• Title/Summary/Keyword: failure behaviors

Search Result 563, Processing Time 0.024 seconds

Stereo-digital image correlation in the behavior investigation of CFRP-steel composite members

  • Dai, Yun-Tong;Wang, Hai-Tao;Ge, Tian-Yuan;Wu, Gang;Wan, Jian-Xiao;Cao, Shuang-Yin;Yang, Fu-Jun;He, Xiao-Yuan
    • Steel and Composite Structures
    • /
    • v.23 no.6
    • /
    • pp.727-736
    • /
    • 2017
  • The application of carbon fiber reinforced polymer (CFRP) in steel structures primarily includes two categories, i.e., the bond-critical application and the contact-critical application. Debonding failure and buckling failure are the main failure modes for these two applications. Conventional electrometric techniques may not provide precise results because of the limitations associated with single-point contact measurements. A nondestructive full-field measurement technique is a valuable alternative to conventional methods. In this study, the digital image correlation (DIC) technique was adopted to investigate the bond behavior and buckling behavior of CFRP-steel composite members. The CFRP-to-steel bonded joint and the CFRP-strengthened square hollow section (SHS) steel column were tested to verify the suitability of the DIC technique. The stereo-DIC technique was utilized to measure continuous deformation. The bond-slip relationship of the CFRP-to-steel interface was derived using the DIC data. Additionally, a multi-camera DIC system consisting of four stereo-DIC subsystems was proposed and applied to the compressive test of CFRP-strengthened SHS steel column. The precise buckling location and CFRP delamination of the CFRP-strengthened SHS steel column were identified. The experimental results confirm that the stereo-DIC technique can provide effective measurements for investigating the behaviors of CFRP-steel composite members.

AE Characteristic under Tensile of Carbon Steel for High-Pressure Pipe (고압배관용 탄소강의 인장시 음향방출 특성)

  • Nam Kiwoo;Lee Siyoon
    • Journal of the Korean Institute of Gas
    • /
    • v.7 no.2 s.19
    • /
    • pp.48-53
    • /
    • 2003
  • This study is to look at the effect for deformation of carbon steel for high-presure pipe, on the AE signals produced by tensile test. Acoustic emission(AE) has been widely used in various fields because of its extreme sensitivity, dynamic detection ability and location of growing defects. We investigated a relationship failure mode and AE signals by tensile test, From the tensile test, we could divide into four ranges of the failure modes of elastic range, yield range, plastic range before $\sigma$u, plastic range after $\sigma$u. And failure behaviors of elastic range, yield range, plastic range before $\sigma$u, plastic range after $\sigma$u could be evaluated in tensile test by AE counts, accumulation counts and time frequency analysis. It is expected to be basic data that can protect a risk according to tensile test and bending of pipe material for pressure vessel, as a real time test of AE.

  • PDF

Experimental study on propagation behavior of three-dimensional cracks influenced by intermediate principal stress

  • Sun, Xi Z.;Shen, B.;Zhang, Bao L.
    • Geomechanics and Engineering
    • /
    • v.14 no.2
    • /
    • pp.195-202
    • /
    • 2018
  • Many laboratory experiments on crack propagation under uniaxial loading and biaxial loading have been conducted in the past using transparent materials such as resin, polymethyl methacrylate (PMMA), etc. However, propagation behaviors of three-dimensional (3D) cracks in rock or rock-like materials under tri-axial loading are often considerably different. In this study, a series of true tri-axial loading tests on the rock-like material with two semi-ellipse pre-existing cracks were performed in laboratory to investigate the acoustic emission (AE) characteristics and propagation characteristics of 3D crack groups influenced by intermediate principal stress. Compared with previous experiments under uniaxial loading and biaxial loading, the tests under true tri-axial loading showed that shear cracks, anti-wing cracks and secondary cracks were the main failure mechanisms, and the initiation and propagation of tensile cracks were limited. Shear cracks propagated in the direction parallel to pre-existing crack plane. With the increase of intermediate principal stress, the critical stress of crack initiation increased gradually, and secondary shear cracks may no longer coalesce in the rock bridge. Crack aperture decreased with the increase of intermediate principal stress, and the failure is dominated by shear fracturing. There are two stages of fracture development: stable propagation stage and unstable failure stage. The AE events occurred in a zone parallel to pre-existing crack plane, and the AE zone increased gradually with the increase of intermediate principal stress, eventually forming obvious shear rupture planes. This shows that shear cracks initiated and propagated in the pre-existing crack direction, forming a shear rupture plane inside the specimens. The paths of fracturing inside the specimens were observed using the Computerized Tomography (CT) scanning and reconstruction.

Failure Behavior of Pin-jointed Cylindrical Composites Using Acoustic Emission Technique (AE기법을 이용한 원통형 복합재의 핀 체결부 파괴거동)

  • Yoon, Sung-Ho;Hwang, Young-Eun;Kim, Chan-Gyu
    • Journal of the Korean Society of Propulsion Engineers
    • /
    • v.16 no.4
    • /
    • pp.9-15
    • /
    • 2012
  • In this paper, the bearing strengths and fracture behaviors of the pin-jointed carbon fiber/epoxy composites were investigated through pin loading test with acoustic emission technique. The composites were fabricated by a filament winding process, and three types of laminated patterns were considered. Type 1 was fabricated with stitch, Type 2 was fabricated without stitich and Type 3 was fabricated with prepregs. According to the results, bearing strength of Type 1 was 3.3% lower than that of Type 2 and that of Type 3 was highest. Type 1 and Type 2 revealed a net-tension failure mode, respectively, whereas Type 3 pattern exhibited a bearing failure mode. Also, acoustic emission energy of the Type 3 was higher than that of the Type 1 and Type 2. Therefore, the Type 3 was found to be structurally safer than the Type 1 and Type 2.

A Study on the Evaluation of Stability due to Ground Deterioration of Slope (사면의 지반 열화로 인한 안정성 평가에 관한 연구)

  • Han, Young-Chul
    • Journal of the Korean Geotechnical Society
    • /
    • v.34 no.12
    • /
    • pp.83-92
    • /
    • 2018
  • The lapse of time may cause in the slope structure various deterioration phenomenon progresses in the ground of slope, and collapse due to deterioration of strength, resulting in a decrease in the service life. The approach to slope stability due to the ground deterioration is a different concept from the existing limit equilibrium analysis, which is limited to the physical characteristics and geometrical structure of ground. In this study, we conducted a comparative analysis of various literature studies related to the slope failure characteristics and behaviors to presented the optimal formulas for shear strength reduction, such as the exponential function, the logarithmic function and the inverse hyperbolic function. And then a case study was performed on cut slope of Gyeongbu High Speed Rail construction site along the Yangsan fault zone, where the slope failure of shale layer vulnerable to deterioration occurred. As a result, it was confirmed that landslide occurred due to reduction of shear strength by deterioration, as safety factor is approx. 1.0 at the time when the slope failure occurred. Based on the comprehensive case study, as a quantitative approach to the evaluation of slope stability due to deterioration of ground, finally we propose a method for evaluating slope stability with optimal strength reduction curves.

Axially-loaded multiplanar tubular KTX-joints: numerical analysis

  • Zhang, Chenhui;Zou, Bo;Yang, Guotao
    • Steel and Composite Structures
    • /
    • v.42 no.2
    • /
    • pp.173-190
    • /
    • 2022
  • With the development of spatial structures, the joints are becoming more and more complex to connect tubular members of spatial structures. In this study, an approach is proposed to establish high-efficiency finite element model of multiplanar KTX-joint with the weld geometries accurately simulated. Ultimate bearing capacity the KTX-joint is determined by the criterion of deformation limit and failure mechanism of chord wall buckling is studied. Size effect of fillet weld on the joint ultimate bearing capacity is preliminarily investigated. Based on the validated finite element model, a parametric study is performed to investigate the effects of geometric and loading parameters of KT-plane brace members on ultimate bearing capacity of the KTX-joint. The effect mechanism is revealed and several design suggestions are proposed. Several simple reinforcement methods are adopted to constrain the chord wall buckling. It is concluded that the finite element model established by proposed approach is capable of simulating static behaviors of multiplanar KTX-joint; chord wall buckling with large indentation is the typical failure mode of multiplanar KTX-joint, which also increases chord wall displacements in the axis directions of brace members in orthogonal plane; ultimate bearing capacity of the KTX-joint increases approximately linearly with the increase of fillet weld size within the allowed range; the effect mechanism of geometric and loading parameters are revealed by the assumption of restraint region and interaction between adjacent KT-plane brace members; relatively large diameter ratio, small overlapping ratio and small included angle are suggested for the KTX-joint to achieve larger ultimate bearing capacity; the adopted simple reinforcement methods can effectively constrain the chord wall buckling with the design of KTX-joint converted into design of uniplanar KT-joint.

The Roles of Service Failure and Recovery Satisfaction in Customer-Firm Relationship Restoration : Focusing on Carry-over effect and Dynamics among Customer Affection, Customer Trust and Loyalty Intention Before and After the Events (서비스실패의 심각성과 복구만족이 고객-기업 관계회복에 미치는 영향 : 실패이전과 복구이후 고객애정, 고객신뢰, 충성의도의 이월효과 및 역학관계 비교를 중심으로)

  • La, Sun-A
    • Journal of Distribution Research
    • /
    • v.17 no.1
    • /
    • pp.1-36
    • /
    • 2012
  • Service failure is one of the major reasons for customer defection. As the business environment gets tougher and more competitive, a single service failure might bring about fatal consequences to a service provider or a firm. Sometimes a failure won't end up with an unsatisfied customer's simple complaining but with a wide-spread animosity against the service provider or the firm, leading to a threat to the firm's survival itself in the society. Therefore, we are in need of comprehensive understandings of complainants' attitudes and behaviors toward service failures and firm's recovery efforts. Even though a failure itself couldn't be fixed completely, marketers should repair the mind and heart of unsatisfied customers, which can be regarded as an successful recovery strategy in the end. As the outcome of recovery efforts exerted by service providers or firms, recovery of the relationship between customer and service provider need to put on the top in the recovery goal list. With these motivations, the study investigates how service failure and recovery makes the changes in dynamics of fundamental elements of customer-firm relationship, such as customer affection, customer trust and loyalty intention by comparing two time points, before the service failure and after the recovery, focusing on the effects of recovery satisfaction and the failure severity. We adopted La & Choi (2012)'s framework for development of the research model that was based on the previous research stream like Yim et al. (2008) and Thomson et al. (2005). The pivotal background theories of the model are mainly from relationship marketing and social relationships of social psychology. For example, Love, Emotional attachment, Intimacy, and Equity theories regarding human relationships were reviewed. As the results, when recovery satisfaction is high, customer affection and customer trust that were established before the service failure are carried over to the future after the recovery. However, when recovery satisfaction is low, customer-firm relationship that had already established in the past are not carried over but broken up. Regardless of the degree of recovery satisfaction, once a failure occurs loyalty intention is not carried over to the future and the impact of customer trust on loyalty intention becomes stronger. Such changes imply that customers become more prudent and more risk-aversive than the time prior to service failure. The impact of severity of failure on customer affection and customer trust matters only when recovery satisfaction is low. When recovery satisfaction is high, customer affection and customer trust become severity-proof. Interestingly, regardless of the degree of recovery satisfaction, failure severity has a significant negative influence on loyalty intention. Loyalty intention is the most fragile target when a service failure occurs no matter how severe the failure criticality is. Consequently, the ultimate goal of service recovery should be the restoration of customer-firm relationship and recovery of customer trust should be the primary objective to accomplish for a successful recovery performance. Especially when failure severity is high, service recovery should be perceived highly satisfied by the complainants because failure severity matters more when recovery satisfaction is low. Marketers can implement recovery strategies to enhance emotional appeals as well as fair treatments since the both impacts of affection and trust on loyalty intention are significant. In the case of high severity of failure, recovery efforts should be exerted to overreach customer expectation, designed to directly repair customer trust and elaborately designed in the focus of customer-firm communications during the interactional recovery process to affect customer trust rebuilding indirectly. Because it is a longer and harder way to rebuild customer-firm relationship for high severity cases, low recovery satisfaction cannot guarantee customer retention. To prevent customer defection due to service failure of high severity, unexpected rewards as a recovery will be likely to be useful since those will lead to customer delight or customer gratitude toward the service firm. Based on the results of analyses, theoretical and managerial implications are presented. Limitations and future research ideas are also discussed.

  • PDF

Determination of cross section of composite breakwaters with multiple failure modes and system reliability analysis (다중 파괴모드에 의한 혼성제 케이슨의 단면 산정 및 제체에 대한 시스템 신뢰성 해석)

  • Lee, Cheol-Eung;Kim, Sang-Ug;Park, Dong-Heon
    • Journal of Korea Water Resources Association
    • /
    • v.51 no.9
    • /
    • pp.827-837
    • /
    • 2018
  • The stabilities of sliding and overturning of caisson and bearing capacity of mound against eccentric and inclined loads, which possibly happen to a composite caisson breakwaters, have been analyzed by using the technique of multiple failure modes. In deterministic approach, mathematical functions have been first derived from the ultimate limit state equations. Using those functions, the minimum cross section of caisson can straightforwardly be evaluated. By taking a look into some various deterministic analyses, it has been found that the conflict between failure modes can be occurred, such that the stability of bearing capacity of mound decreased as the stability of sliding increased. Therefore, the multiple failure modes for the composite caisson breakwaters should be taken into account simultaneously even in the process of deterministically evaluating the design cross section of caisson. Meanwhile, the reliability analyses on multiple failure modes have been implemented to the cross section determined by the sliding failure mode. It has been shown that the system failure probabilities of the composite breakwater are very behaved differently according to the variation of incident waves. The failure probabilities of system tend also to increase as the crest freeboards of caisson are heightening. The similar behaviors are taken place in cases that the water depths above mound are deepening. Finally, the results of the first-order modal are quite coincided with those of the second-order modal in all conditions of numerical tests performed in this paper. However, the second-order modal have had higher accuracy than the first-order modal. This is mainly due to that some correlations between failure modes can be properly incorporated in the second-order modal. Nevertheless, the first-order modal can also be easily used only when one of failure probabilities among multiple failure modes is extremely larger than others.

Testing and Numerical Analysis on the Fracture Characteristics of Composite Adhesive Bonded Single-Lap Joints (복합재료 Single-Lap 본딩 조인트의 파괴 특성에 대한 실험 및 수치해석 연구)

  • 김광수;박재성;장영순;이영무
    • Composites Research
    • /
    • v.16 no.5
    • /
    • pp.45-53
    • /
    • 2003
  • The experimental and numerical investigations on the failure characteristics of the secondary bonded composite single-lap joints were performed. The initiations and growths of cracks were observed using CCD camera and acoustic emission sensor during the tension tests of the joint specimens. The structural behaviors of the specimens were predicted by the geometric nonlinear two-dimensional finite element analysis. The three types of observed initial cracks were included in each finite element models and the strain energy release rates of each specimen models were calculated by VCCT(Virtual Crack Closure Technique) technique. The tension tests showed that the initial cracks occurred in the 60∼90% of final failure loads and the major failure modes of the specimens were adhesive failure and the delamination between the 1st and 2nd ply of laminate. The specimens with the thicker bondline had earlier crack initiation loads but higher crack propagation resistance and eventually better loading capability. The delaminations were mostly observed in the thicker bondline specimens. The mode I values of calculated strain energy release rates were higher than the mode II values in the all specimen models considering the three types of initial cracks. The mode I and total strain energy release rates were calculated as higher values in the order of initial crack in the edge interface, comer interface and delamination between the plies of laminate.

Mechanical Properties and Failure Behavior of Grouting Cements for a $CO_2$-Injection Hole (이산화탄소 주입공 그라우팅 시멘트의 역학적 물성 및 파괴 거동)

  • Park, Mi-Hee;Chang, Chan-Dong;Jo, Yeong-Uk;Choo, Min-Kyoung;Yum, Byoung-Woo
    • The Journal of Engineering Geology
    • /
    • v.21 no.2
    • /
    • pp.147-156
    • /
    • 2011
  • We conducted laboratory experiments to determine the physical and mechanical properties, and the failure behaviors, of cements for use as grouting material in a $CO_2$-injection borehole. Samples with lour different ratios of water to cement mass (0.4, 1, 2, and 3) were tested. The analyzed properties (porosity, sonic velocity, modulus, and compressive and tensile strengths) varied systematically as a function of the ratio of water to cement (w/c), showing a sharp change between w/c ratios of 0.4 and 1. Triaxial compression tests revealed a clear boundary between brittle and ductile failure depending on the w/c ratio and confining pressure. The present results can be utilized as input parameters for numerical models to understand the initial deformation and failure behavior of grouting cements in a $CO_2$-injection borehole.