국내 석탄회 육상매립의 오염 잠재성 평가 (Assessment of potential environmental impact from fly ash landfill)

  • 이상훈
    • 환경영향평가
    • /
    • 제8권4호
    • /
    • pp.25-35
    • /
    • 1999
  • Fly ash, by-product from coal fired power station, has long been regarded as a potential contamination source for heavy metals and inorganics due to their enriched concentrations and associations with particle surface. Feed coal and fly ash samples were collected from two power stations; Yongdong deliang with domestic anthracite coals and Boryong with imported bituminous coals. The coal and fly ash samples were analyzed for chemical composition and mineral components, using XRF and XRD. Batch leaching experiments were conducted by agitating samples with deionised water for 24 hours. Anthracite coals are generally higher in Al and Si contents than bituminous coals. This is due to the higher ash contents of the anthracite coal than bituminous coal. The chemistry of the two fly ash samples shows broadly similar compositions each other, except for the characteristically high contents of Cr in anthracite coal fly ash. Leaching experiments revealed that concentrations of metals gradually decreased with leachings in general. However, measurable amounts of metals were present in the effluent from weathered ash and the samples subjected to the leaching procedure. These metals are likely to indicate that the metals in fly ash were incorporated into glass fraction as well as associated with particle surface of samples. Dissolution of aluminosilicate glass would control releasing heavy metals from fly ash as weathering progresses during landfill with implication of possible groundwater contamination through fly ash landfill.

  • PDF

Efficiency factor of high calcium Class F fly ash in concrete

  • Sata, V.;Khammathit, P.;Chindaprasirt, P.
    • Computers and Concrete
    • /
    • 제8권5호
    • /
    • pp.583-595
    • /
    • 2011
  • This paper studied the cement efficiency factor (k factor) of high calcium Class F fly ash. This k factor represents a unit of fly ash with efficiency equivalent to k unit of cement. The high calcium Class F fly ash was used to replace cement in concrete. The modified Bolomey's law with linear relationship was used for the analysis of the result of compressive strength, cement to water ratio (c/w) and fly ash to water ratio (f/w) by using the multi-linear regression to determine the k factor and other constants in the equations. The results of analysis were compared with the results from other researcher and showed that the k factor of high calcium Class F fly ash depends on the fineness of fly ash, replacement level and curing age. While the amount of CaO content in Class F fly ash not evident. Furthermore, necessary criteria and variables for the determination of the k factor including the use of the k factor in concrete mix design containing fly ash were proposed.

플라이애시 콘크리트의 수화발열 특성과 압축강도 특성에 관한 실험적 연구 (An Experimental Study on Hydration Heat and Strength Properties Concrete with High Volume Fly-Ash)

  • 김우상;김광기;백민수;김우재;정재영;정상진
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2003년도 학술.기술논문발표회
    • /
    • pp.67-71
    • /
    • 2003
  • This study is for the great quantity use of fly-ash. For the producing of high volume concrete from the use of fly-ash, the method of replacement between bonding agents and fine aggregate by fly-ash at the same time was used. It was used that the adiabatic temperature rise of concrete about the mass member which bad been produced by the method that was mentioned before, and the hydration heat of the core test pieces in concrete was measured. Also the core test pieces which were replaced with fly-ash was studied by the compressive streneth's comparison between standard care test pieces and core test pieces. In the case of mass test pieces, hydration heat and the tine to reach the highest temperature were decreased by an increase in replaced fly-ash's amounts of concrete. In addition, among the test pieces having the same amounts of concrete, the test pieces having more replaced amounts of fly-ash's fine aggregate showed higher hydration heat and the increased time to reach the highest temperature. Compressive strength was also increased by hydration heat's decrease according to fly-ash replacement. Replacement of fly-ash was more effective in high temperature environment.

  • PDF

Experimental Investigation of Clay Fly Ash Bricks for Gamma-Ray Shielding

  • Mann, Harjinder Singh;Brar, Gurdarshan Singh;Mann, Kulwinder Singh;Mudahar, Gurmel Singh
    • Nuclear Engineering and Technology
    • /
    • 제48권5호
    • /
    • pp.1230-1236
    • /
    • 2016
  • This study aims to determine the effect of fly ash with a high replacing ratio of clay on the radiation shielding properties of bricks. Some interaction parameters (mass attenuation coefficients, half value layer, effective atomic number, effective electron density, and absorption efficiency) of clay fly ash bricks were measured with a NaI(Tl) detector at 661.6 keV, 1,173.2 keV, and 1,332.5 keV. For the investigation of their shielding behavior, fly ash bricks were molded using an admixture to clay. A narrow beam transmission geometry condition was used for the measurements. The measured values of these parameters were found in good agreement with the theoretical calculations. The elemental compositions of the clay fly ash bricks were analyzed by using an energy dispersive X-ray fluorescence spectrometer. At selected energies the values of the effective atomic numbers and effective electron densities showed a very modest variation with the composition of the fly ash. This seems to be due to the similarity of their elemental compositions. The obtained results were also compared with concrete, in order to study the effect of fly ash content on the radiation shielding properties of clay fly ash bricks. The clay fly ash bricks showed good shielding properties for moderate energy gamma rays. Therefore, these bricks are feasible and eco-friendly compared with traditional clay bricks used for construction.

Experimental study on creep behavior of fly ash concrete filled steel tube circular arches

  • Yan, Wu T.;Han, Bing;Zhang, Jin Q.;Xie, Hui B.;Zhu, Li;Xue, Zhong J.
    • Steel and Composite Structures
    • /
    • 제27권2호
    • /
    • pp.185-192
    • /
    • 2018
  • Fly ash can significantly improve concrete workability and performance, and recycling fly ash in concrete can contribute to a cleaner environment. Since fly ash influences pozzolanic reactions in concrete, mechanical behaviors of concrete containing fly ash differ from traditional concrete. Creep behaviors of fly ash concrete filled steel tube arch were experimentally investigated for 10% and 30% fly ash replacement. The axes of two arches are designed as circular arc with 2.1 m computed span, 0.24 m arch rise, and their cross-sections are all in circular section. Time dependent deflection and strain of loading and mid-span steel tube were measured, and long term deflection of the model arch with 10% fly ash replacement was significantly larger than with 30% replacement. Considering the steel tube strain, compressive zone height, cross section curvature, and internal force borne by the steel tube, the compressive zone height and structural internal forces increased gradually over time due to concrete creep. Increased fly ash content resulted in more significant neutral axis shift. Mechanisms for internal force effects on neutral axis height were analyzed and verified experimentally.

플라이애시를 대량 사용한 콘크리트의 수화열특성 및 강도특성에 관한 연구 (A Study on Hydration Heat Properties and Strength Properties of High Volume Fly-Ash Concrete)

  • 백민수;이영도;정상진
    • 한국건축시공학회지
    • /
    • 제3권3호
    • /
    • pp.135-142
    • /
    • 2003
  • This study is for the great quantity use of fly-ash. For the producing of high volume concrete from the use of fly-ash, the method of replacement between bonding agents and fine aggregate by fly-ash was used at the same time. It was used that the adiabatic temperature rise of concrete about the mass member which had been produced by the method that was mentioned before, and the hydration heat of the core test pieces in concrete was measured. Also the core test pieces which were replaced with fly-ash was studied by the compressive strength's comparison between standard care test pieces and core test pieces. In the case of mass test pieces, hydration heat and the time to reach the highest temperature were decreased by an increase in replaced fly-ash's amounts of concrete. In addition, among the test pieces having the same amounts of concrete, the test pieces having more replaced amounts of fly-ash's fine aggregate showed higher hydration heat and the increased time to reach the highest temperature. Compressive strength was also increased by hydration heat's decrease according to fly-ash replacement. Replacement of fly-ash was more effective in high temperature environment.

Structural performance of concrete containing fly ash based lightweight angular aggregates

  • Pati, Pritam K.;Sahu, Shishir K.
    • Advances in concrete construction
    • /
    • 제13권4호
    • /
    • pp.291-305
    • /
    • 2022
  • The present investigation deals with the production of the innovative lightweight fly ash angular aggregates (FAA) first time in India using local class 'F' fly ash, its characterization, and exploring the potential for its utilization as alternative coarse aggregates in structural concrete applications. Two types of aggregates are manufactured using two different kinds of binders. The manufacturing process involves mixing fly ash, binder, and water, followed by the briquetting process, sintering and crushing them into suitable size aggregates. Tests are conducted on fly ash angular aggregates to measure their physical properties such as crushing value, impact value, specific gravity, water absorption, bulk density, and percentage of voids. Study shows that the physical parameters are significantly enhanced as compared to commercially available fly ash pellets (FAP). The developed FAA are used in concrete vis-à-vis conventional granite aggregates and FAP to determine their compressive, split tensile and flexural strengths. Although being lightweight, the strength parameters for concrete containing FAA are well compared with conventional concrete. This might be due to the high pozzolanic reaction between fly ash angular aggregates and cement paste. Also, RCC beams are cast and the load-deflection behaviour and ultimate load carrying capacity signify that FAA can be suitably used for RCC construction. Hence, the utilization of fly ash as angular aggregates can reduce the dead load of the structure and at the same time serves as a solution for fly ash disposal and mineral depletion problem.

High-Volume 플라이애쉬 콘크리트의 건조수축특성 (Drying Shrinkage of High-Volume Fly Ash Concrete)

  • 최석균;이광명;이진용
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1999년도 학회창립 10주년 기념 1999년도 가을 학술발표회 논문집
    • /
    • pp.195-198
    • /
    • 1999
  • Fly ash is the most common artificial pozzolan, which is a material precipitated electrostatically from the exhaust gases of coal-fired power stations. Fly ash can be used as the supplementary material as well as the material for high performance concrete and hence, the development of high-volume fly ash concrete is imperative. In this study, the characteristics of drying shrinkage of high volume fly ash concrete is investigated. It is found from test results that as the replaced amount of fly ash in concrete is increased, drying shrinkage of concrete is reduced.

  • PDF

많은 양의 플라이애쉬를 혼입한 콘크리트의 굳기전 특성 및 강도 발현 (Fresh Properties and Strength Development of High Volume Fly Ash Concrete)

  • 이진용;최수홍;강석화;이광명
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 가을 학술발표회 논문집(I)
    • /
    • pp.99-104
    • /
    • 1998
  • A study is carried out to investigate the characteristics of concrete various level(0~60%) of fly ash. These results indicate that compressive strength of fly ash concrete seems to be slightly higher than that of ordinary concrete between 7 and 28 days, thereafter the strength of fly ash concrete is significantly higher. In fresh properties of the fly ash concrete, the loss of slump and air content with time up to 120 minutes is lower, but the setting time is increased with increasing fly ash content.

  • PDF

플라이애쉬를 사용한 시멘트 모르터의 강도에 관한 연구 (The Strength of the Portland-Cement Mortar Use of Fly-ash)

  • 서기원;서치호
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1991년도 봄 학술발표회 논문집
    • /
    • pp.19-22
    • /
    • 1991
  • In order to the Utilization of Fly ash, The Properties of cement Mortar use of Fly ash based on Mixing rate, strength of mortar, W/C+F and quantity of Fly ash, Flow value, and unit weight are investigated. So follow result are unit weight of mortar of Fly ash is about 2014 Kg/㎥, Compressive strength of mortar is 50-404 Kg/$\textrm{cm}^2$ and beneficial reference to the utility of domestic Fly ash were obtained.

  • PDF