표준 인장시험과 반복하중 C(T) 시험을 이용한 균열해석에서의 Chaboche 복합경화 모델 결정법 (Determination of Chaboche Cyclic Combined Hardening Model for Cracked Component Analysis Using Tensile and Cyclic C(T) Test Data)

  • 황진하;김훈태;류호완;김윤재;김진원;권형도
    • 한국압력기기공학회 논문집
    • /
    • 제15권2호
    • /
    • pp.31-39
    • /
    • 2019
  • Cracked component analysis is needed for structural integrity analysis under seismic loading. Under large amplitude cyclic loading conditions, the change in material properties can be complex, depending on the magnitude of plastic strain. Therefore the cracked component analysis under cyclic loading should consider appropriate cyclic hardening model. This study introduces a procedure for determining an appropriate cyclic hardening model for cracked component analysis. The test material was nuclear-grade TP316 stainless steel. The material cyclic hardening was simulated using the Chaboche combined hardening model. The kinematic hardening model was determined from standard tensile test to cover the high and wide strain range. The isotropic hardening model was determined by simulating C(T) test under cyclic loading using ABAQUS debonding analysis. The suitability of the material hardening model was verified by comparing load-displacement curves of cyclic C(T) tests under different load ratios.

Application of fiber element in the assessment of the cyclic loading behavior of RC columns

  • Sadjadi, R.;Kianoush, M.R.
    • Structural Engineering and Mechanics
    • /
    • 제34권3호
    • /
    • pp.301-317
    • /
    • 2010
  • This paper studies the reliability of an analytical tool for predicting the lateral load-deformation response of RC columns while subjected to lateral cyclic displacements and axial load. The analytical tool in this study is based on a fiber element model implemented into the program DRAIN-2DX (fiber element). The response of RC column under cyclic displacement is defined by the behavior of concrete, and reinforcing steel under general reversed-cyclic loading. A tri-linear stress-strain relationship for the cyclic behavior of steel is proposed and the improvement in the analytical results is studied. This study only considers the behavior of columns with flexural dominant mode of failure. It is concluded that with the implementation of appropriate constitutive material models, the described analytical tools can predict the response of the columns with reasonable accuracy when compared to experimental data.

내부연결 원추형 임플란트의 육각구조의 유무에 따른 연결부 안정성: 실험적 연구 (Joint stability of internal conical connection abutments with or without hexagon indexes: an in vitro study)

  • 이상운;차민상;이지혜;조리라;박찬진
    • 구강회복응용과학지
    • /
    • 제36권2호
    • /
    • pp.95-103
    • /
    • 2020
  • 목적: 본 연구의 목적은 내부연결 원추형 임플란트의 육각구조 유무가 임플란트 지대주 장축변위와 임플란트 지대주 나사의 풀림토크에 미치는 영향을 평가하고자 하였다. 연구 재료 및 방법: 내부연결 원추형 임플란트를 육각구조를 가진 지대주 그룹(HEX)과 육각구조를 갖지 않는 지대주 그룹(CON)으로 나누고 각 그룹 당 10쌍의 시편을 체결하였다. 지대주 나사를 30 Ncm 조임회전력을 가하여 체결한 뒤 장축변위 및 풀림토크값을 측정하고 250 N 수직적 반복하중을 100,000회 가한 뒤 장축변위 및 풀림토크값을 측정하였다. 각 단계마다 디지털 마이크로미터를 이용하여 임플란트 직경과 수직적 높이를 측정하였고 전자 토크게이지를 이용하여 풀림토크값을 측정하였다. 각 군간의 값의 유의차를 확인하기 위하여 독립 표본 T 검정을 이용하여 통계분석하였다(α = 0.05). 결과: HEX 군은 조임회전력을 가한 뒤 유의하게 높은 장축변위를 나타내였다(P < 0.05). HEX 군과 CON 군은 수직적 반복하중 후 장축변위에 유의한 차이를 보이지 않았다(P = 0.052). HEX 군과 CON 군은 수직적 반복하중 전, 후 풀림토크값 모두 유의한 차이를 보이지 않았다(P = 0.057 and P = 0.138). 모든 그룹에서 반복하중 후 풀림토크값 상실율이 증가하였다(P < 0.05). 결론: 내부연결 원추형 임플란트에서 육각구조를 가진 경우 장축 변위가 더 컸으며, 그 외의 연결부 안정성은 유사하였다. 모든 그룹에서 반복하중 후 풀림토크값 상실율이 증가하였다.

CF8M 스테인리스 강 저주기 환경피로 실험의 주기적 변형률 경화 특성 (Characteristics of the Cyclic Hardening in Low Cycle Environmental Fatigue Test of CF8M Stainless Steel)

  • 정일석;하각현;김태룡;전현익;김영신
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2007년도 춘계학술대회A
    • /
    • pp.17-22
    • /
    • 2007
  • Low-cycle environmental fatigue tests of cast austenitic stainless steel CF8M at the condition of fatigue strain rate 0.04%/sec were conducted at the pressure and temperature, 15MPa, $315^{\circ}C$ of a operating pressurized water reactor. The used test rig was limited to install an extensometer at the gauge length of the cylindrical fatigue specimen inside the small autoclave. So the magnet type LVDT's were used to measure the fatigue displacement at the specimen shoulders inside the high temperature and high pressure water autoclave. However, the displacement and strain measured at the specimen shoulders is different from the one at the gauge length for the geometry and the cyclic strain hardening effect. FEM calculated the displacement and the strain of the gauge length from the data measured at the shoulders. Tensile test properties in elastic and plastic behavior of CF8M material were used in the FEM analysis. A series of low cycle fatigue tests simulating the cyclic strain hardening effect verified that the FEM calculation was well agreed with the simulated tests. The process and method developed in this study would be so useful to produce reliable environmental fatigue curves of CF8M stainless steel in pressurized water reactors.

  • PDF

Protocol for testing of cold-formed steel wall in regions of low-moderate seismicity

  • Shahi, Rojit;Lam, Nelson;Gad, Emad;Wilson, John
    • Earthquakes and Structures
    • /
    • 제4권6호
    • /
    • pp.629-647
    • /
    • 2013
  • Loading protocols have been developed for quasi-static cyclic testing of structures and components. However, it is uncertain if protocols developed for conditions of intense ground shaking in regions of high seismicity would also be applicable to regions of low-moderate seismicity that are remote from the tectonic plate boundaries. This study presents a methodology for developing a quasi-static cyclic displacement loading protocol for experimental bracing evaluation of cold-formed steel stud shear walls. Simulations presented in the paper were based on conditions of moderate ground shaking (in Australia). The methodologies presented are generic in nature and can be applied to other regions of similar seismicity conditions (which include many parts of China, Korea, India and Malaysia). Numerous response time histories including both linear and nonlinear analyses have been generated for selected earthquake scenarios and site classes. Rain-flow cycle counting method has been used for determining the number of cycles at various ranges of normalized displacement amplitude. It is found that the number of displacement cycles of the loading protocol increases with increasing intensity of ground shaking (associated with a longer return period).

유연도법 섬유요소모델에 의한 반복하중을 받는 철근콘크리트 교각의 연성능력 평가 (Evaluation of Ductility Capacity of Reinforced Concrete Bridge Columns Subject to Cyclic Loading Using Flexibility-Based Fiber Element Method)

  • 고현무;조근희;조호현
    • 한국지진공학회논문집
    • /
    • 제6권3호
    • /
    • pp.11-21
    • /
    • 2002
  • 유연도법 섬유요소모델을 통하여 반복하중을 받는 철근콘크리트 교각의 비탄성 이력 거동을 추적하고 직접적인 방법에 의해 변위연성도 평가를 수행하였다. 철근 콘크리트 교각의 극한상태까지의 비탄성 거동을 합리적으로 추적하기 위해 인장강성거동, 기둥-기초면의 불연속 변위 등을 고려하여 철근과 콘크리트의 평균응력-평균변형률 관계, 접촉면요소 등을 실험과 잘 일치하는 기존의 해석 모델을 수정, 적용하였다. 또한 수치해석시 간편하게 적용할 수 있는 직접적인 방법에 의하여 교각의 연성능력을 평가하였으며, 항복변위 및 극한변위의 산출에 영향을 미치는 적분점의 위치, 콘크리트 압쇄 후 강루 철근의 low-cycle fatigue에 의한 파단 시점 등에 대하여 유연도법 섬유요소모델에 적용할 수 있는 값들을 제시하였다. 해석에 의한 변위연성도는 10%이내의 오차를 보이므로, 적용한 해석기법 및 모델에 의한 항복변위 및 극한변위의 평가는 타당하다고 할 수 있다.

Effect of Loading Rate on the Fracture Behavior of Nuclear Piping Materials Under Cyclic Loading Conditions

  • Kim, Jin Weon;Choi, Myung Rak;Kim, Yun Jae
    • Nuclear Engineering and Technology
    • /
    • 제48권6호
    • /
    • pp.1376-1386
    • /
    • 2016
  • This study investigated the loading rate effect on the fracture resistance under cyclic loading conditions to understand clearly the fracture behavior of piping materials under seismic conditions. J-R fracture toughness tests were conducted under monotonic and cyclic loading conditions at various displacement rates at room temperature and the operating temperature of nuclear power plants (i.e., $316^{\circ}C$). SA508 Gr.1a low-alloy steel and SA312 TP316 stainless steel piping materials were used for the tests. The fracture resistance under a reversible cyclic load was considerably lower than that under monotonic load regardless of test temperature, material, and loading rate. Under both cyclic and monotonic loading conditions, the fracture behavior of SA312 TP316 stainless steel was independent of the loading rate at both room temperature and $316^{\circ}C$. For SA508 Gr.1a lowalloy steel, the loading rate effect on the fracture behavior was appreciable at $316^{\circ}C$ under cyclic and monotonic loading conditions. However, the loading rate effect diminished when the cyclic load ratio of the load (R) was -1. Thus, it was recognized that the fracture behavior of piping materials, including seismic loading characteristics, can be evaluated when tested under a cyclic load of R = -1 at a quasistatic loading rate.

댐퍼 스트럿 형상에 따른 의존성 평가 (Dependency Evaluation According to Damper Strut Type)

  • 이현호
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제18권5호
    • /
    • pp.78-86
    • /
    • 2014
  • 본 연구의 목적은 I형 스트럿 및 S형 스트럿 강재댐퍼의 변위 및 속도의존성을 평가하는 것이다. 이를 위하여 12개의 강재댐퍼를 제작하여 의존성 평가를 실시하였으며, 시험 변수는 스트럿 형상, 목표 변위 및 속도이다. 의존성 시험에 의한 반복횟수 평가결과, ASCE 7-10에서 규정한 최소 반복횟수 5회를 충분히 상회하는 것으로 평가되었다. 변위의존성 평가결과, 큰 목표변위 (50mm)의 반복횟수 및 누적에너지소산능력은 적은 목표변위 (25mm)에 비하여 감소하였다. 또한 짧은 목표변위보다 큰 항복강도 및 조기파단을 나타내었다. 속도의존성 평가에서는 빠른 목표속도 (60mm/sec)의 반복횟수 및 누적에너지소산능력이 느린 목표속도 (40mm/sec)에 비하여 감소하였다. 결과적으로 강재댐퍼의 기본 물성, 의존성 평가, 누적에너지소산능력 평가결과, S형 스트럿을 가지는 강재댐퍼의 의존 능력이 I형보다 윌등히 우수한 것으로 평가되었다.

내측연결형 임플란트에 체결한 지대주의 수직침하에 대하여 반복하중이 미치는 영향 (Effect of cyclic loading on axial displacement of abutment into implant with internal tapered connection: a pilot study)

  • 설현우;허성주;곽재영;김성균;한종현
    • 대한치과보철학회지
    • /
    • 제51권4호
    • /
    • pp.315-322
    • /
    • 2013
  • 연구 목적: 내측연결형 임플란트와 지대주의 연결체에 반복하중을 부여하였을 때 수직 침하를 평가하고자 하였다. 연구 재료 및 방법: 외측연결형 임플란트와 내측연결형 임플란트에 세 종류의 시멘트유지형 지대주를 각각 장착하였다. 즉, 외측연결형 지대주(Ext 그룹), 내측연결형 1-piece 지대주(Int-1 그룹), 내측연결형 2-piece 지대주(Int-2 그룹)를 사용하였으며, 각 그룹마다 7개의 시편을 준비하였다. 임플란트-지대주 연결체에 수직하중을 적용하기 위하여 임플란트 받침대에 고정한 후, 4 Hz의 빈도로 $150{\pm}10N$의 반복하중을 가하였다. 수직침하량은 0, 5, 10, 50, 100, 1,000, 5,000, 10,000회의 반복하중 후에 각각 측정하였다. 반복측정분산분석(RM-ANOVA)를 이용하여 반복하중의 영향을 분석하였으며, 패턴변화를 관찰하기 위하여 선형혼합모형(linear mixed model)을 사용하였다. 유의수준은5% 로 설정하였다. 결과: 10,000회 반복하중 후 수직침하량은, Ext 그룹에서 $0.714{\pm}0.488{\mu}m$, Int-1그룹에서 $5.286{\pm}1.604{\mu}m$, Int-2 그룹에서 $11.429{\pm}1.902{\mu}m$를 나타내었다. 패턴분석에서는, Int-1 그룹 및 Int-2 그룹에서 지속적인 수직침하가 관찰되었으며, Ext그룹에서는 수직침하현상이 관찰되지 않았다. 결론:10,000회 반복하중 후의 선형혼합모형을 통한 분석에서, Ext그룹은 수직침하현상을 보이지 않았으나, Int-1 및 Int-2 그룹은 지속적인 수직침하현상을 나타내었다. 또한, Int-2그룹에서 Int-1그룹보다 더 많은 수직침하량이 관찰되었다.

인장하중 및 반복하중을 받는 강재 스프링의 변형 성능 평가 (Evaluation of Deformation Capacity of Various Steel Springs Subjected to Tensile Loading or Uniaxial Cyclic Loading)

  • 권희용;황승현;양근혁;김상희;최용수
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제26권4호
    • /
    • pp.1-10
    • /
    • 2022
  • 이 연구에서는 강재 스프링을 감쇠 장치로써 사용 가능성을 평가하기 위해서, 강재 스프링의 인장 및 반복하중 실험을 수행하였다. 주요 실험변수는 강재의 종류(SAE9254 및 SS275), 스프링상수(700 N/mm, 1,000 N/mm 및 1,400 N/mm) 및 SAE9254의 열처리 유·무이다. 인장 실험 결과, SAE9254로 제작된 강재 스프링의 설계 스프링상수와 측정 스프링상수의 비는 1.08 ~ 1.13이며, SS275로 제작된 강재 스프링의 설계 스프링상수와 측정 스프링상수의 비는 0.86 ~ 0.97로 측정되었다. 항복 이후 열처리 유·무에 따른 SAE9254로 제작된 스프링의 하중-변위 관계 기울기는 약 240 ~ 251 kN/mm 및 92 N/mm 이었으며, SS275로 제작된 스프링의 하중-변위 관계 기울기는 거의 0이었다. 반복하중 실험 결과에서 모든 실험체는 KDS 41 17 00 (2019)에서 요구하는 변위 의존형 감쇠 장치의 적합 조건인 변위 원점에서의 하중 조건, 최대변위에서 하중 조건 그리고 에너지 소산 능력 조건을 모두 만족하였다. 그리고 열처리 안 된 SAE9254 및 SS275로 제작된 강재 스프링의 등가 감쇠비는 열처리 된 SAE9254로 제작된 스프링에 비해 각각 약 2.8배 및 1.9배 높은 수준이었다.