Physicochemical Changes in UV-Exposed Low-Density Polyethylene Films

  • Salem, M.A.;Farouk, H.;Kashif, I.
    • Macromolecular Research
    • /
    • v.10 no.3
    • /
    • pp.168-173
    • /
    • 2002
  • Unstabilized low-density polyethylene (LDPE) films and films formulated with hindered amine light stabilizer (HALS) were exposed to UV-radiation; and the physicochemical changes during photooxidation processes have been investigated using tensile, FTIR spectre-photometric and thermal analytical (DSC) techniques. The dependence of tensile properties (elongation- and stress-at-break), carboxyl index and heat of fusion on UV-irradiation time have been discussed. The use of HALS is found to be effective in maintaining the UV-mechanical properties of the LDPE films. The experimental results showed that there exists no correlation between mechanical properties and carbonyl index, whereas crystallinity correlates well with carbonyl index in unstabilized and stabilized films for irradiation times greater than 100 h. The rate of formation of carbonyl groups is found to be dependent on UV exposure time. Crystallinity of the film samples is strongly influenced by both exposure time and presence of HALS.

Structural Characterization of Silk Fiber Treated with Calcium Nitrate (질산칼슘 처리 농도에 따른 수축견사의 구조특성)

  • 이광길;이용우
    • Journal of Sericultural and Entomological Science
    • /
    • v.39 no.2
    • /
    • pp.186-196
    • /
    • 1997
  • The IR crystallinity index of Calcium nitrate treated silk fiber decreased proportionally to the concentration of calcium nitrate. A partial change of conformation was observed in the concentration of over 46.4-47.6% changing from $\beta$-sheet or to random coil in the crystalline region. This is in coincidence with the result of crystallinity index, which was started to be reduced in the concentration range of 46.4-47.6%. A same trend was observed for the X-ray order factor, birefringence, degree of orientation and surface structure. These structural parameters were remarkably changed on the treatment of silk fibers with concentration of 46.4-17, 6% calcium nitrate. Therefore, it seems that there exists a critical concentration of calcium nitrate in affection the structure and morphology of silk fibers. According to the examination of surface morphology, the fine stripe was observed in the direction of fiber axis at 46.4% concentration. However, the treated concentration was exceeded by 47.6%, the cracks were appeared severely on the fiber surface in the transverse direction as well as fiber axis direction. This result might be related to the tensile properties, specially a tenacity of silk fibers. As a result of quantitative analysis of a dilute acid hydrolysis, three different regions, which are known as a amorphous, semi-crystalline and crystalline region, could be obtained. The hydrolysis rate curves were different with various concentrations of treatment and the relative contents of each region could be calculated.

  • PDF

Improvement of Papermaking Properties of Recycled Fiber with Enzyme (효소처리에 의한 재생섬유의 제지적성 개선)

  • 최윤성;원종명
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.33 no.1
    • /
    • pp.30-37
    • /
    • 2001
  • The effects of enzymatic treatment of recycled fiber were investigated to obtain the basic informations which can be used to improve the papermaking properties of recycled fiber. The recycled fibers were prepared by the repeated handsheet making and disintegrating of hardwood of hardwood and softwood kraft pulp. Novozym 342, Dinimax and Pulpzyme HC were used for enzymatic treatment. The change of fiber length distribution, freeness, contact angle and crystallinity of pulp were measured. The brightness, opacity, breaking and tear index of paper were also measured. The enzymatic treatment decreased long fiber fraction of recycled hardwood fiber, but increased long fiber fraction of recycled softwood fiber. Freeness was decreased with 0.1% enzyme and then increased again with the increase of th enzyme dosage. The improvement of flexibility of recycled fiber was obtained through the decrease of contact angle that is resulted from the decrease of crystallinity of fiber. Brightness and opacity were affected by the type of pulp and enzyme, and dosage of enzyme. Breaking length of recycled hardwood fiber was improved with enzyme treatment, but breaking length of recycled softwood fiber was decreased except for 0.01% Pulpzyme treatment. Tear index was decreased with enzymatic treatment and the lowest decrease was observed with the treatment to Pulpzyme.

  • PDF

Effect of Processing Conditions on the Homogeneity of Partially Degummed Silk Evaluated by FTIR Spectroscopy

  • Kim, Hyun Ju;Chung, Da Eun;Um, In Chul
    • International Journal of Industrial Entomology and Biomaterials
    • /
    • v.26 no.1
    • /
    • pp.54-60
    • /
    • 2013
  • The partial degumming of silk has recently attracted researchers' attention because of its ability to produce silk textiles with new tactile properties, intermediate between the softness of fully degummed silk and the hardness of raw silk. However, it is difficult to obtain partially degummed silk in a homogenously degummed state due to the heterogeneous character of sericin removal. It is also difficult to examine the homogeneity of degumming. In the present study, Fourier transform infrared (FTIR) spectroscopy with attenuated total reflection (ATR) geometry was used to evaluate the effect of processing conditions on the degumming of silk yarns. The crystallinity index, calculated from FTIR spectra, showed an increase with the degumming ratio. Therefore, the homogeneity of degumming could be evaluated by the variation of crystallinity index for 30 different spots in silk yarns. The homogeneity of degumming was influenced by the total degumming time, the content of surfactant, and the liquor rate. No effect was observed upon changing the number of degumming cycles at the same total degumming time.

Effect of heat treatment on the structural characteristics and properties of silk sericin film

  • Park, Chun Jin;Um, In Chul
    • International Journal of Industrial Entomology and Biomaterials
    • /
    • v.37 no.2
    • /
    • pp.36-42
    • /
    • 2018
  • Recently, silk sericin has attracted attention because of its unique properties as a biomaterial, including its UV resistance, moisturizing effect on skin, and wound-healing effect. Therefore, the preparation of sericin in various forms such as gel, film, fiber, and sponge is studied for cosmetic and biomedical applications, and the effect of the preparation conditions on the structure and properties of sericin forms is examined to maximize its performance. In this study, silk sericin films were prepared under different preparation conditions and heat-treated at high temperatures ($100-250^{\circ}C$) to examine the effect of heat treatment on the film structure. The order of the crystallinity index of the untreated sericin film is as follows: F25 (sericin film cast from formic acid) > WE25 (ethanol treated sericin film cast from water at $250^{\circ}C$) > W25 (sericin film cast from water at $250^{\circ}C$) > W100 (sericin film cast from water at $100^{\circ}C$). As the heat-treatment temperature was increased, the color of the sericin films changed gradually from colorless to yellow, brown, and black depending on the temperature. The crystallinity of the sericin film changed after the heat treatment, depending on the preparation condition. Whereas a sericin film cast from formic acid (F25) started to lose its crystallinity at $200^{\circ}C$, thus undergoing the highest loss of crystallinity among the sericin films studied, the rest (W25, WE25, and W100) showed a decrease in crystallinity at $250^{\circ}C$, owing to the disruption of the ${\beta}$-sheet crystallites due to heat.

Conservation status assessment of archaeological bone from Fourier Transform Infrared Spectroscopy and histological Analysis (적외선 분광 분석과 조직 분석을 통한 출토 인골의 보존 상태 평가)

  • Lee, Jeongwon;Kim, Sue Hoon;Kim, Yun-Ji;Cho, Eun Min;Kang, Soyeong
    • 보존과학연구
    • /
    • s.35
    • /
    • pp.87-98
    • /
    • 2014
  • Fourier transform infrared spectroscopy(FTIR-ATR) was applied to chemical analysis for conservation status of 10 human bone remains from Joseon Dynasty. The result of crystallinity index (CI) is $4.25{\pm}0.78$, carbonate to carbonate ratio (C/C) is $0.91{\pm}0.04$ and cabonate content (C/P) is $0.19{\pm}0.06$. The higher histological index (HI) confirmed CI and C/P value was increased and C/C value was reduced. While C/C or C/P values analysis is possible. While DNA analysis can be extracted from the bone, C/C values are lower or C/P values are higher was found to the analysis is possible. Chemical assessment of FTIR and histological index consequence is expected to be applicable as a basis for comprehensive understanding of the conservation status excavated bones.

  • PDF

Variation of Crystalline State in a Stem of Chamaecyparis obtusa E. (편백(Chamaecyparis obtusa E.) 수간내에서의 결정상태의 변이성)

  • Kim, Nam-Hun;Lee, Ki-Yeong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.26 no.4
    • /
    • pp.20-25
    • /
    • 1998
  • Radial variation of crystalline state in a stem of Chamaecyparis obtusa E. was examined by x-ray diffraction analyses. Relative crystallinity and degree of crystallite orientation showed significant differences between juvenile and adult wood. That is, Relative crystallinity increased with increasing the age from pith to about 20th annual ring, after which it reached a more or less constant value. On the other hand, degree of crystallite orientation decreased outward from pith to about 10 years and presented almost a constant value thereafter. Crystal width by Scherrer's equation did not show any significant differences between juvenile and adult wood. Therefore, it was considered that crystallinity index and degree of crystallite orientation by x-ray diffraction method could be used for evaluating wood quality.

  • PDF

The Mineralogy and Chemistry of Clay Minerals of the Middle Ordovician Jigunsan Formation: Implications for the Metamorphic Grade (중부오오도비스기 직운산층 점토광물의 광물학적 및 화학적 연구: 변성정도에 대한 의의)

  • Ko, Hee-Kyeong;Lee, Yong-Il
    • Journal of the Mineralogical Society of Korea
    • /
    • v.4 no.1
    • /
    • pp.32-42
    • /
    • 1991
  • Illite 'crystallinity' and chlorite chemistry are applied to the evaluation of the thermal grade of the Jigunsan Formation. Illite 'crystallinity' value of the formation has the range fom 4.48 to 32.5 in Weaver index (W.I.) and from $0.14{{\Delta}{\circ}}\;2{\Theta}$to $0.03{{\Delta}{\circ}}\;2{\Theta}$in kubler index (K.I). Most of illite 'crystallinity' values in this formation belong to the epizone field (K.I.<$0.21{{\Delta}{\circ}}\;2{\Theta}$). The chemistry and calculated temperature of chlorites from this formation (Fe/(Fe+Mg)=0.45, Tet. Al/Octa. Al=0.84, the calculated temperature=250-270${\circ}C$) are similar to those of epizone chlorites in the literature. The results of this work show that the metamorphic grade of the Jigunsan Formation belongs to the epizone and the formation is believed to have been reached paleotemperatures of at least 300${\circ}C$.

  • PDF

An in Depth Study of Crystallinity, Crystallite Size and Orientation Measurements of a Selection of Poly(Ethylene Terephthalate) Fibers

  • Karacan Ismail
    • Fibers and Polymers
    • /
    • v.6 no.3
    • /
    • pp.186-199
    • /
    • 2005
  • A selection of commercially available poly(ethy1ene terephtha1ate) fibers with different degrees of molecular alignment and crystallinity have been investigated utilizing a wide range of techniques including optical microscopy, infrared spectroscopy together with thermal and wide-angle X-ray diffraction techniques. Annealing experiments showed increased molecular alignment and crystallinity as shown by the increased values of birefringence and melting enthalpies. Crystallinity values determined from thermal analysis, density, unpolarized infrared spectroscopy and X-ray diffraction are compared and discussed in terms of the inherent capabilities and limitations of each measurement technique. The birefringence and refractive index values obtained from optical microscopy are found to decrease with increasing wavelength of light used in the experiments. The wide-angle X-ray diffraction analysis shows that the samples with relatively low orientation possess oriented non-crystalline array of chains whereas those with high molecular orientation possess well defined and oriented crystalline array of chains along the fiber axis direction. X-ray analysis showed increasing crystallite size trend with increasing molecular orientation. SEM images showed micro-cracks on low oriented fiber surfaces becoming smooth on highly oriented fiber surfaces. Excellent bending characteristics were observed with knotted fibers implying relatively easy fabric formation.

Effect of PFI mill and Valley beater refining on cellulose degree of polymerization, alpha cellulose contents, and crystallinity of wood and cotton fibers

  • Hai, Le Van;Park, Hee Jung;Seo, Yung Bum
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.45 no.4
    • /
    • pp.27-33
    • /
    • 2013
  • Manufacturing fabrics from dissolving cellulosic pulp is increasing in these days. For making high quality of cellulose-based fabrics, control of cellulose DP (degree of polymerization), its alpha cellulose content, its brightness, and its crystallinity are important. To process the cellulosic raw material, refining of cellulosic fibers is essential, and it is important to know if refining affects those important cellulose properties. The effects of PFI mill and Valley beater refining on the alpha-cellulose content, cellulose DP, crystallinity, and paper mechanical properties of wood and two different cotton fibers were studied. The results showed that PFI mill refining rarely affected those properties. Fibers refined by a Valley beater displayed a small reduction in fiber length in comparison with those refined by a PFI mill. However, the Valley beater refining method produced almost no changes in cellulose properties, either. The refining process seemed to have very little effect on the cellulose DP, crystallinity index, or alpha-cellulose content until the freeness decreased to around 300 mL CSF for wood and 100 mL CSF for cotton fibers, respectively. There were also no differences in tensile strength development in two refining methods.