Sn-Ag-Bi/Cu 솔더 조인트의 aging시 금속간화합물 성장 거동 (Growth Behavior of Intermetallic Compounds in Sn-Ag-Bi/Cu Solder Joints during Aging)

  • 한상욱;박창용;허주열
    • 한국마이크로전자및패키징학회:학술대회논문집
    • /
    • 한국마이크로전자및패키징학회 2003년도 기술심포지움 논문집
    • /
    • pp.133-137
    • /
    • 2003
  • The effect of Bi additions to the eutectic Sn-3.5Ag solder alloy on the growth kinetics of the intermetallic compound (IMC) layers during solid-state aging of Sn-Ag-Bi/Cu solder joints has been Investigated. The Bi additions enhanced the growth rate of the total IMC layer comprising of $Cu_6Sn_5$ and $Cu_3Sn$ sublayers. This enhanced IMC growth rate was primarily due to the rapid increase In the growth rate of $Cu_6Sn_5$ sublayer. The growth rate of $Cu_3Sn$ sublayers was little influenced and appeared to be retarded by the Bi additions. The observed growth behavior of $Cu_6Sn_5$ and $Cu_3Sn$ sublayers could be understood if the interfacial reaction barrier at the $Cu_6Sn_5/solder$ interface were reduced by the segregation of Bi at the interface.

  • PDF

Some Characteristics of Anisotropic Conductive and Non-conductive Adhesive Flip Chip on Flex Interconnections

  • Caers, J.F.J.M.;De Vries, J.W.C.;Zhao, X.J.;Wong, E.H.
    • JSTS:Journal of Semiconductor Technology and Science
    • /
    • 제3권3호
    • /
    • pp.122-131
    • /
    • 2003
  • In this study, some characteristics of conductive and non-conductive adhesive inter-connections are derived, based on data from literature and own projects. Assembly of flip chip on flex is taken as a carrier. Potential failure mechanisms of adhesive interconnections reported in literature are reviewed. Some methods that can be used to evaluate the quality of adhesive interconnections and to evaluate their aging behavior are given. Possible finite element simulation approaches are introduced and the required critical materials properties are summarized. Response to temperature and moisture, resistance to reflow soldering and resistance to rapid change in temperature and humidity are elaborated. The effect of post cure during accelerated testing is discussed. This study shows that only a combined approach using finite element simulations, and use of appropriate experimental evaluation methods can result in revealing, understanding and quantifying the complex degradation mechanisms of adhesive interconnections during aging.

계육의 숙성 중 Titin의 Z선 영역(Zeugmatin)의 변화 (Postmortem Changes in Z-disk Domain of Titin in the Chicken Muscle)

  • 안동현;박선미
    • 한국축산식품학회지
    • /
    • 제18권4호
    • /
    • pp.292-300
    • /
    • 1998
  • This study was undertaken to determine the influence in the Z-disk domain of titin on the tenderization of meat by the structure change of myofibrillar Z-disks during post-mortem aging. After weakening the structure of Z-disks, the Z-disk region was splitted. As the results, myofibrils were fragmented by mechanical strength. Using indirect immunofluorescence microscopy, we show that the Z-disk domain of titin was disappeared from myofibrils in this period. There phenomenon were also shown by treating myofibrils with a solution containing 0.1mM $Ca^{2+}$. We conclude that change in Z-disk domain of titin is directly effected on the tenderization of meat during post-mortem aging and these change is due to manily calcium ions.

  • PDF

비타민 C가 가용성 콜라겐의 성숙과정에서 Pyridinoline 생성 효소계에 미치는 영향 (The Effect of Ascorbic Acid on the Enzyme Reaction in Pyridinoline Formation during Soluble Collagen Maturation)

  • 김미향
    • 한국식품영양과학회지
    • /
    • 제27권2호
    • /
    • pp.305-312
    • /
    • 1998
  • Normal tensile strength in collagen fibrils is due to intermolecular and intramolecular crosslinks which are known to be altered in aging. Pyridinoline, a mature crosslink which is stable and nonreducible, is derived from two hydroxyallysine and one hydroxylysine residues of collagen fibrils. The excess formation of pyridinoline in collagen is associated with making the tissue stiffer, less soluble and less digestible by enzymes. Lysyl oxidase is the enzyme that initiates the biosynthesis or crosslinks in collagen by catalyzing the oxidative deamination of the lysyl and hydroxylysyl residues in these molecules, and its activity is inhibited by $\beta$-aminopropionitrile(BAPN). Our previous work demonstrated that the pyridinoline content of bone collagen significantly was increased during incubation for 5 weeks at 37$^{\circ}C$ invitro, but it was diecrased by the addition of ascorbic acdi(AsA). In this study, we clarified the specific action of AsA in aging process in vitro enzymatic reaction.

  • PDF

STS 316의 시효 열화 처리와 크리프 거동 특성 (Thermal Aging and Creep Rupture Behavior of STS 316)

  • 임병수
    • 한국생산제조학회지
    • /
    • 제8권4호
    • /
    • pp.123-129
    • /
    • 1999
  • Although type 316 stainless steel is widely used such as in reactors of petrochemical plants and pipes of steam power plants and s attracting attention as potential basic material for the fast breeder reactor structure alloys in nuclear power plants and is attracting attention as potential basic material for the fast breeder reactor structure alloys in nuclear power plants the effect of precipitates which form during the long term exposure at service temperature on creep properties is not known sufficiently. In this study to investigate the creep properties and the influence of prior aging on the microstructure to form precipitates specimens were first solutionized at 113$0^{\circ}C$ for 20 minutes and then aged for different times of 0 hr, 100 hrs, 1000 hrs and 2200 hrs at 75$0^{\circ}C$ After heat treatments tensile tests both at room temperature and $650^{\circ}C$ and constant load creep ruptuere tests were carried out.

  • PDF

열화 메커니즘 규명을 위한 옥외용 실리콘고무의 산성비 성분 열화특성 연구 (A Consideration of Degradation Mechanism of a Effect of the Nitric Solution on the Aging Characteristics of the Outdoor Silicone Rubber)

  • 이정헌
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 춘계학술대회 논문집 센서 박막재료 반도체재료 기술교육
    • /
    • pp.132-136
    • /
    • 2002
  • In this paper, aging characteristics of outdoor silicone rubber insulator resulting from the acid rain have been investigated with regards to nitrate ion $({NO_{3}}^{-1})$. For this purpose, silicone rubber was aged by immersing into the nitric solutions with different level pH during 1500 hours and various tests (tracking, $tan{\delta}$, breakdown voltage, SEM, EDS, contact angle) were performed. It was observed that the degradation was increased to pH 2.5 slightly and at pH 1.5 highly. And thus, it could be expected that there is certain critical point between pH 1.5 and 2.5, which leads to throught degradation.

  • PDF

건강보험 연령별 급여비 추이, 2001-2016 (Trend of Benefit Expenditure in National Health Insurance by Age Group, 2001-2016)

  • 문종윤;박은철
    • 보건행정학회지
    • /
    • 제27권4호
    • /
    • pp.372-374
    • /
    • 2017
  • Korea is one of the fastest aging country in the world. The increase in health expenditure is an inevitable problem in an aging country. We examined trend of benefit expenditure in National Health Insurance (NHI) by age group during 2001 to 2016. The benefit expenditure of NHI was 13.0 trillion won (2001) and 48.7 trillion won (2016); that is 3.76 times to 2001. This rapid increase was mostly due to people aged 65 and over. Proportion of beneficiaries aged 65 and over was 6.9% (2001) and 13.7% (2016), benefit expenditure per capita aged 65 and over was 279 thousand won (2001) and 960 thousand won (2016), and utilization days per capita aged 65 and over 21.44 (2001) and 30.23 (2016). This phenomenon was more pronounced in 75 or 85 aged and over. To contain the health costs for older people, the NHI system should be reformed.

CO, $CO_2$ 가스와 Furan 함유량의 분석을 통한 셀룰로오스 절연지의 열 열화특성 (The Thermal Aging Characteristics of Cellulose Paper using Analysis for CO, $CO_2$ Gas and Furan Compounds)

  • 김재훈;한상옥
    • 전기학회논문지P
    • /
    • 제58권4호
    • /
    • pp.499-504
    • /
    • 2009
  • The analysis for furan compound has provided a complementary technique to dissolved gas analysis(DGA) for monitoring transformers when total concentration of CO and $CO_2$ dissolved in oil only has been evaluated the aging of insulating paper. But, the analysis of furanic compounds by high performance liquid chromatography(HPLC) has been important more than DGA recently. Because it has been known that furanic components in transformer oil have come only from the decomposition of insulating paper. Therefore we have manufactured accelerating aging cell which was aged during 60 hours at 100, 150, 180 and $200^{\circ}C$, respectively, for investigating the characteristics of cellulose paper by thermal using analysis for CO, $CO_2$ and furan compound.

전기적 방법을 이용한 전력용 콘덴서 열화특성 연구 (A Study on the Aging Characteristics of Power Capacitors using Electrical Methods)

  • 김은식;김영욱;김종서;윤철섭;박대희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1998년도 추계학술대회 논문집
    • /
    • pp.199-202
    • /
    • 1998
  • Power capacitors are highly reliable equipment due to their completely enclosed configuration. Aging diagnosis system using partial discharge(PD) and acoustic emission(AE) is being highlighted as a research area for degradation of power capacitors. Their dielectric strength can be however reduced due to some stresses such as over-voltage or thermal degradation of the insulation material during their long period of operation. In this paper, it has been developed to express the AE of the EVENT(average amplitude) and HIT(pulse count) according to the source location. And real time measurement of PD signals for aging diagnosis of power capacitors.

  • PDF

산성비 중 질산 성분에 의한 옥외용 실리콘고무 애자의 열화특성 연구 (An Experimental Investigation of a Effect of the Nitric Solution on the Aging Characteristics of the Outdoor Silicone Rubber Insulator)

  • 이정현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 기술교육위원회 창립총회 및 학술대회 의료기기전시회
    • /
    • pp.28-33
    • /
    • 2001
  • In this paper, aging characteristics of outdoor silicone rubber insulator resulting from the acid rain have been investigated with regards to nitrate ion ($NO^{-1}_{3}$ ). For this purpose, silicone rubber was aged by immersing into the nitric solutions with different level pH during 1500 hours and various tests (tracking, tan $\delta$, breakdown voltage, SEM, EDS, contact angle) were performed. It was observed that the degradation was increased to pH 2.5 slightly and at pH 1.5 highly. And thus, it could be expected that there is certain critical point between pH 1.5 and 2.5, which leads to throught degradation.