• Title/Summary/Keyword: core ceramics

Search Result 85, Processing Time 0.023 seconds

Treatment of rolling cooling waste water by superconductor HGMS method (초전도 자기분리에 의한 냉연공정 폐수처리)

  • Kim, Tae-Hyung;Ha, Dong-Woo;Oh, Sang-Soo;Kim, Young-Hun;Ha, Tae-Wook
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.06a
    • /
    • pp.295-295
    • /
    • 2008
  • This study introduced waste water treatment method applied superconductor HGMS(High Gradient Magnetic Separation). HGMS method treat high efficient method for various waste water. we have surveyed superconducting magnetic separation technology and reviewed the status of related industries using applied superconductivity. We fabricated the prototypes of magnetic matrix filter consisting of stainless steel mesh, which is a core component in the magnetic separation system. In our basic preliminary experiment using HGMS, it was made clear that the fine para-magnetic particles in the rolling colling wasted water obtained from rolling process of POSCO can be separated with high efficiency.

  • PDF

Electrical Properties of $BaTiO_3$ PTC Ceramics with Additional Elements (첨가원소에 따른 $BaTiO_3$ 계 PTC 세라믹스의 전기적 특성)

  • Kim, Hye-Jin;Hong, Youn-Jeong;Lee, Kyu-Mann
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2006.06a
    • /
    • pp.305-306
    • /
    • 2006
  • 자동차의 난방 열원은 HVAC(Heating, Ventilating & Air Conditioning)에 내장되어 있는 히터코어 (Heater Core) 에서 공급하게 되며, 이 히터코어는 엔진에서 가열된 냉각수 열원을 이용하게 된다. 그러나 최근 디젤 엔진의 경우 연소효율의 개선과 CEGR(Cooled Exhaust Gas Recirculation) 시스템의 적용으로 냉각부하가 증가하여 냉각수가 가지는 가용 열원이 기종보다 약 30~40% 정도 저하되고 있다. 따라서 디젤 자동차 및 하이브리드용 자동차의 난방 보조 히터의 국산화 개발이 시급해진 상황이며 초정밀, 고효율 보조 히터의 개발이 요구되고 있다. 현재 적용되고 있는 보조 히터 중에서 PTC 히터는 PTC 소자의 발열을 이용하여 공기를 직접 가열하기 때문에 추가적인 연료소비가 없고 소형 및 저가라는 장점이 있다. PTC 세라믹 소자는 $BaTiO_3$를 모체로 하며, 이의 특성 항상 및 제어를 위해서는 적절한 dopant를 선택하여 균일하게 doping 해야 한다. 지금까지 dopant에 따른 구성 요소 및 역할은 비교적 잘 알려져 있다. 하지만, 자동차용으로 사용되기 위해서는 12V의 저전압에서 동작해야 하며, 또한 소자의 두께가 얇아지게 됨에 따라서 발생하는 전기적 short와 같은 문제점들을 해결하여야 한다. 따라서 본 연구에서는 PTC 세라믹 소자에서 도펀트 종류와 양 조절을 통한 저저항을 확보하고, PTC 세라믹 소자의 박막화를 달성하고자 하였다.

  • PDF

Comparative study in fracture strength of zirconia cores fabricated with three different CAD/CAM systems (3종의 CAD/CAM 시스템에서 지르코니아 코어의 파절 강도에 관한 비교 연구)

  • Shin, Eon-Sick;Lee, Young-Soo;Park, Won-Hee
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.46 no.1
    • /
    • pp.22-30
    • /
    • 2008
  • Purpose: The purpose of this study is to compare three different CAD/CAM systems through the fracture strength of zirconia core and to evaluate the clinical availability of each system. Material and methods: The following three groups of 30 maxillary mesial incisor core for all-ceramics(each group 10) were fabricated as follows: group 1. $Adens^{(R)}$ CAD/CAM system, group 2. $Cerasys^{(R)}$ CAD/CAM system, group 3. 3M $Lava^{(R)}$ CAD/CAM system. All specimens were manufactured consistently thickness 0.5mm and relief $40{\mu}m$. Specimens were subjected to compressive loading on the lingual area by Z250/$SN5S^{(R)}$. Each group's mean and standard deviation were calculated and Kruskal Waillis test, Wilcoxon Rank Sum test were utilized to find out the relationship among the groups. Results: The results were as follows: 1. The mean fracture strength of $Adens^{(R)}$ system was $615.89{\pm}156.1N$, the $Cerasys^{(R)}$ system was $863.98{\pm}151.5N$, and the 3M $Lava^{(R)}$ system was $1143.1{\pm}286.6N$. 2. The fracture strength of the systems showed the significant statistical differences in order of 3M $Lava^{(R)}$ system, $Cerasys^{(R)}$ system, $Adens^{(R)}$ system. Conclusion: In this study, in spite of the differences among the groups, every group showed clinically useful results. It is necessary to study further clinical experiments on a long term basis.

A study on the shear bond strengths of veneering ceramics to the colored zirconia core (착색지르코니아 코어와 전장 도재 사이의 전단결합강도에 관한 연구)

  • Kang, Sun-Nyo;Cho, Wook;Jeon, Young-Chan;Jeong, Chang-Mo;Yun, Mi-Jung
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.47 no.3
    • /
    • pp.312-319
    • /
    • 2009
  • Statement of problem: Delamination of veneering porcelain from underlying ceramic substructures has been reported for zirconia-ceramic restorations. Colored zirconia cores for esthetics have been reported that their bond strength with veneered porcelain is weaker compared to white zirconia cores. Purpose: This study aimed to investigate the shear bond strength by manufacturing the veneering porcelain on the colored zirconia core, using the layering technique and heat-pressing technique, and to evaluate the clinical stability by comparing the result of this with that of conventional metal ceramic system. Material and methods: A Metal ceramic (MC) system was tested as a control group. The tested systems were Katana zirconia with CZR (ZB) and Katana Zirconia with NobelRondo Press (ZP). Thirty specimens, 10 for each system and control, were fabricated. Specimen disks, 3 mm high and 12 mm diameter, were fabricated with the lost-wax technique (MC) and the CAD-CAM (ZB and ZP). MC and ZB specimens were prepared using opaque and dentin veneering ceramics, veneered, 3 mm high and 2.8 mm in diameter, over the cores. ZP specimens were prepared using heat pressing ingots, 3 mm high and 2.8mm in diameter. The shear bond strength test was performed in a Shear bond test machine. Load was applied at a cross-head speed of 0.50 mm/min until failure. Mean shear bond strengths (MPa) were analyzed with the One-way ANOVA. After the shear bond test, fracture surfaces were examined by SEM. Results: The mean shear bond strengths (SD) in MPa were MC control 29.14 (2.26); ZB 29.48 (2.30); and ZP 29.51 (2.32). The shear bond strengths of the tested systems were not significantly different (P > .05). All groups presented cohesive and adhesive failures, and showed predominance of cohesive failures in ceramic veneers. Conclusion: 1. The shear bond strengths of the tested groups were not significantly different from the control group (P >.05). 2. There was no significant different between the layering technique and the heat pressing technique in the veneering methods on the colored zirconia core. 3. All groups presented cohesive and adhesive failures, and showed predominance of cohesive failures in ceramic veneers.

Effect of modeling liquid on the shear-bond strength of zirconia core - porcelain veneer (도재 전용액이 지르코니아 코어-도재 비니어의 전단결합강도에 미치는 영향)

  • Choi, Byung-Hwan;Kim, Im-Sun
    • Journal of Technologic Dentistry
    • /
    • v.36 no.2
    • /
    • pp.83-89
    • /
    • 2014
  • Purpose: This study is to evaluate the effect of modeling liquid on the shear-bond strength between zirconia core and veneering ceramic. Methods: Disk-shaped (diameter: 12.0mm; height: 3.0mm) zirconia were randomly divided into six groups according to the surface conditioning method and whether modeling liquid is used or not to be applied (N=60, n=10 per group): group 1-control group with distilled water(ZD); group 2-control group with modeling liquid(ZM); group 3-airborne particle abrasion with $110-{\mu}m$ $Al_2O_3$(AD) with distilled water; group 4-airborne particle abrasion with $110-{\mu}m$ $Al_2O_3$ with modeling liquid(AM); group 5-liner with distilled water(LD); group $6{\pounds}{\neq}liner$ with modeling liquid(LM). Contact angles were determined by the sessile drop method at room temperature using a contact angle measurement apparatus. The specimens were prepared using dentin veneering ceramics, veneered, 3mm high and 2.8mm in diameter, over the cores. The shear bond strength test was performed in a Shear bond test machine. Load was applied at a cross-head speed of 0.50mm/min until failure. The fractured zirconia surfaces were evaluated by using stereomicroscope (${\times}30$). Collected data were analyzed using SPSS(Statistical Package for Social Sciences) Win 12.0 statistics program. Results: ZD showed the highest contact angle($50.6{\pm}5.4^{\circ}$) and LD showed the lowest value($6.7{\pm}1.3^{\circ}$). Control groups and zirconia liner groups were significantly higher contact angle than liner groups(p<0.05). LD was the highest shear bond strength($43.9{\pm}3.8MPa$) and ZD was the lowest shear bond strength($24.8{\pm}4.9MPa$). Shear bond strengths of control groups and contact angle of liner groups were not significantly different((p>0.05). Liner groups presented adhesive failures. The others groups showed cohesive and adhesive failures. Conclusion: Modeling liquid groups showed lower contact angles and lower shear bond strength compared to those of distilled water groups.

FEA Study on Hoop Stress of Multilayered SiC Composite Tube for Nuclear Fuel Cladding (핵연료 피복관용 다중층 SiC 복합체 튜브의 Hoop Stress 전산모사 연구)

  • Lee, Hyeon-Geun;Kim, Daejong;Park, Ji Yeon;Kim, Weon-Ju
    • Journal of the Korean Ceramic Society
    • /
    • v.51 no.5
    • /
    • pp.435-441
    • /
    • 2014
  • Silicon carbide-based ceramics and their composites have been studied for application to fusion and advanced fission energy systems. For fission reactors, $SiC_f$/SiC composites can be applied to core structural materials. Multilayered SiC composite fuel cladding, owing to its superior high temperature strength and low hydrogen generation under severe accident conditions, is a candidate for the replacement of zirconium alloy cladding. The SiC composite cladding has to retain its mechanical properties and original structure under the inner pressure caused by fission products; as such it can be applied as a cladding in fission reactor. A hoop strength test using an expandable polyurethane plug was designed in order to evaluate the mechanical properties of the fuel cladding. In this paper, a hoop strength test of the multilayered SiC composite tube for nuclear fuel cladding was simulated using FEA. The stress caused by the plug was distributed nonuniformly because of the friction coefficient difference between the inner surface of the tube and the plug. Hoop stress and shear stress at the tube was evaluated and the relationship between the concentrated stress at the inner layer of the tube and the fracture behavior of the tube was investigated.

Electrical Properties and Temperature Stability of Dysprosium and Erbium Co-doped Barium Titanate with Perovskite Structure for X7R MLCCs (Dysprosium과 Erbium이 동시 첨가된 X7R MLCC용 페로브스카이트 BaTiO3의 전기적특성과 온도안정성)

  • Noh, Tai-Min;Kim, Jin-Seong;Ryu, Ji-Seung;Lee, Hee-Soo
    • Journal of the Korean Ceramic Society
    • /
    • v.48 no.4
    • /
    • pp.323-327
    • /
    • 2011
  • The effects of $Dy_2O_3$ and $Er_2O_3$ co-doping on electrical properties and temperature stability of barium titanate ($BaTiO_3$) ceramics were investigated in terms of microstructure and structural analysis. The dielectric constant and the insulation resistance (IR) of 0.7 mol% $Dy_2O_3$ and 0.3 mol% $Er_2O_3$ co-doped dielectrics had about 60% and 20% higher than the values of undoped one, respectively, and the temperature coefficient of capacitance (TCC) met the X7R specification. The addition of $Dy_2O_3$ contributed to electrical properties caused by increase of tetragonality; however, preferential diffusion of $Dy^{3+}$ ions toward A site in $BaTiO_3$ grain exhibited an adverse effect on temperature stability by grain growth. On the other hand, The $Er_2O_3$ addition in $BaTiO_3$ could affect the TCC behavior and the IR with suppression of grain growth caused by reinforcement of grain boundary and electrical compensation. Therefore, the enhanced electrical properties and temperature stability through the co-doping could be deduced from the increase of tetragonality and the suppression of grain growth.

An Effective Modeling of Artificial Teeth Single Cores Prostheses (인공 치아 단일 코아 보철물의 효과적인 모델링)

  • Yoo, Kwan-Hee
    • Journal of the Korea Computer Graphics Society
    • /
    • v.8 no.1
    • /
    • pp.13-20
    • /
    • 2002
  • Recently, there is a great demand for artificial teeth prostheses made of the materials which are sintered at $1500^{\circ}C$ such as zirconia ceramic. Since degree of strength of the materials is very high, however, it is very difficult for technicians to manually fabricate the prostheses for these ceramics. So the prostheses have been fabricated by using CNC(computer numerical control) machines. In doing them by using CNC, it is very important that the prostheses satisfying dentists's requirements are accurately modeled into 3D objects. In this paper, we propose an effective method for modeling single cores such as single caps and Conus cores, which are the main those of artificial teeth prostheses. And we also present the visual examples of 3D models for these single cores modeled by the proposed methods. In special, the method has used Minkowski sum and ZMap for modeling the single cores.

  • PDF

The effect of coloring liquid dipping time on the fracture load and color of zirconia ceramics

  • Orhun, Ekren
    • The Journal of Advanced Prosthodontics
    • /
    • v.9 no.1
    • /
    • pp.67-73
    • /
    • 2017
  • PURPOSE. The aims of the study were to evaluate the fracture load of zirconia core material after dipping in coloring liquid at different time intervals and to compare the color of dipped blocks with that of prefabricated shaded blocks. MATERIALS AND METHODS. 3-unit bridge frameworks were designed digitally. Sixty frameworks were fabricated using uncolored zirconia blocks by CAD/CAM and divided into 4 groups randomly (n = 15). Group 2 (G2) was subjected to coloring liquids for 2 minutes, Group 4 (G4) for 4 minutes, and Group 6 (G6) for 6 minutes. CFS group was not subjected to any coloring procedure. After coloring, color differences between the test groups and a prefabricated shaded zirconia group (CPZ, n = 15) were evaluated by using a spectrophotometer. Fracture test was conducted immediately after shade evaluation with a Testometric test device at a cross-head speed of 1 mm/sec. Statistical analysis for evaluating color and fracture load was performed by using one way ANOVA followed by Tukey HSD test ($P{\leq}.05$). Weibull analysis was conducted for distribution of fracture load. RESULTS. There was no difference in terms of fracture load and color between CFS (1176.681 N) and G2 (985.638 N) group and between CPZ (81.340) and G2 (81.140) group, respectively. Fracture load values of G4 (779.340 N) and G6 (935.491 N) groups were statistically significantly lower than that of CFS group ($P{\leq}.005$). The color values of G4 (79.340) and G6 (79.673) groups were statistically different than that of CPZ group ($P{\leq}.005$). CONCLUSION. Prolonged immersion of zirconia in coloring liquid not only negatively affected the fracture load of the zirconia being tested in the current study but also deteriorated the desired shade of the restoration.

A Study on Ceramic Expression using Silhouette Technique and Decal Technique (실루엣기법과 전사기법을 활용한 융복합적 도자 표현 연구)

  • Kim, Won-Seok;Ro, Hea-Sin;Choi, Jung-Hwa
    • Journal of Digital Convergence
    • /
    • v.15 no.12
    • /
    • pp.495-502
    • /
    • 2017
  • Modern ceramics is exploring the expansion of the area with various expression techniques. The silhouette technique among various expressive decoration techniques is a representative expression technique of object form expression. This emphasizes the outline of the form and expresses it and omits the inner form. It gives simplicity and intensity, and awakens aesthetic sensibility and imagination. Therefore, the researcher designed the material related to the core image of the story by designing it as a silhouette technique by using the "Acorn Story" as a subject and then making the transfer paper by using the vector graphic. The transferred paper was expressed on a ceramic plate by transferring technique. Therefore, I hope that this research, beyond the merely decorative function of ceramic expression, will become a ceramic design that will awaken imagination and aesthetic sensibility in digital information age.