제강 및 열처리 조건이 압력용기강의 피로 및 파괴특성에 미치는 영향 (Influence of Steel-making Process and Heat-treatment Temperature on the Fatigue and Fracture Properties of Pressure Vessel Steels)

  • 고승기;나의균;백태현;박승주;원삼용;이성우
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2001년도 추계학술대회논문집A
    • /
    • pp.87-92
    • /
    • 2001
  • In this paper, high strength pressure vessel steels having the same chemical compositions were manufactured by the two different steel-making processes, such as vacuum degassing(VD) and electro-slag remelting(ESR) methods. After the steel-making process, they were normalized at $955^{\circ}C$, quenched at $843^{\circ}C$, and finally tempered at $550^{\circ}C$ or $450^{\circ}C$, resulting in tempered martensitic microstructures with different yielding strengths depending on the tempering conditions. Low-cycle fatigue(LCF) tests, fatigue crack growth rate(FCGR) tests, and fracture toughness tests were performed to investigate the fatigue and fracture behaviors of the pressure vessel steels. In contrast to very similar monotonic, LCF, and FCGR behaviors between VD and ESR steels, a quite difference was noticed in the fracture toughness. Fracture toughness of ESR steel was higher than that of VD steel, being attributed to the removal of impurities in steel-making process.

  • PDF

SA508 저탄소강과 AISI316 오스테나이트강의 이종 용접부 피로균열 성장 거동에 미치는 열처리 영향 연구 (A Study of the Heat Treatment Effect on the Fatigue Crack Growth Behavior in Dissimilar Weld Metal Joints of SA508 Low-Carbon Steel and AISI316 Austenitic Stainless Steel)

  • 김정석
    • 한국기계가공학회지
    • /
    • 제17권3호
    • /
    • pp.16-21
    • /
    • 2018
  • The effect of heat treatment on the fatigue crack growth behavior in welded joints between the heat-affected zone (HAZ) of SA 508 Cl.3 low-alloy steel and HAZ of AISI 316L stainless steel is investigated. When the crack propagates across SA 508 Cl.3 or AISI 316L SS and HAZ into the weldment, the fatigue crack growth rate (FCGR) in the HAZ region does not change or decrease despite the increase in stress intensity factor ${\Delta}K$. The residual stress at the HAZ region is more compressive than that at the base Δ materials and weldment. The effect of the welding residual stress on the crack growth behavior is determined by performing a residual stress relief heat treatment at $650^{\circ}C$ for 1h and subsequent furnace cooling. The FCG behavior in the HAZ region in the as-welded specimen and the residual stress relief heat-treated specimen is discussed in terms of the welding residual stress.

장기 사용 보일러 헤더의 열화거동 평가에 관한 연구 (Evaluation of Degradation Behavior of the Long-Term Serviced Boiler Header)

  • 권재도;배용탁;최성종
    • 대한기계학회논문집A
    • /
    • 제24권7호
    • /
    • pp.1673-1680
    • /
    • 2000
  • The degradation of a boiler header constructed by a material, 1Cr-0.5Mo steel in a fossil power plant is observed when the header is exposed for a long period to the high temperature and pressure. The present investigations are for evaluating the effect of the degradation on the material, such as its strength changes. Reheat-treated metal is used to compare the mechanical properties of the degraded and that of reheat-treated materials. Through the investigation, following results are obtained 1) the area ratio of ferrite in the reheat-treated material is larger than that of the degraded material, 2) the hardness and tensile strength of the degraded material are lower than that of the reheat-treated material, 3) the ductile-brittle transition temperature(DBTT) increased toward high temperature region, 4) the fatigue crack growth rate(FCGR) of the degraded material is higher than that of the reheat-treated material in the region of low ΔK value while FCGR of the both materials are similar in high ΔK region.