주철본드 다이아몬드 팰렛에 의한 프레스 금형의 고능률 연마가공 (1) (High Efficient Finishing Process for Press Dies by Cast Iron Bonded Diamond Pellet (1))

  • 황찬해;유기태;정해도;안대균
    • 한국정밀공학회지
    • /
    • 제16권3호통권96호
    • /
    • pp.84-90
    • /
    • 1999
  • The finishing process for dies and molds is directly related to finished surface quality, but many parts of process depend on human labor which needs much time and value. So automatic finishing machine has been produced for dies and molds, and applied widely for finishing process. Conventionally finishing machine has applied resin bonded finishing pad as a tool, but the removal ability of pad decreases greatly as finishing process goes on. In the finishing mechanism for dies and molds, finishing process is affected severely by cutting process, so can be divided into removing cusp and smoothing surface process. So, this study investigated the application of cast iron bonded diamond pellet for press dies, which is considered to have better characteristics than the other metal bonded pellets. The finishing characteristics were compared the between finishing pellet and pad. And finishing performance was appraised as the several cutting surfaces.

  • PDF

쾌적조형 부품의 후처리 방안에 관한 연구 (A research on Postprocess Finishing Method of The Rapid Prototyping Parts)

  • 양화준;김성준;장태식;이일엽;이석희
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1997년도 추계학술대회 논문집
    • /
    • pp.83-86
    • /
    • 1997
  • Even as many methods and technologies have been introduced on data generation, parts orientation and layer slicing to acquire the rapid prototyping(RP) parts that have useful surface to satisfy customers' needs such as stylingldesign verification directionlindirect tooling directly from the RP machine, these trials continue to suffer from the surface roughness due to the build characteristics of RP technology. A new postprocess finishing method is suggested in this paper to overcome the surface roughness problem on the surface of the RP parts. To prevent deterioration of dimensional accuracy from the conventional grinding-only, and coating-grinding methods, 4-step surface finishing process is applied. To satisfy the various requirements from the RP oriented industrial f elds, effective procedure, coating material, grmd~ng tools and methods are employed.

  • PDF

Effects of different surface finishing protocols for zirconia on surface roughness and bacterial biofilm formation

  • Lee, Du-Hyeong;Mai, Hang-Nga;Thant, Phyu Pwint;Hong, Su-Hyung;Kim, Jaewon;Jeong, Seung-Mi;Lee, Keun-Woo
    • The Journal of Advanced Prosthodontics
    • /
    • 제11권1호
    • /
    • pp.41-47
    • /
    • 2019
  • PURPOSE. Surface finishing of a zirconia restoration is essential after clinical adjustment. Herein, we investigated the effects of a surface finishing protocol for monolithic zirconia on final roughness and bacterial adherence. MATERIALS AND METHODS. Forty-eight disk-shaped monolithic zirconia specimens were fabricated and divided into four groups (n = 12) based on initial surface treatment, finishing, and polishing protocols: diamond bur+polishing bur (DP group), diamond bur+stone grinding bur+polishing bur (DSP group), no diamond bur+polishing bur (NP group), and no diamond bur+stone grinding bur+polishing bur (NSP group). Initial and final surface roughness was measured with a profilometer, and shown using scanning electron microscope. Bacterial adhesion was evaluated by quantifying Streptococcus mutans in the biofilm. Kruskal-Wallis and Mann-Whitney U tests were used to compare results among groups, and two-way analysis of variance was used to evaluate the effects of grinding burs on final roughness (${\alpha}=.05$). RESULTS. The DP group had the highest final Ra value, followed by the DSP, NP, and NSP groups. Use of the stone grinding bur as a coarse-finishing step significantly decreased final Ra values when a diamond bur was used (P<.001). Omission of the stone grinding bur increased biofilm formation on specimen surfaces. Combining a stone grinding bur with silicone polishing burs produced the smallest final biofilm values, regardless of the use of a diamond bur in initial surface treatment. CONCLUSION. Coarse finishing of monolithic zirconia with a stone grinding bur significantly decreased final Ra values and bacterial biofilm formation when surfaces had been roughened by a diamond bur.

3D 프린터로 출력된 치과용 레진의 자동바렐연마공정에 따른 표면 거칠기 및 연마도 관찰 (Observation of surface roughness and grinding angle by automatic barrel finishing process of dental 3D printed resin)

  • 박유진;정안나
    • 대한치과기공학회지
    • /
    • 제45권2호
    • /
    • pp.39-47
    • /
    • 2023
  • Purpose: This study aimed to confirm the applicability of gloss polishing using automatic barrel finishing with respect to three-dimensional (3D)-printed resin specimens. The surface roughness and grinding angle of the 3D-printed resin specimens were observed with respect to gloss polishing time using automatic dental barrel finishing. Methods: Herein, experiments were conducted on four types of 3D-printed resin specimens. The specimens, with a thickness of 100 ㎛ each, were printed using a 3D printer. Subsequently, light polymerization was performed on these specimens for 15 min. Post this surface treatment, the specimens underwent grinding for 25 min. This process was followed by gloss polishing at 5-min intervals for up to 25 min using automatic dental barrel finishing. The specimens were photographed using a 3D optical microscope, and their surface roughness and grinding angle were measured. Results: The Ra (centerline average roughness) values of all the specimens, except for crown & bridge 10 group and those in the control group that were not polished using automatic barrel finishing, were <0.2 ㎛. However, polishing time needs to be controlled to realize the desired surface roughness and grinding amount considering the hardness of the resin used. Conclusion: Gloss polishing of 3D-printed resin can be realized using automatic dental barrel finishing. However, polishing time needs to be controlled to realize the desired surface roughness and grinding amount considering the hardness of the resin used.

연마방법에 따른 금속의 활택도에 관한 연구 - Atomic Force Microscope를 이용한 - (A STUDY ON SURFACE ROUGHNESS OF METALS ACCORDING TO FINISHING AND POLISHING PROCEDURES - AN ATOMIC FORCE MICROSCOPE ANALYSIS -)

  • 박원규;우이형;최부병;이성복
    • 대한치과보철학회지
    • /
    • 제41권1호
    • /
    • pp.1-19
    • /
    • 2003
  • The surface of metals should be as smooth as possible for optimum comfort, oral hygiene, low plaque retention, and resistance to corrosion. In this study five specimens of each precious metal(type III gold alloy, ceramic gold alloy, and Ag-Pd alloy) were divided into five groups according to finishing and polishing procedures : group 1(sandblaster), group 2(group 1+stone), group 3(group 2+brown rubber), group 4(group 3+green rubber), and group 5(group 4+rouge). Six specimens of each non-precious metal(Co-Cr alloy, Ni-Cr alloy, and Co-Cr-Ti alloy) were divided into six groups: group 1(sandblaster), group 2(group 1+hard stone), group 3(group 2+electrolytic polisher), group 4(group 3+brown hard rubber point), group 5(group 4+green hard rubber point), and group 6(group 5+rouge). Considering factors affecting the rate of abrasion, the same dentist applied each finishing and polishing procedure. In addition, the surface roughness of enamel, resin, and porcelain was evaluated. The effect of finishing and polishing procedures on surface roughness of precious and non-precious metals, enamel, resin, and porcelain was evaluated by means of Atomic Force Microscope(AutoProbe CP. Park Scientific Instruments, U.S.A.) that can image the three dimensional surface profile and measure average surface roughness values of each sample at the same time. The obtained results were as follows : 1. According to finishing and polishing procedures, the surface roughness of type III gold alloy, ceramic gold alloy, and Ag-Pd alloy was decreased in the order of group 1, 2, 3, 4, and 5 (P<0.01). 2. According to finishing and polishing procedures. the surface roughness of Co-Cr alloy, Ni-Cr alloy, and Co-Cr-Ti alloy was decreased in the order of group 1, 2, 3, 4, 5, and 6 (p<0.01). 3. There was not statistically significant difference in the surface roughness among three metals of precious metals in group 1 but was significant difference in group 2, 3, 4, and 5 (P<0.05). 4. There was not statistically significant difference in the surface roughness among three metals of non-precious metals in all groups. 5. When the surface roughness of the smoothest surface of each metal, enamel. porcelain, and resin was compared, porcelain was the smoothest and the surface roughness was decreased in the order of Ni-Cr alloy. Co-Cr alloy. Co-Cr-Ti alloy, resin. Ag-Pd alloy, ceramic gold alloy type III gold alloy, and enamel (P<0.01). The results of this study indicate that the finishing and polishing procedures should be carried out in a logical, systematic sequence of steps and the harder non-precious metals may be less resistance to abrasion than are the softer precious metals.

주차장 바닥용 표면 마감재의 안전성 평가 및 성능기준에 관한 연구 (A Experiment Study for the Standard Performance and Test of Surface Finishing Material for Parking Slab)

  • 김귀태;권시원;곽규성;오상근
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2005년도 춘계 학술기술논문발표대회 논문집
    • /
    • pp.125-131
    • /
    • 2005
  • Recently, to improve condition car park, using surface finishing material for variety color and property epoxy resin, urethane, cement mixed resin mortar or polymeric resin, and so on. However, it is frequent noise and wear out of tier and waterproofing materials, when the car slip or stop in car park, To minimize these cases, It is necessary that reduction of repair cost through performance long term durability of surface finishing material, improvement inside condition such as reduce dirty and car accident and ensurance the expected life of concrete slab in car park. Especially, we have not any tech for quality control, construction tech, production technology for car park surface materials, that's why park slab is not safety and suffer a loss. For this problems, this paper is to test surface finishing materials and as that result, suggest quality standard in the car park.

  • PDF

치과용 바렐연마기의 연마시간에 따른 Co-Cr 합금의 표면거칠기 관찰 (Observations of surface roughness of Co-Cr alloys according to grinding time of dental barrel finishing)

  • 고현정;박유진;최성민
    • 대한치과기공학회지
    • /
    • 제43권3호
    • /
    • pp.93-98
    • /
    • 2021
  • Purpose: The aim of this study was to observe the surface roughness and surface topography of cobalt-chrome (Co-Cr) alloys with grinding time in dental barrel finishing. Methods: This study involved two types of Co-Cr alloys. Specimens were manufactured with the dimensions 10×10×2 mm. Each specimen was cast according to the manufacturer's instructions. The cast alloys were polished for 35 minutes at intervals of five minutes in an automatic barrel finishing. Specimens were imaged with a three-dimensional optical microscope to measure surface roughness. Results: BC specimens and GM specimens had the highest roughness (Ra) values in the ungrained control group, and the lowest Ra values were measured 20 minutes after grinding. Conclusion: The best conditions for grinding Co-Cr alloy using a dental barrel finishing were a weight ratio of polishing media, water, and compound of 150 g:200 g:5 g, and a rotation speed of 450 rpm. Grinding time to obtain appropriate surface roughness should be limited to 15 to 30 minutes.

데님 직물의 워싱 가공 효과에 관한 연구 (A Study on the Washing Finishing Effects of Denim Fabrics)

  • 어미경;서미아
    • 복식문화연구
    • /
    • 제15권5호
    • /
    • pp.852-862
    • /
    • 2007
  • This study was to investigate the physical properties and the external characteristics of denim fabrics(100% cotton non-spun denim, 98% cotton/2% polyurethane spun denim) such as tensile strength, thickness and weight, flex stiffness, surface color and shrinkage. The results of the study were as follows. After examining the change of external characteristics of before and after washing finishing for denim fabrics, denim with bio washing had increased pliability compared to denim without washing finishing but the pliability of the denim did not increase according to the intensity or frequency of washing. The luminance change according to washing finishing was high in the order of bio stone bleach washing, bio stone washing, bio washing and denim without washing finishing and the surface color became brighter in accordance with the increase of intensity and frequency of washing finishing.

  • PDF

사출금형 사상공정의 체계화 (Systematic Finishing Process of Injection Molds)

  • 박민수;김민태;이해성;주종남
    • 한국정밀공학회지
    • /
    • 제21권10호
    • /
    • pp.50-56
    • /
    • 2004
  • Finishing is the final process in molds manufacturing and consumes much process time. Also, it influences on surface quality of molds. But, there are few systematic methods to control the process. In this work, basic experiments were carried out to study the machining characteristics of the finishing tools. From the experiments, critical surface roughness and wear coefficient are suggested to reduce the number of finishing steps and to plan a systematic finishing procedure. Comparison experiments were carried out between the expert's method and the new method, which is based on the results of this research. From the experiments, it is verified that the systematic method takes less time and generates less form error in the machined surface than the worker's method.