• Title/Summary/Keyword: dielectric and piezoelectric properties

Search Result 427, Processing Time 0.021 seconds

Effects on PZT volume fraction on the dielectric and piezoelectric properties with PZT/PVDF O-3 composites (PZT/PVDF O-3형 복합전체에 있어서 PZT 체적비 변화가 유전 및 압전특성에 미치는 영향)

  • 이덕출;김용혁
    • Electrical & Electronic Materials
    • /
    • v.1 no.1
    • /
    • pp.44-53
    • /
    • 1988
  • In this study, PZT/PVDF composites with O-3 phase connectivity were prepared by hot pressing method, and the dielectric and piezoelectric properties as a function of PZT volume fraction were investigated. A modified cubic model was introduced to explain the influence of the PZT volume fraction on the experimentally determined dielectric constant. As A n=0.125, the measured dielectric constant values agreed with the calculated values. It was found that dielectric constant .xi.$_{33}$ and piezoelectric coefficient d$_{33}$ increased with indreasing PZT volume fraction, and hydrostatic piezoelectric figure of merit d/aub h/.g$_{h}$ was improved relative to that of the PZT single phase material.l.l.l.

  • PDF

Piezoelectric and Dielectric Characteristics of PAN-PZT Ceramics with BaCO3Addition (BaCO3첨가량에 따른 PAN-PZI계 세라믹스의 압전 및 유전특성)

  • 박타리;이동균;최지원;강종윤;김현재;윤석진;고태국
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.15 no.4
    • /
    • pp.356-360
    • /
    • 2002
  • The piezoelectric properties of $0.05Pb(Al_{0.5}Nb_{0.5})O_3-0.95Pb(Zr_{0.52}Ti_{0.48})O_3+0.7wt%Nb_2O_5+o.5wt%MnO_2$ ceramics with the additive of BaCO$_3$were investigated. As the addition of BaCO$_3$increased from 0 to 0.4 wt%, the dielectric constant ($\epsilon^T _{33}$), piezoelectric constant ($d_33$), electromechanical coupling factor ($k_p$), and mechanical quality factor ($Q_m$) increased, while the dielectric loss ($tan\delta$) decreased. The highest piezoelectric and dielectric properties were observed at $1200^{\circ}C$ of the sintered temperature with 0.4 wt% of $BaCO_3$, and the properties of $d_33$, $k_p$, and $Q_m$ were 339 pC/N, 60% and 1754, respectively.

Dielectric and piezoelectric properties of low temperature sintering PMN-PZT ceramics for multilayer piezoelectric transformer with $Li_2CO_3$ addition (적층 압전변압기용 저온소결 PMN-PZT 압전세라믹의 $Li_2CO_3$ 첨가에 따른 유전 및 압전특성)

  • Lee, Chang-Bae;Yoo, Ju-Hyun;Park, Chang-Yub;Chung, Kwang-Hyun;Jeong, Yeong-Ho;Paik, Dong-Soo;Jeong, Hoy-Seung
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.07b
    • /
    • pp.821-825
    • /
    • 2004
  • In this paper, in order to develop the low temperature sintering ceramics for multilayer piezoelectric transformer, PMN-PZT ceramcis using $Li_2CO_3$ and $Bi_2O_3$ as sintering aids were manufactured, and their microstructural, dielectric and piezoelectric properties were investigated. The sintering aids were proved to lower the sintering temperature of piezoelectric ceramics due to the effect of $LiBiO_2$ liquid phase. At 0.1wt% $Li_2CO_3$ added specimen sintered at $970[^{\circ}C]$, electromechanical coupling factor(Kp), mechanical quality factor(Qm) and dielectric constant showed the optimum values of 0.50, 2,413 and 1,245, respectively, for multilayer piezoelectric transformer application.

  • PDF

An Analytical Study on Prediction of Effective Properties n Porous and Non-Porous Piezoelectric Composites

  • Lee Jae-Kon
    • Journal of Mechanical Science and Technology
    • /
    • v.19 no.11
    • /
    • pp.2025-2031
    • /
    • 2005
  • Eshelby type micro mechanics model with a newly developed piezoelectric Eshelby tensor is proposed for predicting the effective electroelastic properties of the piezoelectric composite. The model is applied for piezoelectric solids containing both porosities and metal inhomogeneities. The effective electroelastic moduli of the composites such as stiffness, piezoelectric constants, and dielectric constants are predicted by the present model, which are extensively compared with the existing experimental results from the literatures. The validity of Eshelby type model for predicting the effective properties of the composite is thoroughly examined. It can be concluded from this study that a new mechanism is needed to compute correctly the dielectric constants among the effective properties of the composites.

Dielectric and Piezoelectric Properties of (Na,K)$NbO3 Ceramics as a Function of SrTiO3 Substitution (SrTiO3 치환에 따른 (Na,K)NbO3계 세라믹스의 유전 및 압전특성)

  • Lee, Sang-Ho;Yoo, Ju-Hyun;Lee, Yeu-Yong;Song, Hyun-Seon;Mah, Suk-Burm;Kim, Seong-Goo
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.22 no.6
    • /
    • pp.484-488
    • /
    • 2009
  • In this study, in order to develop the lead-free piezoelectric ceramics with high piezoelectric and dielectric properties, $[(K_{0.5}Na_{0.5})_{0.95}Li_{0.05}(Nb_{0.96}Sb_{0.04})]O_3$ ceramics were fabricated using $Ag_2O$ as sintering aid and a conventional mixed oxide process and their piezoelectric and dielectric characteristics were investigated according to the $SrTiO_3$ substitution. $SrTiO_3$ substitution enhanced density, dielectric constant(${\varepsilon}_r$) and electromechanical coupling factor($k_p$). However, mechanical quality factor was deteriorated. And also, Curie temperature ($T_c$), and phase transition temperature($T_p$) were rapidly decreased. At the 0.5 mol% $SrTiO_3$ substitution, density, electromechanical coupling factor($k_p$), dielectric constant(${\varepsilon}_r$) and piezoelectric constant($d_{33}$) of specimen showed the optimum value of $4.437\;g/cm^3$, 0.457, 1294, 265 pC/N, respectively.

Characterization of Elastic, Dielectric and Piezoelectric Properties of piezoelectric Materials

  • Cao, Wenwu
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.11a
    • /
    • pp.13-22
    • /
    • 1999
  • Both the resonance and ultrasonic techniques are standard methods far characterizing the physical properties of piezoelectric materials. However, we found that each technique can only offer a few reliable measurements while the rest often have errors or impossible to implement because of the sample requirements. This paper show that one can use the combination of both techniques to achieve much better accuracy and be able to get the complete set of elastic, dielectric and piezoelectric coefficients using fewer samples. Using an ultrasonic spectroscopy we have also measure the dispersion of the ultrasonic velocity and the attenuation up to 65 MHz. Pb(Zr,Ti)O$_3$[PZT] ceramics were used as examples fur both studies.

  • PDF

PZT-PMN Ceramics for Large Displacement Piezoelectric Devices

  • Lim, Kee-Joe;Park, Jae-Yeol;Lee, Jong-Sub;Kang, Seong-Hwa;Kim, Hyun-Hoo
    • Transactions on Electrical and Electronic Materials
    • /
    • v.5 no.2
    • /
    • pp.76-80
    • /
    • 2004
  • Piezoelectric and dielectric properties as functions of x and y mole ratio in yPb(ZrxTil-x)O$_3$(1-y)Pb(Mn$\_$1/3/Nb/2/3/)O$_3$, ceramics, PZT-PMN, are investigated for large displacement piezoelectric devices. From the experimental results, when y is 0.95 and x is 0.505, the piezoelectric and dielectric properties are maximum, that is, electromechanical coupling coefficient(kp), piezoelectric strain constant(d$\_$33/), permittivity($\varepsilon$$\_$33/$\^$T//$\varepsilon$$\_$0/), and Curie temperature are 58 %, 272 pC/N, 1520 and about 350$^{\circ}C$, respectively. Also, when y is 0.90 and x is 0.50, their properties are 56 %, 242 pC/N, 1220, and 290$^{\circ}C$, respectively. As MgO dopant is added from 0 wt% to 1 wt%, kp increases to 63 % and Qm decreases to 500 at the MgO dopant of 0.1 wt%, and then kp decreases to 57 % as MgO is added.

Piezoelectric and Dielectric Properties of Low Temperature Sintering PMN-PZN-PZT Ceramics according to the Milling Time (밀링 시간에 따른 저온소결 PMN-PZN-PZT 세라믹스의 압전 및 유전특성)

  • Yoo, Ju-Hyun;Lee, Il-Ha;Lee, Kab-Soo
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.20 no.12
    • /
    • pp.1039-1043
    • /
    • 2007
  • In this paper, in order to develop low temperature sintering ceramics for multilayer piezoelectric actuator application, PMN-PZN-PZT ceramics were fabricated using $LiCO_3,\;Bi_2O_3$ and CuO as sintering aids. And also, their piezoelectric and dielectric properties were investigated according to the milling time. All the specimens sintered at $930\;^{\circ}C$ showed tetragonal phases without secondary phases. With increasing milling time, piezoelectric and dielectric characteristic of specimens increased up to 60 hours milling time and then decreased due to the agglomeration of fine particle. Accordingly, it seems that 60 hour is optimum milling condition. At the sintering temperature of $930\;^{\circ}C$ and milling time of 60 hour, density, dielectric constant(${\varepsilon}_r$), electromechanical coupling factor (kp), mechanical quality factor (Qm), piezoelectric d constant showed the optimum value of $7.95\;g/m^3$, 1382, 0.546, 1749, 330 pC/N, respectively for multilayer piezoelectric actuator application.

Effects of Interface Porosity on Dielectric and Piezoelectric Properties of BaTiO3-Polymer Composites of O-3 Type Connectivity (O-3형 BaTiO3-폴리머 복합체의 계면기공율 변화에 따른 유전 및 압전특성)

  • 이형규;김호기
    • Journal of the Korean Ceramic Society
    • /
    • v.26 no.5
    • /
    • pp.617-624
    • /
    • 1989
  • Piezoelectric composites of O-3 connectivity were prepared by thermosetting barium titanate-phenolic resin composite under various cruing pressure. Among three kinds of pore in O-3 type ceramic-polymer composite, such as matrix pores, particle pores, and ceramic-polymer interface pores, the effect of interface porosity on the dielectric and piezoelectric constant was investigated. In pure barium titanate ceramics, the porosity factor of dielectric and piezoelectric constants were 5.7 and 5.0, respectively. However, in BaTiO3-polymer composite, the interface porosity factor of the piezoelectric constant was greater than that of the dielectric constant, interface porosity factor b in d33 was 9.8 and in r 4.6. On the other, piezoelectric voltage constant g33 was independent of the porosity of barium titanate ceramics. But in composite system, the piezoelectric voltage constant g33 was decreased with interface porosity.

  • PDF

The Piezoelectric and Dielectric Properties of PZT-PMFW Piezoelectric Ceramics (PZT-PMFW 압전 세라믹의 압전 및 유전 특성)

  • 이종섭;이문주;이용희;정수현;임기조
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.689-692
    • /
    • 2001
  • In this paper, the pizoelectric and dielectric properties of 0.95Pb(ZrxTil-x)O$_3$- 0.05Pb(Mn$\_$0.2/Fe$\_$0.4/W$\_$0.4/)O$_3$piezoelectric ceramics is investigated as a function of Zr/Ti mole ratio. Also, MPB(Morphotropic Phase Boundary) and optimal sintering temperature is studied using XRD and SEM. As a results, when Zr/Ti mole ratio is 52/48, electromechanical coupling factor, k$\_$p/, is 58[%], permittivity, $\varepsilon$$\^$T/$\_$33//$\varepsilon$0, is 1360 and piezoelectric strain constant, d$\_$33/ is 265[pC/N] and the piezoelectric and dielectric properties become maximum. Phase transition temperature of its ternary piezoelectric system is about 350[$^{\circ}C$]. From the XRD analysis, when Zr/Ti mole ratio is 52/48, tetragonal phase transits to rhombohedral phase. Also, From measuring results of the sintering density, when sintering temperature is 1050[$^{\circ}C$], sintering density become maximum and is about 7930[kg/㎥], and average grain size is about 2-3[$\mu\textrm{m}$].

  • PDF