pp.335-346
    • /
    • 2022
  • Geopolymers are an important alternative material supporting recycling, sustainability, and waste management. Durability properties are among the most critical parameters to be investigated; in this study, the durability of manufactured geopolymer samples under the attack of 10% magnesium sulfate and 10% sodium sulfate solution was investigated. 180 cycles of freezing and thawing were also tested. The experimentally obtained results investigate the durability of geopolymer mortar prepared with fly ash (class F) and alkali activator. Three different quarry dust wastes replaced the river sand aggregate: limestone, marble, and basalt powder as fine filler aggregate in three different replacement ratios of 25%, 50%, and 75% to produce ten series of geopolymer composites. The geopolymer samples' visual appearance, weight changes, UPV, and strength properties were studied for up to 12 months at different time intervals of exposure to sulfate solutions to investigate sulfate resistance. In addition, Scanning Electron Microscopy (SEM), EDS, and XRD were used to study the microstructure of the samples. It was beneficial to include quarry waste as a filler aggregate in durability and mechanical properties. The compact matrix was demonstrated by microstructural analysis of the manufactured specimens. The geopolymer mortars immersed in sodium sulfate showed less strength reduction and deterioration than magnesium sulfate, indicating that magnesium sulfate is more aggressive than sodium sulfate. Therefore, it is concluded that using waste dust interrogation with partial replacement of river sand with fly ash-based geopolymers has satisfactory results in terms of durability properties of freeze-thaw and sulfate resistance.

Estimation of Deterioration Depth of Rock Slope due to Freezing-thawing (동결융해에 의한 암반사면의 열화심도 산정)

  • Baek Yong;Seo Yong-Seok;Jeong Ja-Hyea;Kwon O-Ii
    • The Journal of Engineering Geology
    • /
    • v.15 no.3
    • /
    • pp.325-335
    • /
    • 2005
  • Deterioration depths of rock slope due to freezing-thawing were calculated using the 1-D heat conductivity equation. The temperature distribution analysis was carried out using temperature distribution data for last two years of the five major cities such as Seoul, Daejeon, Pohang, Gwangju and Cangneung. The analysis was performed based on three different types of rocks, sandstone, granite and gneiss. This study has found that the deterioration depths tend to be greater with the increase of the thermal conductivity coefficient in Seoul, Daejeon and Pohang where showing relatively greater temperature deviations. Regarding the influence of rock types, deterioration depths turned out to be greater in Gwangju and Gangneung where show relatively smaller temperature deviations among the five cities, assuming these cities are on the granite with thermal conductivity of $55,200\;cal/m\timesday\times^{\circ}C$. In contrast, for the other rock types, cities of relatively geater temperature deviations show deeper deterioration depth than the others. Deterioration depths of rock slope in Korea due to freezing-thawing fumed out to be around 8.4 m to 10.7 m.

Viability and Acrosomal Status Changes Following Post-thawing Canine Spermatozoa (개 정자의 동결융해 후 생존성 및 첨체의 변화)

  • 이영락;이성림;강태영;최상용
    • Journal of Embryo Transfer
    • /
    • v.18 no.1
    • /
    • pp.51-59
    • /
    • 2003
  • This study was carried out to evaluate the effect of different freezing and thawing rates on the viability, motility and acrosomal changes of frozen canine spermatozoa. The ejaculated semen was extended with Tris-egg yolk buffer containing 8% glycerol and equilibrated for 60 min after cooled to 4$^{\circ}C$ for 58 min. The straws were cryopreserved gradually by slow-cooling at different distance(6, 10 and 17 cm, respectively) from the liquid nitrogen (L$N_2$) to achieve temperature rate of 3, 8.9 and 19$^{\circ}C$ /min. Thawing of the straws was performed in a water bath fur 2 min at 37$^{\circ}C$ and 55$^{\circ}C$ , respectively. The motility of frozen-thawed spermatozoa was assessed by phase-contrast microscopy. To assess their viability and acrosome content, spermatozoa were stained with a vital stain and Fluorescence conjugated lectin Pisum Savitum Agglutinin (FITC/PAS), respectively. Concentration of the ejaculated fresh semen was normal range of 3.44 $\times$ 10$^{8}$ /ml. Freezing temperature were reduced to -110, -70 and -35$^{\circ}C$, as higher distance from liquid nitrogen, 6, 10 and 17 cm, respectively. Freezing at 3$^{\circ}C$/min in distance of 17 cm from liquid nitrogen yielded better motility, viability and rate of intact acrosome than 8.9 or 19$^{\circ}C$/min and the optimal thawing was 37$^{\circ}C$ for 2 min.

Effects of Semen Extender Containing Equex-STM Paste on Post-thaw Motility and Viability of Canine Sperm (Equex-STM paste 첨가 희석액이 개 정액의 동결.융해 후 정자활력 및 생존율에 미치는 영향)

  • 김용준;한종현;유일정;지동범
    • Journal of Veterinary Clinics
    • /
    • v.19 no.1
    • /
    • pp.80-85
    • /
    • 2002
  • This study was performed to investigate the freezomg condition especially focused on extender composition to achieve good post-thaw viability and motility of canine sperm. Semen were collected from 6 male dogs which had been proved to be fertile in the past and were treated for freezing. Equex-STM paste was contained in both the 1st(3%) and the 2nd(7%) diluent and the 2nd diluent was added to the 1st diluent following glycerol equilibration for an hour and a half. To investigate the effect of Equex-STM paste in the extender on post-thaw canine sperm characteristics, the post-thaw viability, motility, and HOS(Hypoosmotic swelling) values were evaluated according to the different composition of extender with or without Equex-STM paste, thawing conditions, and different thawing media added to thawed semen. 1. Canine sperm removed from seminal plasma and frozen )n Sweden extender containing Equex showed higher post-thaw viability, motility, and HOS values than those frozen in the extender containing Equex-STM paste with seminal plasma and those frozen in the extender without Equex and seminal plasma. 2. Canine sperm frozen in Sweden extender containing Equex-STM paste with 5% glycerol showed higher post-thaw viability, motility, and HOS values than those frozen with 3%, 8% glycerol or 5% DMSO. 3. The canine semen frozen in Sweden extender with 5% glycerol and Equex-STM paste showed higher viability, motility, and HOS values when thawed at $70^{\circ}C$ for 8 seconds than when thawed at $37.5^{\circ}C$ for 1 min and at $18-20^{\circ}C$ for 5 min. 4. TFC (tris -fructose-citrate) and PB S (phosphate buffered saline) medium added immediately to thawed canine semen brought better viability, motility, and HOS values for the sperm than those semen added with TGC(tris-glucose-citrate) and no medium. These results indicated that Equex-STM paste in Sweden extender for freezing the canine sperm which were removed from seminal plasma brought good post-thaw viability and motility of canine sperm. Also of the freezing conditions of canine sperm with the same extender containing Equex, the concentration of 5% glycerol, the thawing condition at $70^{\circ}C$ for 8 sec, and TFC and PBS medium added to the thawed semen brought better post-thaw viability and motility of canine sperm than the other conditions used in this study.

Effects of Deep Freezing Temperature for Long-term Storage on Quality Characteristics and Freshness of Lamb Meat

  • Choi, Mi-Jung;Abduzukhurov, Tolibovich;Park, Dong Hyeon;Kim, Eun Jeong;Hong, Geun-Pyo
    • Food Science of Animal Resources
    • /
    • v.38 no.5
    • /
    • pp.959-969
    • /
    • 2018
  • This study investigated the effects of deep freezing and storage temperature ($-50^{\circ}C$, $-60^{\circ}C$, and $-80^{\circ}C$) on the quality and freshness of lamb. To compare the qualities of deep frozen and stored lamb, fresh control and normal freezing conditions ($-18^{\circ}C$) were adopted. As quality and freshness parameters, drip loss (thawing loss and cooking loss), water-holding capacity (WHC), texture profile analysis (TPA), thiobarbituric acid reactive substances (TBARS), and total volatile basic nitrogen (TVBN) were evaluated during 5 months of storage. Temperature influenced the drip loss and WHC, and deep freezing minimized the moisture loss during frozen storage compared to the normal freezing condition. Lamb frozen and stored at deep freezing temperature showed better tenderness than that stored in normal freezing conditions. In particular, lamb frozen at lower than $-60^{\circ}C$ exhibited fresh lamb-like tenderness. Regardless of temperature, evidence of lipid oxidation was not found in any frozen lamb after 5 months, while TVBN was dependent on the applied temperature. Therefore, this study demonstrated that deep freezing could potentially be used to maintain freshness of lamb for 5 months. From the quality and economic aspects, the freezing and storage condition of $-60^{\circ}C$ is estimated as the optimum condition for frozen lamb.

ALC 의 내구성 및 물성개선에 관한 연구

  • 이범재;홍성수;황의환;조헌영;노재성
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1993.10a
    • /
    • pp.65-70
    • /
    • 1993
  • The effect of particle size of Al powder, water repellent agent and finishing agent on frost resistance, absorption ratio and structure of micropore was examined to improve the physical properties and durability of ALC. According as the amount added of water repellent agent was increased, frost resistance was improved and absorption ratio was decreased. From one side freezing /thaw test, finishing agent which has a low vapor permeation located the crack at close indoor point of ALC specimen. ALC produced from fine Al powder has a low volume reduction by scalling and a sound appearance after freezing/thawing test and top surface freezing test, The crystal of tobermorite in ALC matrix was converted to calcium carbonate by carbonation which was accelerated with the decreasing of water content. Since the micropore of ALC was filled up by calcium carbonate, void ratio was reduced and crack was detected after complete carbonation.

  • PDF