• Title/Summary/Keyword: freeze-thaw damage

Search Result 70, Processing Time 0.028 seconds

Strength Development and Freeze-Thaw Resistance of Concrete Incorporating High Volume Blast-Furnace Slag Subjected to Initial Frost Damage (초기동해를 받은 고로슬래그 다량 혼입 콘크리트의 강도발현 및 동결융해 저항성)

  • Koh, Kyung-Taek;Ryu, Gum-Sung
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.6 no.3
    • /
    • pp.79-87
    • /
    • 2011
  • Concrete incorporating high volume blast-furnace slag placed in cold weather regions might be in danger of initial frost damage because dependently on the mix proportions, the setting and the hardening would be remarkably delayed. Therefore, this study investigated to effect of the degree of frost on the strength development and the resistance to freezing and thawing of the concrete incorporating blast-furnace slag when being subjected to freeze at early age. As the experimental results, the concrete incorporating blast-furnace slag attacked by initial frost damage showed the remarkable reduction of both the compressive strength development and the resistance to freezing and thawing. Especially, the resistance to freezing-thawing of the concrete incorporating high volume blast-furnace slag became much lower than that of the normal concrete.

  • PDF

Properties of High Strength Concrete Incorporating Fine Blast Furnace Slag (고로 슬래그 미분말을 사용한 고강도 콘크리트의 특성)

  • Lee, Bong-Hak;Lee, Joo-Hyung;Hong, Chang-Woo
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.40 no.5
    • /
    • pp.59-67
    • /
    • 1998
  • The object of this study is to investigate the strength characteristics and the freeze-thaw resistance of high strength concrete incorporating fine blast furnace slag. Major experimental variables were the water/cement ratio, maximum size of coarse aggregate, and cement types such as ordinary portland and slag cement. The results were as follows ; The workability of fresh concrete incorporating fine blast furnace slag was better than that of OPC(ordinary Portland cement) in terms of slump. The freeze-thaw resistance showed better than that of OPC, keeping more than 90% of relative modules of elasticity after 506 cycles and showing only a hair crack at surface without serious damage. Thus, the fine blast furnace slag might be recycled at concrete to make high strength concrete at fields.

  • PDF

Electrical Resistance Characteristics of Conductive Cement Composite with Deterioration Damage (열화손상이 발생된 전도성시멘트복합체의 전기저항특성)

  • Kim, Young-Min;Lee, Gun Cheol
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2020.11a
    • /
    • pp.149-150
    • /
    • 2020
  • Granting self-sensing performance in a building is an important performance to ensure the degree of damage and safety of the building. Since the current research is being conducted in the state before deterioration loss occurs, it is necessary to confirm whether the self-sensing performance is maintained even in the damaged conductive cement composite. As part of the study, electrical resistance characteristics were analyzed in conductive cement composites in which freeze-thawing and chemical corrosion occurred. As a result, it was found that the change in electrical resistance value due to freeze-thawing was not as large as 1%, and chemical corrosion occurred. It was found that the change in electrical resistance value of the tested specimen increased by about 10%.

  • PDF

Classification of cold regions and analysis of the freeze-thaw repetition cycle based on heat transfer quantity by freezing test (실내동결시험을 통한 열류량 분석에 따른 동결-융해 조건 분석 및 한랭지역의 분류)

  • An, Jai-Wook;Seo, Jeong-Eun;Jung, Min-Hyung;Seong, Joo-Hyun
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.20 no.6
    • /
    • pp.957-972
    • /
    • 2018
  • Tunnels constructed in cold regions can cause serious defects such as cracks and leaks due to external temperature changes in the portals and vents. In order to prevent the freezing damage of the tunnel, appropriate measures should be applied to the section where the freeze damage is concerned. However, the specific criteria and contents for judging whether or not the anti-freeze measures are applied are not presented. In this study, the laboratory freezing tests on the temperature changes of the concrete specimens under freezing conditions were carried out. And the freeze-thaw repetition cycle (F), which can judge the possibility of freezing damage, were presented based on the heat transfer quantity (W) by experimental results of case studies. Also, we propose a classification of cold regions considering the climatic characteristics of Korea for using it to efficient design and maintenance.

Evaluation of Freeze-Thaw Damage on Concrete Using Nonlinear Ultrasound (초음파의 비선형 특성을 이용한 콘크리트 동결융해 손상 평가)

  • Choi, Ha-Jin;Kim, Ryul-Ri;Lee, Jong-Suk;Min, Ji-Young
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.25 no.4
    • /
    • pp.56-64
    • /
    • 2021
  • Leakage due to deterioration and damage is one of the major causes of volume change by freezing and thawing, and it leads micro-cracking and surface scaling in concrete structures. The deterioration of damaged concrete accelerates with the chloride attack. Thus, in the detailed guidelines for facility performance evaluation (2020), the quality of cover concrete and the freeze-thaw (FT) repetition cycle were newly suggested for concrete durability assessment. The quality of cover concrete should be evaluated by the rebound hammer test and the FT repetition cycle should be also considered in the deterioration environmental assessment. This study suggested the application of fast dynamic based nonlinear ultrasound method to monitor initial micro-scale damage under freezing and thawing environment. Concrete specimens were fabricated with different water-cement ratios (40%, 60%) and air contents (1.5% and 3.0%). The compressive strength, rebound number, relative dynamic modulus, and nonlinear ultrasound were measured with different FT cycles. The scanning electron microscopy was also performed to investigate the micro-scale FT damage. As a result, both the rebound number and the relative dynamic modulus had difficulty to detect early damage but the proposed method showed a potential to detect initial micro-scale damage and predict the FT resistance performance of concrete.

A Study on the Freeze-Thaw Resistance of Planting Concrete Using Recycled Aggregate (재생골재를 이용한 식재용 콘크리트의 동결융해저항성에 관한 연구)

  • 이상태;전충근;김경민;최청각;한천구
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2003.05a
    • /
    • pp.233-236
    • /
    • 2003
  • This study is intended to investigate the resistance of frost damage of concrete for planting, which recycled aggregate is used, by freezing in air and thawing in water. According to the results, if AE agent of 0.005% is mixed in making concrete for planting, it is thought that the resistance of frost damage is guaranteed in winter because concrete for planting is not under severe freezing and thawing function, but under natural weather action.

  • PDF

Performance Evaluation of Bridge Deck Materials based on Ordinary Portland Cement Concrete (보통 포틀랜드 콘크리트 기반 교면포장 재료 성능 평가)

  • Nam, Jeong-Hee;Jeon, Seong Il;Kwon, Soo Ahn
    • International Journal of Highway Engineering
    • /
    • v.19 no.6
    • /
    • pp.129-137
    • /
    • 2017
  • PURPOSES : The purpose of this study is to develop bridge deck concrete materials based on ordinary Portland cement concrete, and to evaluate the applicability of the developed materials through material properties tests. METHODS : For field implementation, raw material (cement, fine aggregate, and coarse aggregate) properties, fresh concrete properties (slump and air content), strength (compressive, flexural and bond strength) gain, and durability (freeze-thaw resistance, scaling resistance, and rapid chloride penetrating resistance) performance were evaluated in the laboratory. RESULTS : For the selected binder content of $410kg/m^3$, W/B = 0.42, and S/a = 0.48, the following material performance results were obtained. Considering the capacity of the deck finisher, a minimum slump of 150 mm was required. At least 6 % of air content was obtained to resist freeze-thaw damage. In terms of strength, 51.28 MPa of compressive strength, 7.41 MPa of flexural strength, and 2.56 MPa of bond strength at 28 days after construction were obtained. A total of 94.9 % of the relative dynamic modulus of elasticity after 300 cycles of freeze-thaw resistance testing and $0.0056kg/m^2$ of weight loss in a scaling resistance test were measured. However, in a chloride ion penetration resistance test, the result of 3,356 Coulomb, which exceeds the threshold value of the standard specification (1000 Coulomb at 56 days) was observed. CONCLUSIONS : Instead of using high-performance modified bridge deck materials such as latex or silica fume, we developed an optimum mix design based on ordinary Portland cement concrete. A test construction was carried out at ramp bridge B (bridge length = 111 m) in Gim Jai City. Immediately after the concrete was poured, the curing compound was applied, and then wet mat curing was applied for 28 days. Considering the fact that cracks did not occur during the monitoring period, the applicability of the developed material is considered to be high.

Comparative Study on Freeze-Thaw Durability of General Concrete and Pavement Concrete (일반콘크리트와 포장콘크리트의 동결융해 내구성에 대한 비교 연구)

  • Kim, Hyun-Joong;Lee, Beung-Duk;Lee, Ju-Gang
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.04a
    • /
    • pp.561-564
    • /
    • 2008
  • Concrete scaling is the progressive surface deterioration of susceptible subjected to freeze-thaw cycling in the presence of moisture. Particularly, it has been recognized that chlorides present in deicing agents can significantly increase concrete surface scaling. Domestic area of most be happened chloride deicer damage. Because daily mean temperature is below 0$^{\circ}C$ from the area of domestic most. Use of deicing chemicals has been and will continue to be a major part of highway snow and ice control methods. Chloride-containing chemicals such as calcium chloride or rock salt are main deicers for the road. Extensive use of chloride deicers is, however, not only the source of substantial cost penalties due to their corrosive action and ability to deterioration roadway surface materials but also the source of environmental damages. In this study, Use of (40, 27, 21MPa) pavement concrete analyze freeze-thaw test and scaling on the chlorides present.

  • PDF

Flexural and Cracking Characteristics of Concrete Beams Exposed to Freeze-Thaw Cycles after Patch-Repaired with SHCC (SHCC로 단면 복구후 동결융해에 노출된 콘크리트 보의 휨 및 균열특성)

  • Yun, Hyun-Do;Kim, Sun-Woo;Jeon, Ester;Lee, Young-Oh;Jang, Kwang-Soo;Park, Whan-Shin
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2009.05a
    • /
    • pp.21-22
    • /
    • 2009
  • This paper presents the results of an experimental study on flexural behavior and cracking process of concrete beams subjected to cycles of freezing and thawing after patch-repaired with strain-hardening cement composites (SHCCs). The SHCCs were reinforced with hybrid 0.75% PVA and 0.75% PE fibers. Experimental testing of concrete beams patch-repaired with SHCCs revealed that the SHCC patch-repair system without freeze thaw (FT) exposure showed average 3.31 times increased load carrying capacity and for beams exposed to 300 FT cycles, load carrying capacity increased up to 2.42 times. Cracking damage of SHCC patch-repaired beams mitigated compared to plain concrete beams but this trend decreased under FT exposure.

  • PDF

Fundamental Study on High Strength and High Durability Cement Concrete Pavement: Part II Strength and Durability Evaluations (시멘트콘크리트 포장의 고강도 고내구성을 위한 기초 연구 : Part II 최적배합콘크리트의 강도 및 내구특성 분석)

  • Yun, Kyong-Ku;Park, Cheol-Woo;Hong, Seung-Ho
    • International Journal of Highway Engineering
    • /
    • v.11 no.3
    • /
    • pp.51-60
    • /
    • 2009
  • This study investigates the fresh state characteristics, strength, chloride ion penetration resistance and freeze-thaw resistance of the suggested high strength-high durability cement concrete pavement. The required workability and air content could be achieved by using an appropriate admixtures. However its dosage should be carefully determined through field trial batches. Compressive strength increased with the increased cement content and, in particular, high cement volume concrete continuously developed strength up to 90 days. No clear relationship, however, existed between flexural strength and cement content. Chloride penetration resistance seemed as a function of curing age rather than the cement content. Freeze-thaw resistance test was conducted using two different coolants, tap water and 4% NaCl solution. When the tap water was used no severe damage was observed up to 300 cycles regardless the air content. Under 4% NaCl solution, specimens of 326kg/$m^3$ cement content showed severe damage with surface scaling. Based on the experimental investigations herein, it is highly recommended that the cement content be greater than 400kg/$m^3$ for strength-high durability cement concrete pavement structures.

  • PDF