A novel triazole-functionalized phenolic resin was developed, and its thermal and flame-retardant properties were investigated. The triazole group was incorporated as a pendant unit on the phenolic resin via copper-mediated click chemistry between propargylated phenolic resin and benzyl azide. The newly-developed triazole-functionalized phenolic resin showed higher thermal stability and char yield, together with a reduced total heat release (THR), than the non-functionalized bare phenolic resin, indicating enhanced flame retardancy for the triazole-functionalized phenolic resin.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.20
no.2
/
pp.142-151
/
2007
Non-halogen flame retardant have been focus of extensive research because of environmental problem. Hexakisphenokycyclotriphosphazene was synthesized in order to use as the flame retardant of ABS resin. And using bisphenol A, bisphenol S, and resorcinol, the polymers which contained cyclophosphazene structure were synthesized in order to also use as the flame retardants of ABS resin. All of the synthesized polymers themselves got the excellent flame retardancy. And as the molecular weight of the compound were increased, the thermal stability was increased. But when the synthesized compounds were used as the flame retardants for ABS resin, the lower molecular weight compound in these compounds showed the better flame retardancy and the better physical properties of ABS resin. In case of using resorcinol, it showed the best flame retardancy.
Kim, Hae Young;Shin, Young Jae;Ji, Young Jon;Shin, Jae Sup
Applied Chemistry for Engineering
/
v.17
no.2
/
pp.144-149
/
2006
Non-halogen flame retardants have been the focus of extensive research because of environmental problems. Hexakisp-henoxycyclotriphosphazene was synthesized in order to use as the flame retardant of ABS resin. And using bisphenol A, the polymers containing a cyclotriphosphazene structure were synthesized in order to also use as the flame retardant of ABS resin. All of the synthesized polymers themselves had the excellent flame retardancy. And as their molecular weight and crosslinking density were increased, the thermal stability was increased. But when the synthesized compounds were used as the flame retardant for ABS resin, the lower molecular weight compound in these compounds showed the better flame retardancy and the better physical properties of ABS resin.
The flame retardancy of plywood should be improved as much as possible while minimizing the impact on the bonding strength of plywood. Six commercial flame retardants and three laboratory synthesized phosphorous nitrogen flame retardants were selected. E0, E1 and E2 grade commercial formaldehyde resins (UF) were applied in this study to evaluate the effect of different flame retardants on the curing time of resin, bonding strength, flame retardant performance, and formaldehyde emission of plywood. The results show that the effect of the addition of different flame retardants on the bonding strength of plywood gradually decreased with the increase of the formaldehyde molar ratio of the resin. The effect of flame retardants on the curing time of UF gradually decreased as the mole ratio of formaldehyde increasing, while the amount of formaldehyde emission varied according to the content of formaldehyde in the flame retardant. Compared with plywood without flame retardant, flame retardant of plywood added with phosphorous nitrogen flame retardant was improved.
Magnesium hydroxide-melamine core-shell particles were prepared through the coating of melamine monomer on the surface of magnesium hydroxide in the presence of phosphoric acid. The melamine monomer was dissolved in hot water but recrystallized on the surface of magnesium hydroxide by quenching to room temperature in the presence of phosphoric acid. The core-shell particle was applied to low-density polyethylene/ ethylene vinyl acetate (LDPE/EVA) resin by melt-compounding at $180^{\circ}C$ as flame retardant. The effect of magnesium hydroxide and melamine content has been studied on the flame retardancy of the core-shell particles in LDPE/EVA resin according to the preparation process and purity of magnesium hydroxide. Magnesium hydroxide prepared with sodium hydroxide rather than with ammonia solution revealed higher flame retardancy in core-shell particles with LDPE/EVA resin. At 50 wt% loading of flame retardant, core-shell particles revealed higher flame retardancy compared to that of the exclusive magnesium hydroxide in LDPE/EVA composite, and it was possible to satisfy the V0 grade in the UL-94 vertical test. The synergistic flame retardant effect of magnesium hydroxide and melamine core-shell particles was explained as being due to the endothermic decomposition of magnesium hydroxide and melamine, which was followed by the evolution of water from the magnesium hydroxide and porous char formation due to reactive nitrogen compounds, and carbon dioxide generated from melamine.
Journal of the Korean Applied Science and Technology
/
v.17
no.3
/
pp.203-211
/
2000
Pyrophosphoric lactone modified polyester(PATT) that contains two phosphorous functional groups in one unit base resin structure was synthesized to prepare a non-toxic reactive flame retardant coatings. Then the PATT was cured at room temperature with isocyanate, Desmodur IL, to get a two-component polyurethane flame retardant coatings(PIPUC). Comparing the physical properties of the films of PIPUC with the film of non-flame retardant coatings, there was no degradation observed in physical properties by the introduction of a flame-retarding component into the resin. We found that the char lengths measured by $45^{\circ}$Meckel burner method were $3.1{\sim}4.4cm$ and LOI values recorded $27{\sim}30%$. These results indicate that the coatings prepared in this study is good flame retardant one. The surface structure of coatings investigated with SEM does not show any defects and phase separation.
Journal of Advanced Marine Engineering and Technology
/
v.38
no.9
/
pp.1150-1155
/
2014
To prevent the flame spread in FRP vessel in fire, the engine-room of the vessel should be constructed additionally with laminated fire-retardant resin over 3 times or equivalent insulation materials to former according to the relevant standard for FRP vessel structure. It is surveyed that insulation materials called 'Gel coat' are widely used in FRP fishing vessel, however, test method and its criteria for Gel coat are not clearly establish and have not been evaluated yet, while test method and criteria for fire-retardant resin and fire-retardant polyurethane composite are described in test standard for type-approval. In this study, 3 fire-retardant resins, 4 gel coats, 1 flame-retardant paint and 1 polyurethane composite were selected based on the survey and were evaluated according to both IMO FTP Code part 5 and flame-retardant test. When comparing based on CFE values from flame-spread test, average value for 4 gel coats were lower than that of 3 fire-retardant resins. As for flame-retardant test, there were no significant differences between fire-retardant resin and gel coat, based on charred area.
Proceedings of the Korean Society of Dyers and Finishers Conference
/
2010.03a
/
pp.167-168
/
2010
Non coating type Low melting yarn(L/M PET) not to use the polyurethane resin causing some problems was knitting and evaluated its dyeing characteristics, heat setting properties and flame-retardant properties without flame retardant agent or flame retardant fabric. In order to investigate the dyeing property of fabric of L/M PET, the dyeing of L/M PET was experimented at each different dyeing temperature. Higher exhaustion yield was achieved at lower temperature of L/M PET compared to regular PET. According to result of the study for the heat setting properties of L/M fiber, the K/S value of dyed L/M fiber increased as much as the heat setting temperature did. The experiment for the light fastness reached similar result to dyed PET. However washing fastness in L/M fiber showed lower grade compared with regular PET. flame-retardant efficiency of L/M PET without flame retardant agent or flame retardant fabric measured by $45^{\circ}$ burn test and Contact burn test. The flame?retardant performance of the sample was carried out according to the Korea Fire-fighting Standard.[KOFEIS 1001].
Kim, Jong-In;Park, Jong-Young;Kong, Young-To;Lee, Byoung-Hoo;Kim, Hyun-Joong;Roh, Jeang-Kwan
Journal of the Korean Wood Science and Technology
/
v.30
no.2
/
pp.172-179
/
2002
In this study, two materials treated with a flame retardant were examined for their fire resistance. The first, MDF (medium density fiberboard) was overlaid by an oak sliced veneer, which was either treated by soaking in a 6wt.% solution of flame retardant chemicals (pentabromine-chlorinated paraffin) or non-treated and then was coated with either a flame retardant polyurethane coating or with a common polyurethane coating. The second material, Pinus koraiensis penal was either treated by a spray treatment using a flame retardant solution or non-treated and then was coated with either a flame retardant polyurethane coating or with a common polyurethane coating. Pentabromine-chorinated paraffin chemicals were added (6 part of urethane resin) as the flame retardant chemicals in the polyurethane coatings. In the fire resistance test, the th𝜃(℃·min) decreased with the flame retardant treatment or/and the flame retardant coatings, compared to the untreated sample Weight loss (%) decreased with the flame retardant treatment or/and the flame retardant coatings. The ignition time (sec.) increased and the residual flame time (sec.) decreased with the flame retardant treatment or/and flame retardant coatings. Therefore, the flame retardant treatment or/and flame retardant polyurethane coatings have excellent incombustibility.
The flame retardancy was investigated when the halogenated flame retardant, decabromodiphenyl oxide (DBDPO) and chlorinated paraffin wax (CPW), was added to the polypropylene (PP) / montmorillonite (MMT) nanocomposites. The flame retardancy of polymer resin could be improved not only by addition of flame retardant but also with nanoparticles compositions. The effect of the contents of flame retardant and nanoparticles on the flame retardancy of polypropylene/ montmorillonite nanocomposite systems was thoroughly examined in terms of limited oxygen index (LOI) and cone calorimetry. As a results of cone calorimetry, the heat release rate (HRR) was reduced by the flame retardant DBDPO and CPW, and CPW was a little better than DBDPO. The LOI increased from flammable region (LOI<19) to nonflammable region (LOI>20) for all the flame retardants used in this study. Especially, the improvement in flame retardancy by compounding with PP and MMT was better than that by adding flame retardant to polypropylene. So, the addition of flame retardant after compounding with montmorillonite was more efficient than simple addition of flame retardant.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.