Achillopoulou, Dimitra V.;Kiziridou, Alexandra N.;Papachatzakis, Georgios A.;Karabinis, Athanasios I.
Steel and Composite Structures
/
제22권6호
/
pp.1337-1358
/
2016
The current study focuses on the assessment and interface response of reinforced concrete elements with composite materials (carbon fiber reinforced polymers-CFRPs, glass fiber reinforced polymers-GFRPs, textile reinforced mortars-TRM's, near surface mounted bars-NSMs). A description of the transfer mechanisms from concrete elements to the strengthening materials is conducted through analytical models based on failure modes: plate end interfacial debonding and intermediate flexural crack induced interfacial debonding. A database of 55 in total reinforced concrete columns (scale 1:1) is assembled containing elements rehabilitated with various techniques (29 wrapped with CFRP's, 5 wrapped with GFRP's, 4 containing NSM and 4 strengthened with TRM). The failure modes are discussed together with the performance level of each technique as well as the efficiency level in terms of ductility and bearing/ bending capacity. The analytical models' results are in acceptable agreement with the experimental data and can predict the failure modes. Despite the heterogeneity of the elements contained in the aforementioned database the results are of high interest and point out the need to incorporate the analytical expressions in design codes in order to predict the failure mechanisms and the limit states of bearing capacities of each technique.
콘크리트의 역학적거동은 다양한 종류의 균열의 발생과 전파에 의하여 영향을 받는다. 최근 고성능 콘크리트의 개발이 이루어지면서 계면파괴와 계면역에서의 균열양상에 대한 연구가 중요한 분야로 부각되고 있다. 탄성이며 균질한 재료에 적용되는 균열전파에 대한 규준은 계면역에서 균열이 진전하는 경우는 유효하지 않으며 이 경우에는 콘크리트에서 균열전파를 예측하기 위하여 구성재료들의 파괴인성과 그들 사이 계면의 파괴인성의상대적인 크기를 고려하여야 한다. 본 논문에서는 계면균열선단에서 계면파괴역학변수인 에너지해방률과 하중위상각을 수치해석방법을 이용하여 구하는 방법과 계면에서의 균열전파의 예측을 위한 에너지해방률에 기초를 둔 파괴규준을 제안하였다. 계면역에서의 균열양상을 조사하기 위하여 계면균열을 가진 이상복합모델에 대한 실험과 수치해석연구를 수행하였으며 대체적으로 실험결과와 규준을 이용하여 예측한 결과가 서로 일치하는 결과를 얻었다.
This paper reports the experimental results of three through bolt beam-column connections under pure shear forces using modified push-out tests. The investigated specimens include extended end-plates and six through-bolts connecting square concrete-filled steel tubular column (S-CFST) to steel beams. The main goal of this study is to investigate if and how the mechanical shear connectors, such as steel angles and stud bolts, contribute to the shear transfer mechanisms in the steel-concrete interface of the composite column. The contribution of shear studs and steel angles to improve the shear resistance of steel-concrete interface in through-bolt connections was investigated using tests. The results showed that their contribution is not significant when the beam-column connection is included in the push-out tests. The specimens failed by pure shear of the long bolts, and the ultimate load can be predicted using the shear resistance of the bolts under shear forces. The predicted values of load allowed obtaining a good agreement with the tests results.
Steel plate bonding technique is most widely used in strengthening of existing concrete structures, but it has inherently a problem of the premature failure such as interface separation and rip off. So far, many studies have been arid out in the manner of laboratory tests for the reinforced concrete beams to find out he mechanism of the premature failure. However, in order to verify the characteristics of the premature failure, more reasonable local investigations are needed rather than such relatively global experimental works. In this study, therefore, the double lap test which simulate the pure shear loadings and the half beam tests which consider combined flexure-shear force have been done. There are, however, difficulties in getting the normal stress caused to premature failure, so that finite element analysis was performed, too. In numerical study, material nonlinearity was considered, and the interface element was applied to model the interface between steel plate and adhesive. From the results of experimental and numerical studies, a realistic failure criterion on the separation of steel plates has been derived.
The interface necessarily exists in joints using cement mortar, UP(Unsaturated Polyester : UP) mortar and SBR(SBR-latex) mortar. Characteristics of shear transfer in joint interface consisting of different materials are studied with experimental and analytical methods. The uniaxial compressive shear experiments are accomplished with various angle of inclination (35, 45, 55, 65, 75°), materials of old and new-cast mortar. In this study, The results are as follows ① Mohr-coulomb's slip theory be applied to the interface consisting different materials ② The cohesion of UP mortar is superior to that f cement mortar, SBR mortar.
Haeri, Hadi;Sarfarazi, Vahab;Zhu, Zheming;Marji, Mohammad Fatehi;Masoumi, Alireza
Smart Structures and Systems
/
제23권1호
/
pp.81-90
/
2019
The shear behavior of soil-concrete interface is mainly affected by the surface roughness of the two contact surfaces. The present research emphasizes on investigating the effect of roughness of soil-concrete interface on the interface shear behavior in two-layered laboratory testing samples. In these specially prepared samples, clay silt layer with density of $2027kg/m^3$ was selected to be in contact a concrete layer for simplifying the laboratory testing. The particle size testing and direct shear tests are performed to determine the appropriate particles sizes and their shear strength properties such as cohesion and friction angle. Then, the surface undulations in form of teeth are provided on the surfaces of both concrete and soil layers in different testing carried out on these mixed specimens. The soil-concrete samples are prepared in form of cubes of 10*10*30 cm. in dimension. The undulations (inter-surface roughness) are provided in form of one tooth or two teeth having angles $15^{\circ}$ and $30^{\circ}$, respectively. Several direct shear tests were carried out under four different normal loads of 80, 150, 300 and 500 KPa with a constant displacement rate of 0.02 mm/min. These testing results show that the shear failure mechanism is affected by the tooth number, the roughness angle and the applied normal stress on the sample. The teeth are sheared from the base under low normal load while the oblique cracks may lead to a failure under a higher normal load. As the number of teeth increase the shear strength of the sample also increases. When the tooth roughness angle increases a wider portion of the tooth base will be failed which means the shear strength of the sample is increased.
본 연구에서는 2번에 분리타설된 교량 슬래브의 휨 및 전단거동 특성에 대한 실험연구를 수행하였다. 분리타설된 슬래브의 거동은 구콘크리트의 표면상태, 다우웰 철근량 및 접착층의 부착강도에 의해 큰 영향을 받게 되므로, 본 연구에서는 이와 같은 변수를 변화시켜 실험을 수행하였다. 본 연구결과 초기균열이 발생할때까지는 콘크리트의 표면상태 및 다우웰 철근량에 따라 구조거동에 큰 차이를 보이지 않으나, 극한하중상태에 도달하면 구콘크리트의 표면상태가 양호하고 아크릴수지 처리와 다우웰 철근이 많을수록 분리타설된 슬래브는 일체로 거동하는 것으로 나타났다. 따라서, 본 연구결과는 앞으로 교량에서 2층으로 분리타설하는 철근콘크리트 슬래브의 설계를 위한 유용한 자료와 토대를 제시하고 있다.
Belaidi, Amina;Hacene, Mohammed Amine Boukli;Kadri, El-Hadj;Taleb, Omar
Advances in concrete construction
/
제11권3호
/
pp.231-238
/
2021
The present work aims at investigating the effects of using various fine mineral additions as partial replacement to Portland cement on the tribological properties of concrete. To achieve this goal, concrete mixtures were prepared with different percentages (10, 20 and 30%) of limestone fillers (LF) and natural pozzolana (NP), and (20, 40 and 60%) of blast furnace slag (BFS). The interface yield stress (τ0) and viscous constants (η) that allow characterizing friction at the concrete-pipe wall interface were determined using a rotational tribometer. In addition, the compositions of the boundary layers that formed in the pumping pipes of the different concretes under study were also identified and analyzed. The experimental results obtained showed that the concretes studied have a linear tribological behavior that can be described by the Bingham model. Furthermore, the use of different mineral additions, especially limestone fillers and blast furnace slags, even at high rates, had a beneficial effect on the optimization of the volume of paste present in the boundary layer, which made it possible to significantly reduce the viscous constant of concrete. However, a maximum rate of 10% of natural pozzolana was recommended to achieve tribological properties that are favorable to the pumpability of concrete.
Li Zhou;Kai Su;Ding-wei Liu;Yin-quan Li;Hong-ze Zhu
Structural Engineering and Mechanics
/
제86권1호
/
pp.139-156
/
2023
The reinforced concrete lining in the hydraulic pressure tunnel tends to crack during the water-filling process. The lining will be detached from the surrounding rock due to the inner water exosmosis along concrete cracks. From the previous research achievements, the cohesive element is widely adopted to simulate the concrete crack but rarely adopted to simulate the lining-rock interface. In this study, the zero-thickness cohesive element with hydro-mechanical coupling property is not only employed to simulate the traditional concrete crack, but also innovatively introduced to simulate the lining-rock interface. Combined with the indirect-coupled method, the hydro-mechanical coupling algorithm of the reinforced concrete lining in hydraulic pressure tunnels is proposed and implemented in the finite element code ABAQUS. The calculated results reveal the cracking mechanism of the reinforced concrete lining, and match well with the observed engineering phenomenon.
In this study, the influence of the lateral pressure on the interface shear transfer of concrete has been investigated experimentally. A total of 21 specimens has been tested at the laboratory. The lateral pressure intensities in the tests have been taken as 0, 7, 14, 28, and 35kg/$\textrm{cm}^2$ for the specimens, the compressive strengths of which are either 180, 400 or 550kg/$\textrm{cm}^2$. The linear regression analysis based on the test results has shown relatively good agreements with the values given in the shear friction theory.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.