• Title/Summary/Keyword: elongation properties

검색결과 1,481건 처리시간 0.026초

실리카-실란이 클로로부틸 방진고무 복합소재의 기계적 물성 증가에 미치는 영향 (Effects of Silica-Silane for CIIR Vibration Isolation Compound upon Increased Mechanical Properties)

  • 김성민;김광제
    • 폴리머
    • /
    • 제39권1호
    • /
    • pp.107-113
    • /
    • 2015
  • 클로로부틸(CIIR) 방진고무 복합소재 내에서 실리카-실란이 기계적 물성과 점탄성에 미치는 영향을 평가하였다. 실리카-실란이 첨가된 경우, 방진고무의 핵심물성 중 하나인 인열강도는 13%, 파단 신장률은 14%씩 각각 증가하였다. 그 외 인장강도 및 경도 등은 비슷한 값을 보였다. 점탄성 관찰로부터 인열강도 및 파단 신장률의 증가는 실리카-실란의 첨가에 의한 복합소재 내 실리카와 클로로부틸간 3차원 사슬구조의 형성에 따른 것으로 판단되었다. 인열강도 및 파단 신장률의 향상에 관한 메커니즘을 논의하였다.

Effect of treatment temperature on mechanical properties of silk textiles made with silk/polyurethane core-spun yarn

  • Bae, Yeon Su;Um, In Chul
    • International Journal of Industrial Entomology and Biomaterials
    • /
    • 제33권2호
    • /
    • pp.108-112
    • /
    • 2016
  • Silk has been used extensively in textile applications because of its good luster and feel. However, the low elongation and elastic recovery of silk has limited its use in a wider variety of textile applications. In this study, silk textile samples were made with a highly twisted silk/polyurethane core-spun yarn. They were immersed in water and dried at different temperatures, and the effect of treatment temperature on the mechanical properties of the silk textile was examined. It was found that the water temperature strongly affected the morphology and mechanical properties of the silk textile, whereas the drying temperature did not. As the water temperature was increased, the weft silk yarn became tangled and the interval between warp yarns decreased, resulting in shrinkage of the silk textile. When the silk textile was immersed in water at high temperature (i.e., $100^{\circ}C$), the elongation of the textile increased eight-fold as compared to an untreated silk textile. The maximum elastic recovery ratio of the silk textile was 96.7%.

그라파이트/구리 복합재료의 기계적 특성에 미치는 그라파이트 형상과 복합재료 제조방법의 영향 (Effects of Graphite Shape and Composite Fabricating Method on Mechanical Properties of Graphite/Copper Composites)

  • 손유한;한준현
    • 한국재료학회지
    • /
    • 제28권10호
    • /
    • pp.601-609
    • /
    • 2018
  • To study the effects of graphite shape and the composite fabricating method on the mechanical properties of graphite/copper (Gr/Cu) composites, a copper composite using graphite flakes or graphite granules as reinforcing phases is fabricated using mechanical mixing or electroless plating method. The mechanical properties of the Gr/Cu composites are evaluated by compression tests, and the compressive strength and elongation of the Gr/Cu composites using graphite granules as a reinforcing phase are compared with those of Cu composites with graphite flakes as a reinforcing phase. The compressive yield strength or maximum strength of the Gr/Cu composites with graphite granules as a reinforcing phase is higher than that of the composites using graphite flakes as a reinforcing phase regardless of the alignment of graphite. The strength of the composite produced by the electroless plating method is higher than that of the composite material produced by the conventional mechanical mixing method regardless of the shape of the graphite. Using graphite granules as a reinforcing phase instead of graphite flakes improves the strength and elongation of the Gr/Cu composites in all directions, and reduces the difference in strength or elongation according to the direction.

Mod. 440A 마르텐사이트 스테인리스강의 기계적 성질에 미치는 템퍼링의 영향 (The effect of Tempering on the Mechanical Properties of Mod. 440A Martensitic Stainless Steel)

  • 권순두;김영철;강창룡
    • 열처리공학회지
    • /
    • 제26권3호
    • /
    • pp.120-125
    • /
    • 2013
  • In this study, the effect of tempering treatment on the mechanical properties in modified 440A steel has been investigated. The amount of remaining carbide decreased with increasing the austenitizing treatment temperature, and all carbides were completely dissolved at $1250^{\circ}C$. The amount of remaining carbide decreased with increasing the time of austenitizing, but the carbide remained insoluble up to 120 minutes at $1050^{\circ}C$. With increasing the tempering temperature, tensile strength decreased, and elongation increased slowly, while hardness rapidly decreased, and impact value unchanged and then rapidly increased over $500^{\circ}C$. The strength and hardness slowly decreased, while the elongation and impact absorbed energy increased with increasing the tempering time. $Cr_{23}C_6$ type carbide was precipitated and sharp decrease of elongation and toughness by tempering did not appear.

마르텐사이트와 오스테나이트의 2상 조직을 갖는 고 Mn 오스테나이트계 스테인리스강의 인장성질 (Tensile Properties of High Mn Austenitic Stainless Steel with Two Phases of Martensite and Austenite)

  • 김영화;강창룡
    • 한국해양공학회지
    • /
    • 제27권4호
    • /
    • pp.9-13
    • /
    • 2013
  • The tensile properties of high manganese austenitic stainless steel with the two phase structures of deformation-induced martensite and reversed austenite were studied. Reversed austenite with an ultra-fine grain size of less than $0.3{\mu}m$ was obtained by reversion treatment. The two phases structures of deformation-induced martensite and reversed austenite were obtained by an annealing treatment in the range of $500^{\circ}C-700^{\circ}C$ for various times in 70% cold- rolled high-manganese austenitic stainless steel. The volume fraction of the reversed austenite increased rapidly with increases in the annealing temperature and time. In the stainless steel with the two phases of austenite and martensite, the strength decreased rapidly, while the elongation increased slowly and then rapidly increased with an increase in the volume fraction of the reversed austenite. Therefore, the strength and elongation were strongly controlled by the volume fraction of reversed austenite. A good combination of high strength and elongation could be obtained by the mixed structure of reversed austenite and deformation-induced martensite.

25Cr-7Ni-2Mo-4W 슈퍼 2상 스테인리스강의 기계적 성질에 미치는 R상의 영향 (Effect of R Phase Formation on the Mechanical Properties of 25Cr-7Ni-2Mo-4W Super Duplex Stainless Steel)

  • 이병찬;강창룡
    • 한국재료학회지
    • /
    • 제24권8호
    • /
    • pp.401-406
    • /
    • 2014
  • In this study, we investigated the precipitation behavior of the R-phase precipitated at the initial stage of aging and its effects on the mechanical properties of 25%Cr-7%Ni-2%Mo-4%W super duplex stainless steel. The R-phase was mainly precipitated at the interface of ferrite/austenite phases and inside of the ferrite phase during the initial stage of aging. It was transformed into the ${\sigma}$-phase with an increase of the aging time. The ferrite phase was decomposed into a new austenite(${\gamma}_2$)phase and the ${\sigma}$-phase by an aging treatment. The R phase was an intermetallic compound showing higher molybdenum and tungsten concentrations than the matrix and also showed higher molybdenum and tungsten concentrations than the ${\sigma}$ phase. In the initial stage of aging, precipitation of the R-phase did not change the hardness, the strength and the elongation. The hardness and the strength increased upon a longer aging time, but the elongation rapidly decreased. These results show that the R-phase did not significantly affect the hardness and the strength, though it did influence the elongation.

Properties of Carbon Black/SBR Rubber Composites Filled by Surface Modified Carbon Blacks

  • Dai, Shuang-Ye;Ao, Ge-You;Kim, Myung-Soo
    • Carbon letters
    • /
    • 제8권2호
    • /
    • pp.115-119
    • /
    • 2007
  • Properties of carbon blacks and carbon black/SBR rubber composites filled by surface modified carbon blacks were examined. Although the specific surface area of carbon blacks increased after the surface modifications with heat, acid, and base, there were no obvious changes in resistivity. The composites filled by heat treated carbon blacks showed a higher tensile strength and elongation than those filled by raw blacks. The acid and base treated carbon blacks filled composites also showed higher tensile strength but similar elongation values with those filled by raw blacks. With increasing loading ratio, both tensile strength and elongation increased, and appeared a maximum value at 30-40 phr. Modulus at 300% strain remained increasing with further loading of carbon blacks. At the same loading, the heat treated black filled composites showed similar modulus values with composites filled by raw blacks but for base and acid treated black filled composites much higher values were obtained. After the surface modification, the functional groups which played an important role in reinforcement action were changed.

Linear Low Density Polyethylene (LLDPE)/Zeolite Microporous Composite Film

  • Jagannath Biswas;Kim, Hyun;Soonja Choe;Patit P. Kundu;Park, Young-Hoon;Lee, Dai-Soo
    • Macromolecular Research
    • /
    • 제11권5호
    • /
    • pp.357-367
    • /
    • 2003
  • The linear low density polyethylene (LLDPE)/zeolite composite using novel inorganic filler, zeolite, is prepared by a conventional compounding procedure using a twin-screw extruder. The observed scanning electron microscopic (SEM) morphology shows a good dispersion and adhesion of zeolite in the LLDPE matrix. The mechanical properties in terms of the Young's modulus, the yield stress, the impact strength, and the elongation at break were enhanced with a successive increment of zeolite content up to 40 wt%. The X-ray diffraction measurement is of supportive for the improved mechanical properties and the complex melt viscosity is as well. Upon applying a certain level of strain on the composites, the dewetting, the air hole formation and its growth are characterized. The dewetting originates around the filler particles at low strain and induces elliptical micropores upon further stretching. The microporosity such as the aspect ratio, the number and the total area of the air holes is also characterized. Thus, the composites loaded 40 % zeolite and 300 % elongation may be applicable for breathable microporous films with improved modulus, impact and yield stress, elongation at break, microporosity and air hole properties.

Incoloy 825 합금의 기계적 성질에 미치는 열간 단조비와 용체화 온도의 영향 (Effect of Hot Forging Ratio and Solution Treatment Temperature on the Mechanical Properties of Incoloy 825 Alloy)

  • 김도훈;박영태;손영민;강창룡
    • 열처리공학회지
    • /
    • 제31권5호
    • /
    • pp.213-219
    • /
    • 2018
  • This study was carried out to investigate the effect of hot forging ratio and solution treatment temperature on the mechanical properties of incoloy 825 alloy. With an increasing of the hot forging ratio, grain size and range of grain size was decreased. With an increasing of the solution treatment temperature after 90% forging, grain size and range of grain size was increased. Cr carbides and Ti nitrides was precipitated at below $900^{\circ}C$ and volume fraction of precipitate was increased with an decreasing of the solution treatment temperature. With an increasing of the hot forging ratio, hardness, tensile strength and elongation, toughness was increased. With an increasing of the solution treatment temperature after 90% forging, hardness and strength was increased, elongation and toughness was decreased by grain refinement. With an increasing of the forging ratio, effect of solution treatment temperature on the hardness, strength and elongation was small, but on the toughness was large.

콘크리트 표면강화 에폭시의 장기특성 평가 (An Estimation of the Long-Term Properties of Epoxy Used for Reinforcing Surface in Concrete)

  • 김성욱;김도겸;이장화;김근경;김상조
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1999년도 학회창립 10주년 기념 1999년도 가을 학술발표회 논문집
    • /
    • pp.183-186
    • /
    • 1999
  • Up to date, it is difficult to estimate the consistence of properties on the epoxy liner in service time because an estimation of the long term environment-deterioration with aging has not been processed. In the study, the estimation on epoxy liner is carried by the physical test 7 rounds. There are the elongation the and the crack bridging test in the part of physical tests. An elongation test is carried out with epoxy membrane and a crack bridging test is carried out with specimen painted epoxy on concrete. The subjects of test and estimation are a containment quality system and a fibre-glass reinforced system. The materials of these systems are a Robber added Epoxy, a Silica added Epoxy, and a Fiber reinforced Epoxy. Ensuring the test data, properties of epoxy liner was estimated and the change of properties was predicted on epoxy liners.

  • PDF