• Title/Summary/Keyword: fiber wood

Search Result 479, Processing Time 0.025 seconds

Characteristics of Culm Anatomy and Dimensional Variation in Genus Phyllostachys Grown Damyang District, Korea (담양지방(潭陽地方) 왕대속(屬) 4종(種)의 조직(組織) 및 간내(稈內) 변이성(變異性))

  • Lee, Jae-Ki;Park, Sang-Jin
    • Journal of the Korean Wood Science and Technology
    • /
    • v.15 no.3
    • /
    • pp.14-23
    • /
    • 1987
  • This study was carried out to investigate the anatomical characteristics, the radial and axial variation of the cell dimension and bulk density for four bamboo species used as the major material of bamboo products in Korea; Phyllostachys(P.bambusoides, P.edulis, P.nigra var.henonis, and Pnigra). The results obtained were summarized as follows; 1) In the outer part of culm, the mophological difference of cell diameter and distribution were not acknowledged. However, gum-like substance was occurred In the epidermis, hypodermis, cortex and metaxylem vessel of P.nigra, while it was occured only in the metaxylem vessel of P.edulis. 2) The protoxylem vessel in the central zone of culm-wall could be in the two types; the first type consisted of 4-5 small cell pieces occurred in P.edulis and P.nigra var. henonis, the second type of 1-2 large cell pieces in P.bambusoides and P.nigra. And transition of cell diameter from the vascular bundle sheath to the ground tissue was gradually enlarged in P.nigra and P.edulis but abruptly in P.bambusoides and P.nigra var. henonis. 3) Thin-wall tyloses were well developed in the outer and central zone of culm-wall in four species. 4) Compared with the central part of culm-wall, the number of parenchyma cells and the amount of the vascular bundle sheaths per unit area were a few in the inner part. The inner part nearest to the pith cavity was consisted of thick-well parenchyma cell. 5) The dimensional variations of metaxylem vessel and parenchyma cell in the radial direction were decreased from the inner part to the epidermis in all species observed. 6) The fiber length was the maximum in the central zone and its diameter was increased from the inner part to the outer part. In the axial variation. fiber length was slightly increased from the base and then decresed slowly toward the top, and its diameter was reverse. 7) The axial variation of the bulk density was continuously increased from the base toward the top and its radial variation was rapidly increased from the inner part to the epidermis.

  • PDF

Cell Wall Micropore Loading of Pulp Fibers (펄프 섬유의 세포벽 미세공극 충전)

  • Lee, Jong-Man;Jo, Byoung-Muk
    • Journal of the Korean Wood Science and Technology
    • /
    • v.20 no.4
    • /
    • pp.57-64
    • /
    • 1992
  • The unique cell wall micropores of pulp fiber can be utilized as loading site in variety of important practical application which could be the basis of new papermaking technologies. One of these includes the manufature of paper containing higher levels of in situ filler precipitated. Hardwood pulp fiber were first impregnated with the solution of sodium carbonate($Na_2CO_3$). The micropores in cell wall of pulp fibers were filled with the liquid salt solution. The second calcium nitrate($Ca(NO_3)_2$) solution formed an insoluble calcium carbonate($CaCO_3$) precipitate within the cell wall micropores by interacting with the first sodium carbonate solution. The effects of chemical concentration and dryness of pulp fibers on the retention of cell wall micropore loaded filler were investigated. The paper properties of cell wall micropore loaded pulp fibers were compared with those of conventionally loaded and lumen loaded pulp fibers. Also the presense of the fillers within the cell wall micropore was observed by SEM. Increasing the chemical concentration to generate the calcium carbonate increased the retention of filler in cell wall micropore loaded pulp fibers. The particle size distribution of precipitated calcium carbonate ranged from $0.1{\mu}m$ to $80{\mu}m$. But, the average particle size of cell wall micropore loaded calcium carbonate was $4{\mu}m$. The paper made from never dried pulp fibers, the cell wall micropores which were filled with calcium carbonate, had better mechanical and optical properties than those of conventionally loaded or lumen loaded pulp fibers.

  • PDF

The Improvement of Wet Strength Properties of Sheet by N-Chlorocarbamoylethylation (N-chlorocarbamoylethyl화에 의한 sheet의 습윤강도 향상효과)

  • Jeong, Myung-Joon;Jo, Byoung-Muk;Oh, Jung-Soo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.27 no.3
    • /
    • pp.63-72
    • /
    • 1999
  • For the purpose of improving the wet strength properties of paper, cellulosic fibers were modified by the processes of carbarmoylethylation and N-chlorocarbamoylethylation. Carbamoylethylated cellulose was prepared by the reaction of acrylamide with cellulosic fibers under the alkali catalyst, and N-chlorocarbamoylethylated cellulose was prepared by the addition of sodium hypochlorite into the carbamoylethylated cellulose. In carbamoylethylation reaction, the conditions of NaOH concentration, temperature and acrylamide addition rate were considered to be important factors. An initial reactivity and degree of substitution(DS) in carbamoylethylation of cellulosic fibers were effective according to increasing the addition rates of alkali, acrylamide and the temperature condition of $40^{\circ}C$. The effective wet strength properties by N-chlorocarbamoylethylation of cellulosic fibers were indicated under the conditions of DS 0.06. The wet strength of sheet was improved to 85% at the 100% basis of dry strength. From the photograph of scanning electron microscopy, fiber cuttings on the edge of sheet sample used in tensile strength testing were found in the N-chlorocarbamoylethylated sheet, due to the improvement of fiber bonding strength. The hypochlorite treatment was effective in the recycling of N-chlorocarbamoylethylated sheet, and was reduced the wet strength of sheet to be able to reslush.

  • PDF

The Dyeing Properties of Woody Fiber Regenerated from Waste MDF by Reactive Dyes (반응성염료에 의한 폐MDF 재생 목질섬유의 염색특성)

  • Ju, Seon-Gyeong;Roh, JeongKwan
    • Journal of the Korean Wood Science and Technology
    • /
    • v.47 no.2
    • /
    • pp.163-177
    • /
    • 2019
  • This study aims to review the relations between the dyeing conditions (i.e., dye concentration, addition amounts of salt and alkali, and dyeing temperature) and dyeing properties and color fastness to light for identifying the optimal dyeing conditions when dyed regenerated woody fibers were obtained through the defibration of waste medium density fiberboard (MDF) using reactive Red H-E3B (Bis-monochlorotriazine (MCT)/MCT type) and reactive Red RB133% (Bis-MCT/Vinyl sulphone type). The dyeing yield (K/S) obtained using two types of reactive dyes increased as the dye concentration increased by 1-10% (on the weight of fiber (OWF)). In addition, the K/S of H-E3B was higher than that of RB133% irrespective of the dye concentration. The color difference of H-E3B after ultraviolet (UV) radiation was lower than that of RB133%, denoting good resistance to discoloration by UV. As the amount of sodium sulfate increased, the color difference and K/S also increased, and the adequate salt content was determined to be 50-70 g/L. Further, the color difference and K/S significantly increased only the addition of 2 g/L of sodium carbonate; however, almost no difference was observed when more than 2 g/L of sodium carbonate was added. The addition amount of sodium carbonate was adequate 5-10 g/L to dyeing the fiber and the pH at this addition level was 10. The dyeing yield of H-E3B increased when the dyeing temperature increased; however, it subsequently decreased after the dyeing temperature became $80^{\circ}C$. The dyeing yield of RB133% was almost the same up to $60-70^{\circ}C$ but declined subsequently. Thus, the adequate temperatures were $80^{\circ}C$ and $60^{\circ}C$ for H-E3B and RB133%, respectively. If the waste MDF woody fiber was dyed under the aforementioned optimal conditions, dyed regenerated woody fiber can be obtained having the following colors: 1.5 to 2.0R with the H-E3B dye and 9.6 to 10.0 PR with RB133%.

APPLICATION OF TIME-OF-FLIGHT NEAR INFRARED SPECTROSCOPY TO WOOD

  • Tsuchikawa, Satoru;Tsutsumi, Shigeaki
    • Proceedings of the Korean Society of Near Infrared Spectroscopy Conference
    • /
    • 2001.06a
    • /
    • pp.1182-1182
    • /
    • 2001
  • In this study, the newly constructed optical measurement system, which was mainly composed of a parametric tunable laser and a near infrared photoelectric multiplier, was introduced to clarify the optical characteristics of wood as discontinuous body with anisotropic cellular structure from the viewpoint of the time-of-flight near infrared spectroscopy (TOF-NIRS). The combined effects of the cellular structure of wood sample, the wavelength of the laser beam λ, and the detection position of transmitted light on the time resolved profiles were investigated in detail. The variation of the attenuance of peak maxima At, the time delay of peak maxima Δt and the variation of full width at half maximum Δw were strongly dependent on the feature of cellular structure of a sample and the wavelength of the laser beam. The substantial optical path length became about 30 to 35 times as long as sample thickness except the absorption band of water. Δt ${\times}$ Δw representing the light scattering condition increased exponentially with the sample thickness or the distance between the irradiation point and the end of sample. Around the λ=900-950 nm, there may be considerable light scattering in the lumen of tracheid, which is multiple specular reflection and easy to propagate along the length of wood fiber. Such tendency was remarkable for soft wood with the aggregate of thin layers of cell walls. When we apply TOF-NIRS to the cellular structural materials like wood, it is very important to give attention to the difference in the light scattering within cell wall and the multiple specular-like reflections between cell walls. We tried to express the characteristics of the time resolved profile on the basis of the optical parameters for light propagation determined by the previous studies, which were absorption coefficient K and scattering coefficient S from Kubelka-Munk theory and n from nth power cosine model of radiant intensity. The wavelength dependency of the product of K/S and n, which expressed the light-absorbing and -scattering condition and the degree of anisotropy, respectively, was similar to that of the time delay of peak maxima Δt. The variation of the time resolved profile is governed by the combination of these parameters. So, we can easily find the set of parameters for light propagation synthetically from Δt.

  • PDF

Anatomical Characteristics of Black and White Charcoal Manufactured in Korea (국내산 흑탄과 백탄의 해부학적 특성)

  • Kwon, Sung-Min;Kwon, Gu-Joong;Lee, Sung-Jae;Kim, Nam-Hun
    • Journal of Forest and Environmental Science
    • /
    • v.23 no.1
    • /
    • pp.57-63
    • /
    • 2007
  • Anatomical characteristics of black and white charcoal of Quercus variabilis and Quercus mongolica manufactured by a Korean traditional kiln were investigated by scanning electron microscopy. In both charcoal, the earlywood vessels shrank in tangential direction, whereas the other cells didn't change. However, in the case of latewood vessels, black charcoal did not show tangential direction shrinkage, but white charcoal did. The wood fiber were changed severly in shape due to the excessive shrinkage. Tyloses in early wood vessel were still shown unchanged shape in both charcoals. Cell wall of ray parenchyma was observed and their shapes were severly distorted. Voids between ray parenchyma were observed in white charcoal, which maybe due to high temperature in white charcoal. Moreover, lumen diameters in the uniseriate ray and multiseriate ray were decreased at the high charring temperature. These results showed that the low charcoal yield of the white charcoal compared to the black charcoal was caused by decrease of cell dimensions as well as loss of wood components associated with the carbonization temperature.

  • PDF

Effect of High-molecular-weight Maleic Anhydride-grafted Polylactic Acid Compatibilizer on the Properties of Polylactic acid-based Wood Polymer Composites (말레산 무수물로 그래프트된 고분자량의 폴리락트산 상용화제가 폴리락트산 기반의 합성목재에 미치는 영향)

  • Han, Dong-Heon;Lee, Jong In;Oh, Seung-Ju;Nam, Byeong Uk;Bae, Jin Woo
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.22 no.6
    • /
    • pp.275-282
    • /
    • 2021
  • High-molecular-weight maleic anhydride-grafted polylactic acids (HMMA-g-PLA) compatibilizers were prepared by melt grafting in a twin screw extruder using di(tert-butyl-perxoyisopropyl)benzene (PK-14; as initiator), maleic anhydride (MA), and divinylbenzene (DVB). To determine the properties of the prepared HMMA-g-PLA compatibilizers, Fourier transform infrared (FTIR), Melt index (MI), and back-titration analyses were performed. On increasing DVB concentration, grafting yield of HMMA-g-PLA increased but MI decreased because 𝛽-scission of PLA was restrained by the DVB, and thus, the molecular weight of HMMA-g-PLA increased. PLA-based wood-plastic composites (WPCs) were prepared using HMMA-g-PLA by melt blending through a single screw extruder. The flexural and impact strengths of WPCs compatibilized with HMMA-g-PLA were greater than those of WPCs produced without HMMA-g-PLA. Scanning electron microscope (SEM) studies indicated that increased mechanical properties were caused by excellent interfacial adhesion between PLA and wood fibers due to the addition of HMMA-g-PLA. However, rather high contents of HMMA-g-PLA reduced the mechanical properties of WPCs. We believe that lower molecular-weight of HMMA-g-PLA added as an compatibilizer, compared with PLA polymer, caused the reduction of mechanical properties.

Alkali Pulping Charactics of Moso Bamboo(Phyllostachys pubescens Mazel) with Various Ages (맹종죽의 죽령별 알칼리 펄프화 특성)

  • Yoon, Seung-Lak;Jo, Hyun-Jin;Park, Byung-Su;Kang, Ha-Young;Kang, Kyu-Young
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.38 no.3 s.116
    • /
    • pp.29-37
    • /
    • 2006
  • To use bamboo in the pulp industry, the anatomical characteristics of 60-day-old, 1-year-old, 2-year-old, and 3-year-old moso bamboo (Phyllostachys pubescens Mazel), and the characteristics of fiber and sheet of alkali pulp made of moso bamboo were investigated. Moso bamboo is composed of metaxylens and parenchyma cells in the inner part of the wall, and thick-walled small bundle sheathes near the outer walls. Moso bamboo showed the heterogeneity in anatomical structure. The longest fibers were shown in the middle part, and the widest width in the inner part. The lignin contents were 14.4% in 60-day-old bamboo, which was not lignified yet. The lignin contents in bamboo above 1 year were approximately 35%. The yields of alkali pulp of moso bamboo were in the range between 41 and 47%, and the yields tend to decrease with the increase of ages. The lignin contents of 60-day-old bamboo were 2.1% and those of bamboo above 1 year showed approximately 4% to 5% increment. The length, width, and curl index of fiber in alkali pulp appeared to be similar in all ages. However, coarseness increased slightly with the increase of bamboo ages. The distribution of long fiber was shown much in 60-year-old bamboo. The optical and mechanical properties of moso bamboo tended to decrease with the increase of bamboo age.

Study on the Mechanical Properties of Lumber Reinforced with Glass-Fiber (유리섬유로 보강된 제재목의 기계적 성질에 대한 연구)

  • Cha, Jae-Kyung
    • Journal of the Korea Furniture Society
    • /
    • v.20 no.4
    • /
    • pp.281-289
    • /
    • 2009
  • This research examined the technical feasibility of composite that had two layers of fiberglass reinforcement to enhance the load carrying capacity of lumber. Specimens were prepared from standard lumber made of thinning crop trees such as Larix kaempferi, Pinus koraiensis, and P. rigida. Results indicated that bending properties, hardness, and wood screw withdrawal load of low density lumber from the P. koraiensis increased as the number of layers of fiberglass reinforcement increased. Composite produced by VARTM method showed the MOE increased in all specimens, while the MOR differed on the location, whether the 2-layers of FRP is put on tensile zone or compressive zone. The MOR of high density lumber from Larix kaempferi and P. rigida decreased when they placed into tensile zone, but low density lumber from P. koraiensis increased in same location. The bending toughness only increased high density lumber of Larix kaempferi as the number of layers of fiberglass reinforcement increased. The technique developed by this study may increase an opportunity to use small diameter log with low density for commercial purposes.

  • PDF

Characteristics of pre-extracted hemicelluloses from Korean mixed wood by hot water and alkali solution and its effect on handsheet properties (열수 및 알칼리 용액을 이용하여 국산 목재 칩으로부터 선추출한 헤미셀룰로오스의 특성과 이에 따른 수초지 물성 변화)

  • Seo, Dong-Il;Lee, Sang-Hoon;Sim, Kyu-Jeong;Lee, Hak-Lae;Youn, Hye-Jung
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.43 no.5
    • /
    • pp.60-67
    • /
    • 2011
  • Hemicelluloses pre-extracted from Korean mixed wood chip were investigated as a wet-end additive. Hemicelluloses dissolved in hot water and alkali solution were isolated by ethyl alcohol precipitation from pre-extractives. They showed molecular weight of 9,000 ~ 27,000 g/mol as revealed by size exclusion chromatography. The reduction of molecular weight through hot water extraction was caused by autohydrolysis. Chemical composition of the hemicelluloses were analyzed with high-performance liquid chromatography and UV-Vis spectroscopy. As the surface charge of isolated hemicelluloses were negative, the adsorption of hemicelluloses onto softwood unbleached kraft pulp fiber was promoted by poly-DADMAC. The physical properties of handsheets increased as the molecular weight of hemicellulose increased. On the other hands, the optical property decreased with hemicellulose adsorption.