• 제목/요약/키워드: ferroelectric film

검색결과 513건 처리시간 0.025초

A Study of the Ferroelectric Properties of PbZr0.4Ti0.6O3 (PZT) Grains Using Kelvin Force Microscopy Analysis

  • Heo, Jin-Hee
    • Transactions on Electrical and Electronic Materials
    • /
    • 제11권6호
    • /
    • pp.275-278
    • /
    • 2010
  • We have examined the Ferroelectric properties of $PbZr_{0.4}Ti_{0.6}O_3$ (PZT) grains by monitoring the surface potential through the utilization of Kelvin force microscopy. Hysteretic and time dependent behaviors of small and large grains were compared with each other. The smaller grain yields had smaller values of surface potential. However, the normalized voltage versus surface potential behavior indicates that the smaller grains became saturated earlier with respect to the writing voltages than did the larger grains. On the other hand, the surface potential hysteresis loop obtained from the smaller grains showed a similar shape to what might be obtained from a Zr rich PZT film. In contrast the hysteresis loop of the larger grain looks like that obtained from a Ti-rich film. In addition, the time dependent behaviors of the smaller grains also revealed a better response than the response of larger grains. The overall ferroelectric properties of the smaller grains seem better than corresponding properties for larger grains. The Ti/Zr ratio of the PZT film which was examined in this study was 60/40.

두께 변화에 따른 BST 박막의 특성 (The Properties of BST Thin Films by Thickness)

  • 홍경진;민용기;조재철
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집 Vol.14 No.1
    • /
    • pp.455-458
    • /
    • 2001
  • The thin films of high pemitivity in ferroelectric materials using a capacitor are applied to DRAMs and FRAMs. (Ba, Sr)$TiO_3$ thin films as ferroelectric materials were prepared by the sol-gel method and made by spin-coating on the Pt/Ti/$SiO_2/Si$ substrate at 4,000 [rpm] for 10 seconds. The devices of BST thin films to composite $(Ba_{0.7},Sr_{0.3})TiO_3$ were fabricated by changing of the depositing layer number on $Pt/Ti/SiO_2/Si$ substrate. The thin film capacitor to be ferroelectric devices was investigated by structural and electrical properties. The thickness of BST thin films at each coating numbers 3, 4 and 5 times was $2500[\AA]$, $3500[\AA]$, $3800[\AA]$. The dielectric factor of thin film when the coating numbers were 3, 4 and 5 times was 190, 400 and 460 on frequency l[MHz]. The dielectric loss of BST thin film was linearly increased by increasing of the specimen area.

  • PDF

$BaMgF_4$/Si 구조를 이용한 비휘발성 메모리용 MFSFET의 제작 및 특성 (Fabrication and Properties of MFSFET′s Using $BaMgF_4$/Si Structures for Non-volatile Memory)

  • 이상우;김광호
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제10권10호
    • /
    • pp.1029-1033
    • /
    • 1997
  • A prototype MFSFET using ferroelectric fluoride BaMgF$_4$as a gate insulator has been successfully fabricated with the help of 2 sheets of metal mask. The fluoride film was deposited in an ultrai-high vacuum system at a substrate temperature of below 30$0^{\circ}C$ and an in-situ post-deposition annealing was conducted for 20 seconds at $650^{\circ}C$ in the same chamber. The interface state density of the BaMgF$_4$/Si(100) interface calculated by a MFS capacitor fabricated on the same wafer was about 8$\times$10$^{10}$ /cm$^2$.eV. The I$_{D}$-V$_{G}$ characteristics of the MFSFET show a hysteresis loop due to the ferroelectric nature of the BaMgF$_4$film. It is also demonstrated that the I$_{D}$ can be controlled by the “write” plus which was applied before the measurements even at the same “read”gate voltage.ltage.

  • PDF

The ferroelectric and fatigue properties in Gd-modified bismuth titanate (BGT) thin films deposited by liquid delivery MOCVD

  • Kang Dong-Kyun;Park Won-Tae;Kim Byong-Ho
    • 한국반도체및디스플레이장비학회:학술대회논문집
    • /
    • 한국반도체및디스플레이장비학회 2006년도 춘계학술대회
    • /
    • pp.190-193
    • /
    • 2006
  • Gadolinium-substituted bismuth titanate, $Bi_{3.3}Gd_{0.7}Ti_{3}O_{12}$, thin films were successfully fabricated on Pt(111)/Ti/$SiO_2$/Si(100) substrates by a MOCVD process. Fabricated BGT thin films were found to be random oriental ions, which were confirmed by X-ray diffraction and scanning electron microscope analysis. The remanent polarization value ($2P_r$) of the BGT thin film annealed at $720^{\circ}C$ was $45.13{\mu}C/cm^2$, at an applied voltage of 5 V. The BGT thin film exhibits a good fatigue resistance up to $1{\times}10^{11}$ switching cycles at a frequency of 1 MHz with applied voltage of 5 V. These results indicate that the randomly oriented BGT thin film is a promising candidate among ferroelectric materials useful in lead-free nonvolatile ferroelectric random access memory applications.

  • PDF

두께 변화에 따른 BST 박막의 특성 (The Properties of BST Thin Films by Thickness)

  • 홍경진;민용기;조재철
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집
    • /
    • pp.455-458
    • /
    • 2001
  • The thin films of high permitivity in ferroelectric materials using a capacitor are applied to DRAMs and FRAMs. (Ba, Sr)TiO$_3$ thin films as ferroelectric materials were prepared by the sol-gel method and made by spin-coating on the Pt/Ti/SiO$_2$/Si substrate at 4,700 [rpm] for 10 seconds. The devices of BST thin films to composite (Ba$\_$0.7/Sr$\_$0.3/)TiO$_3$ were fabricated by changing of the depositing layer number on Pt/Ti/SiO$_2$/Si substrate. The thin film capacitor to be ferroelectric devices was investigated by structural and electrical properties. The thickness of BST thin films at each coating numbers 3, 4 and 5 times was 2500[${\AA}$], 3500[${\AA}$], 3800[${\AA}$]. The dielectric factor of thin film when the coating numbers were 3, 4 and 5 times was 190, 400 and 460 on frequency 1[MHz]. The dielectric loss of BST thin film was linearly increased by increasing of the specimen area.

  • PDF

$Bi_{3.25}La_{0.75}Ti_{3}O_{12}$ (BLT) 박막의 CMP 메커니즘 연구 (A Study on CMP Mechanism of $Bi_{3.25}La_{0.75}Ti_{3}O_{12}$ (BLT) Thin Films)

  • 신상헌;고필주;김남훈;이우선
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2006년도 제37회 하계학술대회 논문집 C
    • /
    • pp.1450-1451
    • /
    • 2006
  • In this paper, we first applied the chemical mechanical polishing (CMP) process to the planarization of ferroelectric film in order to obtain a good planarity of electrode/ferroelectric film interface. $Bi_{3.25}La_{0.75}Ti_{3}O_{12}$ (BLT) ferroelectric fan was fabricated by the sol-gel method. Removal rate and non-uniformity (WIWNU%) were examined by change of silica slurries pH(10.3, 11.3, 12.3). Surface roughness of BLT thin films before and after CMP process was inquired into by atomic force microscopy (AFM). Effects of silica slurries pH(10.3, 11.3, 12.3) were investigated on the CMP performance of BLT film by the surface analysis of X-ray photoelectron spectroscopy(XPS).

  • PDF

Hf0.5Zr0.5O2 강유전체 박막의 다양한 분극 스위칭 모델에 의한 동역학 분석 (Switching Dynamics Analysis by Various Models of Hf0.5Zr0.5O2 Ferroelectric Thin Films)

  • 안승언
    • 한국재료학회지
    • /
    • 제30권2호
    • /
    • pp.99-104
    • /
    • 2020
  • Recent discoveries of ferroelectric properties in ultrathin doped hafnium oxide (HfO2) have led to the expectation that HfO2 could overcome the shortcomings of perovskite materials and be applied to electron devices such as Fe-Random access memory (RAM), ferroelectric tunnel junction (FTJ) and negative capacitance field effect transistor (NC-FET) device. As research on hafnium oxide ferroelectrics accelerates, several models to analyze the polarization switching characteristics of hafnium oxide ferroelectrics have been proposed from the domain or energy point of view. However, there is still a lack of in-depth consideration of models that can fully express the polarization switching properties of ferroelectrics. In this paper, a Zr-doped HfO2 thin film based metal-ferroelectric-metal (MFM) capacitor was implemented and the polarization switching dynamics, along with the ferroelectric characteristics, of the device were analyzed. In addition, a study was conducted to propose an applicable model of HfO2-based MFM capacitors by applying various ferroelectric switching characteristics models.

솔-젤 회전 코팅법을 이용한 강유전성 $BaTiO_3$ 박막제조 (Preparation of Ferroelectric $Cr_3C_2$ Thin Film Using Sol-Gel Spin Coating Process)

  • 배호기;고태경
    • 한국세라믹학회지
    • /
    • 제31권7호
    • /
    • pp.795-803
    • /
    • 1994
  • Ferroelectric BaTiO3 thin film was produced using BaTi-ethoxide sol. This sol was prepared from BaTi-ethoxide by a partial hydrolysis with ammonia as a basic catalyst and ethylene glycol as a chelating agent. BaTiO3 thin film was prepared from three continuous spin-coating layers of the sol on bare Si(100) wafer at 2500 rpm followed by pyrolysis at $700^{\circ}C$ for 30 min. After the heat treatment, the film was 0.200$\pm$0.010 ${\mu}{\textrm}{m}$ thick and its grain size was 0.059 ${\mu}{\textrm}{m}$. On the other hand, electrical properties were measured for BaTiO3 thin film separately prepared on Au-deposited silicon wafer. The dielectric constant and loss of the BaTiO3 thin film at room temperature was 150~160 and 0.04 respectively, which was measured at 10 kHz and oscillation level of 0.1 V. In the measurements of the dielectric properties at high temperatures, it was observed that the capacitance of the thin film increases steeply, while the dielectric loss reaches maximum around 1$25^{\circ}C$, which corresponds a phase transition from tetragonal to cubic BaTiO3.

  • PDF

스크린 프린팅법으로 제작한 PZT후막의 강유전 특성 (The Ferroelectric properties of PZT thick film by preparation Screen Printing)

  • 강정민;조현무;이성갑;이상헌;이영희;배선기
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2004년도 하계학술대회 논문집 Vol.5 No.2
    • /
    • pp.656-658
    • /
    • 2004
  • Pb$(Zr_{0.8}Ti_{0.2})TiO_3$ powder were prepared by the sol-gel method using a solution of Pb-acetate, Zr n-propoxide and Ti iso-propoxide. PZT thick film were fabricated by the screen printing method, and the structural and ferroelectric properties asafunting of the sintering temperature were studied. PZT film thickness, obtained by four screen printing, was approximately $70\sim90{\mu}m$. The relative dielectric constant and the dielectric loss of the PZT thick film sintered at $1050^{\circ}C$t were approximately 676 and 1.4%, respectively. The remanent polarization and the coercive field of the PZT thick film sintered at $1050^{\circ}C$ were $21.15{\mu}C/cm^2$ and 10.1 kV/cm, mapetively