$Al_2O_3$$Al_2O_3$ -$SiC_w$ 복합재료의 동적 및 정적 파괴인성에 관한 연구 (Dynamic and Quasi-Static Fracture Toughness of $Al_2O_3$ and $Al_2O_3$ Ceramic Matrix Composite Reinforced with Sic Whiskers)

  • 조경목;이성학;표성규;장영원
    • 한국세라믹학회지
    • /
    • 제27권4호
    • /
    • pp.457-464
    • /
    • 1990
  • This paper presents the influence of the loading rate on the room temperature fracture toughness of a brittle Al2O3 and a SiC whisker reinforced Al2O3 composite. Dynamic fracture toughness tests were conduced using compressive fatigue pre-cracked notched round bars loaded in tension to produce a stress intensity rate K1=106 MPa√m/sec. The experimental results show that for each loading rate the fracture toughness values obtained for the ceramic matrix composite are higher than the corresponding values for the single phase alumina. In addition, both the reinforced and unreinforced ceramic are singnificantly tougher under dynamic loading than static loading. This dynamic and quasi-static fracture initiation behaviro can be interpreted by identifying quantitatively the mode of fractuer initiation as a function of loading rate.

  • PDF

The effect of nonlinear groundwater flow on DNAPL migration in a rough-walled single fracture

  • 지성훈;이항복;여인욱;이강근
    • 한국지하수토양환경학회:학술대회논문집
    • /
    • 한국지하수토양환경학회 2005년도 총회 및 춘계학술발표회
    • /
    • pp.68-71
    • /
    • 2005
  • We conducted simple experiments to consider the influence of nonlinear groundwater flow on Trichloroethylene (TCE) as Dense Non-Aqueous Phase Liquid (DNAPL) migration in a rough walled single fracture. A glass replica of a granite sample containing a rough single fracture was made and experiments were conducted over a range of Re. Observations are compared to the results of TCE migration tests that were conducted in two parallel glass plates over the same range of Re. Results show nonlinear groundwater flow in a single fracture affect TCE migration path and residual saturation of TCE.

  • PDF

놋취가 있는 복합적층판의 잔류강도 해석 (Residual strength analysis for notched composite laminates)

  • 김성준;황인희
    • 한국항공운항학회지
    • /
    • 제20권1호
    • /
    • pp.103-111
    • /
    • 2012
  • This study reviews several fracture models for predicting the residual strength of notched composite laminates. Representative experimental results on the residual strength of composite laminates containing a notch subjected to static uniaxial tensile loading have been collected from open literature. And notched strength data for T300/5208 are analyzed. The various parameters associated with the fracture models have been determined for laminates. Notched strength data sets are compared with fracture models and the applicability of the different fracture models in predicting the notched strength of composite laminates is discussed. And static tests have been performed on 2.0mm depth notched specimen. And the test results are compared with analysis models.

A coupled damage-viscoplasticity model for the analysis of localisation and size effects

  • Georgin, J.F.;Sluys, L.J.;Reynouard, J.M.
    • Computers and Concrete
    • /
    • 제1권2호
    • /
    • pp.169-188
    • /
    • 2004
  • A coupled damage-viscoplasticity model is presented for the analysis of localisation and size effects. On one hand, viscosity helps to avoid mesh sensitivity because of the introduction of a length scale in the model and, on the other hand, enables to represent size effects. Size effects were analysed by means of three-point bending tests. Correlation between the fracture energy parameter measured experimentally and the density fracture energy modelling parameter is discussed. It has been shown that the dependence of nominal strength and fracture energy on size is determined by the ligament length in comparison with the width of the fracture process zone.

초소형 무연 단일 솔더볼 연결부의 전단강도 평가 (Evaluation of Shear Strength of a Miniature Lead-free Single Solder Ball Joint)

  • 주세민;김호경
    • 한국안전학회지
    • /
    • 제25권6호
    • /
    • pp.14-21
    • /
    • 2010
  • A miniature single solder ball joint is designed to mimic the actual solder joints used in the micro-electric industries. Shear tests were conducted to evaluate the mechanical behavior of miniature single solder joints at intermediate strain rates from $0.019\;s^{-1}$ to $2.16\;s^{-1}$ at room temperature. The shear fracture strength of the present solder ball joints generally increased with increasing shear strain rate, ranging from 32 to 51MPa. This behavior is affected by the sensitivity of bulk solder strength to strain rate. Shear fracture mode changed from brittle to partial ductile (failure inside the bulk solder) with an increase of shear speed. The unloading shear fracture toughness is generally consistent with the measure of the amount of bulk solder on the fractured surface.

A fracture criterion for high-strength steel cracked bars

  • Toribio, J.
    • Structural Engineering and Mechanics
    • /
    • 제14권2호
    • /
    • pp.209-221
    • /
    • 2002
  • In this paper a fracture criterion is proposed for cracked cylindrical samples of high-strength prestressing steels of different yield strength. The surface crack is assumed to be semi-elliptical, a geometry very adequate to model sharp defects produced by any subcritical mechanism of cracking: mechanical fatigue, stress-corrosion cracking, hydrogen embrittlement or corrosion fatigue. Two fracture criteria with different meanings are considered: a global (energetic) criterion based on the energy release rate G, and a local (stress) criterion based on the stress intensity factor $K_I$. The advantages and disadvantages of both criteria for engineering design are discussed in this paper on the basis of many experimental results of fracture tests on cracked wires of high-strength prestressing steels of different yield strength and with different degrees of strength anisotropy.

세라믹/금속 접합재에 대한 정적강도의 파괴역학적 평가 (Evaluation of Static Strength Applying to Fracture Mechanics on Ceramic/Metal bonded Joint)

  • 김기성
    • 한국생산제조학회지
    • /
    • 제5권4호
    • /
    • pp.53-62
    • /
    • 1996
  • Recently, ceramic / metal bonded joints have led to inccreasing use of structural materials such as automobile, heat engine in various industries. In this paper, a method to analyze an interface crack under both residual stresses and applied loading was proposed. and some results of boundary element method(BEM) analysis Were presented, Fracture thoughness tests of ceramic/metals bonded joints with an interface crack Were carried out, and the stress intensity factors of these joints Ware analyzed by BEM. Also crack propagtion direction was simulated numerically by using BEM. Crack propagation angle was able to easily determine based on the maximum stress concept. The prediction of fracture strength by the fracture thoughness of the ceramics/metals bonded joints was proposed.

  • PDF

고속철도용 차륜재의 파괴 역학적 특성 (Fracture Mechanics Characteristics of Wheel Materials for High Speed Train)

  • 권석진;서정원;허현무;권성태
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2005년도 추계학술대회 논문집
    • /
    • pp.20-23
    • /
    • 2005
  • The service demands of railway vehicles have become severe in recent years due to a general increase in operating speeds. It is very important to evaluate the fracture mechanics characteristics with respect to high-speed train wheel. In the present study, fracture mechanics characterization tests were carried out in accordance with various wheel materials. The result shows that fracture mechanics characteristic should be considered in the design code of the wheel materials.

  • PDF

Evaluation of Fracture Behavior of SA-516 Steel Welds Using Acoustic Emission Analysis

  • Na, Eui-Gyun;Ono, Kanji;Lee, Dong-Whan
    • Journal of Mechanical Science and Technology
    • /
    • 제20권2호
    • /
    • pp.197-204
    • /
    • 2006
  • The purpose of this study is to evaluate the AE characteristics for the basemetal, PWHT (post-weld heat treatment) and weldment specimens of SA-516 steel during fracture testing. Four-point bending and AE tests were conducted simultaneously. AE signals were emitted in the process of plastic deformation. AE signal strength and amplitude of the weldment was the strongest, followed by PWHT specimen and basemetal. More AE signals were emitted from the weldment samples because of the oxides, and discontinuous mechanical properties. AE signal strength and amplitude for the basemetal or PWHT specimen decreased remarkably compared to the weldment because of lower strength. Pre-cracked specimens emitted even lower event counts than the corresponding blunt notched specimens. Dimple fracture from void coalescence mechanism is associated with low-level AE signal strength for the basemetal or PWHT. Tearing mode and dimple formation were shown on the fracture surfaces of the weldment, but only a small fraction produced detectable AE.

혼합모드하에서의 레일강의 파괴거동 (Fracture Behavior of Rail Steel under Mixed Mode Loading)

  • 장동일;김성훈
    • 대한토목학회논문집
    • /
    • 제14권4호
    • /
    • pp.761-769
    • /
    • 1994
  • 열차 바퀴의 접촉하중에 의해 레일이 받는 하중형식은 모드 I과 모드 II가 조합된 혼합모드 하중 상태로서 본 연구에서는 레일강의 피로파괴거동을 규명하기 위해 Richard가 개발한 혼합모드 파괴시험편 및 시험 지-그(Jig)를 이용하여 파괴시험을 실시하였으며 그 결과로부터 혼합모드에 대한 용력강도계수의 상관관계를 이용하여 균열성장경로를 평가하고 기제안된 다양한 파괴기준을 비교하였다. 그 결과, 레일강의 균열성장경로는 최대원주응력설과 변형에너지밀도설을 파괴기준은 주변형률설을 따름을 알 수 있었다.

  • PDF