Since non-corrosive Fiber Reinforced Polymer(FRP) tendons have been in increasing use for underground and coastal structures constantly contacted with fresh water or sea water because of their superiority to metallic ones in corrosion-resistance, new non-metallic anchoring system for FRP tendons has been developed and investigated to verify the effectiveness of tendon force, which consist of mainly FRP pipes and Highly Expansive Mortar(HEM). The major factors considered in this experiment were expansive pressures of HEM during its hydration, sleeve lengths and types, and anchoring methods of tendon. New anchoring system were investigated from the pull-out tests. The pull-out procedures of the FRP tendons in the various pipe filled with HEM were analyzed and improved ideas were suggested to develop novel non-metallic anchoring system for FRP tendons The pull-out tests for the FRP tendon and new non-metallic anchoring system were conducted. The results show that non-metallic anchoring system for the FRP tendon has been more stablized due to the gradual expansive pressrure of HEM, as tims goes. Since tile lower stiffness of FRP pipes causes the weakness of anchoring force, it requires the increase of stiffness using a carbon fiber or an increased section area.
본 연구에서는 철근콘크리트 구조의 FRP를 이용한 보강에서 낮은 내화성능을 개선하기 위한 방안을 찾기 위하여, 보강된 FRP의 외부를 내화보강하는 방법에 대한 내화실험을 실시하였다. 특히 철근콘크리트 부재의 피복에 홈을 형성하여 FRP를 매입하는 보강 즉, NSM 보강을 대상으로 하였다. 실험에서의 주요 변수는 보강방법과 사용 내화재료로서, Perlite계 재료를 표면에 분사하여 보강하는 방법, Calcium silicate계 보드로 표면에 부착하는 방법, 그리고 추가로 홈내부에 Polymer mortar 또는 Calcium silicate조각을 삽입하여 보강하는 방법으로 보강한 뒤 가열로 내부의 온도변화에 따른 열전달을 관찰하였다. 실험결과, Perlite계 내화뿜칠로 표면을 보강하는 경우보다 Calcium Silicate계 내화보드로 표면을 보강하는 방법이 효과적인 것으로 나타났다. 홈 내부의 에폭시가 유리전이온도에 도달할 때의 외부 표면온도 $820^{\circ}C$까지 내화단열성능을 확보할 수 있는 것으로 나타났다.
이 연구는 부착형 정착 장치를 갖는 CFRP(carbon fiber reinforced polymer) 긴장재의 정착에 관한 실험 연구이다. 적절한 채움재를 도출하기 위해 예비 실험을 수행하였고, 에폭시 또는 콘크리트 모르타르와 같은 5종의 재료가 채움재로 사용되었다. 실험 결과 무수축 모르타르를 사용한 시편에서 최대 인장강도를 보이므로 이 연구에서는 CFRP 긴장재용 강관 몰드의 채움재로써 무수축 모르타르를 결정하였다. 예비 실험으로 도출된 채움재를 이용하여 강관 몰드의 적정 제원을 도출하기 위해 외경, 두께 및 길에 대한 추가 실험을 수행하였다. 이 실험을 통해 무수축 모르타르를 사용한 강관 몰드의 적정 제원이 도출되었고, 이러한 제원의 강관 몰드로 정착된 CFRP 긴장재는 안정적인 인장 성능을 보였다.
For the last decade many bridges and buildings have experienced flexural strengthening with the fiber reinforced polymer(FRP) bonding system, demands for increasing heavy traffic loads and the changing of the code application. Of the many strengthening systems, NSM(near surface mounted) system with FRP has become attractive and popular way of strengthening for the existed RC structures and many studies and applications of this technique have significantly increased all over the world. Meanwhile, polymer mortar that contains much of the same ingredients as cement but includes the addition of certain polymer resins for enhancing desired physical properties, has been used as an alternative adhesive. This paper focuses on flexural behaviour of CFRP-bar NSM system with variables such as kinds of adhesive, anchorage, sectional aspect ratio. Based on the test results and test-to-predicted ratio, this paper provides researchers and practical engineers a fundamental knowledge and intuition.
재활용 PET와 fly-ash를 이용하여 두 가지 종류의 고분자 몰타르(PMM)를 제조하였다. 재활용 PET의 조성을 변화시켜 경성(rigid) polymer-modified mortar(PMM)와 연성(flexible) PMM을 제조하였다. 마찰계수 측정을 포함하는 기계적 특성과 흡음 특성을 조사하였고 상업적 PMM인 에폭시 PMM과 PET PMM을 비교하였다. 기계적 특성들의 결과로부터 경성 PMM이 상업적인 PET PMM에 비하여 우수함을 알 수 있었다. 흡음계수 측정에서 경성 PMM과 연성 PMM 모두 상업적인 PMM에 비하여 매우 우수한 흡음 특성을 보여주었다. 또한, 마찰계수 측정결과는 경성 PMM이 바닥재의 활용에 적절하다는 것을 보여주었다.
시멘트 모르타르의 내마모성, 여러 피착체에 대한 부착성능, 내화학성, 내수성 등의 많은 성능을 개선시키는 데 폴리머 디스퍼젼은 매우 유용한 재료로서 본 실험에 사용한 SBR은 상업적으로 국내에서 생산되고 있는 시멘트 적용성이 우수한 재료이다. 본 실험에서는 시멘트 모르타르에 높은 유동성을 유도하여 자기 평활성을 가지도록 고유동화제와 SBR을 사용하여 시험체를 제작하였으며 SBR에 의한 시험체의 부착강도의 발현 특성을 파악하고자 하였으며 SBR에 의해 개질된 자기 평활성을 가지는 시멘트 모르타르는 재령의 증가에 따라 부착강도는 증가하는 현상을 보여주었으며 파괴형상을 보면 재령이 증가함에 따라 시험체에서 보다는 계면과 피착체에서 외부 인장력에 대하여 파괴가 일어났다. 현재 사무실, 공장, 주차장 등의 바닥 마감재로 널리 사용되고 있는 합성 고분자계 재료인 에폭시 수지나 폴리우레탄 제품은 연도변화가 심하여 가사시간이 상당히 짧다는 것을 확인할 수 있었으며 이에 반하여 본 연구의 시험체는 충분한 가사시간을 확보할 수 있는 이점을 가진 재료로 여겨진다.
Steel plate-masonry composite structure is a newly-developed type of structural technique applicable to existing masonry buildings by which the load-bearing walls can be removed for large spaces. This kind of structure has been used in practice for its several advantages, but experimental investigation on its elements is nearly unavailable in existing literature. This paper presents an experimental study on the flexural behaviour of four steel plate-masonry composite beams loaded by four-point bending. Test results indicate that failure of the tested beams always starts from the local buckling of steel plate, and that the tested beams can satisfy the requirement of service limit state. In addition, the assumption of plane section is still remained for steel plate prior to local buckling or steel yielding. By comparative analyses, it was also verified that the working performance of the beam is influenced by the cross-section of steel plate, which can be efficiently enhanced by epoxy adhesive rather than cement mortar or nothing at all. Besides, it was also found that the contribution of the encased masonry to the flexural capacity of the composite beam cannot be ignored when the beam is injected with epoxy adhesive.
This study evaluated the fire resisting capacity and post-fire serviceability of the concrete beams retrofitted by near surface mounted method(NSM) using GFRP plates. Main parameters in the test are grout materials and fire exposure. For the test, two types of grout materials between concrete substrate and GFRP plate were used; flame resisting epoxy and filling mortar. Four RC beam specimens were made and two of them were exposed to fire according to real scale fire curve proposed KS F 2257. After the fire exposure test, flexural test were performed to investigate the flexural performance of concrete beams including strength and deformation. From the test results, it was found that the beam retrofitted by NSM-GFRP presented higher flexural strength than that of the beam without retrofit, which indicates NSM-GFRP retrofit technologies is effective to maintain flexural strength even after fire exposure. In addition, the specimens grouted by epoxy showed good performance in strength but bad performance in ductility.
In this study, the behavior of R/C beam strengthened with carbon fiber laminate(C.F.L) is analyzed from the test results. Test parameters are the width, the thickness and the length of C.F.L. and method of construction. The failure mode and ultimate load are analyzed from these measured data. Test results shows that the peak moment of specimens strengthened with C.F.L is increased to 1.43~1.90 times of that of non-rehabilitation specimen. The wider lap width, larger amount of rehabilitation materials, the larger strength is obtained.
The main goal of this study was to develop a convenient strengthening technique for retrofitting of reinforced concrete members. For this purpose a new retrofitting material so-called prefabricated-HSPRCC (high performance steel plate reinforced cementitious composite) panel was developed by using high performance concrete and perforated steel plate. Prefabricated-HSPRCC composes advantages of steel and high performance concrete. The prefabricated-HSPRCC panels were either only bonded on the specimens using epoxy mortar or anchored to the specimen by steel bolts as well as bonding. Effect of different variations such as prefabricated-HSPRCC panel thicknesses, steel plate thicknesses, puncture orientation of perforated steel plate, existence of anchorage etc. were studied through a simple experimental work. The behaviour of the specimens under vertical point load was also studied by using simple mechanics. The retrofitted specimens were found to exhibit much better performance both in terms of strength and deformation capability. The anchorage application was found to positively affect this improved performance. Furthermore, as a result of the tests the best parameters of prefabricated-HSPRCC plate for improving strength and deformation capacities were determined.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.