Effect of Acid Treatment of Graphitized Carbon on Carbon Corrosion in Polymer Electrolyte Membrane Fuel Cells (결정성 탄소의 산처리가 고분자연료전지의 성능과 내구성에 미치는 영향 평가)

  • Oh, Hyung-Suk;Han, Hak-Soo;Kim, Han-Sung
    • Journal of the Korean Electrochemical Society
    • /
    • v.12 no.2
    • /
    • pp.181-188
    • /
    • 2009
  • Pt catalyst was adsorbed on Carbon nanofiber (CNF) by modified polyol method after acid treatment of the carbon support with $HNO_3$ and $H_{2}SO_{4}$. As the time for acid treatment increases, more oxygen functional groups on carbon surface were produced which improve the loading amount and dispersion of Pt catalyst on carbon supports. In order to inspect the effect of CNF acid treatment time on electrochemical corrosion, constant potential of 1.4 V was applied to a single cell for 30 min and the amount of $CO_2$ emitted was monitored with on-line mass spectrometry. According to the results of our experiment, more $CO_2$ was produced with Pt/ oxidized-CNF catalyst in compared to that with unoxidized-CNF. Increasing acid treatment time also induces the more $CO_2$ emission. Besides, performance degradation after corrosion test expanded with severer carbon corrosion. From the observed results, it can be concluded that the acid treatment of CNF is beneficial to catalyst loading, but it also is a significant factor declining the fuel cell durability by accelerating electrochemical oxidation of carbon support.

Influence of Filling Density in the Positive Active-material on the Cycle-life Performance of the Tubular Type Gelled Valve Regulated Lead Acid Batteries (튜브식 겔형 납축전지에 있어서 활물질 밀도에 따른 싸이클 수명 특성)

  • Yoon, Youn-Saup;Kim, Byung-Kwan;Lee, Soo;Kim, Kyu-Tea
    • Applied Chemistry for Engineering
    • /
    • v.10 no.3
    • /
    • pp.415-418
    • /
    • 1999
  • The characteristics of VRLA (valve regulated Iead-acid) battery with the tubular positive plate and gel type electrolyte were examined as a function of active material filling density. The filling density of positive plate was 3.2 g/mL, 3.4 g/mL, and 3.6 g/mL, respectively. These VRLA batteries were cycled with 100% DOD (depth of discharge) at the $C_5/5$ rate, followed by IU-type recharge with $I_{max}=0.2C_{10}/10$ and a final voltage V=2.40 V/cell. The test was performed in a thermostatic room at $25{\pm}1^{\circ}C$. The result indicated that the initial capacity was independent of active material filling density, i.e., the highest initial capacity was 3.4 g/mL of filling density and the lowest was 3.6 g/mL. On aspect of the cycle-life performance of the VRLA battery, the filling density of 3.6 g/mL was similar to that of 3.4 g/mL in the positive plate, and both were higher than that of 3.2 g/mL. Water-loss and degradation of the VRLA battery were decreased according to an increase of the filling density in the positive plate. The optimum filling density of the active material was 3.4~3.6 g/mL.

  • PDF

Development Feasibility of Water-Floating Fungicide Formulation for the Control of Sheath Blight(Caused by Rhizotonia solani) in Rice (수도(水稻) 문고병방제용(紋枯病防除用) 수면부유제(水面浮遊劑)의 개발(開發) 가능성(可能性)에 관(關)한 연구(硏究))

  • Oh, Byung-Youl;Kim, Jin-Hwa
    • Applied Biological Chemistry
    • /
    • v.31 no.3
    • /
    • pp.226-233
    • /
    • 1988
  • Some physico-chemical properties and biological activities of new fungicide formulations were tested to investigate a feasibility of water-floating formulation development for sheath blight control in rice. Pencycuron[1-(4-chlorobenzyl)-1-cyclopentyl-3-phenylurea] and flutolanil$({\alpha},{\alpha},{\alpha}$-trifluoro-3'-isopropoxy-O-toluanilide) were chosen as toxicants for the formulations. Vegetable oil and surface active agents were used as a floating agent and spreader, respectively. All the formulations tested showed an excellent spreadability on the water having over $35cm^2/mg$ and were chemically stable, which the degradation rates of active ingredients were less than 10% after 12 weeks of storage at $50^{\circ}C$. Most of the applied test formulation of pencycuron was retained within 0.5cm of the surface paddy water, while that of flutolanil was vertically dispersed in the water. Inhibition activity of the tested pencycuron formulation on the sclerotia germination of the pathogen in paddy water was maintained over 30 days after the formulation treatment. Control effect of 4% pencycuron water-floating formulated with surface active agent of hydro-lipophyllic balance 4.3 on the disease in rice was equal to the reference fungicide(pencycuron 25% WP) when the former was treated one day before the transplantation of rice seedlings. Overflowing the submerged paddy water after the formulation treatment resulted in a deterious effect on the disease control.

  • PDF

In vivo Metabolism of Endosulfan in Carp (Cyprinus carpio) (In vivo 시험에 의한 잉어체내 $^{14}C-endosulfan$의 대사)

  • Lee, K.B.;Shim, J.H.;Suh, Y.T.
    • Applied Biological Chemistry
    • /
    • v.37 no.3
    • /
    • pp.203-209
    • /
    • 1994
  • When $^{14}C-{\alpha}-endosulfan$ was incubated with carp liver, kidney and gut preparations, it was metabolized to water soluble and organosoluble metabolites. In an in vitro test, endosulfan was converted to endosulfan ${\alpha}-hydroxyether$ (EHE), endosulfan alcohol (EA) and endosulfan ether (EE). The addition of NADPH resulted in rapid conversion of endosulfan to the metabolites in 105,000 g soluble fraction and microsomes. However, the rate of metabolism of endosulfan in liver, kidney and gut supplemented with NADPH as a cofactor was higher in the 105,000 g soluble fraction than that in the microsomes of carp under incubation conditions. The enzymes probably involved in the metabolism of endosulfan include the glutathione S-transferase (GST) and the mixed function oxidases (MFO), based on the evidence that addition of either GSH or NADPH increased the degradation of endosulfan.

  • PDF

Dissolution Profile Analysis of Hydroxypropyl Methylcellulose-based Vitamin C Tablets (Hydroxypropyl methylcellulose를 활용한 비타민 C 지속성 정제의 용출 특성 분석)

  • Cha, Ja-Hyun;Hong, Jun-Kee;Lee, Sung-Wan;Cha, Jae-Uk;Ko, Won-Hwa;Baek, Hyon-Ho;Park, Hyun-Jin
    • Korean Journal of Food Science and Technology
    • /
    • v.44 no.3
    • /
    • pp.274-279
    • /
    • 2012
  • The objective of this study was to develop oral matrix tablets for the sustained release of vitamin C. In this study hydroxypropyl methylcellulose (HPMC) has been utilized as an excipient, as it is one of the most widely used polymers, for use during long periods of time in formations. The vitamin C tablet formulation depends on the molecular weight and concentration of sustained-delivery in HPMC. Anti-oxidants have been added as a dissolution medium in order to prevent vitamin C degradation in water. The dissolution test was carried out in a distilled water medium, and the release model equation was applied to analyze the vitamin C release pattern. The results demonstrated that the release and lasting power of vitamin C tablets, containing HPMC, lasted for more than 12 h.

Structural Integrity Evaluation of Mechanically Fastened FRP Beams Under the Effects of Sustained Loads and Environments (지속하중과 환경영향을 받은 MF-FRP 보강보의 구조건전성 평가)

  • Lee, Jae-Ha;Kim, Woo-Seok
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.18 no.1
    • /
    • pp.10-18
    • /
    • 2014
  • Mechanically fastening FRP (MF-FRP) strips using nails and anchors, has been shown to provide a more ductile behavior to the strengthened structural element than using bonded FRP. To further advance the state of the knowledge on this strengthening method, the current study examined environmental effects for six months on MF-FRP beams. Reinforced concrete beams strengthened with mechanically fastened FRP strips and subjected to sustained loads for six months were exposed to outdoor weather and constant high temperatures ($40^{\circ}C$). For comparison, the behavior of RC beam with and without sustained loads was evaluated. Results from flexural tests did not show any significant degradation or change of failure mode as a result of sustained load and of environmental effects such as high temperatures and outdoor weather over a period of six months. Failure of the beams was governed by FRP delamination followed by concrete crushing as not much load applied to the nail and anchors because of slip effects.

Performance Based Evaluation of Concrete Strength and Freeze-Thaw Resistance from Wind Speed - Sunlight Exposure Time Effect (풍속과 일조시간에 따른 콘크리트의 강도 및 동결융해 저항성 성능중심평가)

  • Kim, Tae-Kyun;Choi, Seung-Jai;Choi, Ji-Hun;Kim, Jang-Ho Jay
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.21 no.1
    • /
    • pp.49-58
    • /
    • 2017
  • The phenomena that we experience in everyday life such as snow, rain, wind, and temperature are referred to as weather, and the average state of atmospheric phenomena that occur over a long period of time in a specific region is referred to as climate. In addition, significant variation of climate compared to the average state is referred to as climate change. Concrete structures can have various problems when exposed to elements. Among the problems, the freeze-thaw problem due to extreme climatic factors such as heavy rain and snowfall has become a particularly significant issue recently. The concrete that has been subjected to repeated freeze-thaw rather than too high or low temperature shows serious degradation of durability, and the performance of structures with degraded performance is difficult to recover. Therefore, in this study, concrete durability performance with respect to freeze-thaw from curing conditions change due to wind speed and sunshine exposure time. Concrete freeze-thaw experiment are performed. using wind speed and sunlight exposure time. Also, performance based evaluation through the satisfaction curve based on the freeze-thaw test results are performed.

Perchlorate Removal by River Microorganisms in Industrial Complexes (산업단지지역 하천 미생물에 의한 퍼클로레이트 제거)

  • Jo, Kang-Ick;Ahn, Yeonghee
    • Korean Chemical Engineering Research
    • /
    • v.52 no.1
    • /
    • pp.92-97
    • /
    • 2014
  • Perchlorate ($ClO_4^-$) is an emerging contaminant of soil/groundwater and surface water. $ClO_4^-$ has been shown to inhibit iodide uptake into the thyroid gland and cause a reduction in thyroid hormone production. $ClO_4^-$ is highly soluble and very stable in water. Biodegradation by $ClO_4^-$-reducing bacteria (PRB) is considered the most important factor in natural attenuation of $ClO_4^-$. Rivers in an industrial complex have potential to be contaminated with $ClO_4^-$ discharged from point or non-point sources. In this study, water samples were taken from the rivers running through the Gumi industrial complexes and used for batch test to analyze $ClO_4^-$-degradation potential of river microorganisms. The results of 83-h batch culture showed that $ClO_4^-$-removal efficiency of all samples was 0.77% or less without addition of an external electron ($e^-$) donor. However $ClO_4^-$-removal efficiency was higher when an $e^-$ donor (acetate, thiosulfate, $S^0$, or $F^0$) was added into the batch culture, showing up to 100% removal efficiency. The removal efficiency was various depending on type of $e^-$ donor and site of sampling. When acetate was used as an $e^-$ donor, the highest $ClO_4^-$-removal efficiency was observed among the $e^-$ donors used in this study, suggesting that activity of heterotrophic PRB was dominant. The results of this study provide basic information on natural attenuation of $ClO_4^-$ by river microorganisms. The information can be useful to prepare a strategy to enhance efficiency of $ClO_4^-$ biodegradation for in situ bioremediation.

Design and Development of VDL Mode-2 D8PSK Modem (VDL Mode-2 D8PSK 모뎀 설계 및 개발)

  • Gim, Jong-Man;Choi, Seoung-Duk;Eun, Chang-Soo
    • The Journal of Korean Institute of Communications and Information Sciences
    • /
    • v.34 no.11C
    • /
    • pp.1085-1097
    • /
    • 2009
  • We present a structure and design method of the D8PSK modem compatible with the VDL mode-2 standard and performance test results of the developed modem. In VDL mode-2, the raised cosine filter is used only in the transmitter and a general low pass filter is used in the receiver. Consequently, we can not achieve ISI reduction but can have better spectrum characteristics. Although there is 1~2 dB performance degradation with an un-matched filter compared to that with a matched filter, it is more important to minimize adjacent channel interference in narrow band communications. The transmit signal is generated digitally to avoid the problems(I/Q imbalance and DC offset etc.) of analog modulators. In addition the digital down converter using digital IF sampling technique is adopted for the receiver. This paper contains the overall configuration, design method and simulation results based in part on the previously proposed structures and algorithms. It is confirmed that the modem transmits and receives messages successfully at a speed of max. 870 km/h over ranges of up to 310 km through the ground and in-flight communication tests.

Designed of rPP/d2w®/ZnO Nanocomposite Flexible Film for Food Packaging and Characterization on Mechanical and Antimicrobial Properties (산화분해촉매를 함유한 rPP/ZnO 나노컴포지트 유연식품포장필름 제조 및 물성 특성 연구)

  • Lee, Jin-kyoung;Gil, Bo-min;Lee, Dong-jin;Lee, Ik-mo
    • KOREAN JOURNAL OF PACKAGING SCIENCE & TECHNOLOGY
    • /
    • v.24 no.1
    • /
    • pp.1-11
    • /
    • 2018
  • In this study, pro-oxidant($d2w^{(R)}$) and rPP/ZnO nanocomposite flexible films for food packaging were prepared, and their mechanical and antimicrobial properties were investigated. As a result, the carbonyl index and hydroxyl index increased with exposured time to heat and UV rays. Surface analysis showed that the addition of zinc oxide improved the dispersibility and compatibility of the polymer, so that the surface of the composite film was smooth and the zinc oxide particles were smaller than the compared film. And it kept the physical properties by heat and UV ray blocking effect, and it worked to reduce decomposition. In the antimicrobial activity test, the microbial reduction rate was 3 logs or more at the use concentration of zinc oxide. The tensile strength was increased and the elongation was decreased. Oxidative degradability of multi-layered film in UV exposured for 72 hours, the molecular weight of the film decreased by 75.6%, 1,294 g/mol Mn and 5,920 g/mol Mw. In the safety analysis of food packaging materials, we obtained that are in standard of polypropylene, a food contact material of domestic law.