플렉서블 능동구동형 유기전계발광(Flexible AMOLED) 디스플레이 개발에 있어 핵심기술이라 할 수 있는 high barrier 특성을 갖는 고분자 기판, 능동구동 소자 및 flexible OLED 제작 기술에 대한 연구를 수행하였다. Polyacryl/SiON 복합층을 사용하여 OLED에 적합한 barrier 특성(투습율 : $10^{-5}\;{\sim}\;10^{-6}\;g/m^2-day$)을 가진 고분자 기판을 개발하였으며 이와 더불어 ULTPS TFT, OTFT 및 flexible OLED 소자를 구현하였다.
In this paper we will outline the opportunities for flexible OLED devices, both for display and solid-state lighting applications. We will present our recent data, and discuss future challenges, for low power consumption phosphorescent OLED technology fabricated on flexible substrates to enable a new generation of energy efficient electronic devices.
Kim, Han-Ki;Moon, Jong-Min;Kim, Ji-Hwim;Kim, Jang-Joo;Kang, Jae-Wook
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2007.06a
/
pp.401-402
/
2007
The preparation and characteristics of ITO anode films grown using a linear facing target sputtering (FTS) technique for use in organic light emitting diodes (OLED) and flexible OLED is described. The electrical, optical, and work function of the ITO anode, which was prepared by linear FTS at room temperature, were comparable to those of commercial ITO anode films. In particular, linear FTS-grown ITO films shows very smooth surface without defects such as pin hole and cracks due to low substrate temperature. Furthermore OLED with the linear FTS-grown ITO anode film shows comparable electrical and optical properties to those of OLED with the commercial crystalline-ITO anode film. This suggested that linear FTS is promising thin film technology for preparing high quality anode film in OLEDs and flexible OLEDs.
A new flexible TFT backplane structure with improved mechanical reliability is proposed. Amorphous indium-gallium-zinc-oxide (a-IGZO) thin film transistors based on this structure have been fabricated on a polyimide substrate, and the resultant mechanical durability has been evaluated in a cyclic bending test. The panel can withstand 10,000 bending cycles at a bending radius of 5 mm without any noticeable TFT degradation. After 10K bending cycles, the change of threshold voltage, mobility, sub-threshold slope, and gate leakage current were only -0.22V, -0.13$cm^2$/V-s, -0.05V/decade, and $-3.05{\times}10^{-13}A$, respectively.
Kim, KwanDo;Jang, SeokHee;Kim, JongMin;Chang, SangMok
Korean Chemical Engineering Research
/
v.50
no.3
/
pp.574-581
/
2012
The relatively short lifetime is a major obstruction for the commercial applications of OLED. One of the reason for the short lifetime is that the organic materials are interacted with water or oxygen in the atmosphere. Protection of water or oxygen from diffusing into the organic material layers are necessary to increase the lifetime of OLED. Although encapsulation of OLED with glass or metal cans has been established, passivation methods of OLED by organic/inorganic thin films are still being developed. In this paper we have developed in-situ passivation system and thin film passivation method using PECVD by which deposition can be performed at room temperature. We have analyzed the characteristics of the passivated OLED device also. The WVTR (Water Vapor Transmission Rate) for the inorganic thin film mono-layer can be reached down to $1{\times}10^{-2}g/m^2{\cdot}day$ and improved lifetime can be obtained. Thin film passivation methods are expected to be applied to flexible display.
Top-emitting organic light-emitting diode (TEOLED) was fabricated on flexible substrate of PES film. Aluminum and Chromium multilayer was used as an anode of TEOLED and the TEOLEDs of Cr(20nm)/Al(100nm)/Cr(20nm)/NPB(60nm)/Alq(60nm)/LiF(1nm)/Al(2nm)/Ag(20nm)/NPB(200nm) has been fabricated on PES film and Si wafer for control device. The TEOLED on PES film which had good anode surface morphology, showed very similar device characteristics to that on Si wafer.
Advanced mobile communication devices require a bright, high information content display in a small, light-weight, low power consumption package. In this paper we will outline our progress towards developing such a low power consumption active-matrix flexible OLED ($FOLED^{TM}$) display. Our work in this area is focused on three critical enabling technologies. The first is the development of a high efficiency long-lived phosphorescent OLED ($PHOLED{TM}$) device technology, which has now proven itself to be capable of meeting the low power consumption performance requirements for mobile display applications. Secondly, is the development of flexible active matrix backplanes, and for this our team are employing poly-Si TFTs formed on metal foil substrates as this approach represents an attractive alternative to fabricating poly-Si TFTs on plastic for the realization of first generation flexible active matrix OLED displays. Unlike most plastics, metal foil substrates can withstand a large thermal load and do not require a moisture and oxygen permeation barrier. Thirdly, the key to reliable operation is to ensure that the organic materials are fully encapsulated in a package designed for repetitive flexing. We also present progress in operational lifetime of encapsulated T-PHOLED pixels on planarized metal foil and discuss PHOLED encapsulation strategy.
In this study, we have investigated the structural and electrical characteristics of IZO thin films deposited under hydrogen atmosphere on flexible substrate for the OLED (organic light emitting diodes) devices. For this purpose, PES was used for flexible substrate and IZO thin films were deposited by RF magnetron sputtering under hydrogen ambient gases (Ar, $Ar+H^2$) at room temperature. In order to investigate the influences of the hydrogen, the flow rate of hydrogen in argon mixing gas has been changed from 0.1sccm to 0.5sccm. All the samples show amorphous structure regardless of flow rate. The electrical resistivity of IZO films increased with increasing flow rate of $H^2$ under $Ar+H^2$. All the films showed the average transmittance over 85% in the visible range. The OLED device was fabricated with different IZO electrodes made by configuration of IZO/$\acute{a}$-NPD/DPVB/$Alq_3$/LiF/Al to elucidate the performance of IZO substrate. OLED devices with the amorphous-IZO (a-IZO) anode film show good current density-voltage-luminance characteristics. This suggests that flat surface roughness and low electrical resistivity of a-IZO anode film lead to more efficient anode material in OLED devices.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2006.06a
/
pp.491-492
/
2006
We report on the fabrication of organic-based flexible display using an amorphous IZO anode grown at room temperature. The IZO anode films were grown by a conventional DC reactive sputtering on polycarbonate (PC) substrate at room temperature using a synthesized IZO target in a Ar/$O_2$ ambient. X-ray diffraction examination results show that the IZO anode film grown at room temperature is complete amorphous structure due to low substrate temperature. It is shown that the $Ir(ppy)_3$ doped flexible organic light emitting diode (OLED) fabricated on the IZO anode exhibit comparable current-voltage-luminance characteristics to OLED fabricated on conventional ITO/glass substrate. These findings indicate that the IZO anode film grown on PC substrate is a promising anode materials for the fabrication of organic based flexible displays.
Proceedings of the Materials Research Society of Korea Conference
/
2009.05a
/
pp.36.1-36.1
/
2009
OLED(organic light emitting diode)는 차세대 평판 디스플레이로 전자종이, 입는 디스플레이 등 flexible한 디스플레이로도 주목받고 있다. 하지만, OLED의 가장 큰 단점 중의 하나가 수분과 산소에 매우 민감하다는 것으로 이것은 OLED의 lifetime과 연결된다. 따라서 이에 대한 mechanism의 확립이 필요하다. 따라서 본 연구에서는, flexible한 OLED에 적용되는 금속 코팅막의 적층구조 및 기판의 노출온도에 따른 금속 코팅막의 수분침투 특성에 대해 MOCON의 weight gain test (WGT)를 통해 barrier layer에 대해 평가하고 이에 대한 mechanism을 확립하는데 그 목적이 있다. 금속 코팅막은 OLED의 cathode와 anode 재료로 많이 사용되는 Al과 ITO를 sputter장비를 이용해 single layer와 multi-layer의 두 가지 구조로 PET기판에 증착하였다. 또한, 노출온도에 따른 특성을 알아보고자 bare PET / ITO coated PET(single layer $50{\mu}m$) / Al coated PET(single layer $200{\mu}m$)의 세 가지 시편을 제작하였다. 이 시편을 각각 $25^{\circ}C$, $37.8^{\circ}C$, $50^{\circ}C$의 온도에서 test를 진행하였고 이 과정을 100%RH, 70%RH, 40%RH조건의 수분조건에서 진행하여 각각의 수분조건에서 각각의 온도에 따른 금속 코팅막의 수분침투 특성에 대한 mechanism을 확립하였다. 적층구조에 따른 수분침투 특성 평가 결과 multi-layer가 single layer보다 더 우수한 수분침투의 barrier 특성을 나타냈었다. 그리고 각 온도에 따른 test결과 온도가 증가할수록 barrier의 특성이 나빠짐이 보였다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.