• 제목/요약/키워드: flexural test

검색결과 1,908건 처리시간 0.052초

전단보강에 따른 일방향 중공슬래브의 휨 성능 평가 (Evaluation on Flexural Performance of One-Way Hollow Slabs according to the Shear Reinforcement)

  • 유유진;석근영;김기철;강주원
    • 한국공간구조학회논문집
    • /
    • 제14권2호
    • /
    • pp.79-86
    • /
    • 2014
  • The purpose of this study is intended to determine the validity of shear reinforcement by evaluating flexural performance in the hollow slab. The hollow slab is relatively light and second moment of inertia is large. Due to these characteristics, it can be used to slab system efficiently. Therefore the prediction of the structural behaviors is very important because of decrease of shear and flexural strength which is caused by hollow section of slab interior. In this study, the flexural test were performed to analyze the flexural capacity of the hollow slab w/ or w/o shear reinforcement. A total of six full scale specimens were tested. These specimens have three cases of reinforcing bar ratio, 0.009, 0.018 and 0.024. To verify the flexural behavior such as ultimate load, load-deflection and crack pattern, the flexural experiment were tested by using loading frame. Experimental results have shown that the flexural behavior are depend on the reinforcing bar ratio. Also the hollow slab with shear reinforcement have shown flexural behavior. Therefore, it is appropriate that the hollow slab is reinforced by shear reinforcement to improve the flexural performance of the hollow slab.

현장인발시험을 통한 섬유형 쏘일네일의 거동특성 평가 (Evaluation of Behavior Characteristics of Geosynthetic Fiber Nail System from the Field Pull-Out Tests)

  • 김홍택;박시삼;조병국;정성필
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2004년도 춘계학술발표회
    • /
    • pp.342-347
    • /
    • 2004
  • Excavation nearby the existing structures is being performed vigorously to get the greatest use of land along with fast economic growth in the downtown area. The application of soil nailing system gradually increases because of an advantage of soil nailing system adjacently constructed in the existing structures. In this study, friction resistance by pull-out is considered as main resistance except resistance formed by flexural rigidity of nail observing that resistance of flexural rigidity is about $0{\sim}15\;%$ of whole safety factor according to degree of flexural rigidity in general soil nail wall and application of geosynthetic fiber soil nailing system is evaluated through laboratory tensile strength test and field pull-out test.

  • PDF

변형에폭시계 재료를 사용한 하부증대 보의 구조적 성능 (Structural Performance of Flexural Members Enlarged with Epoxy Mortar System at Soffit)

  • 홍건호;조하나;신영수;정혜교
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 가을 학술발표대회 논문집(III)
    • /
    • pp.833-838
    • /
    • 1998
  • This paper is aimed to investigate structural performance of flexural members enlarged with epoxy mortar at soffit. Main test variables are steel ratio and interface treatment method and six test beams are tested to investigate the effect of each test variables on maximum load capacity, load-deflection and moment-curvature relationship, interface behavior and failure mode. Test results show that section enlarged beams can carry almost same load of the monolithic beams with same size and the flexural stiffness and cracking moments are increased about 2.5 times and 50 to 70%of failure moment in comparison with same sized control beam, respectively. However, deflections and curvatures are decreased at the same load and interface fractures are not discovered at the ultimate load.

  • PDF

주철근비에 따른 고강도 콘크리트 보의 휨거동 (The Effect of Longitudinal Steel Ratio on Flexural Behavior of Reinforced High Strength Concrete Beams)

  • 김진근;박찬규
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1994년도 봄 학술발표회 논문집
    • /
    • pp.71-76
    • /
    • 1994
  • Eight singly reinforced high strength concrete beams were tested to investigate their flexural behavior. The variable is tensile steel raio. The test results are presented in terms of load-deformation behavior, ductility indexes, and cracking patterns. The flexural strengths obtained experimentally are compapred to the analytical results, and good agreements are obtained. The flexural design provisions of the ACI Building Code are found to be adequate to predict the strength of reinforced high-strength concrete beams.

  • PDF

An Experimental Study on the Flexural Strength of Fiber Reinforced Concrete Structures

  • Chai, Won-Kyu
    • International Journal of Safety
    • /
    • 제11권2호
    • /
    • pp.26-28
    • /
    • 2012
  • In this thesis, fracture tests were carried out in order to investigate the flexural strength behavior of FRC(fiber reinforced concrete) structures. FRC beams were used in the tests, the initial crack load and the ultimate load of the beams were observed under the static loading. According to the results, the ultimate loads increase with the fiber content, and these tendency is clear in the specimens with large fiber aspect ratio. From the results of the regression analysis, practical formulae for predicting the flexural strength of FRC were suggested.

Compressive and Flexural Properties of Hemp Fiber Reinforced Concrete

  • Li, Zhijian;Wang, Lijing;Wang, Xungai
    • Fibers and Polymers
    • /
    • 제5권3호
    • /
    • pp.187-197
    • /
    • 2004
  • The compressive and flexural properties of hemp fiber reinforced concretes (FRC) were examined in this paper. Natural hemp fiber was mixed using dry and wet mixing methods to fabricate the FRC. Mechanical properties of the FRC were investigated. The main factors affecting compressive and flexural properties of the FRC materials were evaluated with an orthogonal test design. Fiber content by weight has the largest effect. The method for casting hemp FRC has been optimised. Under the optimum conditions, compressive strength increased by 4 %, flexural strength increased by 9 %, flexural toughness increased by 144 %, and flexural toughness index increased by 214 %.

유리 섬유의 첨가에 따른 자가중합 및 열중합 의치상용 레진의 강화효과 (Effect of Reinforcement of Glass fiber on Auto and Heat polymerized denture base resin)

  • 유상희;김연수;최운재;전종남
    • 대한치과기공학회지
    • /
    • 제31권4호
    • /
    • pp.37-43
    • /
    • 2009
  • This study evaluated the effect of concentration of glass fiber reinforcement on the flexural properties of auto and heat polymerized denture base resin. The test specimens($64{\times}10{\times}3.3mm$) were made of auto and heat polymerized resin(Vertex, Dentimax, Netherlands). Glass fiber(ER 270FW, Hankuk Fiber Glass, Korea) were used to reinforce the denture base resin. The 2.6%, 5.3% and 7.9% volume pre-impregnated fiber were located at the bottom of specimen. The test specimens(n=7) of each group were stored in distilled water at $37^{\circ}C$ for 50 hours before test. The flexural strength and modulus were measured by an universal testing machine(Z020, Zwick, Germany) at a crosshead speed of 5 mm/min in a three-point bending mode. The data was analyzed by one-way ANOVA and the Duncan's multiple range test(${\alpha}$=0.05). The difference of auto polymerized resin groups and heat polymerized resin groups were statistically analyzed by t-test(${\alpha}$=0.05). Glass fiber showed significant reinforcing effects on auto and heat polymerized resin. For flexural strength and modulus, auto polymerized resin was the highest in 7.9% volume, while heat polymerized resin was the highest in 5.3% volume. In this study, glass fiber at 7.9% volume ratio showed most effective reinforcing effect on auto polymerized resin and glass fiber at 5.3% volume ratio showed most effective reinforcing effect on heat polymerized resin in terms of flexural strength and flexural modulus.

  • PDF

미세입자 분사마모 표면처리가 Fiber-Reinforced Composite 포스트의 굴곡 강도에 미치는 영향 (Influence of airborne-particle abrasion on flexural strength of fiber-reinforced composite post)

  • 심은주;김진우;조경모;박세희
    • 구강회복응용과학지
    • /
    • 제32권1호
    • /
    • pp.24-31
    • /
    • 2016
  • 목적: 미세입자 분사마모 표면처리가 Fiber-Reinforced Composite (FRC) 포스트의 굴곡강도에 미치는 영향을 평가하는 것이다. 연구 재료 및 방법: 두 종류의 FRC 포스트 (DT Light Post, Size 2, Bisco Inc. / RelyX Fiber Post, Size 3, 3M ESPE)를 사용하여 표면처리에 따라 6개의 그룹으로 무작위 분류하였다. 표면처리를 위해 $30{\mu}m$ Rocatec Soft와 $50{\mu}m$ aluminum oxide를 사용하였다. 표면처리 후 편평한 5 mm 부분을 만능시험기로 3점 굽힘시험을 시행하여 FRC 포스트의 굴곡강도와 굴곡계수를 측정하고 통계분석하였다. 결과: FRC포스트의 미세입자 분사마모 표면처리가 FRC포스트의 굴곡강도와 굴곡계수에는 영향을 미치지 않음을 알 수 있었다. 결론: 임상가들이 FRC포스트에 대하여 미세입자 분사마모 표면처리를 하여도 포스트의 굴곡강도와 굴곡계수에는 영향을 미치지 않으면서 접착강도를 높일 수 있을 근거 중의 하나가 될 수 있을 것이다.

해석적 방법에 의한 강섬유 보강 초고성능 콘크리트(UHPFRC) 휨부재의 강도 평가 (Strength Evaluation of UHPFRC Flexural Member by Analytical Method)

  • 박우진;황훈희
    • 한국안전학회지
    • /
    • 제28권2호
    • /
    • pp.55-59
    • /
    • 2013
  • The analytical model was constituted to evaluate the flexural strength of UHPFRC(ultra high performance fiber reinforced concrete) member. The analytical approach was attemped to study the effect of the joint and the result compared with the experimental study to verify the analytical model. The calculated value tends to underestimate about 23%~25% in comparison with the experimental result of the jointed test member because the bond stress between precast UHPFRC and cast-in-place UHPFRC surface is not considered in the analytical model. But in the case of the continuous test member, the analytical model provides reasonable results for the flexural strength of UHPFRC member.

재하상태에 따른 강판보강공법의 휨 보강효과 (Flexural Rehabilitation Effect of Pre-loaded RC Beams Strengthened by Steel Plate)

  • 한복규;홍건호;신영수;조하나
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1999년도 학회창립 10주년 기념 1999년도 가을 학술발표회 논문집
    • /
    • pp.701-704
    • /
    • 1999
  • The purpose of this study was to investigate the effectiveness of the flexural rehabilitation of the pre-loaded reinforced concrete beams strengthened by the steel plate. Main test parameters were the existence and the magnitude of the pre-loading at the flexural of rehabilitation and the tensile reinforcement ratio of the specimens. Seven beam specimens were tested to investigate the effectiveness of the rehabilitation method. Test results showed that the ultimate load capacities of the pre-loaded specimens were higher than not-pre-loaded specimens at the rehabilitation. The cause of the pharameter was analyzed if is suggested that the bond failure between the concrete and the strengthening steel plate occured prior to the yielding of the tension reinforcement. The member flexural stiffnesses, were similar regardless of the load conditions at retrofit and failure modes showed brittle aspect caused by rip-off failure.