• 제목/요약/키워드: dental casting alloys

검색결과 70건 처리시간 0.022초

TiN피막 코팅된 치과주조용 합금의 부식거동 (Corrosion Behaviors of TiN Coated Dental Casting Alloys)

  • 조호형;박근형;김원기;최한철
    • 대한금속재료학회지
    • /
    • 제47권2호
    • /
    • pp.129-137
    • /
    • 2009
  • Corrosion behaviors of TiN coated dental casting alloys have been researched by using various electrochemical methods. Three casting alloys (Alloy 1: 63Co-27Cr-5.5Mo, Alloy 2: 63Ni-16Cr-5Mo, Alloy 3: 63Co-30Cr-5Mo) were prepared for fabricating partial denture frameworks with various casting methods; centrifugal casting(CF), high frequency induction casting(HFI) and vacuum pressure casting(VP). The specimens were coated with TiN film by RF-magnetron sputtering method. The corrosion behaviors were investigated using potentiostat (EG&G Co, 263A. USA) in 0.9% NaCl solution at $36.5{\pm}1^{\circ}C$. The corrosion morphologies were analyzed using FE-SEM and EDX. Alloy 1 and Alloy 2 showed the ${\alpha}-Co$ and ${\varepsilon}-Co$ phase on the matrix, and it was disappeared in case of TiN coated Alloy 1 and 2. In the Alloy 3, $Ni_2Cr$ second phases were appeared at matrix. Corrosion potentials of TiN coated alloy were higher than that of non-coated alloy, but current density at passive region of TiN coated alloy was lower than that of non-coated alloy. Pitting corrosion resistances were increased in the order of centrifugal casting, high frequency induction casting and vacuum pressure casting method from cyclic potentiodynamic polarization test.

치과주조용 Ti-X%Cu(X=2,5,10)합금의 미세조직 및 경도 (Microstructure and Hardness of Ti-X%Cu(X=2,5,10) Alloys for Dental Castings)

  • 정종현
    • 대한치과기공학회지
    • /
    • 제31권3호
    • /
    • pp.9-14
    • /
    • 2009
  • This study evaluated the mechanical properties of Ti-Cu alloys with the hope of developing an alloy for dental casting with better mechanical properties than unalloyed titanium. Ti-Cu alloys with four concentrations of Cu(2,5,10wt%) were made in an argon-arc melting furnace. The microstructure and micro-Vickers hardness were determined. X-ray diffraction pattern test was performed on the polished specimens. The microstructure of 2%Cu and 5%Cu alloys are shown acicular ${\alpha}Ti$ phase formed on the surfaces of previously formed $\beta$grains. The 10%Cu alloys has essentially a eutectoid structure; this structure includes lamella of ${\alpha}Ti$ and $Ti_2Cu$ phase that transformed from ${\alpha}Ti$ at the eutectoid temperature. The micro-Vickers hardness of CP Ti specimens was significantly(p<0.05) lower than that of any of the other alloys. Among the Ti-Cu alloys, the 10%Cu alloys exhibited a significantly(p<0.05) higher hardness value. but lower than that of Ti-6%Al-4%V alloy. From these results, it was concluded that new alloys for dental castings should be designed as Ti-Cu based alloys if other properties necessary for dental castings were obtained.

  • PDF

치과용 주조 합금의 방전가공에 따른 표면 성분 변화 (Elemental alteration of the surface of dental casting alloys induced by electro discharge machining)

  • 장용철;이명곤
    • 대한치과기공학회지
    • /
    • 제31권1호
    • /
    • pp.55-61
    • /
    • 2009
  • Passive fitting of meso-structure and super-structures is a predominant requirement for the longevity and clinical success of osseointegrated dental implants. However, precision and passive fitting has been unpredictable with conventional methods of casting as well as for corrective techniques. Alternative to conventional techniques, electro discharge machining(EDM) is an advanced method introduced to dental technology to improve the passive fitting of implant prosthesis. In this technique material is removed by melting and vaporization in electric sparks. Regarding the efficacy of EDM, the application of this technique induces severe surface morphological and elemental alterations due to the high temperatures developed during machining, which vary between $10,000{\sim}20,000^{\circ}C$. The aim of this study was to investigate the morphological and elemental alterations induced by EDM process of casting dental gold alloy and non-precious alloy used for the production of implant-supported prosthesis. A conventional clinical dental casting alloys were used for experimental specimens patterns, which were divided in three groups, high fineness gold alloy(Au 75%, HG group), low fineness gold alloy(Au 55%, LG group) and nonprecious metal alloy(Ni-Cr, NP group). The UCLA type plastic abutment patterns were invested with conventional investment material and were cast in a centrifugal casting machine. Castings were sandblasted with $50{\mu}m\;Al_2O_3$. One casting specimen of each group was polished by conventional finishing(HGCON, LGCON, NPCON) and one specimen of each group was subjected to EDM in a system using Cu electrodes, kerosene as dielectric fluid in 10 min for gold alloy and 20 min for Ni-Cr alloy(HGEDM. LGEDM, NOEDM). The surface morphology of all specimens was studied under an energy dispersive X-ray spectrometer (EDS). The quantitative results from EDS analysis are presented on the HGEDM and LGEDM specimens a significant increase in C and Cu concentrations was found after EDM finishing. The different result was documented for C on the NPEDM with a significant uptake of O after EDM finishing, whereas Al, Si showed a significant decrease in their concentrations. EDS analysis showed a serious uptake of C and Cu after the EDM procedure in the alloys studied. The C uptake after the EDM process is a common finding and it is attributed to the decomposition of the dielectric fluid in the plasma column, probably due to the development of extremely high temperatures. The Cu uptake is readily explained from the decomposition of Cu electrodes, something which is also a common finding after the EDM procedure. However, all the aforementioned mechanisms require further research. The clinical implication of these findings is related with the biological and corrosion resistance of surfaces prepared by the EDM process.

  • PDF

베릴륨 불포함 치과 주조용 니켈-크롬 합금 중 금속의치상용 합금과 금속소부도재관용 합금의 부식에 관한연구 (Corrosion of the non-beryllium dental casting Ni-Cr alloys for the denture base framework metal and the porcelain-fused-to-metal crown)

  • 김홍식;송재상;박수철
    • 대한치과기공학회지
    • /
    • 제34권4호
    • /
    • pp.337-344
    • /
    • 2012
  • Purpose: This study examined the corrosion level by alloy type and pH, and used the corrosion levels as the dental health data. The study utilized one Ni-Cr alloy for the full and removable partial denture metal frameworks and two Ni-Cr alloys for porcelain-fused-to-metal crown, among the non-beryllium dental casting non-precious Ni-Cr alloys. Methods: The alloy specimens were manufactured in $10cm^2$ and stored in the corrosive solution(pH 2.2-4.4) in the electrical water bath($37^{\circ}C$) for seven days. Afterwards, the metal ions were quantitatively analyzed using the ICP. Results: Of the three metal alloys, Bellabond-Plus$^{(R)}$alloy and SOLIBOND N$^{(R)}$alloy, with 22% or higher chrome chemical contents, had higher corrosion resistance than Jdium-100$^{(R)}$alloy with 20% chrome chemical content. In all three alloys, the corrosion of Ni was highest, and metal ion corrosion was higher in the pH 2.2 corrosive solution. Conclusion: Although Ni-Cr alloy was not very corrosive, a Ni-allergic patient should not have Ni-Cr alloy prosthesis. The Ni-Cr alloy for porcelain-fused-to-metal crown should be designed for the dental porcelain to cover the whole crown.

치과 도재용착 주조관용 비귀금속 합금의 반복주조가 기계적 특성 및 미세조직에 미치는 영향 (A Study on How Cyclic Casting of Base Metal Alloy for Dental Ceramic Crown May Effects upon Its Mechanical Properties and Microstructure)

  • 최운재;신무학;정희선;고명원
    • 대한치과기공학회지
    • /
    • 제25권1호
    • /
    • pp.9-20
    • /
    • 2003
  • Using a nickel-chrome casting alloy called 'Rexillium V' which is also available as base metal alloy for dental ceramic crown, 4 types of mixtures(A, B, C, D) with old and new metal were prepared for cyclic casting. The results of cyclic casting can be outlined as follows: 1. For Vickers hardness after casting, specimen A and D tended to have lower hardness in the course of cyclic casting, while specimen B and C tended to higher hardness. 2. The results of X-ray diffraction analysis showed that major crystal phase contained nickelchrome compounds and carbide. 3. The observation results of SEM photographs after cyclic casting show that there was a significant tendency to have similar structures among experimental groups. 4. The results of EDX analysis after cyclic casting showed that there were little differences in chemical composition between parent metal and base metal alloy. Although industrial nickel-chrome cast alloy did not show any significant change in material properties even through cyclic casting over several times, it is recommended that more there be more in-depth studies on how to detect any potential corrosion, discoloration and toxication of dental ceramic crown implanted in patient's oral cavity.

  • PDF

치과 보철물 제작시 사용되는 Sprue의 재료 및 형태가 비귀금속 합금의 주조성에 미치는 영향에 관한 연구 (A Study on the Castability of Base Metal Alloys Which Sprue Shape and materials used in the Production of Dantal Prosdontics)

  • 최운재;신무학;김연수
    • 대한치과기공학회지
    • /
    • 제21권1호
    • /
    • pp.87-96
    • /
    • 1999
  • In order to examine the influence of sprue(used to make crown supplements) on casting, 3 kinds of sprue materials(wax, wood, plastic) and 3 types of sprue(round, square, triangle) were made and buried and cast, then the comparison and analysis of casting characters among sprue materials and among sprue type show the following results : 1. The comparison of casting characters in accordance with sprue materials shows wax sprue of 83.3%, wood sprue 81.3%, and plastic sprue of 80.7%, Wax sprue was the bast materials for casting, However there was no statistically significant difference of casting characters among was, plastic and wood. 2. The comparison of casting in accordance with sprue types shows square sprue of 94.0%, round sprue of 86.9% and triangle sprue of 84.2%. square sprue had a best casting character. 3. When a ring cast using wood sprue was classified from burying materials. its cutting of casting body and sprue indicated much more than any other sprue material. It seems to be caused by the influence of wood residuals and carbon occurrence.

  • PDF

Ti-Pd계 합금의 미세조직변화에 따른 부식거동 (Corrosion Behavior of Ti-Pd System Alloys by Microstructural changes)

  • 차성수;곽동주;남상용
    • 대한치과기공학회지
    • /
    • 제30권2호
    • /
    • pp.9-16
    • /
    • 2008
  • The surface microstructural changes, mechanical properties and corrosion resistance of Ti-Pd alloys for dental biomaterials have been investigated. Ti, Ti-Pd alloys were melted in arc furnace and the corrosion resistance of Ti-Pd alloys was evaluated by anodic polarization test. The surface microstructural changes and mechanical properties of Ti-Pd alloys were analysed by scanning electron microscope and Vickers micro-hardness tester. The vickers hardnees of pure Ti improved by addition of Pd but Ti-25Pd alloy showed decreasing compared with Ti-15Pd. And anodic polarization and potentiostatic test were conducted in 5% HCl to quantify the resistance to corrosion with the addition of Pd, There was no significant difference in corrosion resistance between pure Ti, Ti-5Pd and Ti-15Pd alloy. However, Ti-25Pd alloy showed decreasing compared with pure Ti in corrosion resistance. From these results, it was concluded that newly formulated Ti-15Pd experimental alloy have adequate hardness and high corrosion resistance, and this alloy is promising candidate for a successful dental casting alloy.

  • PDF

Titanium Ions Released from Oral Casting Alloys May Contribute to the Symptom of Burning Mouth Syndrome

  • Park, Yang Mi;Kim, Kyung-Hee;Lee, Sunhee;Jeon, Hye-Mi;Heo, Jun-Young;Ahn, Yong-Woo;Ok, Soo-Min;Jeong, Sung-Hee
    • Journal of Oral Medicine and Pain
    • /
    • 제42권4호
    • /
    • pp.102-108
    • /
    • 2017
  • Purpose: Many metal ions released from dental casting alloys have been reported to influence the intraoral symptoms of oral lichen planus (OLP) and burning mouth syndrome (BMS). The aim of this study was to investigate the relationship between salivary metal ion levels and the prosthetic duration as well as to evaluate the time-dependent morbid effects of metal ions in OLP and BMS patients. Methods: Three study groups consist of the following subjects respectively: 17 OLP patients, 12 BMS patients, and 12 patients without oral symptoms. The salivary concentrations of 13 metal ions (copper, cobalt, zinc, chromium, nickel, aluminum, silver, iron, titanium [Ti], platinum, tin, palladium, and gold) were measured by Laser Ablation Microprobe Inductively coupled Plasma Mass Spectrometry. Results: The Ti ions had statistically significant differences among the groups with a prosthetic duration of less than 5 years. There were no significant differences between all ion levels among the groups wearing dental cast alloys for over 5 years. In the BMS group, the level of Ti ions in patients with prosthetic restorations less than 5 years old were significantly high (p<0.05). Conclusions: In the BMS group, 3-60 months during which salivary Ti levels were higher were matched with the duration of burning symptoms ($15.6{\pm}17.1months$). Furthermore, Ti ions were statistically high in the oral cavity of BMS patients fitted with dental casting alloys for 5 years. These results suggest that Ti ions released from dental implants and oral prostheses could attribute to burning sensation of BMS.